JIS G3101 SS540 Steel Plate | JIS G3101 Steel - SHH STEEL

JIS G3101 SS540 Steel Plate

JIS G3101 SS540 is a hot-rolled general structural steel. It is the highest-tensile JIS G 3101 grade. The name marks a 540 N/mm² tensile minimum, not yield. Table 3 gives 540 N/mm² minimum tensile strength. Yield is 400 N/mm² up to 16 mm and 390 N/mm² through 40 mm. Plate thickness is limited to 40 mm. Carbon is 0.30 % max and manganese is 1.60 % max. SHH STEEL produces and exports this steel plate to the ordered thickness, tests and documentation.
Equivalent Grades:
Hot-rolled general structural steel, 540 N/mm² tensile class (SS540)
Heat Treatment
As-rolled; no required normalizing.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
Conclusion

What is JIS G3101 SS540 Steel Plate?

JIS G3101 SS540 Steel Plate is a hot-rolled steel for general structures under JIS G 3101, Rolled steels for general structure. Figures on this page follow Table 1 (types and applicable sizes), Table 2 (ladle analysis) and Table 3 (mechanical properties) of JIS G 3101:2015. The current listed edition is JIS G 3101:2024; that listing is cited only for status and revision and is not used here as the acceptance table. JIS G 3101:2015 places plate and bar mechanical properties in one Table 3. The formal grades are SS330, SS400, SS490 and SS540. This page is SS540. The number in the grade name is the specified minimum tensile strength in N/mm², not the yield strength.

The standard covers hot-rolled steels used in bridges, ships, vehicles and other structures, together with hot-extruded sections under a separate annex. For SS540, Table 1 of JIS G 3101:2015 limits steel plates, strip, sections and flats to 40 mm thickness or less, and bars to a diameter, side or distance across flats of 40 mm or less. This article is written for plate supply under the structural-plate hub; bar rows from the same 2015 Table 3 are printed separately so they are not mixed with the plate rows.

JIS G 3101 does not require a fully killed practice and does not require the product to be normalized. If a heat treatment has been applied, the standard only gives sampling rules for that heat-treated lot. It does not turn normalizing into the delivery condition of the grade.

SHH STEEL produces and exports JIS G3101 SS540 Steel Plate to the ordered thickness, tests and documentation. A related published range is Structural Steel Plates.

Material specification for JIS G3101 SS540 Steel Plate

The items below follow JIS G 3101. Thickness, width, length and the inspection document are stated on the enquiry rather than listed here as stock or capacity ranges.

Parameter Detail
Standard JIS G 3101, Rolled steels for general structure. Technical tables: JIS G 3101:2015. Current listing (status only): JIS G 3101:2024. The 2024 listing is not used here as the acceptance table
Grade SS540. The number is the minimum tensile strength in N/mm² (1 N/mm² = 1 MPa), not a yield class
Formal set Four grades: SS330, SS400, SS490 and SS540. This page is SS540
Product form Table 1 of JIS G 3101:2015 limits steel plates, strip, sections and flats to 40 mm thickness or less, and bars to a diameter, side or distance across flats of 40 mm or less
Scope on this page Plate, strip, sections and flats 40 mm or less; bars 40 mm or less
Delivery condition Hot-rolled general structural steel. The standard does not require normalizing and does not require a fully killed practice
Chemistry basis Table 2 ladle analysis (溶鋼分析). Product-analysis deviations are not printed in Table 2 and are not invented here
Mechanical basis Table 3 of JIS G 3101:2015. Plate, strip, flat and section rows and bar rows are printed as two groups from that single table
Impact JIS G 3101 does not specify Charpy absorbed-energy values
Dimensional standards JIS G 3193 for plates and strip. If not otherwise specified, cut-edge width uses tolerance A of JIS G 3193 Table 7 and length uses tolerance A of Table 8
Our supply We produce and export SS540 as steel plate to the thickness, tests and documentation agreed on the order

Chemical composition of JIS G3101 SS540 Steel Plate

The ladle analysis shall comply with Table 2 of JIS G 3101:2015. The row below is the SS540 ladle-analysis row of that table.

Element SS540 ladle analysis, JIS G 3101 Table 2 (mass %)
C 0.30 max.
Mn 1.60 max.
P 0.040 max.
S 0.040 max.

Table 2 of JIS G 3101:2015 specifies carbon and manganese for SS540, together with phosphorus and sulfur. Alloying elements other than those listed in Table 2 may be added as necessary.

Table 2 is a ladle-analysis table. This page does not invent product-analysis deviation numbers.

Mechanical properties and thickness limits

Under clause 5 of JIS G 3101:2015, yield point or proof strength, tensile strength, elongation and bendability shall comply with Table 3. The tables below are the SS540 rows of that single table, grouped so plate rows and bar rows are not mixed. Values are in N/mm²; 1 N/mm² = 1 MPa. The number in SS540 is the tensile class, not a single yield value for every thickness.

