Q390E steel plate GB/T 1591 high-strength low-alloy plate stock at SHH STEEL supplier yard

Q390E Steel Plate GB/T 1591 Supplier

Q390E is the −40°C impact quality of GB/T 1591 Q390 high-strength low-alloy plate: 390 MPa minimum yield (≤16 mm), 490 – 650 MPa tensile and KV2 ≥ 34 J at −40°C. SHH STEEL supplies Q390E for cold-climate structures, and can deliver it as Q390NE or Q390ME under GB/T 1591-2018 when the drawing calls for the current edition.
Keywords
Q390E, Q390E steel plate, GB/T 1591 Q390E, Q390E plate, Q390 E, Q390E equivalent, Q390E -40 impact, Q390NE, Q390ME, Q390E supplier
Equivalent Grades:
ASTM A572 Gr.55 / EN 10025-4 S420ML (closest)
Share:
Overview
Buyer Question
Specification
Chemical Composition
Product Analysis
Mechanical Properties
Equivalent Grades
Grade Comparison
Carbon Equivalent
Applications
Testing & Certificates
Sizes & Stock
Processing
Ordering
Why SHH STEEL
FAQ
Conclusion

What does Q390E mean today?

Q390E is the −40°C quality letter of the Q390 family. It was a standard grade in GB/T 1591-2008. In GB/T 1591-2018 the E letter for Q390 is no longer offered in the hot-rolled condition: it is published as Q390NE (normalized / normalized rolled) and Q390ME (thermomechanical rolled). Many tenders, steel lists and older design codes still write “Q390E”, so the name is very much alive in the market.

When you order Q390E from SHH STEEL we confirm which edition your project needs. For new projects we normally recommend certifying to the 2018 edition as Q390NE or Q390ME with the −40°C test, so the certificate matches the current standard.

SHH STEEL is a producer and exporter of structural plate and a sales agent for well-known Chinese mills. We keep Q390E plate in our own processing warehouse in Shanghai for cutting, drilling, shot blasting and priming. Q390E belongs to our GB/T 1591 plate range; see also our high-strength low-alloy plates overview.

Q390E in GB/T 1591-2018: why the grade disappeared from hot-rolled

The 2018 revision tied the toughest quality letters to controlled delivery conditions: hot-rolled Q390 stops at D, and −40°C Q390 is produced as N or M. Mills still roll to “Q390E” for buyers who quote GB/T 1591-2008 – say which you need.

Q390E specification at a glance

Item Q390E requirement
Standard GB/T 1591-2008 (Q390E) – current edition replaces it with Q390NE / Q390ME
Steel type High-strength low-alloy structural steel, killed
Minimum yield ReH (≤16 mm) 390 MPa
Tensile strength Rm (≤100 mm) 490 – 650 MPa
Impact test KV2 ≥ 34 J at −40°C, longitudinal
Thickness range (SHH STEEL) 6 – 150 mm
Width / length 1 500 – 4 020 mm / 6 000 – 18 000 mm
Dimensions & tolerance GB/T 709 (EN 10029 / ASTM A6 on request)
Certificate EN 10204 3.1 (3.2 with third-party inspection)

Q390E chemical composition (heat analysis)

Element Q390E heat analysis, % max Role
C ≤ 0.20 strength and hardenability; kept ≤0.20 for weldability
Si ≤ 0.50 deoxidiser, adds some strength
Mn ≤ 1.70 main strengthening element; with C sets the CEV
P ≤ 0.025 impurity; lower in the tougher quality letters
S ≤ 0.020 impurity; forms MnS that hurts through-thickness and impact values
Nb ≤ 0.07 grain refiner, precipitation strengthening
V ≤ 0.20 precipitation strengthening, helps thick plate keep yield
Ti ≤ 0.20 fixes N, refines grain in the HAZ
Cr ≤ 0.30 residual / minor alloy
Ni ≤ 0.50 residual; helps low-temperature toughness
Cu ≤ 0.30 residual; limited for hot shortness
Mo ≤ 0.10 residual / minor alloy
N ≤ 0.015 kept low; free N harms toughness
Als ≥ 0.015 fine-grain practice, required for D/E

Values below are the GB/T 1591-2008 Q390E heat analysis; Q390NE / Q390ME under the 2018 edition have their own tables (P ≤ 0.025, S ≤ 0.020 for NE). Nb, V and Ti may be used alone or in combination; for Q390/Q420 the sum Nb+V+Ti is limited to 0.22%. Where Cu is used as a residual element the mill must report it. Values are for the ladle (heat) analysis printed on the certificate.

