KR RF32 (KR RF32) higher-strength hull structural steel plate, yield 315 N/mm², tensile 440–590 N/mm², Charpy at −60 °C, stamped KR RF32 with Korean Register–endorsed certificates. SHH STEEL supplies stock and mill-roll plate in China with cutting, multi-class and 3.2 inspection.
Keywords
KR RF32 steel plate, KR FH32 steel plate, KR RF32 shipbuilding steel plate, KR RF32 marine plate, FH32 hull steel, Korean Register FH32 plate, RA/RD/RE/RF 32 marine plate, Korean Register Rules Pt 2 hull steel
Equivalent Grades:
ASTM A131 Grade FH32; ABS FH32; DNV NV F32; LR FH32; BV FH32; NK KF32; CCS F32 / FH32; RINA Grade FH32; GB 712 Grade FH32
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Impact Test and Condition of Supply
Thickness Tolerance
Stock
Equivalent Grades
Grade Selection
Applications and Fabrication
Testing and Inspection
Specification Mistakes
Buyer Concerns
How to Order
FAQ
Conclusion

KR RF32 (KR RF32) shipbuilding steel plate — overview

Technical Reviewer: Jack | SHH STEEL Material Solutions Department · Updated: 2026-10-27

KR RF32 is Korean Register’s −60 °C higher-strength hull steel (IACS FH32 equivalent), with the tighter F-column chemistry of UR W11 — lower C, P and S and a nitrogen cap. It is ordered for ice-class and Arctic LNG/shuttle tonnage built under KR class. Strength level 32 means minimum yield 315 N/mm², tensile 440–590 N/mm² and elongation 22 % min. (A5). The letter F fixes Charpy V-notch testing at −60 °C. In commercial enquiries it is called KR RF32 shipbuilding steel plate; “KR FH32” is a common but unofficial way of writing it.

Equivalent grades: KR RF32 ≈ ASTM A131 Grade FH32 ≈ ABS FH32 ≈ DNV NV F32 ≈ LR FH32 ≈ BV FH32 ≈ CCS F32 / FH32 ≈ NK KF32 ≈ RINA FH32 ≈ GB 712 Grade FH32 (all class-approved, stamped by the issuing society).

KR RF32 is selected when the scantling needs the 32 yield band and the KR material class assigns −60 °C toughness. Ordinary-strength KR RA–RE stay at 235 N/mm² and cannot replace RF32 without a drawing change. In the KR ladder for strength 32: RA32 0 °C → RD32 −20 °C → RE32 −40 °C → RF32 −60 °C; within the F letter, RA32 → RA36 → RA40-style steps raise yield from 315 to 355 to 390 N/mm².

Plates that pass mill tests under KR survey are stamped with the KR mark and RF32 (stencils sometimes add the IACS form FH32 for the yard; plus Z or U where through-thickness or ultrasonic requirements apply) and are supplied with a mill certificate the KR Surveyor endorses. SHH STEEL supplies KR RF32 from Chinese mills that hold KR works approval for the grade, from stock in common sizes or from a mill rolling cycle, with KR survey arranged at the mill.

KR RF32 plate: specification summary

ItemKR RF32 / RF32 data
Rule basisKR Rules Pt 2; IACS UR W11 higher-strength Grade FH32 (KR Rules Pt 2 paragraph cross-refs UNCERTAIN without local KR Rules text)
Official KR designationRF32 (R prefix = KR rolled hull steel); IACS / ABS-style equivalent FH32 — write RF32 on KR-class POs
Related product standardASTM A131/A131M Grade FH32 — product standard only; not KR class approval
Strength levelhigher strength 32, yield 315 N/mm² min., tensile 440–590 N/mm²
Toughness classFH / R → Charpy at −60 °C
Plate thickness primarily coveredup to 100 mm under IACS UR W11 scope for plates; greater thickness by special consideration (see UNCERTAIN)
Deoxidationkilled, fine grain practice (UR W11)
Impact testCharpy V at −60 °C; frequency and supply condition per UR W11 / KR Rules Pt 2 tables
MarkingKR RF32 / KR RF32; plus Z / U / TM where ordered and qualified
TMCP Ceq (indicative UR W11 / industry practice)≤ 0.36 % for t ≤ 50 mm; ≤ 0.38 % for 50 < t ≤ 100 mm (TM steels) — confirm on mill approval / PO
Thickness toleranceIACS UR W13 as adopted by KR (minus tolerance commonly 0.3 mm class — confirm on PO; see UNCERTAIN)
Certificatemill certificate endorsed by the KR Surveyor; EN 10204 3.1 / 3.2 on request

Size range. Common market thicknesses for RF32 are about 6–80 mm (heavier plates available as per mill approval), widths 1500–3500 mm. Exact maximum thickness for a given delivery condition is as per standard and mill certificate / KR works approval. Ask for confirmation above 100 mm.