Property, Table 3 of JIS G 3101:2015 (plates, strip, flats and sections) SS540
Yield point or proof strength, 16 mm or less 400 N/mm² min.
Yield point or proof strength, over 16 mm up to 40 mm 390 N/mm² min.
Tensile strength 540 N/mm² min.
Elongation, 5 mm or less, No. 5 test piece 16 % min.
Elongation, over 5 mm up to 16 mm, No. 1A test piece 13 % min.
Elongation, over 16 mm up to 40 mm, No. 1A test piece 17 % min.
Bend test 180°, inner radius 2.0 times the thickness, No. 1 test piece (No. 3 may be used at 5 mm thickness or less)
Property, Table 3 of JIS G 3101:2015 (bars) SS540
Yield point or proof strength, 16 mm or less 400 N/mm² min.
Yield point or proof strength, over 16 mm up to 40 mm 390 N/mm² min.
Tensile strength 540 N/mm² min.
Elongation, diameter, side or distance across flats 25 mm or less, No. 2 test piece 13 % min.
Elongation, diameter, side or distance across flats over 25 mm up to 40 mm, No. 14A test piece 16 % min.
Bend test 180°, inner radius 2.0 times the diameter, side or distance across flats, No. 2 test piece

For sections, thickness is the thickness at the test-piece location. For bars, round bars use the diameter, square bars use the side and hexagonal bars use the distance across flats. The outside of a bend test piece shall be free from cracks. The bend test itself may be omitted at the manufacturer’s discretion unless the purchaser specifies it, but the bend property must still be satisfied.

JIS G 3101 does not specify Charpy absorbed energy. This page does not invent a joule value or a test temperature.

Delivery conditions for JIS G3101 SS540 Steel Plate

JIS G 3101 is a specification for hot-rolled steels for general structure:

  • The products are supplied as hot-rolled general structural steel.
  • The standard does not require a fully killed deoxidation practice.
  • The standard does not require normalizing as the delivery condition.
  • If a heat treatment has been applied, test-piece grouping follows that heat-treated lot. That rule is not a normalizing guarantee.
  • Unless otherwise specified, the inspection document is an inspection certificate 3.1 to JIS G 0415.

Do not treat a quenched-and-tempered plate, a normalized pressure-vessel plate, or a JIS G 3106 SM welded-structure grade as the automatic delivery condition of this part.

We produce and export SS540 as hot-rolled steel plate within 40 mm thickness.

Welding and fabrication

JIS G 3101 does not prescribe preheat temperatures, heat-input limits or a carbon-equivalent maximum. Table 2 specifies carbon (0.30 % max.) and manganese (1.60 % max.) for SS540, which is tighter than the SS330, SS400 and SS490 rows. That still does not turn this page into a welding procedure. This page does not invent a welding procedure or a calculated CEV.

Steels specified for welded structures are written to JIS G 3106 (SM grades) and other welding-oriented standards. Those names are not automatic substitutes for SS540.

Form, finish and dimensions

Dimensions, shape, mass and tolerances follow JIS G 3193 for plates and strip, JIS G 3192 for sections, JIS G 3194 for flats and JIS G 3191 for bars. If width and length are not otherwise specified, cut-edge plate width uses tolerance A of JIS G 3193 Table 7 and plate length uses tolerance A of Table 8. This page does not reprint those tolerance tables and does not list stock sizes or mill-capacity ranges.

We produce and export SS540 to the dimensions and surface requirements agreed on the enquiry.

Applications and specification limits

SS540 is specified for general structural parts that name JIS G 3101 and this grade, including bridges, ships, vehicles and similar structures written to that standard. Allowable design stresses and any toughness rule come from the construction code or the purchaser specification. JIS G 3101 itself does not specify Charpy values.

Table 3 of JIS G 3101:2015 requires a 180° bend with an inner radius of 2.0 times the thickness on plate products and a 180° bend with an inner radius of 2.0 times the diameter, side or distance across flats on bars. Those two row groups belong to the same table and are printed separately so they are not mixed.

This page is not ASTM A36 plate, not EN 10025-2 S235 or S275 plate, and not a JIS G 3106 SM welded-structure grade. It is also not an automatic match for Chinese Q235 names.

Compare JIS G3101 SS540 Steel Plate with other steel products

JIS G3101 SS540 Steel Plate is a JIS G 3101 general structural steel identified by its tensile class, not by a single yield number. The comparison uses three products we already publish. They are related by engineering use or similar names, not equivalents. Unpublished JIS G 3101 sibling grades are not linked here.

