SHH STEEL supplies GB/T 713.7-2023 stainless steel and heat-resisting steel plates and coils for pressure equipment as Factory-Direct Supply and export. This part replaces GB/T 24511-2017 and covers austenitic, ferritic and duplex grades for boilers, pressure vessels and related equipment. Common grades include S30403, S31603, S32168, S22053 and S25073.S30403, S31603, S32168, S22053, S25073, 304 316 Hot-rolled and cold-rolled supply, including thinner cold-rolled strip from 0.30 mm. Competitive mill price, cut-to-size service, fast delivery and full MTCs.

GB/T 713.7 022Cr23Ni4MoCuN (S23043) stainless steel plate at SHH STEEL warehouse

GB/T 713.7 022Cr23Ni4MoCuN S23043 Pressure Vessel Stainless Plate

GB/T 713.7 022Cr23Ni4MoCuN (S23043) is a lean duplex stainless steel plate for pressure equipment, equivalent in family to ASTM A240 2304. Under GB/T 713.7-2023 it is delivered solution treated with Rp0.2 ≥400 MPa and Rm ≥ 600 MPa (Table 17). SHH STEEL supplies it in 0.30 – 100 mm, cut to size, with heat and product analysis on EN 10204 3.1 or 3.2 certificates.
View More
GB/T 713.7 022Cr25Ni7Mo4N (S25073) stainless steel plate at SHH STEEL warehouse

GB/T 713.7 022Cr25Ni7Mo4N S25073 Pressure Vessel Stainless Plate

GB/T 713.7 022Cr25Ni7Mo4N (S25073) is a super duplex stainless steel plate for pressure equipment, equivalent in family to ASTM A240 2507. Under GB/T 713.7-2023 it is delivered solution treated with Rp0.2 ≥550 MPa and Rm ≥ 800 MPa (Table 17). SHH STEEL supplies it in 0.30 – 100 mm, cut to size, with heat and product analysis on EN 10204 3.1 or 3.2 certificates.
View More
GB/T 713.7 022Cr22Ni5Mo3N (S22253) stainless steel plate at SHH STEEL warehouse

GB/T 713.7 022Cr22Ni5Mo3N S22253 Pressure Vessel Stainless Plate

GB/T 713.7 022Cr22Ni5Mo3N (S22253) is a duplex stainless steel plate for pressure equipment, equivalent in family to ASTM A240 S31803. Under GB/T 713.7-2023 it is delivered solution treated with Rp0.2 ≥450 MPa and Rm ≥ 620 MPa (Table 17). SHH STEEL supplies it in 0.30 – 100 mm, cut to size, with heat and product analysis on EN 10204 3.1 or 3.2 certificates.
View More
GB/T 713.7 022Cr23Ni5Mo3N (S22053) stainless steel plate at SHH STEEL warehouse

GB/T 713.7 022Cr23Ni5Mo3N S22053 Pressure Vessel Stainless Plate

GB/T 713.7 022Cr23Ni5Mo3N (S22053) is a duplex stainless steel plate for pressure equipment, equivalent in family to ASTM A240 2205. Under GB/T 713.7-2023 it is delivered solution treated with Rp0.2 ≥450 MPa and Rm ≥ 620 MPa (Table 17). SHH STEEL supplies it in 0.30 – 100 mm, cut to size, with heat and product analysis on EN 10204 3.1 or 3.2 certificates.
View More
GB/T 713.7 08Cr21Ni11Si2CeN (S30859) stainless steel plate at SHH STEEL warehouse

GB/T 713.7 08Cr21Ni11Si2CeN S30859 Pressure Vessel Stainless Plate

GB/T 713.7 08Cr21Ni11Si2CeN (S30859) is a heat-resisting austenitic stainless steel plate for pressure equipment, equivalent in family to ASTM A240 S30815. Under GB/T 713.7-2023 it is delivered solution treated with Rp0.2 ≥310 MPa and Rm ≥ 600 MPa (Table 16). SHH STEEL supplies it in 0.30 – 100 mm, cut to size, with heat and product analysis on EN 10204 3.1 or 3.2 certificates.
View More
GB/T 713.7 015Cr21Ni26Mo5Cu2 (S39042) stainless steel plate at SHH STEEL warehouse

GB/T 713.7 015Cr21Ni26Mo5Cu2 S39042 Pressure Vessel Stainless Plate

GB/T 713.7 015Cr21Ni26Mo5Cu2 (S39042) is a super-austenitic stainless steel plate for pressure equipment, equivalent in family to ASTM A240 904L. Under GB/T 713.7-2023 it is delivered solution treated with Rp0.2 ≥220 MPa and Rm ≥ 490 MPa (Table 16). SHH STEEL supplies it in 0.30 – 100 mm, cut to size, with heat and product analysis on EN 10204 3.1 or 3.2 certificates.
View More
GB/T 713.7 015Cr20Ni18Mo6CuN (S31252) stainless steel plate at SHH STEEL warehouse

