KR Steel Plates

Product Showcase

KR Steel Plates Carbon Steel Plates

SHH STEEL offers KR Rules-compliant KR AH32/DH32/EH36 steel plates. Korean Register Rules for Steel Ships specify materials, welding, and construction for classed vessels, ensuring seaworthiness. Certified quality, competitive prices, customizable. Trust SHH STEEL!

KR RF51 shipbuilding steel plate to Korean Register (KR) rules, stacked hull plates

KR RF51 Shipbuilding Steel Plate

KR RF51 (RF51) extra-high-strength hull structural steel plate, yield 500 N/mm², tensile 610–770 N/mm², Charpy at −60 °C, stamped KR RF51 / KR RF51 with Korean Register–endorsed certificates. SHH STEEL supplies mill-roll plate in China with cutting, multi-class and 3.2 inspection.
View More
KR RE51 marine steel plate per Korean Register (KR) rules at SHH STEEL warehouse

KR RE51 Shipbuilding Steel Plate

KR RE51 (RE51) extra-high-strength hull structural steel plate, yield 500 N/mm², tensile 610–770 N/mm², Charpy at −40 °C, stamped KR RE51 / KR RE51 with Korean Register–endorsed certificates. SHH STEEL supplies mill-roll plate in China with cutting, multi-class and 3.2 inspection.
View More
KR RD51 shipbuilding steel plate to Korean Register (KR) rules, stacked hull plates

KR RD51 Shipbuilding Steel Plate

KR RD51 (RD51) extra-high-strength hull structural steel plate, yield 500 N/mm², tensile 610–770 N/mm², Charpy at −20 °C, stamped KR RD51 / KR RD51 with Korean Register–endorsed certificates. SHH STEEL supplies mill-roll plate in China with cutting, multi-class and 3.2 inspection.
View More
KR RA51 marine steel plate per Korean Register (KR) rules at SHH STEEL warehouse

KR RA51 Shipbuilding Steel Plate

KR RA51 (RA51) extra-high-strength hull structural steel plate, yield 500 N/mm², tensile 610–770 N/mm², Charpy at 0 °C, stamped KR RA51 / KR RA51 with Korean Register–endorsed certificates. SHH STEEL supplies mill-roll plate in China with cutting, multi-class and 3.2 inspection.
View More
KR RF47 shipbuilding steel plate to Korean Register (KR) rules, stacked hull plates

KR RF47 Shipbuilding Steel Plate

KR RF47 (RF47) extra-high-strength hull structural steel plate, yield 460 N/mm², tensile 570–720 N/mm², Charpy at −60 °C, stamped KR RF47 / KR RF47 with Korean Register–endorsed certificates. SHH STEEL supplies mill-roll plate in China with cutting, multi-class and 3.2 inspection.
View More
KR RE47 shipbuilding steel plate to Korean Register (KR) rules, stacked hull plates

KR RE47 Shipbuilding Steel Plate

KR RE47 (RE47) extra-high-strength hull structural steel plate, yield 460 N/mm², tensile 570–720 N/mm², Charpy at −40 °C, stamped KR RE47 / KR RE47 with Korean Register–endorsed certificates. SHH STEEL supplies mill-roll plate in China with cutting, multi-class and 3.2 inspection.
View More
KR RD47 shipbuilding steel plate to Korean Register (KR) rules, stacked hull plates

KR RD47 Shipbuilding Steel Plate

KR RD47 (RD47) extra-high-strength hull structural steel plate, yield 460 N/mm², tensile 570–720 N/mm², Charpy at −20 °C, stamped KR RD47 / KR RD47 with Korean Register–endorsed certificates. SHH STEEL supplies mill-roll plate in China with cutting, multi-class and 3.2 inspection.
View More
Close view of KR RA47 hull structural steel plate, Korean Register (KR) rules

KR RA47 Shipbuilding Steel Plate

KR RA47 (RA47) extra-high-strength hull structural steel plate, yield 460 N/mm², tensile 570–720 N/mm², Charpy at 0 °C, stamped KR RA47 / KR RA47 with Korean Register–endorsed certificates. SHH STEEL supplies mill-roll plate in China with cutting, multi-class and 3.2 inspection.
View More
KR RF43 marine steel plate per Korean Register (KR) rules at SHH STEEL warehouse

KR RF43 Shipbuilding Steel Plate

KR RF43 (RF43) extra-high-strength hull structural steel plate, yield 420 N/mm², tensile 530–680 N/mm², Charpy at −60 °C, stamped KR RF43 / KR RF43 with Korean Register–endorsed certificates. SHH STEEL supplies mill-roll plate in China with cutting, multi-class and 3.2 inspection.
View More
Close view of KR RE43 hull structural steel plate, Korean Register (KR) rules

KR RE43 Shipbuilding Steel Plate

KR RE43 (RE43) extra-high-strength hull structural steel plate, yield 420 N/mm², tensile 530–680 N/mm², Charpy at −40 °C, stamped KR RE43 / KR RE43 with Korean Register–endorsed certificates. SHH STEEL supplies mill-roll plate in China with cutting, multi-class and 3.2 inspection.
View More
Close view of KR RD43 hull structural steel plate, Korean Register (KR) rules

KR RD43 Shipbuilding Steel Plate

KR RD43 (RD43) extra-high-strength hull structural steel plate, yield 420 N/mm², tensile 530–680 N/mm², Charpy at −20 °C, stamped KR RD43 / KR RD43 with Korean Register–endorsed certificates. SHH STEEL supplies mill-roll plate in China with cutting, multi-class and 3.2 inspection.
View More
KR RA43 shipbuilding steel plate to Korean Register (KR) rules, stacked hull plates

KR RA43 Shipbuilding Steel Plate

KR RA43 (RA43) extra-high-strength hull structural steel plate, yield 420 N/mm², tensile 530–680 N/mm², Charpy at 0 °C, stamped KR RA43 / KR RA43 with Korean Register–endorsed certificates. SHH STEEL supplies mill-roll plate in China with cutting, multi-class and 3.2 inspection.
View More

Shipbuilding Steel Plates

SHH STEEL, a premier Shipbuilding Steel Plates exporter, produces and exports shipbuilding steel plates for marine vessels and offshore structures. Our plates, such as AH36 and DH36, provide high strength, toughness, and corrosion resistance, meeting ABS and BV standards. With a 5,000-ton inventory, we guarantee 3–5 day delivery for in-stock items, backed by SGS/TUV inspections and mill certificates. Choose SHH STEEL for reliable marine-grade steel plates and custom maritime solutions.

Shipbuilding Steel Plates

SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

    *

    *

    *

    *


    X