JIS G 3101 SS490 Equal and Unequal Steel Angles | JIS G 3101 Steel Angles - SHH STEEL

JIS G 3101 SS490 Equal and Unequal Steel Angles

JIS G 3101 SS490 steel angle is a general structural equal-leg or unequal-leg section named for a 490–610 N/mm² tensile range, not for a 490 N/mm² yield. Yield is 285 N/mm² up to 16 mm and 275 N/mm² between 16 mm and 40 mm. Dimensions follow JIS G 3192. SHH STEEL supplies these angles to the grade, designation, edition and certificate named on the order.
Keywords
JIS G 3101 SS490 Steel Angle, SS490 equal angle, SS490 unequal angle, JIS G 3192 angle, 490 N/mm² structural angle
Equivalent Grades:
Near-equivalents only, not automatic substitutes: SS400 is a lower-tensile grade in the same standard; SS540 is a higher-tensile grade with a 40 mm thickness cap; SM490 is a different JIS standard (G 3106); Q355B; S355JR.
Share:
General Description
Material Specification
Available Sizes of SS490 Equal Leg Steel Angles
Available Sizes of SS490 Unequal Leg Steel Angles
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Stock and Supply
FAQ
Conclusion

What is JIS G 3101 SS490 Steel Angle?

JIS G 3101 SS490 steel angle is a hot-rolled equal-leg or unequal-leg section in general structural steel SS490. The material standard is JIS G 3101, Rolled steels for general structure. The chemical and mechanical figures on this page are those of the issued JIS G 3101:2015 tables. JIS G 3101:2024 is the current listed edition, issued 20 February 2024; the edition named on the order governs acceptance. Dimensions, mass and tolerances for these angles are those of JIS G 3192:2024. SHH STEEL supplies these angles to the grade, designation, edition and certificate named on the order.

The number in the grade name is the specified tensile strength in N/mm² (1 N/mm² = 1 MPa), not a yield class. Formal grades in the standard are SS330, SS400, SS490 and SS540. This page is SS490. It is not the JIS G 3101 SS400 steel angle page, not a JIS G 3106 SM490 steel angle, and not a data sheet for SS490 steel plate.

These angles are filed under JIS G3101 in the steel angle profiles category of steel structural profiles. The same grade in plate form is listed separately; do not use the plate page as an angle data sheet.

This page covers Equal and Unequal Steel Angles in JIS G 3101 SS490. The Equal Leg Steel Angles (JIS G 3192 Table 8) and Unequal Leg Steel Angles (Tables 9 and 10) follow JIS G 3192; the material standard does not by itself define the dimensions.

Material, Dimensions and Tolerances for SS490 Angles

Keep the material specification and the dimensional standard distinct. JIS G 3101 is the material standard. The ladle-analysis and mechanical figures used here are those of the issued JIS G 3101:2015 tables (Table 2 and Table 3). JIS G 3101:2024 is the current listed edition; the edition named on the order governs acceptance. JIS G 3192:2024 is the shape standard for these angles. A documented special combination is valid only if every requirement of each named standard is met. Matching a nominal 100 mm or 4 in leg is not a substitution method.

JIS G 3101 does not require a fully killed practice and does not require the product to be normalized. If a heat treatment has been applied, the standard gives sampling rules for that heat-treated lot; it does not turn normalizing into the delivery condition of the grade.

JIS G 3101 SS490 Equal Leg Steel Angles

The tables list the complete tabulated standard angle series in JIS G 3192:2024: Table 8 equal-leg angles, 40 sizes from 25×25×3 to 250×250×35; Table 9 unequal-leg angles, 13 sizes from 90×75×9 to 150×100×15; and Table 10 unequal-leg unequal-thickness angles, 7 sizes from 200×90×9×14 to 400×100×13×18. Each table carries footnote a: the listed sizes are representative, and sizes other than those listed are agreed between the purchaser and the supplier. Use the tables to identify and estimate, not as a rolling programme for SS490. Mid-range equal legs such as 75×75 and 100×100 are the usual enquiry core; the 25×25 and 30×30 families, the 250×250 rows, and the Table 10 series should be confirmed size by size.

Table 10 is a separate series and is not a subset of Table 9. Root and toe radii r1 and r2 are tabulated standard dimensions in these JIS series and are shown. Theoretical mass uses a density of 7.85 g/cm³. This page does not invent rows that Tables 8, 9 and 10 do not list. SS490 in Table 1 of the issued JIS G 3101:2015 text has no tabulated thickness cap for sections. The 255 N/mm² and 245 N/mm² yield bands are kept because a special bar over 40 mm or 100 mm could be agreed; none of the tabulated G 3192 series reach those thicknesses.

75×75×9 has a 9 mm leg, so the 285 N/mm² yield band applies. 150×150×15 remains in that first band. 150×150×19 and 200×200×20 have 19 mm and 20 mm legs, so the minimum yield is 275 N/mm², not 285 N/mm². On Table 10 the usual thickness basis is the thicker leg t2. Annex JA of JIS G 3101 applies to sections whose leg length is under 40 mm: in Table 8, that is the 25×25 and 30×30 families, which shall be reviewed against Annex JA in the edition named on the order. The numeric Annex JA values are not restated here, and this page does not extend Annex JA to legs of 40 mm or larger.

Equal-leg angles — Table 8, 40 sizes

Swipe horizontally to view all dimensions.

Designation (A×A×t) A (mm) t (mm) r1 (mm) r2 (mm) Area (cm²) Mass (kg/m)
25×25×3 25 3 4 2 1.427 1.12
30×30×3 30 3 4 2 1.727 1.36
40×40×3 40 3 4.5 2 2.336 1.83
40×40×5 40 5 4.5 3 3.755 2.95
45×45×4 45 4 6.5 3 3.492 2.74
45×45×5 45 5 6.5 3 4.302 3.38
50×50×4 50 4 6.5 3 3.892 3.06
50×50×5 50 5 6.5 3 4.802 3.77
50×50×6 50 6 6.5 4.5 5.644 4.43
60×60×4 60 4 6.5 3 4.692 3.68
60×60×5 60 5 6.5 3 5.802 4.55
65×65×5 65 5 8.5 3 6.367 5.00
65×65×6 65 6 8.5 4 7.527 5.91
65×65×8 65 8 8.5 6 9.761 7.66
70×70×6 70 6 8.5 4 8.127 6.38
75×75×6 75 6 8.5 4 8.727 6.85
75×75×9 75 9 8.5 6 12.69 9.96
75×75×12 75 12 8.5 6 16.56 13.0
80×80×6 80 6 8.5 4 9.327 7.32
90×90×6 90 6 10 5 10.55 8.28
90×90×7 90 7 10 5 12.22 9.59
90×90×10 90 10 10 7 17.00 13.3
90×90×13 90 13 10 7 21.71 17.0
100×100×7 100 7 10 5 13.62 10.7
100×100×10 100 10 10 7 19.00 14.9
100×100×13 100 13 10 7 24.31 19.1
120×120×8 120 8 12 5 18.76 14.7
130×130×9 130 9 12 6 22.74 17.9
130×130×12 130 12 12 8.5 29.76 23.4
130×130×15 130 15 12 8.5 36.75 28.8
150×150×12 150 12 14 7 34.77 27.3
150×150×15 150 15 14 10 42.74 33.6
150×150×19 150 19 14 10 53.38 41.9
175×175×12 175 12 15 11 40.52 31.8
175×175×15 175 15 15 11 50.21 39.4
200×200×15 200 15 17 12 57.75 45.3
200×200×20 200 20 17 12 76.00 59.7
200×200×25 200 25 17 12 93.75 73.6
250×250×25 250 25 24 12 119.4 93.7
250×250×35 250 35 24 18 162.6 128

JIS G 3101 SS490 Unequal Leg Steel Angles

Table 9 and Table 10 continue the same JIS G 3192:2024 series for SS490. An unequal angle such as 100×75×10 is not a 100×100 equal angle, and it is not an ASTM L-shape of a similar inch size. SS490 in Table 1 of the issued JIS G 3101:2015 text has no tabulated thickness cap for sections. The 255 N/mm² and 245 N/mm² yield bands are kept because a special bar over 40 mm or 100 mm could be agreed; none of the tabulated G 3192 series reach those thicknesses.

Unequal-leg angles — Table 9, 13 sizes

Swipe horizontally to view all dimensions.

Designation (A×B×t) A (mm) B (mm) t (mm) r1 (mm) r2 (mm) Area (cm²) Mass (kg/m)
90×75×9 90 75 9 8.5 6 14.04 11.0
100×75×7 100 75 7 10 5 11.87 9.32
100×75×10 100 75 10 10 7 16.50 13.0
125×75×7 125 75 7 10 5 13.62 10.7
125×75×10 125 75 10 10 7 19.00 14.9
125×75×13 125 75 13 10 7 24.31 19.1
125×90×10 125 90 10 10 7 20.50 16.1
125×90×13 125 90 13 10 7 26.26 20.6
150×90×9 150 90 9 12 6 20.94 16.4
150×90×12 150 90 12 12 8.5 27.36 21.5
150×100×9 150 100 9 12 6 21.84 17.1
150×100×12 150 100 12 12 8.5 28.56 22.4
150×100×15 150 100 15 12 8.5 35.25 27.7

Unequal-thickness angles — Table 10, 7 sizes

Swipe horizontally to view all dimensions.

