What is GOST 9941 10Х23Н18 Seamless Stainless Steel Pipe
GOST 9941-81 is the Soviet / CIS product standard for seamless cold-/warm-deformed corrosion-resistant steel pipes — geometry, tensile floors, and acceptance in one document. Grade 10Х23Н18 sits in the austenitic heat-resisting 25-20 class set under Table 3. Russian 25Cr-20Ni heat-resisting seamless pipe under the cold-/warm-deformed standard.
SHH STEEL can produce and supply GOST 9941 10Х23Н18 as cold-/warm-deformed seamless pipe across the enquiry OD×wall band (within the mark’s diameter cap), heat-treated by default (without HT only when the PO waives it), descaled or bright-finished, and documented on mill certificates tied to GOST 5632 cast analysis and Table 3 tensile results. Duty focus: 25-20 class heat-resisting austenitic seamless pipe for furnace and hot-gas lines.
Shop language may still say “310 pipe,” yet that commercial alias does not select GOST 5632 cast limits, cold-/warm-deformed tensile floors, or GOST 9941 marking. The purchase order has to name GOST 9941 and 10Х23Н18 so the mill applies the correct analysis, optional heat treatment, mechanical floors, and stencil. Design caution: sulphur-bearing atmospheres attack chromium films — check the gas analysis before copying a 310S note.
Scope discipline: 10Х23Н18 is cold-/warm-deformed seamless pipe under GOST 9941, not hot-deformed GOST 9940 and not an ASTM A312 order by default. Sister marks often compared on the same RFQ include 08Х20Н14С2, 12Х18Н12Т, 17Х18Н9. Role reminder: 25-20 class heat-resisting austenitic seamless pipe for furnace and hot-gas lines. Diameter note: cold/warm Table 1 practice.
Inside this GOST 9941 series, compare GOST 9941 08Х20Н14С2, GOST 9941 12Х18Н12Т, GOST 9941 17Х18Н9. Hub: GOST 9941. Related hot-deformed product page: GOST 9940 10Х23Н18 (different Rm/δ5 and HT default — not interchangeable by certificate). ASTM/ASME related pipe pages (not interchangeable by default): ASTM A312 TP310S.
10Х23Н18 sourcing notes should keep forms separate: open Stainless Steel Pipes and Tubes for pipes/tubes and Stainless Steel Sheets and Plates for sheets/plates, then use ASTM A240 Type 310S only when the flat form is required. Keep 10Х23Н18 acceptance text on the governing pipe/tube standard.
Chemical Composition of GOST 9941 10Х23Н18
Cast analysis for GOST 9941 10Х23Н18 is not printed inside 9941 itself — clause 2.2 points to GOST 5632. Key windows on a typical certificate include C ≤0.10, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.020, Ni 17.00–20.00, Cr 22.00–25.00. SHH STEEL ties the heat number on the pipe marking to the same cast line on the MTC. Commercial alias 310 / UNS S31000 family (approx). Corrosion thread: oxidation and carburisation resistance dominate; aqueous chlorides are secondary.
Chemical limits for 10Х23Н18 appear in the table underneath (GOST 5632-2014 extract). Source priority is the paid GOST 5632 table if your client cites a different edition footnote — send it before the heat is melted. Duty thread: 25-20 class heat-resisting austenitic seamless pipe for furnace and hot-gas lines.
| Grade | C | Si | Mn | P | S | Ni | Cr |
|---|---|---|---|---|---|---|---|
| 10Х23Н18 | ≤0.10 | ≤1.00 | ≤2.00 | ≤0.035 | ≤0.020 | 17.00–20.00 | 22.00–25.00 |
Cast analysis windows from GOST 5632 (chemistry is not tabulated inside GOST 9941-81). Sulphur may be tightened to ≤0.020% when the order states the pipe is intended for welding.
Mechanical Properties of GOST 9941 10Х23Н18
Ambient tensile floors for 10Х23Н18 come from GOST 9941-81 Table 3: Rm min 529 N/mm², elongation δ5 min 35% (yield not normalised in Table 3). Note: Yield not normalised in Table 3. These are delivery-condition values at room temperature, not elevated-temperature design allowables. SHH STEEL reports actual tensile results on the mill document for the ordered test unit. Family: austenitic heat-resisting 25-20 class. Caution: sulphur-bearing atmospheres attack chromium films — check the gas analysis before copying a 310S note.