KR RF32 (KR RF32) chemical composition (heat and product analysis)

ElementHeat (ladle) analysis, %Product (check) analysis, %Note
C0.16 max.numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificateFH group
Mn0.90–1.60numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificate
Si0.10–0.50numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificatemin. waived if acid-soluble Al ≥ 0.015 %
P0.025 max.numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificatetighter for FH
S0.025 max.numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificatetighter for FH
Al (acid soluble) min.0.015 min. acid-solublenumeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificategrain refining
Nb0.02–0.05 when used singlynumeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificatewhen used singly; combined minima in UR W11
V0.05–0.10 when used singlynumeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificatewhen used singly
Ti0.02 max.numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificateneed not be reported unless intentionally added
Cu0.35 max.numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificate
Cr0.20 max.numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificate
Ni0.80 max.numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificateFH allows higher Ni than AH/DH/EH
Mo0.08 max.numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificate
N0.009 max. (0.012 if Al present)numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificateFH specifies N max.

Product (check) analysis column: KR Rules (Part 2) specify heat (ladle) limits; no numeric product-analysis tolerance is tabulated in the rule text reviewed, so product (check) limits are agreed on the order or taken from the approved mill specification and certificate.

Source: IACS UR W11 higher-strength chemistry tables (ladle samples), adopted by Korean Register for KR RF32 in Rules for the Classification of Steel Ships Pt 2 (KR paragraph numbers UNCERTAIN). The full grain-refining and residual set (Al, Nb, V, Ti, Cu, Cr, Ni, Mo, N) is shown so you can check every row on the certificate. AH/DH/EH share one chemistry column; FH is tighter on C, P, S and adds N control with higher Ni allowance. Toughness is differentiated by impact temperature and supply routes, not by separate C/Mn caps within AH/DH/EH. Product (check) analysis numeric tolerances are not tabulated in UR W11; when required, agree tolerances at enquiry. TMCP steels must also meet the applicable Ceq / Pcm limits on the mill approval — ask for Ceq on the certificate.

KR RF32 tensile properties

PropertyRequirement (IACS UR W11)
Tensile strength Rm440–590 N/mm²
Yield strength ReH315 N/mm² min.
Elongation A522 % min.
Impact test temperature−60 °C

Alternative flat-specimen elongations by thickness (indicative UR W11 / industry table for strength 32):

Thickness (mm)≤5>5–10>10–15>15–20>20–25>25–30>30–40>40–50
Elongation min. %1416171819202122

Same tensile band applies to A/AH, D/DH, E/EH and F/FH 32; only impact temperature and chemistry group (FH vs AH/DH/EH) change across the letter.

KR RF32: Charpy at −60 °C and supply condition

ThicknessLong. avg. at −60 °CTrans. avg. at −60 °C
t ≤ 50 mm31 J22 J
50 < t ≤ 70 mm38 J26 J
70 < t ≤ 100 mm46 J31 J

Source: IACS UR W11 impact table for higher-strength Grade FH32 (full-size; either direction acceptable unless specified). Energies rise with thickness — a 60 mm plate must meet higher values than a 20 mm plate at the same −60 °C. Condition of supply and impact lot size depend on grain-refining practice and thickness (AR/CR/N/TM/QT as permitted). For TMCP RF32, respect Ceq caps ≈ 0.36 % (t≤50) / 0.38 % (50

Thickness tolerance and surface condition

Korean Register applies IACS UR W13 thickness tolerances unless the PO states otherwise (often 0.3 mm minus class — confirm on PO; see UNCERTAIN). Plus/flatness/width/length per agreed standard (ASTM A6, EN 10029 or GB/T 709). Surface quality per EN 10163 or equivalent accepted by KR; state primer/surface class on receipt if needed.

