Close view of KR RD56 hull structural steel plate, Korean Register (KR) rules

KR RD56 Shipbuilding Steel Plate

KR RD56 (RD56) extra-high-strength hull structural steel plate, yield 550 N/mm², tensile 670–835 N/mm², Charpy at −20 °C, stamped KR RD56 / KR RD56 with Korean Register–endorsed certificates. SHH STEEL supplies mill-roll plate in China with cutting, multi-class and 3.2 inspection.
Keywords
KR RD56 steel plate, KR RD56 shipbuilding steel plate, KR RD56 marine plate, RD56 extra high strength hull steel, Korean Register RD56 plate, Korean Register RA43 RF70, KR Rules Pt 2 hull steel
Equivalent Grades:
ASTM A131 (no direct); ABS DH55 / DQ56; DNV NV D550; LR DH55 / LR/DH55; BV D550; NK KD550; CCS DH550; RINA per rules; GB 712 Grade DH550
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Impact Test and Condition of Supply
Thickness Tolerance
Stock
Equivalent Grades
Grade Selection
Applications and Fabrication
Testing and Inspection
Specification Mistakes
Buyer Concerns
How to Order
FAQ
Conclusion

KR RD56 / KR RD56 shipbuilding steel plate — overview

Technical Reviewer: Jack | SHH STEEL Material Solutions Department · Updated: 2026-10-28

KR RD56 is the Korean Register −20 °C extra-high-strength grade at 550 N/mm² yield; KR prints it as RD56, with the R prefix and a two-digit class number. The strength band follows IACS Unified Requirement W16; KR implements it in the Rules for the Classification of Steel Ships, Pt 2 (Materials). Minimum yield is 550 N/mm², tensile 670–835 N/mm², elongation 16 % min., Charpy at −20 °C. It sits above the RA–RF 40 higher-strength family (max. 390 N/mm² under UR W11). Commercial enquiries use KR RD56 or KR RD56 shipbuilding steel plate.

Equivalent grades: KR RD56 ≈ ASTM A131 (no direct grade at this strength) ≈ ABS DH55 / DQ56 ≈ DNV NV D550 ≈ LR DH55 ≈ BV D550 ≈ CCS DH550 ≈ NK KD550 ≈ RINA D550 ≈ GB 712 Grade DH550 (all class-approved, stamped by the issuing society).

Naming note: KR’s EHS numbers 43 / 47 / 51 / 56 / 63 / 70 follow the ABS-style official yield-class numbering (420 → 43, 460 → 47, 500 → 51, 550 → 56, 620 → 63, 690 → 70), so 550 N/mm² becomes RD56. ABS titles the same band DH55 commercially (official DQ56); DNV and CCS use DH550; BV uses D550 (no H); LR uses DH55. ASTM A131 has no grade at this strength. The 43…70 mapping is consistent with ABS practice but is UNCERTAIN against a local KR Rules text — confirm the exact designation on the mill’s KR approval certificate before ordering.

KR RD56 is almost always produced TM or QT by a KR-approved mill to order rather than taken from open stock. SHH STEEL sources extra-high-strength plate from mills with Korean Register approval for the grade, under Surveyor attendance, with optional multi-class (ABS/DNV/LR/BV) and EN 10204 3.2.