GB/T 713.7 015Cr20Ni18Mo6CuN S31252 Pressure Vessel Stainless Plate

GB/T 713.7 015Cr20Ni18Mo6CuN (S31252) is a super-austenitic stainless steel plate for pressure equipment, equivalent in family to ASTM A240 S31254. Under GB/T 713.7-2023 it is delivered solution treated with Rp0.2 ≥310 MPa and Rm ≥ 655 MPa (Table 16). SHH STEEL supplies it in 0.30 – 100 mm, cut to size, with heat and product analysis on EN 10204 3.1 or 3.2 certificates.
View More
GB/T 713.7 022Cr19Ni13Mo3 (S31703) stainless steel plate at SHH STEEL warehouse

GB/T 713.7 022Cr19Ni13Mo3 S31703 Pressure Vessel Stainless Plate

GB/T 713.7 022Cr19Ni13Mo3 (S31703) is a 3-4% molybdenum austenitic stainless steel plate for pressure equipment, equivalent in family to ASTM A240 317L. Under GB/T 713.7-2023 it is delivered solution treated with Rp0.2 ≥205 MPa and Rm ≥ 520 MPa (Table 16). SHH STEEL supplies it in 0.30 – 100 mm, cut to size, with heat and product analysis on EN 10204 3.1 or 3.2 certificates.
View More
GB/T 713.7 06Cr19Ni13Mo3 (S31708) stainless steel plate at SHH STEEL warehouse

GB/T 713.7 06Cr19Ni13Mo3 S31708 Pressure Vessel Stainless Plate

GB/T 713.7 06Cr19Ni13Mo3 (S31708) is a 3-4% molybdenum austenitic stainless steel plate for pressure equipment, equivalent in family to ASTM A240 317. Under GB/T 713.7-2023 it is delivered solution treated with Rp0.2 ≥205 MPa and Rm ≥ 520 MPa (Table 16). SHH STEEL supplies it in 0.30 – 100 mm, cut to size, with heat and product analysis on EN 10204 3.1 or 3.2 certificates.
View More
GB/T 713.7 06Cr25Ni20 (S31008) stainless steel plate at SHH STEEL warehouse

GB/T 713.7 06Cr25Ni20 S31008 Pressure Vessel Stainless Plate

GB/T 713.7 06Cr25Ni20 (S31008) is a heat-resisting austenitic stainless steel plate for pressure equipment, equivalent in family to ASTM A240 310S. Under GB/T 713.7-2023 it is delivered solution treated with Rp0.2 ≥205 MPa and Rm ≥ 520 MPa (Table 16). SHH STEEL supplies it in 0.30 – 100 mm, cut to size, with heat and product analysis on EN 10204 3.1 or 3.2 certificates.
View More
GB/T 713.7 06Cr23Ni13 (S30908) stainless steel plate at SHH STEEL warehouse

GB/T 713.7 06Cr23Ni13 S30908 Pressure Vessel Stainless Plate

GB/T 713.7 06Cr23Ni13 (S30908) is a heat-resisting austenitic stainless steel plate for pressure equipment, equivalent in family to ASTM A240 309S. Under GB/T 713.7-2023 it is delivered solution treated with Rp0.2 ≥205 MPa and Rm ≥ 515 MPa (Table 16). SHH STEEL supplies it in 0.30 – 100 mm, cut to size, with heat and product analysis on EN 10204 3.1 or 3.2 certificates.
View More
GB/T 713.7 07Cr18Ni11Nb (S34779) stainless steel plate at SHH STEEL warehouse

GB/T 713.7 07Cr18Ni11Nb S34779 Pressure Vessel Stainless Plate

GB/T 713.7 07Cr18Ni11Nb (S34779) is a controlled-carbon stabilized austenitic stainless steel plate for pressure equipment, equivalent in family to ASTM A240 347H. Under GB/T 713.7-2023 it is delivered solution treated with Rp0.2 ≥205 MPa and Rm ≥ 515 MPa (Table 16). SHH STEEL supplies it in 0.30 – 100 mm, cut to size, with heat and product analysis on EN 10204 3.1 or 3.2 certificates.
View More