KR RF32 plate stock in China

Thickness (mm)Width (mm)Length (mm)ConditionApprox. quantityLocation
61800 / 20006000 / 8000AR / CR / N / TM100+ tChina
81800 / 20008000 / 12000AR / CR / N / TM200+ tChina
102000 / 22008000 / 12000AR / CR / N / TM200+ tChina
122000 / 2200 / 250012000AR / CR / N / TM200+ tChina
142000 / 220012000AR / CR / N / TM100+ tChina
162000 / 250012000AR / CR / N / TM200+ tChina
202000 / 250012000AR / CR / N / TM100+ tChina
252200 / 250012000AR / CR / N / TM100+ tChina
30220010000 / 12000AR / CR / N / TM100+ tChina
40220010000AR / CR / N / TM50+ tChina
5022008000 / 10000AR / CR / N / TM50+ tChina

Quantities are approximate and change daily (indicative — confirm before booking); all stock plates carry KR RF32 marking and KR-endorsed mill certificates when sold as KR class plate. Sizes outside the table (for example 3000 mm width, 60–100 mm thickness, or fixed lengths for a cutting plan) are produced in the next mill rolling cycle, typically 3–6 weeks including KR survey. Send your size list and we will reply with what is in stock and what must be rolled.

Packing. Plates are bundled by size with steel strapping, marked with heat number, grade and KR stamp, and shipped in containers (up to about 11.8 m) or break bulk for longer plates.

KR RF32 equivalents in other rules and standards

Standard / societyDesignationComment
KR (Korean Register)KR RF32this page; official KR designation RF32 (IACS FH32); stamped under KR survey
GB 712GB 712 Grade FH32Chinese product standard; not class approval by itself
ASTM A131/A131MASTM A131/A131M Grade FH32A131 lists AH–FH 32/36/40; product standard only
ABSABS FH32IACS UR W11 higher-strength; live product page
DNVDNV NV F32IACS UR W11; live product page
LRLR FH32 / LR/FH32IACS UR W11; live product page
BVBV FH32IACS UR W11; live product page
NK (ClassNK)NK KF32ClassNK KF32
CCSCCS F32 / FH32IACS UR W11; live CCS product page
RINARINA Grade FH32confirm exact designation per RINA rules
Structural (indicative)S275JRland structural; no class marking

These are comparisons, not substitutions. Multi-class stamps (KR + ABS / DNV / LR / BV) require joint survey before rolling. Other KR siblings in the 32 band are linked via KR until each product page is live.

KR RF32 vs other KR hull grades

Pick RF32 when the drawing specifies higher-strength grade FH32 (KR writes FH32 as RF32). Do not substitute ordinary Grade A/B unless the designer recalculates scantlings — yield differs (315 vs 235). Within the 32 band, letter choice is toughness: A/AH 0 °C → D/DH −20 °C → E/EH −40 °C → F/FH −60 °C. Within the FH letter, strength steps 32 → 36 → 40 raise yield from 315 to 355 to 390 N/mm².

For yields above 390 N/mm² KR moves to extra-high strength (IACS UR W16): RA43…RF70, numbered by ABS-style yield class (420 → 43 … 690 → 70; UNCERTAIN vs local KR text) rather than CCS/DNV FH420 or BV A420.

When KR RF32 is the right choice: typical uses are low-temperature service: Arctic and polar-class hulls, ice belts and offshore units in cold regions where −60 °C toughness is specified. The Charpy temperature (−60 °C) is fixed by the letter, and the strength by the number (ReH 315 N/mm²). Pick the strength from the scantling calculation and the letter from the material class and design temperature on the approved drawing.

Applications, cutting and welding of KR RF32

Typical uses: low-temperature service: Arctic and polar-class hulls, ice belts and offshore units in cold regions where −60 °C toughness is specified; weight-saving vs ordinary-strength plate in large tankers, bulkers and container ships built to KR class. See offshore platform steel plates when primary offshore grades apply.

Welding: higher-strength hull steels need approved higher-strength consumables matched to −60 °C weld-metal toughness; preheat and heat input follow the approved WPS and often track Ceq/Pcm from the mill certificate. TMCP RF32 must respect the Ceq caps noted above. Cutting by oxy-fuel/plasma/laser is routine; thick FH plate may need hydrogen control — follow mill recommendations.

Processing notes for KR RF32: cold forming is routine within normal shipyard radii. Line heating and fairing of TMCP plate should stay within the temperature limits recommended by the mill, because overheating can reduce the strength gained in controlled rolling. Check the delivery condition on the certificate before planning hot forming.

Certificates, KR survey and third-party inspection

Every plate is tested and marked at the mill under Korean Register survey; the mill certificate lists heat number, ladle chemistry, Ceq where applicable, tensile results (ReH ≥ 315 N/mm², Rm 440–590 N/mm², A ≥ 22 %), Charpy at −60 °C, delivery condition and plate numbers, endorsed by the Surveyor. Optional EN 10204 3.2, UT (U), Z-direction, multi-class with ABS/DNV/LR/BV.

On receipt: verify KR RF32 (or KR RF32) stamp, −60 °C impact data, energies for the delivered thickness band, thickness within UR W13 / PO tolerance, KR Surveyor endorsement present — not a mill-only certificate.