KR RD56 plate: specification summary

ItemKR RD56 / RD56 data
Rule basisKR Rules Pt 2 (extra-high / high-strength hull steel); IACS UR W16 strength band (see UNCERTAIN for KR Rules Pt 2 paragraph cross-refs without local KR Rules text)
Official KR designationRD56 (R prefix + ABS-style yield-class number 56; = 550 N/mm² band) — UNCERTAIN vs local KR text
IACS strength bandUR W16, yield 550 N/mm² (DH550 in DNV/CCS naming)
Yield / tensile / elongation550 / 670–835 N/mm² / 16 % min.
Impact−20 °C; ≈ 55 J L or 37 J T average (IACS UR W16 / aligned tables — confirm on mill certificate)
Deoxidationfully killed, fine grain; N-binding elements per manufacturing specification
Delivery conditionTM or QT (N/CR routes only where specifically approved) — within mill approval thickness limits
MarkingKR RD56 / KR RD56 (plus delivery-condition / Z / U where ordered)
UTcommonly required for thicker EHS plate (e.g. ≥15 mm) — agree standard (EN 10160 / ASTM A578) on PO
Thickness toleranceIACS UR W13 as adopted by KR (confirm class on PO; see UNCERTAIN)
Certificatemill certificate endorsed by the KR Surveyor; includes Ceq/CET/Pcm as applicable; EN 10204 3.1 / 3.2 on request

Maximum plate thickness depends on delivery condition and the mill’s KR approval sheet — typically TM up to about 100–150 mm and QT higher, but treat the approval limit as governing (UNCERTAIN without local KR Rules text). Primary commercial scope we quote is within ~100 mm unless the mill approval and KR survey confirm otherwise.

KR RD56 chemical composition (heat analysis — full alloy set)

ElementHeat (ladle) analysis, %Product (check) analysis, %Note
C0.21 max. (often 0.14–0.20 by route/condition; TM/QT may tighten)numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificateTM/QT and letter routes may tighten C — UNCERTAIN exact KR Rules Pt 2 table without local PDF
Mn1.70 max. (typically 1.00–1.70; QT route may differ)numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificateas per mill approval / UR W16 envelope
Si0.55 max. (QT may allow up to ~0.80 — confirm on mill approval)numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificate
P0.025 max. (some EQ-style routes tighter — confirm)numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificateEQ-style routes may be tighter
S0.025 max. (some EQ-style routes tighter — confirm)numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificateEQ-style routes may be tighter
Al (acid soluble / total)0.015 min. acid-soluble / ≈0.020 total Al (fine-grain; Al/N control unless other N-binders)numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificategrain refining / N control
Nb0.05 max. (when used; combined microalloy caps apply)numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificatewhen intentionally added
V0.10 max. (when used; combined caps apply)numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificatewhen intentionally added
Ti0.05 max. (when used; combined caps apply)numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificatewhen intentionally added
Cu0.50 max. (route-dependent; often ≤0.35 in practice)numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificate
Cr0.20–0.25 max. (route-dependent)numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificate
Ni2.00 max. or per mill approval (often lower on AH/DH routes)numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificate
Mo0.08–0.50 (route-dependent; QT may allow higher)numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificate
B0.005 max. (when intentionally added)numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificatereport when intentionally added
N0.015 max. (tighter control when Al is the sole N-binder)numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificateAl/N practice unless other N-binders
Nb+V+Ti (combined)Nb+V+Ti typically < 0.26 % for N/TM routes (not QT) — confirm UR W16 / mill approvalnot applicable (calculated from heat analysis)combined microalloy cap
Ceq / CET / PcmCeq / CET / Pcm maxima by category and condition on mill approval — report on certificatenot applicable (calculated from heat analysis)report on certificate; choice agreed mill/purchaser

Product (check) analysis column: KR Rules (Part 2) specify heat (ladle) limits; no numeric product-analysis tolerance is tabulated in the rule text reviewed, so product (check) limits are agreed on the order or taken from the approved mill specification and certificate.

Source: IACS UR W16 chemistry envelope (ABS 2-1-8 Table 4A aligned — the same yield-class numbering KR follows) as implemented by Korean Register for KR RD56 — exact ladle limits depend on delivery condition (TM vs QT) and toughness letter. Class work follows the KR / UR W16 envelope on the mill approval. Values above are the rule envelope with every alloy / microalloy row listed; the purchase order and mill approval sheet govern. Product analysis: as per standard and mill certificate. All intentionally added elements and Ceq (or CET/Pcm) are to be reported. Flagged UNCERTAIN where a local KR Rules text was not available to quote paragraph numbers.