Product (finished plate) analysis and check tolerances for Q390E

A check analysis drilled from the finished plate may differ slightly from the ladle analysis. GB/T 1591 refers to GB/T 222 for the permitted deviations. The table applies them to the Q390E limits. The deviation applies to one side of a limit only.

Element Heat analysis limit, % Permitted deviation Product analysis limit, %
C ≤ 0.20 +0.02 ≤ 0.22
Si ≤ 0.50 +0.03 ≤ 0.53
Mn ≤ 1.70 +0.1 ≤ 1.80
P ≤ 0.025 +0.005 ≤ 0.030
S ≤ 0.020 +0.005 ≤ 0.025
Nb ≤ 0.07 +0.01 ≤ 0.08
V ≤ 0.20 +0.02 ≤ 0.22
Ti ≤ 0.20 +0.01 ≤ 0.21
Cr ≤ 0.30 +0.05 ≤ 0.35
Ni ≤ 0.50 +0.05 ≤ 0.55
Cu ≤ 0.30 +0.05 ≤ 0.35
Mo ≤ 0.10 +0.01 ≤ 0.11
N ≤ 0.015 +0.002 ≤ 0.017
Als ≥ 0.015 −0.005 ≥ 0.010

If your inspector tests a plate in a third-party lab, compare the result with the right-hand column, not with the heat analysis.

Q390E mechanical properties by thickness

Thickness, mm Yield ReH, MPa min Tensile Rm, MPa Elongation A, % min (long. / trans.)
≤ 16 390 490 – 650 21 / 20
> 16 – 40 380 490 – 650 21 / 20
> 40 – 63 360 490 – 650 20 / 19
> 63 – 100 340 490 – 650 20 / 19
> 100 – 150 320 470 – 620 19 / 18
Quality Test temperature KV2 longitudinal, J min KV2 transverse, J min
E −40°C 34 27

Yield drops with thickness because thick plate cools slower and gets less rolling reduction. Design with the value for your actual thickness, not the headline 390 MPa. Impact tests use 10×10 mm specimens for plate ≥ 12 mm; thinner plate uses sub-size specimens with reduced values. Tensile tests on plate are transverse by default.

Q390E equivalent grades: EN, ASTM, JIS

System Grade Comment
ASTM ASTM A572 Gr.55 Requires S5 Charpy at −40°C
EN 10025-4 EN 10025-4 S420ML (closest) −50°C 27 J, 420 MPa
EN 10025-3 EN 10025-3 S355NL Lower-strength −50°C reference
GB/T 1591-2018 Q390NE / Q390ME Current names for −40°C Q390

“Equivalent” means similar, not identical. Strength classes, impact temperatures and delivery conditions differ between standards. A plate can be dual-certified only if one heat meets both books in full; ask us before you assume it.

Q390E vs Q355E vs Q420E

Grade Yield ≤16 mm, MPa Tensile ≤100 mm, MPa Impact
Q355E 355 470 – 630 −40°C
Q390E 390 490 – 650 −40°C
Q420E 420 520 – 680 −40°C

Q390E vs Q355E: both at −40°C, but 390 vs 355 MPa yield. Q390E vs Q420E: Q420E adds 30 MPa. Q390E vs Q390ND: drop to −20°C if your lowest service temperature allows – it saves cost and lead time.

