Product Showcase
GB/T 713.7-2023 Stainless Steel Products
SHH STEEL supplies GB/T 713.7-2023 stainless steel and heat-resisting steel plates and coils for pressure equipment as Factory-Direct Supply and export. This part replaces GB/T 24511-2017 and covers austenitic, ferritic and duplex grades for boilers, pressure vessels and related equipment. Common grades include S30403, S31603, S32168, S22053 and S25073.S30403, S31603, S32168, S22053, S25073, 304 316 Hot-rolled and cold-rolled supply, including thinner cold-rolled strip from 0.30 mm. Competitive mill price, cut-to-size service, fast delivery and full MTCs.
-
GB/T 713.7 06Cr18Ni11Nb S34778 Pressure Vessel Stainless Plate
GB/T 713.7 06Cr18Ni11Nb (S34778) is a stabilized austenitic stainless steel plate for pressure equipment, equivalent in family to ASTM A240 347. Under GB/T 713.7-2023 it is delivered solution treated with Rp0.2 ≥205 MPa and Rm ≥ 515 MPa (Table 16). SHH STEEL supplies it in 0.30 – 100 mm, cut to size, with heat and product analysis on EN 10204 3.1 or 3.2 certificates.View More -
GB/T 713.7 07Cr19Ni11Ti S32169 Pressure Vessel Stainless Plate
GB/T 713.7 07Cr19Ni11Ti (S32169) is a controlled-carbon stabilized austenitic stainless steel plate for pressure equipment, equivalent in family to ASTM A240 321H. Under GB/T 713.7-2023 it is delivered solution treated with Rp0.2 ≥205 MPa and Rm ≥ 515 MPa (Table 16). SHH STEEL supplies it in 0.30 – 100 mm, cut to size, with heat and product analysis on EN 10204 3.1 or 3.2 certificates.View More -
GB/T 713.7 06Cr18Ni11Ti S32168 Pressure Vessel Stainless Plate
GB/T 713.7 06Cr18Ni11Ti (S32168) is a stabilized austenitic stainless steel plate for pressure equipment, equivalent in family to ASTM A240 321. Under GB/T 713.7-2023 it is delivered solution treated with Rp0.2 ≥205 MPa and Rm ≥ 520 MPa (Table 16). SHH STEEL supplies it in 0.30 – 100 mm, cut to size, with heat and product analysis on EN 10204 3.1 or 3.2 certificates.View More -
GB/T 713.7 022Cr17Ni12Mo2N S31653 Pressure Vessel Stainless Plate
GB/T 713.7 022Cr17Ni12Mo2N (S31653) is a low-carbon, nitrogen-strengthened austenitic stainless steel plate for pressure equipment, equivalent in family to ASTM A240 316LN. Under GB/T 713.7-2023 it is delivered solution treated with Rp0.2 ≥205 MPa and Rm ≥ 515 MPa (Table 16). SHH STEEL supplies it in 0.30 – 100 mm, cut to size, with heat and product analysis on EN 10204 3.1 or 3.2 certificates.View More -
GB/T 713.7 06Cr17Ni12Mo2N S31658 Pressure Vessel Stainless Plate
GB/T 713.7 06Cr17Ni12Mo2N (S31658) is a nitrogen-strengthened austenitic stainless steel plate for pressure equipment, equivalent in family to ASTM A240 316N. Under GB/T 713.7-2023 it is delivered solution treated with Rp0.2 ≥240 MPa and Rm ≥ 550 MPa (Table 16). SHH STEEL supplies it in 0.30 – 100 mm, cut to size, with heat and product analysis on EN 10204 3.1 or 3.2 certificates.View More -
GB/T 713.7 06Cr17Ni12Mo2Ti S31668 Pressure Vessel Stainless Plate
GB/T 713.7 06Cr17Ni12Mo2Ti (S31668) is a stabilized austenitic stainless steel plate for pressure equipment, equivalent in family to ASTM A240 316Ti. Under GB/T 713.7-2023 it is delivered solution treated with Rp0.2 ≥205 MPa and Rm ≥ 520 MPa (Table 16). SHH STEEL supplies it in 0.30 – 100 mm, cut to size, with heat and product analysis on EN 10204 3.1 or 3.2 certificates.View More -