KR RD56 tensile and impact properties

PropertyRequirement (IACS UR W16 aligned)
Yield strength ReH (or Rp0.2)550 N/mm² min.
Tensile strength Rm670–835 N/mm²
Elongation (transverse, 5.65√A)16 % min.
Impact test temperature−20 °C
Impact energy (indicative)55 J L or 37 J T average

Final acceptance values are as per standard and mill certificate under KR survey. For thick plate, additional mid-thickness tensile/impact positions may apply — confirm at enquiry. Test frequency is typically each heat-treatment batch of same cast/condition/thickness.

Delivery condition and toughness for KR RD56

Charpy temperature is fixed by the grade letter: DH → −20 °C. Indicative average energy 55 / 37 J (L/T) from IACS UR W16 aligned tables — confirm exact figures on the KR-endorsed certificate. Unlike UR W11 higher-strength tables, EHS energies are usually stated as a single pair rather than rising through many thickness bands; thick-plate mid-thickness rules may still apply.

Allowed delivery conditions are primarily TM and QT within the mill’s approved thickness. Vacuum degassing is commonly required for higher categories and for thicker plate — follow the mill approval. State TM or QT on the PO; do not leave delivery condition blank for RD56.

Thickness tolerance and surface condition

Korean Register applies IACS UR W13 unless the PO states otherwise (confirm minus class on PO; see UNCERTAIN). Surface repair limits follow the applicable KR / UR rules; state primer/surface class on receipt if needed. For QT plate, avoid notching cut edges; follow mill cutting recommendations.

KR RD56 plate — mill-roll supply in China

Thickness (mm)Width (mm)Length (mm)ConditionApprox. quantityLocation
102000 / 22008000 / 12000TM / QT200+ tChina
122000 / 2200 / 250012000TM / QT200+ tChina
142000 / 220012000TM / QT100+ tChina
162000 / 250012000TM / QT200+ tChina
202000 / 250012000TM / QT100+ tChina
252200 / 250012000TM / QT100+ tChina
30220010000 / 12000TM / QT100+ tChina
40220010000TM / QT50+ tChina
5022008000 / 10000TM / QT50+ tChina

Extra-high grades such as KR RD56 are rarely held as open stock; the table shows the size bands we quote against scheduled mill rolls. Quantities are indicative. All plates sold as KR class carry KR RD56 marking and a Korean Register–endorsed mill certificate. Typical mill lead time including KR survey is about 6–10 weeks (commercial estimate — confirm per quote). Send your size list and we will reply with the next available rolling slot.

Packing. Plates are bundled by size with steel strapping, marked with heat number, grade and KR stamp, and shipped in containers (up to about 11.8 m) or break bulk for longer plates.

KR RD56 equivalents in other rules and standards

Standard / societyDesignationComment
KR (Korean Register)KR RD56this page; KR uses RA43…RF70 (ABS-style class numbers — UNCERTAIN)
GB 712GB 712 Grade DH550Chinese product standard EHS band; not class approval
ASTM A131/A131MASTM A131/A131M — no direct Grade RD56A131 stops at FH40
ABSABS DH55 / DQ56commercial DH55 / official DQ56
DNVDNV NV D550DNV titles DH550 for this yield band
LRLR DH55 / LR/DH55LR titles DH55 (AH69 not AH70 / AH690)
BVBV D550BV titles D550 (no H — A420 not AH420)
NK (ClassNK)NK KD550NK KD550
CCSCCS DH550IACS UR W11; live CCS product page
RINARINA (per rules)EHS name not verified from local RINA PDF

These are comparisons, not substitutions. Always write the KR stamp KR RD56 on the PO, plus any additional society stamps you need. Other KR EHS siblings are linked via KR until each product page is live.