Designation (A×B×t1×t2) A (mm) B (mm) t1 (mm) t2 (mm) r1 (mm) r2 (mm) Area (cm²) Mass (kg/m)
200×90×9×14 200 90 9 14 14 7 29.66 23.3
250×90×10×15 250 90 10 15 17 8.5 37.47 29.4
250×90×12×16 250 90 12 16 17 8.5 42.95 33.7
300×90×11×16 300 90 11 16 19 9.5 46.22 36.3
300×90×13×17 300 90 13 17 19 9.5 52.67 41.3
350×100×12×17 350 100 12 17 22 11 57.74 45.3
400×100×13×18 400 100 13 18 24 12 68.59 53.8

SS490 Chemical Composition for Angles (Table 2)

The ladle analysis shall comply with Table 2 of JIS G 3101, using the issued 2015 figures given below. JIS G 3101:2024 is the current listed edition; the edition named on the order governs. The SS490 row is the same row as SS330 and SS400: only phosphorus and sulfur have maxima. Carbon and manganese are shown as having no tabulated requirement. Silicon is not a tabulated column on that row. This page does not invent carbon or manganese windows from mill catalogues or from the SS540 row.

Element SS490 ladle analysis, Table 2 (mass %)
C No specified requirement
Mn No specified requirement
P, max 0.050
S, max 0.050

Elements shown as having no tabulated requirement, and alloying elements not listed in Table 2, may be added as necessary. Table 2 is a ladle-analysis table. The issued 2015 text recovered for this page specifies ladle analysis only and does not give a separate numeric product-analysis table. This page does not invent one.

SS490 Angle Mechanical Properties: Yield, Tensile and Elongation

Mechanical properties of SS490 plates, strip, flats and sections follow Table 3 of the issued JIS G 3101:2015 text, which is a single mechanical table that includes plate, strip, flat, section and bar rows. These angles use the plate, strip, flat and section rows, not the bar rows. The recovered 2015 Table 3 notes do not add an upper-yield or 0.2% proof-stress instruction, and this page does not add one. Thickness for a section is the thickness at the test-piece location; on these pages the usual basis for selecting a yield band is the leg thickness t, or the thicker leg t2 on Table 10.

Property Table 3 requirement for SS490 sections
Minimum yield, t ≤ 16 mm 285 N/mm²
Minimum yield, 16 mm < t ≤ 40 mm 275 N/mm²
Minimum yield, 40 mm < t ≤ 100 mm 255 N/mm²
Minimum yield, t > 100 mm 245 N/mm²
Tensile strength, all those bands 490–610 N/mm²
Elongation, t ≤ 5 mm 19% min, test piece No. 5
Elongation, 5 mm < t ≤ 16 mm 15% min, test piece No. 1A
Elongation, 16 mm < t ≤ 50 mm 19% min, test piece No. 1A
Bend 180°, inner radius 2.0 × thickness, test piece No. 1 (No. 3 may be used at 5 mm and under)

A 2015 Table 3 note reduces the No. 4 elongation on plates thicker than 90 mm; that is a plate rule and is not extended here to invent a section value. This page does not reprint a No. 4 elongation percentage, because that figure was not recovered from the issued 2015 table image. The 255 N/mm² and 245 N/mm² yield bands do not appear among the tabulated G 3192 sizes on this page, all of which have a leg thickness of 35 mm or less. JIS G 3101 does not specify Charpy absorbed-energy values. The bend test may be omitted unless the purchaser specifies it; the steel still has to satisfy the bendability requirement, and the outside of the bend piece must be free of cracks.

Delivery, Inspection and Identification of SS490 Angles

SS490 angles are commonly supplied as-rolled. If not otherwise specified at the time of order, the default inspection document is a JIS G 0415 inspection certificate 3.1. The document should identify JIS G 3101 and its edition, the grade SS490, the G 3192 designation, the heat number, the ladle analysis and the tensile results. An EN 10204 type 3.1 request is usually satisfied by that 3.1 document; type 3.2 or nominated third-party attendance can be added when the order requires it. Length is a matter for the rolling programme and the order, often in the region of 6–12 m; those lengths are enquiry ranges, not a stock list. A SS490 plate certificate does not identify an angle.