Yield strength is numerically normalised in GOST 9941 only for 12Х18Н10Т (≥216 N/mm²) when the purchaser orders it — for 10Х23Н18, treat Rp0.2 as an ordered extra unless that mark exception applies. Thick-wall pipes with D/s ≤8 on thirteen named marks may reduce Rm by 19.6 N/mm² per Table 3 note 1. Density 7.95 g/cm³. Role: 25-20 class heat-resisting austenitic seamless pipe for furnace and hot-gas lines.
| Grade | Rm min (N/mm²) | Rp0.2 min (N/mm²) | δ5 min (%) | Density (g/cm³) | Max OD note |
|---|---|---|---|---|---|
| 10Х23Н18 | 529 | — (not normalised) | 35 | 7.95 | cold/warm Table 1 practice |
Ambient values from GOST 9941-81 Table 3 for 10Х23Н18. Yield not normalised in Table 3. Delivery: heat-treated by default (clause 2.3); without HT only by purchaser request. Heat-treatment guidance: Solution anneal / family HT mandatory by default (GOST 9941 clause 2.3); without HT only when purchaser orders it — then mech by agreement.
Seamless Pipe Manufacture of GOST 9941 10Х23Н18
Seamless is not optional wording for 10Х23Н18: GOST 9941 covers cold- and warm-deformed seamless corrosion-resistant pipe. Hot-deformed sisters of related marks live under GOST 9940-81 with different tensile floors. SHH STEEL will not quietly substitute a welded or hot-pierced-only route under a 9941 PO.
Austenitic heats take solution annealing with rapid cool as the default HT path under 9941; skip inventing a without-HT shipment unless the PO freezes that exception. Heat-treatment note for 10Х23Н18: Solution anneal / family HT mandatory by default (GOST 9941 clause 2.3); without HT only when purchaser orders it — then mech by agreement. Scale removal follows when ordered; clause defaults do not automatically pickle every pipe. Duty thread: 25-20 class heat-resisting austenitic seamless pipe for furnace and hot-gas lines.
When dual documentation against ASTM A312 is requested for a related chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Size context for 10Х23Н18: cold-/warm heat-resisting sizes — thinner wall than cold-/warm-deformed 9940 sister. Diameter cap: cold/warm Table 1 practice.
Dimensions and Tolerances for GOST 9941 10Х23Н18
SHH STEEL aligns nominal OD, wall, length type, and precision class (ordinary / high) for 10Х23Н18 before the mill slot is locked. Table 1 lists the cold-/warm OD×wall grid (smaller OD and thinner walls than GOST 9940), with measured length limits per size cell. Size hint: cold-/warm heat-resisting sizes — thinner wall than cold-/warm-deformed 9940 sister. Mark cap: cold/warm Table 1 practice.
OD tolerance is ±1.5% (ordinary) or ±1.0% (high). Wall minus tolerance reaches 15% on many gauges — design min wall with that minus in view. Curvature limits: 1.5 / 2 / 4 mm per metre by wall band. Duty thread: 25-20 class heat-resisting austenitic seamless pipe for furnace and hot-gas lines.
Equivalent Grades for GOST 9941 10Х23Н18
Lock 10Х23Н18 on the PO when the datasheet owner wants GOST 9941 seamless stainless steel pipe (cold-/warm-deformed). Commercial talk as 310 / UNS S31000 family (approx) is fine in emails; mill paperwork must still show GOST 9941 10Х23Н18. Application framing: reformer outlets, furnace coils, and high-temperature CIS process pipe short of true nickel alloys.
| System | Designation | Notes |
|---|---|---|
| GOST 9941 | 10Х23Н18 | Governing pipe grade for this page |
| Commercial / UNS (body only) | 310 / UNS S31000 family (approx) | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A312 related | 310 chemistry family | Related chemistry — different product standard; not interchangeable by default |
| EN / other | EN 1.4845 | Starting point for comparison only; no automatic dual-cert |
When the service outgrows 10Х23Н18, move to a sister rather than stretching the alias: GOST 9941 08Х20Н14С2, GOST 9941 12Х18Н12Т, GOST 9941 17Х18Н9. Apps context: reformer outlets, furnace coils, and high-temperature CIS process pipe short of true nickel alloys. Full list under GOST 9941. Sister grades in the same series each carry their own chemistry row and must be ordered by their own designation (10Х23Н18).
Heat Treatment and Delivery Condition for GOST 9941 10Х23Н18
10Х23Н18 is delivered heat-treated by default (clause 2.3); without HT only by purchaser request under GOST 9941. Guidance: Solution anneal / family HT mandatory by default (GOST 9941 clause 2.3); without HT only when purchaser orders it — then mech by agreement. Fabricator heat treatment after hot bending should chase the same family practice. Weld thread: 310-class fillers; control ferrite and hot cracking on thick wall.