KR RD56 vs higher-strength and other EHS grades

Use RD56 when scantlings need yield 550 N/mm². Do not substitute RA40/RE40 (390 N/mm² under UR W11) without redesign. Within the 56 class, letter choice is toughness: RA 0 °C → RD −20 °C → RE −40 °C → RF −60 °C. Neighbouring KR strengths are RD51 / RD63 — swapping strength needs class approval of the drawing change.

When KR RD56 is the right choice: typical uses are extra-high-strength members assigned −20 °C toughness on the KR material class table — thicker primary strakes and ice-strengthened structure at extra-high yield — weight-critical hull girder strakes, polar and ice-class primary structure, and offshore units where 550 N/mm² is specified. See offshore platform steel plates for related offshore grades.

Applications and welding notes for KR RD56

Typical uses: extra-high-strength members assigned −20 °C toughness on the KR material class table — thicker primary strakes and ice-strengthened structure at ReH 550 N/mm²; strength deck and shell of large container ships and gas carriers where EHS is specified; ice-belt and polar primary structure; selected offshore members. See offshore platform steel plates.

Welding: KR RD56 is an extra-high-strength steel supplied TM or QT. Welding must follow a procedure qualified for this grade and approved by KR. Ceq/CET/Pcm from the ladle analysis govern hydrogen control, preheat, interpass and heat-input windows. Too much heat input can lower HAZ strength and toughness in QT plate. We send the certificate values before shipment so your welding engineer can confirm the procedure fits. We do not give generic preheat temperatures.

Processing notes: KR RD56 owes its strength to TM or QT processing. Hot forming or stress relieving above the tempering temperature can lower the properties, so any heat treatment after delivery must be agreed with the mill and KR. Cold forming and bending radii should follow the mill’s data sheet. Thermal cutting parameters follow mill recommendations so the cut edge is not damaged.

Certificates, KR survey and third-party inspection

KR survey at the mill; certificate includes ladle chemistry (full alloy set + Ceq/CET/Pcm as applicable), tensile (ReH ≥ 550, Rm 670–835, A ≥ 16 %), Charpy at −20 °C, delivery condition, UT if ordered, and plate identity. Optional EN 10204 3.2 and multi-class with ABS/DNV/LR/BV.

On receipt: verify KR RD56 stamp, −20 °C impact data, energies ≥ ordered/certified minima, thickness within tolerance, KR Surveyor endorsement, UT report if required.

Charpy acceptance for KR RD56 (IACS UR W16 aligned; actual results as per standard and mill certificate):

Thickness t (mm)Test temperatureAverage energy, longitudinal (J min.)Average energy, transverse (J min.)
as per UR W16 / mill approval (typically t/4 position)−20 °C5537

For thickness above ~100 mm, additional mid-thickness rules may apply — confirm at enquiry. If the PO asked for 3.2, the inspector’s report must name the witnessed tests and plate numbers.

Common mistakes when ordering KR RD56 / KR RD56

  • Ordering “KR 56” or “KR 550” without the letter — toughness class missing
  • Writing DH550 or D550 on a KR PO — the KR designation is RD56; the mill must stamp KR RD56
  • Writing ABS DH55 or DNV DH550 or LR DH55 or BV D550 on a KR-class PO without arranging that society’s survey (wrong stamp)
  • Leaving delivery condition blank (TM vs QT changes price, mill and properties)
  • Expecting ASTM A131 dual certification at this strength (A131 has no EHS grade)
  • Skipping UT on thick EHS plate when the yard specification requires it
  • Missing KR Surveyor endorsement on the mill certificate (mill-only or product-standard papers are not KR class approval)
  • Omitting alloy / microalloy rows (Al, Nb, V, Ti, Cu, Cr, Ni, Mo, B, N) from the certificate check

Write the KR grade (RD56), TM/QT, impact temperature, UT level and certificate type into the PO.