Material Alloy / type Delivery condition Mechanical requirements Typical service Substitution limit
JIS G3101 SS540 Steel Plate (this product) JIS G 3101 SS540; ladle analysis to Table 2; tensile class 540 N/mm² Hot-rolled general structural steel; normalizing not required Table 3 of JIS G 3101:2015: tensile 540 N/mm² min.; yield 400 N/mm² min. at 16 mm or less; 390 N/mm² min. over 16 mm up to 40 mm; 180° bend General structural plate specified to JIS G 3101 SS540 Not interchangeable with Q235, S235 or A36 names unless the project specification allows it
ASTM A36 Steel Plate From our A36 page: A36 carbon structural steel plate From our A36 page: carbon structural steel plate From our A36 page: min yield 250 MPa From our A36 page: construction, bridges and general fabrication Not an equivalent. A36 is identified by a yield minimum on that page; SS540 is identified by a tensile class under JIS G 3101
EN 10025-2 S235JR Steel Plate From our S235JR page: EN 10025-2 non-alloy structural steel From our S235JR page: non-alloy structural steel From our S235JR page: 235 MPa yield strength Structural plate specified to EN 10025-2 S235JR Not an equivalent. SS400 is not an automatic S235JR match, and SS540 must be ordered to JIS G 3101
EN 10025-2 S275JR Steel Plate From our S275JR page: EN 10025-2 non-alloy structural steel From our S275JR page: non-alloy structural steel From our S275JR page: 275 MPa yield strength Structural plate specified to EN 10025-2 S275JR Not an equivalent. A similar yield band on one thickness does not make the two stamps interchangeable

A related published range: Structural Steel Plates.

Equivalent and related grades by country

The designations below are near names or related national plates, not certified or automatic equivalents. Chemistry, thickness, delivery condition, bend rules and the required stamp must match the project specification before a substitution is considered. Unpublished JIS G 3101 siblings are named as plain text only.

Country / region Standard Grade Similarity and key differences Substitution caveat
Japan JIS G 3101 SS540 This hot-rolled general structural steel. The formal list is SS330, SS400, SS490 and SS540. The number is the minimum tensile strength, not the yield. Specify JIS G 3101, this named grade, product form (plate, strip, section, flat or bar), thickness and the inspection document.
Japan JIS G 3106 SM400, SM490 or another named SM grade Rolled steels for welded structures, with their own chemistry and toughness rules, not the SS series of JIS G 3101. Do not treat an SM name as an automatic SS match.
Europe EN 10025-2 S235JR or S275JR From our live pages: S235JR has a 235 MPa yield; S275JR has a 275 MPa yield. Not an automatic equivalent of SS400 or of SS540. See EN 10025-2 S235JR Steel Plate and EN 10025-2 S275JR Steel Plate.
United States ASTM A36/A36M A36 From our A36 page: min yield 250 MPa, used in construction, bridges and general fabrication. Not an automatic equivalent. See ASTM A36 Steel Plate.
China GB/T 700 Q235 names used in catalogues Chinese carbon structural steels written to GB/T 700, not to JIS G 3101. This site does not currently publish a Q235B product page, so no Q235 link is offered. SS400 is not an automatic Q235 match. Do not substitute on the name alone.

Why choose SHH STEEL for JIS G3101 SS540 Steel Plate

  • We produce and export JIS G 3101 SS540 hot-rolled steel plate
  • We review the enquiry for edition, grade, product form and thickness within 40 mm
  • We keep the tensile-class grade name distinct from yield-based names such as S235 or Q235
  • We do not invent carbon or manganese limits where Table 2 marks them as not specified, and we do not invent a Charpy value
  • We match documentation to what the purchase order requires

How to enquire for JIS G3101 SS540 Steel Plate

Item What to specify
Standard and grade JIS G 3101, SS540. Name the edition required by the project. Figures on this page follow JIS G 3101:2015 Table 1, Table 2 and Table 3
Product form Plate, strip, section, flat or bar. State which form is required. Plate and bar rows from Table 3 are printed separately
Thickness and dimensions Thickness, width and length. Table 1 limits this grade to 40 mm
Delivery condition Hot-rolled general structural steel. Do not assume fully killed or normalized supply unless the order says so
Chemistry Table 2 ladle analysis. Carbon 0.30 % max. and manganese 1.60 % max. apply
Mechanical tests Table 3 tension and bend of JIS G 3101:2015. Write a bend-test request if the test itself must be performed rather than omitted
Documentation State the inspection document type if it is not the default 3.1 certificate
Processing Cutting or other processing only when requested

Request a quotation

Contact SHH STEEL for a quotation for JIS G 3101 SS540 hot-rolled steel plate. Please include your required quantity, thickness, width and length, delivery destination and preferred delivery schedule so we can review your production and export requirements.

Specify JIS G 3101, SS540, and the edition required by the project. Figures on this page follow JIS G 3101:2015 Table 1, Table 2 and Table 3. The grade name is a tensile class (540 N/mm²), not a single yield number. Table 1 limits this grade to 40 mm.

If your enquiry compares SS540 with ASTM A36, EN 10025-2 S235JR or EN 10025-2 S275JR, identify each product clearly. We will review the differences in standard, tensile class, yield-by-thickness rules and chemistry rather than assume that similar names are interchangeable.

For a detailed quotation, email your material specification, quantity and delivery requirements to our team.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X