GB/T 713.7-2023 Stainless Steel Products

GB/T 713.7 022Cr27Ni2Mo4NbTi S12763 Pressure Vessel Stainless Plate GB/T 713.7 019Cr23MoTi S12362 Pressure Vessel Stainless Plate GB/T 713.7 019Cr23Mo2Ti S12361 Pressure Vessel Stainless Plate GB/T 713.7 019Cr19Mo2NbTi S11972 Pressure Vessel Stainless Plate
GB/T 713.7 06Cr13 S11306 Pressure Vessel Stainless Plate GB/T 713.7 06Cr13Al S11348 Pressure Vessel Stainless Plate GB/T 713.7 022Cr21Ni3Mo2N S22153 Pressure Vessel Stainless Plate GB/T 713.7 03Cr22Mn5Ni2MoCuN S22294 Pressure Vessel Stainless Plate
GB/T 713.7 022Cr19Ni5Mo3Si2N S21953 Pressure Vessel Stainless Plate GB/T 713.7 03Cr25Ni6Mo3Cu2N S25554 Pressure Vessel Stainless Plate GB/T 713.7 022Cr25Ni7Mo4WCuN S27603 Pressure Vessel Stainless Plate GB/T 713.7 022Cr25Ni6Mo2N S22553 Pressure Vessel Stainless Plate
GB/T 713.7 022Cr23Ni4MoCuN S23043 Pressure Vessel Stainless Plate GB/T 713.7 022Cr25Ni7Mo4N S25073 Pressure Vessel Stainless Plate GB/T 713.7 022Cr22Ni5Mo3N S22253 Pressure Vessel Stainless Plate GB/T 713.7 022Cr23Ni5Mo3N S22053 Pressure Vessel Stainless Plate
GB/T 713.7 08Cr21Ni11Si2CeN S30859 Pressure Vessel Stainless Plate GB/T 713.7 015Cr21Ni26Mo5Cu2 S39042 Pressure Vessel Stainless Plate GB/T 713.7 015Cr20Ni18Mo6CuN S31252 Pressure Vessel Stainless Plate GB/T 713.7 022Cr19Ni13Mo3 S31703 Pressure Vessel Stainless Plate
GB/T 713.7 06Cr19Ni13Mo3 S31708 Pressure Vessel Stainless Plate GB/T 713.7 06Cr25Ni20 S31008 Pressure Vessel Stainless Plate GB/T 713.7 06Cr23Ni13 S30908 Pressure Vessel Stainless Plate GB/T 713.7 07Cr18Ni11Nb S34779 Pressure Vessel Stainless Plate
GB/T 713.7 06Cr18Ni11Nb S34778 Pressure Vessel Stainless Plate GB/T 713.7 07Cr19Ni11Ti S32169 Pressure Vessel Stainless Plate GB/T 713.7 06Cr18Ni11Ti S32168 Pressure Vessel Stainless Plate GB/T 713.7 022Cr17Ni12Mo2N S31653 Pressure Vessel Stainless Plate
GB/T 713.7 06Cr17Ni12Mo2N S31658 Pressure Vessel Stainless Plate GB/T 713.7 06Cr17Ni12Mo2Ti S31668 Pressure Vessel Stainless Plate GB/T 713.7 07Cr17Ni12Mo2 S31609 Pressure Vessel Stainless Plate GB/T 713.7 022Cr17Ni12Mo2 S31603 Pressure Vessel Stainless Plate
GB/T 713.7 06Cr17Ni12Mo2 S31608 Pressure Vessel Stainless Plate GB/T 713.7 05Cr19Ni10Si2CeN S30450 Pressure Vessel Stainless Plate GB/T 713.7 06Cr19Ni9NbN S30478 Pressure Vessel Stainless Plate GB/T 713.7 022Cr19Ni10N S30453 Pressure Vessel Stainless Plate
GB/T 713.7 06Cr19Ni10N S30458 Pressure Vessel Stainless Plate GB/T 713.7 07Cr19Ni10 S30409 Pressure Vessel Stainless Plate GB/T 713.7 022Cr19Ni10 S30403 Pressure Vessel Stainless Plate GB/T 713.7 06Cr19Ni10 S30408 Pressure Vessel Stainless Plate
Stainless Steel Sheets and Plates

Stainless Steel Sheets and Plates

SHH STEEL, a leading Stainless Steel Sheets and Plates exporter, produces and exports stainless steel sheets (0.3–6 mm) and plates (>6 mm) for marine, chemical, and structural applications. Our products, like 304 and 316L (ASTM A240), offer corrosion resistance and durability. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Trust SHH STEEL for 316L stainless steel plates and custom solutions for your projects.

Stainless Steel Sheets and Plates

SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

    *

    *

    *

    *


    X