Sourcing KR RD56: buyer concerns and SHH STEEL solutions

ConcernHow SHH STEEL handles it
Fake class plateKR-approved mills only; traceable KR RD56 stamp + certificate; 3.2 on request
Payment riskT/T or L/C; inspection before balance
Mill minimum / long lead timecombine sizes on one heat where possible; weekly photo updates; clear rolling-slot confirmation before deposit
Welding / heat-input risksend ladle Ceq/CET/Pcm before shipment; support WPS review with mill data
Prep before shipcutting, bevelling, drilling, machining in our workshop (follow mill cutting notes for QT)

How to order KR RD56 plate

Specify KR RD56 (KR RD56), delivery condition TM or QT, thickness × width × length × qty, Z/U/UT level, multi-class, certificate type, port. Send to SHH STEEL.

Sample PO line: “Steel plate to KR Rules for the Classification of Steel Ships, Pt 2, Grade RD56 (KR RD56), delivery condition [TM/QT], 30 × 2500 × 12000 mm, 10 pcs, marked KR RD56 / KR RD56, certificate endorsed by KR Surveyor, EN 10204 3.2 [if required], UT [EN 10160 / ASTM A578 level], CIF [port].”

FAQ

What sizes and minimum order quantity can you supply for KR RD56 / KR RD56 plate?
KR RD56 is ordered as Korean Register extra-high-strength grade RD56 (IACS UR W16 band, 550 N/mm²). The plate is fully killed, and the maximum thickness depends on the delivery condition (TM or QT) and the mill’s KR approval. In practice KR RD56 is nearly always produced by an approved mill to order rather than taken from stock, so a mill minimum per heat or rolling usually applies. Send thickness × width × length × quantity per size and we will say whether the order fits a scheduled rolling or needs its own heat. Small balance quantities can sometimes ride on another RD56 order.
How is KR RD56 certified, and can you arrange EN 10204 3.2 or dual-class with ABS/DNV/LR/BV?
Every plate is made by a KR-approved mill under Korean Register survey. It is die-stamped or stencilled KR RD56 / KR RD56 with the heat or plate number, and the mill test certificate is endorsed by the KR Surveyor. The certificate gives ladle chemistry (full alloy set including Al, Nb, V, Ti, Cu, Cr, Ni, Mo, B, N where applicable), Ceq/CET/Pcm as applicable, tensile (ReH ≥ 550 N/mm², Rm 670–835 N/mm², A ≥ 16 %), Charpy at −20 °C, delivery condition, UT if ordered, and plate identity. An ASTM A131 or GB 712 product certificate alone is not KR class approval. If your contract asks for EN 10204 3.2, we arrange it before rolling. Dual or multi-class (e.g. KR + ABS, DNV, LR or BV) must be booked before testing. 3.2 cannot be added afterwards.
What is the impact test temperature and energy for KR RD56 / KR RD56, and do thickness limits apply?
KR RD56 is tested at −20 °C with an indicative average of at least 55 J longitudinal or 37 J transverse (IACS UR W16 aligned tables). Impact specimens typically come from the quarter-thickness position (t/4). For thicker plates, KR / UR W16 may require additional positions. Rule maximum thickness depends on whether the plate is TM or QT and on mill approval, so give the delivery condition as well as the thickness, and we will check the approved mill’s range before quoting. Final values are as per standard and mill certificate (see UNCERTAIN).
What welding and preheat guidance applies to KR RD56?
KR RD56 is an extra-high-strength steel (yield ≥ 550 N/mm²) supplied TM or QT. Welding must follow a procedure qualified for this grade and approved by KR. Ceq is calculated from the ladle analysis and limited by the approval chemistry; the mill may also report CET or Pcm for low-carbon TM/QT steel. Hydrogen control, preheat, interpass temperature and heat-input windows come from the approved WPS and the mill’s recommendations. Too much heat input can lower HAZ strength and toughness in QT plate. We send the certificate values before shipment so your welding engineer can confirm the procedure fits.
What is the delivery time for KR RD56 plate?
KR RD56 is normally rolled to order. Typical commercial lead time is about 6–10 weeks from confirmed PO and deposit, depending on the mill rolling schedule, QT capacity, UT and any 3.2 witness. Ocean transit comes on top of that. This is a commercial estimate, not a rule value, and we confirm it with each quotation. Every week, your coordinator sends the rolling, heat-treatment, testing and stamping status with photos. Delays are reported as soon as the mill tells us, not at the shipping date.
Which payment terms do you accept for KR RD56, and how is my deposit protected?
We accept T/T or L/C at sight. With T/T, the usual terms are a 30 % deposit and the balance against the documents or after inspection. You or your inspector can check the KR RD56 stamping, the dimensions and the Surveyor-endorsed certificate before you pay the balance. With L/C, payment is tied to the presented documents. For first orders we can start with a smaller trial lot. The proforma invoice shows the grade (KR RD56 / KR RD56), TM/QT, sizes and certificate type.
Why is it called RD56 and not DH550, and what are the equivalents?
Korean Register numbers its extra-high-strength grades by yield class in the ABS style: 550 N/mm² → 56, so the grade is RD56 (UNCERTAIN against local KR text — confirm on the mill approval). CCS DH550 and DNV use DH550. ASTM A131/A131M stops at FH40, so it has no direct equivalent. ABS DH55 / DQ56 is the usual ABS counterpart. DNV NV D550 is the DNV counterpart (DNV titles DH550). LR DH55 / LR/DH55 is the LR counterpart (LR titles DH55). BV D550 is the BV counterpart (BV titles D550 without H). NK KD550 and CCS DH550 are the NK/CCS counterparts. RINA EHS names are written “per rules” until verified. GB 712 Grade RD56 is listed in the GB 712 EHS band but is not class approval by itself. Always write KR RD56 on the PO, plus any additional society stamps you need.
Can you cut, bevel or machine KR RD56 plates, and how are they packed for export?
Yes. In our workshop we can flame, plasma or laser cut RD56 to drawings, bevel weld edges (V, X or K preparation to your angle and land), drill and machine. Every cut piece keeps traceability: we transfer the KR RD56 marking and heat number before cutting, and the cutting list is tied to the mill certificate. For QT extra-high-strength plate, thermal cutting parameters follow the mill’s recommendations so the cut edge is not damaged. For export, plates are bundled with steel straps and timber spacers, marked with grade, size and heat number, and loaded in containers or as break-bulk. See SHH STEEL for our processing capabilities.