GB/T 713.7 07Cr17Ni12Mo2 S31609 Pressure Vessel Stainless Plate
GB/T 713.7 07Cr17Ni12Mo2 (S31609) is a controlled-carbon (H-grade) austenitic stainless steel plate for pressure equipment, equivalent in family to ASTM A240 316H. Under GB/T 713.7-2023 it is delivered solution treated with Rp0.2 ≥220 MPa and Rm ≥ 515 MPa (Table 16). SHH STEEL supplies it in 0.30 – 100 mm, cut to size, with heat and product analysis on EN 10204 3.1 or 3.2 certificates.View More -
GB/T 713.7 022Cr17Ni12Mo2 S31603 Pressure Vessel Stainless Plate
GB/T 713.7 022Cr17Ni12Mo2 (S31603) is a low-carbon austenitic stainless steel plate for pressure equipment, equivalent in family to ASTM A240 316L. Under GB/T 713.7-2023 it is delivered solution treated with Rp0.2 ≥210 MPa and Rm 520 – 680 MPa (Table 16). SHH STEEL supplies it in 0.30 – 100 mm, cut to size, with heat and product analysis on EN 10204 3.1 or 3.2 certificates.View More -
GB/T 713.7 06Cr17Ni12Mo2 S31608 Pressure Vessel Stainless Plate
GB/T 713.7 06Cr17Ni12Mo2 (S31608) is a molybdenum-bearing 17-12-2 austenitic stainless steel plate for pressure equipment, equivalent in family to ASTM A240 316. Under GB/T 713.7-2023 it is delivered solution treated with Rp0.2 ≥220 MPa and Rm 520 – 680 MPa (Table 16). SHH STEEL supplies it in 0.30 – 100 mm, cut to size, with heat and product analysis on EN 10204 3.1 or 3.2 certificates.View More -
GB/T 713.7 05Cr19Ni10Si2CeN S30450 Pressure Vessel Stainless Plate
GB/T 713.7 05Cr19Ni10Si2CeN (S30450) is a heat-resisting austenitic stainless steel plate for pressure equipment, equivalent in family to ASTM A240 S30415. Under GB/T 713.7-2023 it is delivered solution treated with Rp0.2 ≥290 MPa and Rm ≥ 600 MPa (Table 16). SHH STEEL supplies it in 0.30 – 100 mm, cut to size, with heat and product analysis on EN 10204 3.1 or 3.2 certificates.View More -
GB/T 713.7 06Cr19Ni9NbN S30478 Pressure Vessel Stainless Plate
GB/T 713.7 06Cr19Ni9NbN (S30478) is a nitrogen-strengthened austenitic stainless steel plate for pressure equipment. Under GB/T 713.7-2023 it is delivered solution treated with Rp0.2 ≥275 MPa and Rm ≥ 585 MPa (Table 16). SHH STEEL supplies it in 0.30 – 100 mm, cut to size, with heat and product analysis on EN 10204 3.1 or 3.2 certificates.View More -
GB/T 713.7 022Cr19Ni10N S30453 Pressure Vessel Stainless Plate
GB/T 713.7 022Cr19Ni10N (S30453) is a low-carbon, nitrogen-strengthened austenitic stainless steel plate for pressure equipment, equivalent in family to ASTM A240 304LN. Under GB/T 713.7-2023 it is delivered solution treated with Rp0.2 ≥205 MPa and Rm ≥ 515 MPa (Table 16). SHH STEEL supplies it in 0.30 – 100 mm, cut to size, with heat and product analysis on EN 10204 3.1 or 3.2 certificates.View More
GB/T 713.7-2023 Stainless Steel Products
Stainless Steel Sheets and Plates
SHH STEEL, a leading Stainless Steel Sheets and Plates exporter, produces and exports stainless steel sheets (0.3–6 mm) and plates (>6 mm) for marine, chemical, and structural applications. Our products, like 304 and 316L (ASTM A240), offer corrosion resistance and durability. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Trust SHH STEEL for 316L stainless steel plates and custom solutions for your projects.
Stainless Steel Sheets and Plates
X