Weldability and Surface Condition of SS490 Angles

SS490 is a general structural steel intended to be welded, bolted or otherwise fabricated when the procedure is suitable for the thickness and the joint. JIS G 3101 does not table a carbon-equivalent limit or a Charpy value for this grade. This page does not prescribe a welding procedure or a preheat chart. The as-rolled surface is mill scale. Blast, paint or galvanizing is an order option. Cutting, punching, forming or coating can be reviewed when that specification is sent with the enquiry.

JIS G 3192 Shape Tolerances and Theoretical Mass

Dimensional and mass tolerances for these angles are those of JIS G 3192, not of JIS G 3101 itself. This article does not reproduce the millimetre tolerance tables; acceptance is against the edition of G 3192 named on the order. Root and toe radii in the tables are tabulated standard dimensions in this series. Settlement on theoretical or weighed mass should follow the contract.

Applications and Service Limits

SS490 steel angles are used where a general structural L-section in this tensile class is specified: frames, bracing, towers, shops and fabrications that name JIS G 3101 SS490 rather than SS400, SS540 or a welded-structure grade such as SM490. The grade is not specified here as a pressure-vessel or nuclear-safety material. Durability comes from the coating or fire-protection system named on the order, not from the SS490 designation itself.

SS490 Angle Compared with SS400, Plate and Other 50 ksi-Class Grades

SS400 steel angle is a lower-tensile grade in the same standard (400–510 N/mm²) and can use the same G 3192 series. SS490 steel plate is the same grade in a different product form. JIS G 3106 SM490 steel angle is a welded-structure grade with its own chemistry and toughness practice; it is not an SS490 certificate. S355JR and Q355B are useful export comparisons only if chemistry, toughness and the shape standard are also satisfied.

Near-Equivalents: Not Automatic Substitutes

The comparisons above are for orientation. They are not a licence to substitute one grade, one certificate or one shape system for another. SS490 chemistry is only P and S have maxima. Use the sister pages for their own standards.

Stock and Supply of SS490 Steel Angles from SHH STEEL

SHH STEEL supplies JIS G 3101 SS490 equal-leg and unequal-leg steel angles as an export trading house, coordinating mill production and project procurement. The useful work on this product is to keep SS490 distinct from SS400 and from JIS G 3106 grades, to select the correct yield band from the leg thickness, and to align the G 3192 designation, the edition and the inspection document before a rolling programme is committed.

Sizes, lengths and certificates are confirmed per enquiry. The tables are the standard G 3192 series, not a list of pieces on the floor. Mid-range 75×75 and 100×100 sizes are the usual core; 25×25, 250×250 and Table 10 sizes are confirmed per line.

Sections can be sourced from mills that SHH STEEL buys from, including Masteel, Rizhao Steel, Laiwu (Shandong Steel Laiwu) and Tung Ho Steel, among others when the programme matches the order. Those mills do not each roll every equal or unequal size in SS490. If cutting, punching, forming or a coating system is required, include that specification for review. Export packing and container loading can be arranged to the packing list agreed for the shipment.

SS490 Steel Angle FAQs

Does the name SS490 mean a 490 N/mm² yield?
No. The number is the specified tensile class. Table 3 gives a tensile range of 490–610 N/mm². The minimum yield is 285 N/mm² up to 16 mm and 275 N/mm² between 16 mm and 40 mm, with lower figures only in thicker bands that the tabulated G 3192 series does not reach.
Are carbon and manganese limited for SS490?
Table 2 of the issued JIS G 3101:2015 text does not specify numerical carbon or manganese maxima for SS490. Only phosphorus (0.050% max) and sulfur (0.050% max) are listed. Do not copy the SS540 carbon and manganese maxima onto this grade.
Is SM490 the same as SS490?
No. SM490 is specified in JIS G 3106, a different standard written for welded structures. An SM490 certificate is not an SS490 certificate, even when both can be furnished as G 3192 angles.
Is an equal angle interchangeable with an unequal angle of the same long-leg length?
No. A 100×100 equal angle and a 100×75 unequal angle are different sections. Table 10 is also a separate series, not a subset of Table 9.
Which inspection document is default?
If not otherwise specified at the time of order, JIS G 0415 inspection certificate 3.1 is the default. The document should name JIS G 3101 and its edition, SS490, the G 3192 designation, the heat analysis and the tensile results.

Request a Quotation for JIS G 3101 SS490 Steel Angle

JIS G 3101 SS490 steel angle is a general structural L-section whose tensile class is 490–610 N/mm². Nominate the equal or unequal G 3192 size and the material to JIS G 3101 SS490, naming the edition on the order. This page uses the issued 2015 tables; 2024 is the current listing. The tables are reference dimensions, not a rolling list. Send the designation list, edition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response