Cooling type matters — austenitics need rapid cool after solution treatment when HT is ordered; ferritic/martensitic anneal practice follows air or slow-cool notes. Duty thread: 25-20 class heat-resisting austenitic seamless pipe for furnace and hot-gas lines. Density 7.95 g/cm³ for weight calcs. Field heat treatment of 10Х23Н18 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. This paragraph is locked to 10Х23Н18 duty: 25-20 class heat-resisting austenitic seamless pipe for furnace and hot-gas lines.
Corrosion Resistance of GOST 9941 10Х23Н18
Corrosion behaviour of GOST 9941 10Х23Н18 tracks its austenitic heat-resisting 25-20 class balance: oxidation and carburisation resistance dominate; aqueous chlorides are secondary. Intergranular corrosion testing is a purchaser option under GOST 9941, not an automatic coupon on every lot. Design caution: sulphur-bearing atmospheres attack chromium films — check the gas analysis before copying a 310S note.
For heat-facing austenitics, oxidation resistance may dominate over aqueous IGC talk; for Mo austenitics, chlorides dominate; for ferritics, mild aqueous and weld practice dominate. 10Х23Н18 is filed as austenitic heat-resisting 25-20 class. Caution: sulphur-bearing atmospheres attack chromium films — check the gas analysis before copying a 310S note.
Applications of GOST 9941 10Х23Н18 Seamless Pipe
Applications of GOST 9941 10Х23Н18 seamless pipe centre on reformer outlets, furnace coils, and high-temperature CIS process pipe short of true nickel alloys. Role summary: 25-20 class heat-resisting austenitic seamless pipe for furnace and hot-gas lines. When a related chemistry is required under ASTM A312, open those sister pages — acceptance text is not automatic.
Downstream fabricators should inherit the same Cyrillic grade symbol on cut lists so informal latinised substitutions do not creep in. Primary application sketch: reformer outlets, furnace coils, and high-temperature CIS process pipe short of true nickel alloys. Duty thread: 25-20 class heat-resisting austenitic seamless pipe for furnace and hot-gas lines.
Weldability of GOST 9941 10Х23Н18
10Х23Н18 ships as seamless mill product, but fabricator joints on spools still need a qualified WPS. Shop guidance: 310-class fillers; control ferrite and hot cracking on thick wall. Mill heat treatment of the pipe does not replace qualified welding procedures on site joints. Procedure qualification for 10Х23Н18 should use the same product form and wall class as production, including the cold-/warm-deformed seamless finish that will ship. Corrosion framing beside 10Х23Н18: oxidation and carburisation resistance dominate; aqueous chlorides are secondary.
Filler selection should match or over-alloy the base chemistry as the WPS demands. Heat input, interpass temperature, and shielding follow the family — austenitic heat-resisting 25-20 class — not a single shop habit. Caution: sulphur-bearing atmospheres attack chromium films — check the gas analysis before copying a 310S note. Consumable lot control and shielding-gas notes for 10Х23Н18 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Weld-shop note tied to 10Х23Н18: 310-class fillers; control ferrite and hot cracking on thick wall.
Surface Finishes for GOST 9941 10Х23Н18
On 10Х23Н18, cosmetics never outrank correct heat treatment. Passivation and polish are sequenced after the anneal that qualifies the pipe. Duty locked here: 25-20 class heat-resisting austenitic seamless pipe for furnace and hot-gas lines. Name which surface carries each finish callout. Passivation and polish are sequenced only after heat-treatment evidence is already on the certificate for 10Х23Н18.
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard pipe mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
Do not polish over unresolved defects on 10Х23Н18; inspection comes before cosmetics. Passivation after pickle or shop welding is good practice in chloride-lean service, but GOST 9941 acceptance still rests on correct heat treatment. Pack away from carbon-steel contact. Final visual release still rejects grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed (10Х23Н18).
Inspection and Testing for GOST 9941 10Х23Н18
Inspection for GOST 9941 10Х23Н18 covers dimensions and appearance on every pipe; tensile on two pipes per party; flattening or expanding on one when ordered; IGC on two when ordered. Hydrostatic and ultrasonic tests run when the purchaser asks. Documents follow GOST 10692 with chemistry taken from the billet certificate.