Charpy acceptance for KR RF32 by thickness (IACS UR W11; actual results as per standard and mill certificate):

Thickness t (mm)Test temperatureAverage energy, longitudinal (J min.)Average energy, transverse (J min.)
t ≤ 50−60 °C3122
50 < t ≤ 70−60 °C3826
70 < t ≤ 100−60 °C4631

If UT or 3.2 was ordered, check the UT report and inspector’s plate list as well.

Common mistakes when ordering KR RF32 (KR RF32)

  • Ordering “KR 32” without the letter — toughness class missing
  • Writing FH32 (ABS/CCS style) on a KR PO without stating KR RF32 — the KR certificate and stamp read RF32
  • Accepting ordinary-strength Grade A/B certificates for a RF32 PO
  • Accepting a FH32 certificate from another society (or a product-standard paper) where KR RF32 is specified
  • Ignoring TMCP Ceq caps on TM plate
  • FH chemistry (tighter P/S, N) not checked when the PO says FH
  • Coil-cut plate without coil approval
  • Missing KR endorsement on the MTC
  • Writing DNV NV F32 or LR/FH32 on a KR-class PO without arranging that society’s survey

Write the KR grade (RF32), delivery condition, impact temperature and certificate type into the PO.

Sourcing KR RF32: buyer concerns and SHH STEEL solutions

ConcernHow SHH STEEL handles it
Fake class plateKR-approved mills only; traceable KR RF32 stamp + certificate; 3.2 on request
Payment riskT/T or L/C; inspection before balance
Mixed sizes / gradesRF32 combined with KR Grade A/B/D/E or other A–FH sizes in one container
Lead time visibilityweekly photo updates from dedicated coordinator
Prep before shipcutting, bevelling, drilling, machining in our workshop

How to order KR RF32 plate

Specify KR RF32 (KR RF32), delivery condition (AR/CR/N/TM/QT as applicable), thickness × width × length × qty, Z/U, multi-class, certificate type, port. Send to SHH STEEL.

Sample PO line: “Steel plate to KR Rules for the Classification of Steel Ships, Pt 2, Grade RF32 (KR RF32), delivery condition [AR/CR/N/TM/QT], 20 × 2500 × 12000 mm, 30 pcs, marked KR RF32, certificate endorsed by KR Surveyor, EN 10204 3.2 [if required], UT [if required], CIF [port].”