Q390E carbon equivalent (CEV) and weldability

Thickness, mm ≤ 30 > 30 – 63 > 63 – 150 > 150 – 250
CEV max, % (heat analysis) 0.45 0.47 0.48 —

CEV = C + Mn/6 + (Cr+Mo+V)/5 + (Ni+Cu)/15. Real heats from our mills usually come in around 0.40 – 0.44 on 20 – 40 mm plate. Q390 plate welds with standard E50/E55-class consumables (AWS E7018 / E8018 type, ER50-6 / ER55 wire). Preheat of 50 – 100°C is common above 25 mm or in restrained joints; low-hydrogen practice is the key point.

Where Q390E earns its price

Q390E plate is used for arctic and high-altitude structures, LNG plant secondary steel, low-temperature machinery, polar vessels’ non-class structure, power transmission towers in northern regions.

For building columns with through-thickness loads, compare with Q390GJC building plate to GB/T 19879, which adds Z-direction and yield-ratio control.

How Q390E is tested and certified

Each lot carries tensile, Charpy at −40°C and chemistry results. Batches are by heat, thickness and delivery condition, up to 60 t. Optional: Z15/Z25/Z35 through-thickness to GB/T 5313, UT, product analysis, SGS/BV/TÜV witness for EN 10204 3.2.

Q390E plate sizes we supply

Form Thickness, mm Width, mm Length, mm
Mill plate 6 – 150 1 500 – 4 020 6 000 – 18 000
Shanghai stock (common) 8, 10, 12, 14, 16, 20, 25, 30, 40, 50 2 000 / 2 200 / 2 500 8 000 – 12 000
Cut pieces 6 – 150 to drawing to drawing

Mill orders usually take 30 – 45 days from rolling schedule. Stock sizes can ship within a week after cutting.

Cutting and processing Q390E in our Shanghai warehouse

  • Flame, plasma and CNC laser cutting to drawings; bevelling for welding
  • Drilling, bending and rolling of shells
  • Shot blasting Sa 2.5 and shop primer or full paint system
  • Ultrasonic testing to GB/T 2970, EN 10160 or ASTM A578

Processed plates keep heat numbers traceable to the mill certificate.

How to order Q390E correctly

State: standard and edition (GB/T 1591-2008 Q390E or GB/T 1591-2018 Q390NE/Q390ME), thickness × width × length, quantity, tolerance standard, any UT or Z-grade, certificate type and marking. Writing the edition avoids the most common certificate dispute we see.

Why buy Q390E from SHH STEEL

SHH STEEL works as an agent for well-known Chinese mills, so we can book rolling slots for non-stock sizes and still offer warehouse stock for urgent orders. Our team checks every certificate against GB/T 1591 before shipment. We export to Southeast Asia, the Middle East, Africa, Europe and South America, packed for sea freight with sea-worthy marking.

FAQ

Is Q390E still in GB/T 1591-2018?
Not as a hot-rolled grade. The 2018 edition uses Q390NE and Q390ME for −40°C; Q390E remains a GB/T 1591-2008 grade.
What is Q390E equivalent to?
EN 10025-4 S420ML is the closest European match; ASTM A572 Gr.55 with S5 Charpy at −40°F is a US comparison.
What impact energy does Q390E need?
KV2 ≥ 34 J at −40°C, longitudinal.
Q390E vs Q390D: what is the difference?
Same strength; E is tested at −40°C instead of −20°C and has tighter P and S.
What is the yield strength of Q390E?
390 MPa minimum up to 16 mm, decreasing with thickness.
Can SHH STEEL certify Q390E as Q390NE?
Yes, when the heat and delivery condition meet the 2018 Q390NE table; we confirm before rolling.

Conclusion

Q390E is a legacy −40°C 390 MPa HSLA plate grade of GB/T 1591 with 490 – 650 MPa tensile and −40°C Charpy impact. Check the thickness-dependent yield, the CEV and the product analysis tolerances when you write your purchase order.

SHH STEEL supplies Q390E mill-direct and from our Shanghai processing warehouse, with EN 10204 3.1 certificates. Related pages: Q355E, Q420E, Q390NE, EN 10025-4 S420ML and our GB/T 1591 plate range. Send us your sizes for a quotation.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X