Conclusion

KR RD56 is extra-high-strength hull steel (IACS UR W16 band; KR yield-class number 56): yield 550 N/mm², tensile 670–835 N/mm², Charpy at −20 °C, marking KR RD56. Whatever the IACS family name, only a KR Surveyor-endorsed certificate makes it KR class steel. Lock on the order: TM or QT, UT level, Ceq/CET/Pcm reporting, multi-class and 3.2.

SHH STEEL supplies KR RD56 plate rolled by Chinese mills that hold Korean Register works approval for the grade, so every plate carries the KR RD56 stamp and a Surveyor-endorsed certificate traceable to its heat. Sizes are scheduled into the mill rolling cycle with KR survey arranged at the mill. On request we add EN 10204 3.2 certificates with third-party witness (TÜV, SGS, LR or another agency) and joint certification with ABS, DNV, LR, BV, NK, KR or RINA.

We accept T/T or L/C payment, with inspection before the balance is paid. Small quantities in several sizes, or KR RD56 with neighbouring KR EHS sizes or RA–RF 40 where the drawing allows, can be combined in one container. A dedicated coordinator sends production and shipping updates with photos, and our own workshop cuts to size, bevels, drills and machines plates before shipment so they arrive ready for fabrication.

Request a quotation: send SHH STEEL the grade (KR RD56 / KR RD56), thickness, width, length, quantity per size and destination port, plus any multi-class, Z/U or 3.2 certificate requirement. We reply with price, available stock and lead time.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *



    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *