JIS G 3101 SS540 Equal and Unequal Steel Angles
What is JIS G 3101 SS540 Steel Angle?
JIS G 3101 SS540 steel angle is a hot-rolled equal-leg or unequal-leg section in general structural steel SS540. The material standard is JIS G 3101, Rolled steels for general structure. The chemical and mechanical figures on this page are those of the issued JIS G 3101:2015 tables. JIS G 3101:2024 is the current listed edition, issued 20 February 2024; the edition named on the order governs acceptance. Dimensions, mass and tolerances for these angles are those of JIS G 3192:2024. SHH STEEL supplies these angles to the grade, designation, edition and certificate named on the order.
The number in the grade name is the specified tensile strength in N/mm² (1 N/mm² = 1 MPa), not a yield class. Formal grades in the standard are SS330, SS400, SS490 and SS540. This page is SS540. It is not the JIS G 3101 SS400 steel angle page, not a JIS G 3106 SM490 steel angle, and not a data sheet for SS540 steel plate.
These angles are filed under JIS G3101 in the steel angle profiles category of steel structural profiles. The same grade in plate form is listed separately; do not use the plate page as an angle data sheet.
This page covers Equal and Unequal Steel Angles in JIS G 3101 SS540. The Equal Leg Steel Angles (JIS G 3192 Table 8) and Unequal Leg Steel Angles (Tables 9 and 10) follow JIS G 3192; the material standard does not by itself define the dimensions.
Material, Dimensions and Tolerances for SS540 Angles
Keep the material specification and the dimensional standard distinct. JIS G 3101 is the material standard. The ladle-analysis and mechanical figures used here are those of the issued JIS G 3101:2015 tables (Table 2 and Table 3). JIS G 3101:2024 is the current listed edition; the edition named on the order governs acceptance. JIS G 3192:2024 is the shape standard for these angles. A documented special combination is valid only if every requirement of each named standard is met. Matching a nominal 100 mm or 4 in leg is not a substitution method.
JIS G 3101 does not require a fully killed practice and does not require the product to be normalized. If a heat treatment has been applied, the standard gives sampling rules for that heat-treated lot; it does not turn normalizing into the delivery condition of the grade.
JIS G 3101 SS540 Equal Leg Steel Angles
The tables list the complete tabulated standard angle series in JIS G 3192:2024: Table 8 equal-leg angles, 40 sizes from 25×25×3 to 250×250×35; Table 9 unequal-leg angles, 13 sizes from 90×75×9 to 150×100×15; and Table 10 unequal-leg unequal-thickness angles, 7 sizes from 200×90×9×14 to 400×100×13×18. Each table carries footnote a: the listed sizes are representative, and sizes other than those listed are agreed between the purchaser and the supplier. Use the tables to identify and estimate, not as a rolling programme for SS540. Mid-range equal legs such as 75×75 and 100×100 are the usual enquiry core; the 25×25 and 30×30 families, the 250×250 rows, and the Table 10 series should be confirmed size by size.
Table 10 is a separate series and is not a subset of Table 9. Root and toe radii r1 and r2 are tabulated standard dimensions in these JIS series and are shown. Theoretical mass uses a density of 7.85 g/cm³. This page does not invent rows that Tables 8, 9 and 10 do not list. Table 1 of the issued JIS G 3101:2015 text limits SS540 sections to 40 mm thickness or less (t or t2 in JIS G 3192). Every tabulated row on this page has a leg thickness of 35 mm or less, and Table 10 t2 is 18 mm or less, so the listed series sits inside that cap. A special thicker leg is outside this grade.
75×75×9 has a 9 mm leg, so the 400 N/mm² yield band applies. 150×150×15 remains in that first band. 150×150×19 and 200×200×20 have 19 mm and 20 mm legs, so the minimum yield is 390 N/mm², not 400 N/mm². On Table 10 the usual thickness basis is the thicker leg t2. Annex JA of JIS G 3101 applies to sections whose leg length is under 40 mm: in Table 8, that is the 25×25 and 30×30 families, which shall be reviewed against Annex JA in the edition named on the order. The numeric Annex JA values are not restated here, and this page does not extend Annex JA to legs of 40 mm or larger.
