NM600 Wear-Resistant Steel Plate | GB/T 24186 Wear-Resistant Steel - SHH STEEL

NM600 Wear-Resistant Steel Plate

NM600 wear-resistant steel plate is the hardest grade in GB/T 24186, 570–640 HBW and up to 60 mm thick, for extreme abrasion with little impact. SHH STEEL can produce and supply NM600, NM600D and NM600E plate from China.
Keywords
nm600 steel plate, nm600 wear-resistant steel plate, nm600 hardness, nm600 equivalent, nm600 vs ar600, GB/T 24186 NM600, nm600d, nm600e
Equivalent Grades:
AR600 (commercial hardness class); SSAB Hardox (brand standard) Hardox 600; related GB/T 24186 grade NM550 (not identical)
Standard
GB/T 24186-2022, usually quenched and tempered (Q+T)
Grade
NM600 / NM600D (−20 °C) / NM600E (−40 °C)
Share:
Overview
Designation
Chemical Composition
Hardness and Mechanical Properties
Dimensions and Tolerances
Delivery Condition
Equivalent Grades
Applications
Fabrication
Surface Finishes
Inspection and Testing
Stock
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is NM600 Wear-Resistant Steel Plate (GB/T 24186)

Technical Reviewer: Jack | SHH STEEL Material Solutions Department · Updated: 2026-11-02

NM600 wear-resistant steel plate is the hardest grade in GB/T 24186 and should be treated as a wear tool rather than a construction steel. NM is the Pinyin initials of Nai Mo, meaning wear-resistant; 600 is the nominal Brinell class. GB/T 24186-2022 sets its surface hardness at 570–640 HBW and limits the thickness to 60 mm — the narrowest range in the standard, because through-hardening thicker plate to this level is not practical.

SHH STEEL can produce and supply NM600 wear-resistant steel plate to GB/T 24186, quenched on Chinese mill lines and hardness-tested per batch, with NM600D and NM600E when an agreed low-temperature impact test is required. Most NM600 we ship is cut into tiles and strips in our workshop by water-jet or controlled thermal cutting.

Use NM600 where abrasion is relentless and impact is nearly absent: fine ore and sand slurries, sliding coke, cement raw meal, glass cullet. It is almost always mounted on a tougher backing plate.

The next grade down, with a little more toughness, is NM550 Wear-Resistant Steel Plate. Family hub: GB/T 24186; category: Wear-Resistant Steel Plates.

Material Specification and Designation: NM, NM600D and NM600E

NM600 is the base grade; NM600D and NM600E are tested at −20 °C and −40 °C. As for NM550, Table 5 note a leaves the impact energy to agreement, so a D or E order must state the joules required.

Order wording: GB/T 24186-2022, NM600 (or NM600D / NM600E with agreed KV2), quenched, sizes, quantity, certificate. Tensile values for NM600 are also by agreement under Table 6 note a.

Because 600 HBW plate is brittle compared with the lower grades, the D/E letters guarantee only test behaviour at temperature — they do not make NM600 an impact-resistant plate.

Chemical Composition of NM600 Wear-Resistant Steel Plate

NM600 ladle chemistry per Table 2 and Table 3 is shown below.

Element (mass %) NM600 (Table 2, ladle) NM600D/E (Table 3, ladle)
C ≤ 0.45 ≤ 0.45
Si ≤ 0.70 ≤ 0.7
Mn ≤ 1.90 ≤ 1.9
P ≤ 0.020 ≤ 0.015
S ≤ 0.010 ≤ 0.005
Cr ≤ 1.60 ≤ 1.60
Ni ≤ 2.00 ≤ 2.0
Mo ≤ 0.80 ≤ 0.80
Ti ≤ 0.050 ≤ 0.05
B 0.0005–0.0060 0.0005–0.0060
Als ≥ 0.010 ≥ 0.015
CEV (≤ 50 mm / > 50 mm) not capped in Table 2 ≤ 0.84 / ≤ 0.94

This is the richest grade: carbon up to 0.45 %, Mn 1.90 %, Cr 1.60 %, Ni 2.00 % and Mo 0.80 %. The carbon level alone explains the 570+ HBW hardness. NM600D/E holds the same carbon, tightens P to 0.015 % and S to 0.005 %, and its CEV caps of 0.84 % up to 50 mm and 0.94 % above are by far the highest in the standard.

Additional alloying elements must be declared (7.1.2), with Cu ≤ 0.30 % and As ≤ 0.08 % residuals (7.1.3). At these CEV levels, conventional structural welding is not realistic.

Hardness and Mechanical Properties of NM600 Steel Plate

Table 4 gives a single band for NM600 and NM600D/E up to 60 mm. Hardness is tested after removing the decarburized layer.

Grade Thickness (mm) Surface hardness (HBW) Centre hardness (HBW)
NM600 / NM600D/E ≤ 60 570–640 510–640

Impact and tensile are both by agreement for this grade, as summarised below.

Property GB/T 24186-2022 value Status
Charpy KV2, NM600D (−20 °C) / NM600E (−40 °C) energy by agreement (Table 5 note a) Temperature fixed by D/E; value agreed in contract
Transverse tensile Rm / A50mm by agreement Table 6 note a — no default values for NM600

Bend testing does not apply to NM600 (Table 7 note a). Practically, the plate should not be formed at all. Impact, where agreed, follows the mean-of-three rule with one value down to 70 %.

Thickness, Dimensions and Tolerances for NM600 Plate

Table 1 limits NM600 and NM600D/E to 60 mm. GB/T 709-2019 governs dimensions and tolerances, with Class H flatness default and Class L by agreement.

NM600 demand is concentrated in 6–30 mm, cut into tiles, strips and segments. Accurate flatness helps tiles seat on the backing structure without rocking.

Delivery Condition and Heat Treatment of NM600 Wear Plate

Clause 7.3 lists the permitted conditions; NM600 is supplied quenched, sometimes with a very low temper. Residual stress is high, so plates should be lifted and stored carefully and never dropped.

Hot-rolled-before-heat-treatment plate is not mechanically tested (7.4.6). Batches: one grade, heat, thickness, delivery condition and heat-treatment cycle, up to 60 t.

Equivalent Grades: NM600 vs AR600 vs Hardox 600 (SSAB Hardox)

NM600 is compared with AR600 and Hardox 600 under the SSAB Hardox brand standard. They are similar 570–640 HBW hardness-class products, not drop-in identical; each follows a different document.

Designation / family Typical hardness class Notes for enquiry
GB/T 24186 NM600 / NM600D / NM600E 570–640 HBW (≤ 60 mm surface) Governing standard; impact energy by agreement
Commercial AR600 ~600 HBW class Commercial name; maker data governs
SSAB Hardox brand standard — Hardox 600 ~570–640 HBW class (brand data) Brand plate under SSAB Hardox; similar hardness class, not drop-in identical
GB/T 24186 NM550 520–580 HBW Slightly tougher grade in the same standard

Agree substitutions before production, and write the GB/T 24186 grade and any agreed impact on the order. Peer ranges are orientation only. Related grade: NM550 Wear-Resistant Steel Plate; AR-side category: AR400/AR500.

Wear Performance and Applications of NM600 Plate

NM600 serves extreme low-impact abrasion: slurry pipe and pump liners, sand and mineral classifier liners, cement raw-meal and clinker cooler chute tiles, glass-cullet handling, and wear segments on screw conveyors and mixer paddles.

If impact is present, NM600 will chip or crack. Many plants combine NM600 tiles in the sliding zone with NM450 or NM500 in the impact zone.

Cutting, Joining and Handling of ~600 HBW Plate

Welding NM600 into structure is generally avoided. Tiles are usually bolted, plug-welded with austenitic consumables under a qualified procedure, or bonded. Where welding is unavoidable, preheat, dry low-hydrogen practice and slow cooling are essential.

Abrasive water-jet is the preferred cutting method; thermal cutting needs preheat and slow cooling to avoid edge cracks. Drilling is impractical; holes are cut by water-jet or thermally. Forming is not possible.

Surface Finishes and Surface Condition for NM600 Plate

Clause 7.5: no cracks, blisters, scabs, laps, inclusions or visible lamination; dressing within half the thickness tolerance; no welding repair; light scale acceptable; GB/T 14977 by agreement.

NM600 is supplied with mill surface in nearly all cases.

Finish / condition Typical supply Order note
As quenched mill surface Standard supply Adequate for tiles
Water-jet cut tiles SHH STEEL workshop No heat-affected edge
Thermally cut blanks with preheat Larger pieces Slow cooling required
GB/T 14977 surface class By agreement (7.5.4) Write the class on the order

Hardness checks need a ground spot below the decarburized layer.

Inspection and Testing for NM600 Wear-Resistant Steel Plate

Table 8: chemistry per heat, hardness per batch, Charpy against agreed energy for NM600D/E, NDT by agreement; tensile only if agreed; no bend test.

SHH STEEL issues EN 10204 3.1 certificates and arranges 3.2 witness on request. On receipt, check hardness, plate edges for cracks and any agreed impact values.

Stock and Sizes of NM600 Plate SHH STEEL Can Supply

NM600 is a specialist grade with limited stock. SHH STEEL keeps small tonnages of liner thicknesses and produces most orders to mill schedule. Quantities are approximate.

Thickness (mm) Width (mm) Length (mm) Condition Approx. quantity Location
6–10 1500 / 2000 6000 Q 50+ t China
12–20 2000 6000 Q 50+ t China
25–40 2000 6000 Q mill schedule China
> 40–60 (incl. NM600D/E) 2000 6000 Q mill schedule China

Water-jet cut tiles to drawing are our most common NM600 supply.

Why Choose SHH STEEL for NM600 Wear-Resistant Steel Plate

SHH STEEL produces and supplies NM600 with batch hardness testing and precise water-jet cutting, and we review the wear duty before quoting so the hardest grade is used only where it works.

EN 10204 3.1 / 3.2 certificates and third-party inspection are available.

Supply Capability

SHH STEEL can produce and supply NM600 / NM600D / NM600E up to 60 mm thick per Table 1, quenched, with GB/T 709 dimensions and tile cutting. Compare NM550 Wear-Resistant Steel Plate or see the GB/T 24186 hub.

FAQ

What is NM600 steel plate?
NM600 is the hardest GB/T 24186 wear-resistant plate, nominal 600 HBW, up to 60 mm thick, for extreme low-impact abrasion.
What is the hardness of NM600?
570–640 HBW surface up to 60 mm, with centre hardness 510–640 HBW by agreement; the same band covers NM600D/E.
What is the chemical composition of NM600?
Table 2 maxima: C 0.45, Si 0.70, Mn 1.90, P 0.020, S 0.010, Cr 1.60, Ni 2.00, Mo 0.80, Ti 0.050 %, B 0.0005–0.0060 %, Als ≥ 0.010 %. NM600D/E: P 0.015, S 0.005, CEV ≤ 0.84 / 0.94 %.
What are the equivalent grades of NM600?
AR600 and Hardox 600 under the SSAB Hardox brand standard are similar hardness-class products, not drop-in identical.
Can NM600 be welded?
Not as a structural steel. Tiles are bolted, plug-welded with austenitic filler under a qualified procedure, or bonded.
Where can I get an NM600 data sheet?
This page summarises GB/T 24186-2022; the mill certificate shows heat chemistry, hardness and any agreed tests.
What is the difference between NM600, NM600D and NM600E?
D and E add Charpy tests at −20 °C and −40 °C with contract-agreed energy and follow Table 3 chemistry.
Why is NM600 limited to 60 mm?
Table 1 limits it to 60 mm because thicker plate cannot be reliably hardened through to 570–640 HBW.
Is tensile testing required for NM600?
No default values exist; tensile properties are by agreement under Table 6 note a.
How is NM600 cut?
Abrasive water-jet is preferred; thermal cutting requires preheat and slow cooling. SHH STEEL supplies cut tiles to drawing.

Conclusion

NM600 is the hardest GB/T 24186 grade: 570–640 HBW, up to 60 mm, with impact and tensile by agreement. It is a liner tile material for pure abrasion and must be cut and fixed with care.

SHH STEEL can produce and supply NM600 / NM600D / NM600E from China, cut to tiles. Email admin@steelspecs.com with drawings and port.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response