FAQ

What sizes and minimum order quantity can you supply for KR RF32 (KR RF32) plate?
IACS UR W11 lists FH32 plate primarily up to 100 mm; thicker plate needs special KR consideration. Most enquiries we receive for RF32 are 8–60 mm thick, 1800–3000 mm wide and 6000–12000 mm long. Popular sizes can come from China stock carrying the KR RF32 marking, with no fixed minimum. A mill rolling for a special width, thickness above roughly 60 mm or a Z-grade normally needs a minimum quantity per size, which we confirm per order. We can combine several sizes, or RF32 with other hull grades, to reach a rolling or container quantity.
How is KR RF32 certified, and can you arrange EN 10204 3.2 or dual-class with ABS/DNV/LR/BV?
Every plate is made by a KR-approved mill under Korean Register survey. It is die-stamped or stencilled KR RF32 / KR RF32 with the heat or plate number, and the mill test certificate is endorsed by the KR Surveyor. The certificate gives the ladle chemistry, the tensile results (ReH ≥ 315 N/mm², Rm 440–590 N/mm², A ≥ 22 %), the Charpy results at −60 °C, the delivery condition and the plate identity. An ASTM A131 or GB 712 certificate for FH32 alone is not KR class approval. If your contract asks for EN 10204 3.2, we arrange it before rolling. Dual or multi-class (KR + ABS, DNV, LR or BV) must be booked before testing. 3.2 cannot be added after testing, so please state it on the enquiry.
What is the impact test temperature and energy for KR RF32, and do thickness limits apply?
KR RF32 is tested at −60 °C. Required average energies (longitudinal/transverse, J min.) under IACS UR W11 rise with thickness: ≤50 mm 31/22; 50–70 mm 38/26; 70–100 mm 46/31. This matters when you order thick RF32: a 60 mm plate must meet higher values than a 20 mm plate at the same −60 °C. The test lot size and the permitted delivery condition (AR, CR, N, TM or QT) follow the UR W11 / KR Rules Pt 2 supply table. Above 100 mm, agree data positions and energies with KR. Results are as per standard and mill certificate.
What welding and preheat guidance applies to KR RF32?
KR RF32 needs higher-strength welding consumables approved for −60 °C weld-metal toughness. For TMCP plate, Ceq is commonly capped near 0.36 % (t ≤ 50 mm) and 0.38 % (50 < t ≤ 100 mm) under UR W11 practice; above 100 mm it is agreed at mill approval. N or AR plate of the same grade may have a higher actual Ceq, so the delivery condition affects how easy the plate is to weld. Preheat, interpass temperature and heat input must follow your KR-approved WPS. We send the mill certificate’s ladle analysis and Ceq before shipment so the welding engineer can confirm the procedure qualifies. We do not give generic preheat temperatures.
What is the delivery time for KR RF32 plate?
Stock sizes of KR RF32 can usually be cut, inspected and loaded in about 7–15 days. Mill-rolled orders typically take about 3–6 weeks plus inspection, depending on thickness, delivery condition and the mill schedule. These are commercial estimates, confirmed with each quote. If 3.2 witness or multi-class survey is required, we book the inspector when we place the mill order so testing is not delayed. A dedicated coordinator sends weekly progress photos until the bill of lading is issued.
Which payment terms do you accept for KR RF32, and how is my deposit protected?
We accept T/T or L/C at sight. With T/T, the usual terms are a 30 % deposit and the balance against the documents or after inspection. You or your inspector can check the KR RF32 stamping, the dimensions and the Surveyor-endorsed certificate before you pay the balance. With L/C, payment is tied to the presented documents. For first orders we can start with a smaller trial lot. The proforma invoice shows the grade (KR RF32 / KR RF32), sizes and certificate type.
Why does KR write RF32 instead of FH32, and what are the equivalent grades?
Korean Register uses an R prefix for rolled hull steels, so the IACS UR W11 grade FH32 appears in KR Rules and on KR certificates as RF32. Our title uses the official RF32; FH32 is the familiar cross-society name. KR RF32 corresponds to ASTM A131/A131M Grade FH32, ABS FH32, DNV NV F32, LR FH32 / LR/FH32, BV FH32, NK KF32, CCS F32 / FH32, RINA Grade FH32 (confirm RINA designation per rules), and GB 712 Grade FH32. All share yield 315 N/mm², tensile 440–590 N/mm² and a Charpy test at −60 °C under IACS UR W11. Even so, a plate is only accepted by the society whose stamp and certificate it carries. Order KR RF32 for KR class, or ask for multi-class when one stock must serve several projects. GB 712 or A131 certificates alone do not replace the KR RF32 stamp.
Can you cut, bevel or machine KR RF32 plates, and how are they packed for export?
Yes. In our workshop we can flame, plasma or laser cut RF32 to drawings, bevel weld edges (V, X or K preparation to your angle and land), drill and machine. Every cut piece keeps traceability: we transfer the KR RF32 marking and heat number before cutting, and the cutting list is tied to the mill certificate. For export, plates are bundled with steel straps and timber spacers, marked with grade, size and heat number, and loaded in containers or as break-bulk. Shot blasting and shop primer are available on request. See SHH STEEL for our processing capabilities.

Conclusion

KR RF32 / KR RF32 is higher-strength hull steel under KR Rules for the Classification of Steel Ships, Pt 2 and IACS UR W11: yield 315 N/mm², tensile 440–590 N/mm², Charpy at −60 °C, marking KR RF32. FH32 is the cross-society name for the same IACS grade, but only the KR RF32 stamp and KR-endorsed certificate are accepted for KR class. Lock on the order: delivery condition, impact lot size, TMCP Ceq if TM, product analysis if needed, multi-class and 3.2.

SHH STEEL supplies KR RF32 plate rolled by Chinese mills that hold Korean Register works approval for the grade, so every plate carries the KR RF32 stamp and a Surveyor-endorsed certificate traceable to its heat. Common thicknesses are available from stock; other sizes are scheduled into the mill rolling cycle with KR survey arranged at the mill. On request we add EN 10204 3.2 certificates with third-party witness (TÜV, SGS, LR or another agency) and joint certification with ABS, DNV, LR, BV, NK, KR or RINA.

We accept T/T or L/C payment, with inspection before the balance is paid. Small quantities in several sizes, or KR RF32 mixed with KR RA/RB/RD/RE or other RA–RF 32/36/40 sizes, can be combined in one container. A dedicated coordinator sends production and shipping updates with photos, and our own workshop cuts to size, bevels, drills and machines plates before shipment so they arrive ready for fabrication.

Request a quotation: send SHH STEEL the grade (KR RF32 / KR RF32), thickness, width, length, quantity per size and destination port, plus any multi-class, Z/U or 3.2 certificate requirement. We reply with price, available stock and lead time.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *



    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *



      X