Equal-leg angles — Table 8, 40 sizes
Swipe horizontally to view all dimensions.
JIS G 3101 SS540 Unequal Leg Steel Angles
Table 9 and Table 10 continue the same JIS G 3192:2024 series for SS540. An unequal angle such as 100×75×10 is not a 100×100 equal angle, and it is not an ASTM L-shape of a similar inch size. Table 1 of the issued JIS G 3101:2015 text limits SS540 sections to 40 mm thickness or less (t or t2 in JIS G 3192). Every tabulated row on this page has a leg thickness of 35 mm or less, and Table 10 t2 is 18 mm or less, so the listed series sits inside that cap. A special thicker leg is outside this grade.
Unequal-leg angles — Table 9, 13 sizes
Swipe horizontally to view all dimensions.
Unequal-thickness angles — Table 10, 7 sizes
Swipe horizontally to view all dimensions.
SS540 Chemical Composition for Angles (Table 2)
The ladle analysis shall comply with Table 2 of JIS G 3101, using the issued 2015 figures given below. JIS G 3101:2024 is the current listed edition; the edition named on the order governs. Unlike SS400 and SS490, the SS540 row specifies carbon and manganese as well as phosphorus and sulfur.
These are maxima, not typical heat results, and they are not an invitation to describe the grade as “containing 0.30% carbon and 1.60% manganese.” Alloying elements not listed in Table 2 may be added as necessary. Table 2 is a ladle-analysis table. The issued 2015 text recovered for this page specifies ladle analysis only and does not give a separate numeric product-analysis table. This page does not invent one.
SS540 Angle Mechanical Properties: Yield, Tensile and Elongation
Mechanical properties of SS540 plates, strip, flats and sections follow Table 3 of the issued JIS G 3101:2015 text, and they stop at 40 mm, in line with Table 1. These angles use the plate, strip, flat and section rows of that table, not the bar rows. The recovered 2015 Table 3 notes do not add an upper-yield or 0.2% proof-stress instruction, and this page does not add one. Thickness for a section is the thickness at the test-piece location; on these pages the usual basis for selecting a yield band is the leg thickness t, or the thicker leg t2 on Table 10.
There is no Table 3 yield or elongation band above 40 mm for SS540, and this page does not invent one. JIS G 3101 does not specify Charpy absorbed-energy values. The bend test may be omitted unless the purchaser specifies it; the steel still has to satisfy the bendability requirement, and the outside of the bend piece must be free of cracks.
Delivery, Inspection and Identification of SS540 Angles
SS540 angles are commonly supplied as-rolled. If not otherwise specified at the time of order, the default inspection document is a JIS G 0415 inspection certificate 3.1. The document should identify JIS G 3101 and its edition, the grade SS540, the G 3192 designation, the heat number, the ladle analysis and the tensile results. An EN 10204 type 3.1 request is usually satisfied by that 3.1 document; type 3.2 or nominated third-party attendance can be added when the order requires it. Length is a matter for the rolling programme and the order, often in the region of 6–12 m; those lengths are enquiry ranges, not a stock list. A SS540 plate certificate does not identify an angle.
Weldability and Surface Condition of SS540 Angles
SS540 is a general structural steel intended to be welded, bolted or otherwise fabricated when the procedure is suitable for the thickness and the joint. JIS G 3101 does not table a carbon-equivalent limit or a Charpy value for this grade. This page does not prescribe a welding procedure or a preheat chart. The as-rolled surface is mill scale. Blast, paint or galvanizing is an order option. Cutting, punching, forming or coating can be reviewed when that specification is sent with the enquiry.
JIS G 3192 Shape Tolerances and Theoretical Mass
Dimensional and mass tolerances for these angles are those of JIS G 3192, not of JIS G 3101 itself. This article does not reproduce the millimetre tolerance tables; acceptance is against the edition of G 3192 named on the order. Root and toe radii in the tables are tabulated standard dimensions in this series. Settlement on theoretical or weighed mass should follow the contract.
Applications and Service Limits
SS540 steel angles are used where a general structural L-section in this tensile class is specified: frames, bracing, towers, shops and fabrications that name JIS G 3101 SS540 rather than SS400, SS540 or a welded-structure grade such as SM490. The grade is not specified here as a pressure-vessel or nuclear-safety material. Durability comes from the coating or fire-protection system named on the order, not from the SS540 designation itself.
SS540 Angle Compared with SS400, Plate and Other 50 ksi-Class Grades
SS400 and SS490 are lower-tensile grades in the same standard and can use the same G 3192 series, but they do not carry the SS540 40 mm thickness cap or the SS540 carbon and manganese maxima. SS540 steel plate is the same grade in a different product form. A572 Grade 50 steel angle and S355JR are useful export comparisons only if chemistry and the shape standard are also satisfied; they are not SS540 certificates.
Near-Equivalents: Not Automatic Substitutes
The comparisons above are for orientation. They are not a licence to substitute one grade, one certificate or one shape system for another. SS540 chemistry is C 0.30 max, Mn 1.60 max, with tighter P and S. Use the sister pages for their own standards.
Stock and Supply of SS540 Steel Angles from SHH STEEL
SHH STEEL supplies JIS G 3101 SS540 equal-leg and unequal-leg steel angles as an export trading house, coordinating mill production and project procurement. The useful work on this product is to keep SS540 distinct from SS400 and from JIS G 3106 grades, to select the correct yield band from the leg thickness, and to align the G 3192 designation, the edition and the inspection document before a rolling programme is committed.
Sizes, lengths and certificates are confirmed per enquiry. The tables are the standard G 3192 series, not a list of pieces on the floor. Mid-range 75×75 and 100×100 sizes are the usual core; 25×25, 250×250 and Table 10 sizes are confirmed per line.
Sections can be sourced from mills that SHH STEEL buys from, including Masteel, Rizhao Steel, Laiwu (Shandong Steel Laiwu) and Tung Ho Steel, among others when the programme matches the order. Those mills do not each roll every equal or unequal size in SS540. If cutting, punching, forming or a coating system is required, include that specification for review. Export packing and container loading can be arranged to the packing list agreed for the shipment.
SS540 Steel Angle FAQs
-
Does the name SS540 mean a 540 N/mm² yield?
- No. The number is the specified tensile minimum, 540 N/mm², with no tabulated tensile maximum in Table 3. The minimum yield is 400 N/mm² up to 16 mm and 390 N/mm² between 16 mm and 40 mm.
-
Can I order an SS540 angle thicker than 40 mm?
- Not under Table 1 of the issued JIS G 3101:2015 text, which limits SS540 sections to 40 mm thickness or less. JIS G 3101:2024 is the current listed edition; the edition named on the order governs. The tabulated G 3192 series on this page is inside that cap. A thicker special would be outside this grade.
-
Is SS540 just a stronger SS490?
- It is a higher-tensile grade in the same standard, but the chemistry row is also different: SS540 specifies carbon 0.30% max and manganese 1.60% max, with tighter phosphorus and sulfur, and it has the 40 mm thickness cap. An SS490 certificate is not an SS540 certificate.
-
Is an equal angle interchangeable with an unequal angle of the same long-leg length?
- No. A 100×100 equal angle and a 100×75 unequal angle are different sections. Table 10 is also a separate series, not a subset of Table 9.
-
Which inspection document is default?
- If not otherwise specified at the time of order, JIS G 0415 inspection certificate 3.1 is the default. The document should name JIS G 3101 and its edition, SS540, the G 3192 designation, the heat analysis and the tensile results.
Request a Quotation for JIS G 3101 SS540 Steel Angle
JIS G 3101 SS540 steel angle is a general structural L-section whose tensile class is 540 N/mm² minimum. Nominate the equal or unequal G 3192 size and the material to JIS G 3101 SS540, naming the edition on the order. This page uses the issued 2015 tables; 2024 is the current listing. The tables are reference dimensions, not a rolling list. Send the designation list, edition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.