Marking includes 10Х23Н18, manufacturer, size, and GOST 9941. Traceability from stencil to MTC is part of supply, not an upgrade. Use: reformer outlets, furnace coils, and high-temperature CIS process pipe short of true nickel alloys. Non-conforming 10Х23Н18 lengths are segregated and retested or rejected under GOST 9941 rather than reworked into unmarked stock. Size practice for 10Х23Н18 remains cold-/warm heat-resisting sizes — thinner wall than cold-/warm-deformed 9940 sister.
Packaging and Shipping for GOST 9941 10Х23Н18
Packaging for 10Х23Н18 uses wooden boxes, plywood cases, or bundled frames with waterproof wrapping as the OD and finish demand. Soft separators protect descaled and polished surfaces. Ends receive caps or bevel protectors when ordered. Bundle tickets for 10Х23Н18 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Application context for 10Х23Н18 stays reformer outlets, furnace coils, and high-temperature CIS process pipe short of true nickel alloys.
Carbon-steel strapping never contacts the stainless OD without a barrier. Mixed-grade bundles are forbidden when chemistry integrity matters. Caution: sulphur-bearing atmospheres attack chromium films — check the gas analysis before copying a 310S note. Desiccant and wrap choices for 10Х23Н18 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Application context for 10Х23Н18 stays reformer outlets, furnace coils, and high-temperature CIS process pipe short of true nickel alloys.
Shipping documents list GOST 9941, 10Х23Н18, sizes, quantities, heat numbers, and certificate type. SHH STEEL coordinates inland trucking and FOB/CIF packing scopes as the order states. Role: 25-20 class heat-resisting austenitic seamless pipe for furnace and hot-gas lines. Claims handling for 10Х23Н18 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Corrosion framing beside 10Х23Н18: oxidation and carburisation resistance dominate; aqueous chlorides are secondary.
Why Choose SHH STEEL
SHH STEEL can produce and supply GOST 9941 10Х23Н18 with the cold-/warm-deformed seamless route, heat-treatment choice, and tests named on your enquiry — not a bait-and-switch alias. Mill partners run stainless seamless hot capacity covering this mark’s OD band. Duty focus: 25-20 class heat-resisting austenitic seamless pipe for furnace and hot-gas lines.
Technical sales can map 10Х23Н18 against sisters 08Х20Н14С2, 12Х18Н12Т, 17Х18Н9 and live ASTM A312 pages without pretending standards are identical. Inspection coordination and export packing are in-house habits, not afterthoughts. Ask for a written acknowledgement that names 10Х23Н18, precision class, and heat-treatment yes or no before melt. SHH STEEL can make 10Х23Н18 to that written scope.
Supply Capability
SHH STEEL can produce and supply GOST 9941 10Х23Н18 across enquiry-oriented OD × wall bands (within cold/warm Table 1 practice), in the cold-/warm-deformed seamless route, with certificates and optional tests as ordered. Summary capability follows in the table; stock language below is an RFQ map, not a frozen tonnage catalogue.
| Item | Capability |
|---|---|
| Standard | GOST 9941-81 seamless cold- and warm-deformed corrosion-resistant steel pipes |
| Grade | 10Х23Н18 (GOST 5632 chemistry; alias 310 / UNS S31000 family (approx)) |
| Product form | Seamless pipe only — cold-/warm-deformed (hot-deformed = GOST 9940) |
| Delivery condition | heat-treated by default (clause 2.3); without HT only by purchaser request |
| Documents | Quality document per GOST 10692 / EN 10204 3.1 style as ordered |
| Typical size practice | Cold-/warm Table 1 OD×wall (smaller/thinner than 9940); mark note: cold/warm Table 1 practice |
| Precision | Ordinary, high, or elevated (indices per marking examples) |
| Tests | Tensile per party; hydro / UT / flatten / IGC / yield when ordered |
Stock / Available sizes
SHH STEEL can produce and supply GOST 9941 10Х23Н18. Stock / Available sizes: enquiry band typically aligns with GOST 9941 Table 1 OD×wall practice, with ordinary or high precision as ordered. For 10Х23Н18, practical fast-track sizes often sit inside the mark’s diameter cap — send the OD × wall list for a firm acknowledgement. Context: cold-/warm heat-resisting sizes — thinner wall than cold-/warm-deformed 9940 sister. Cap: cold/warm Table 1 practice.
Cut lengths, bevels, special NDT, IGC, and HT extras add lead time — call them early. Sisters often quoted alongside: 08Х20Н14С2, 12Х18Н12Т, 17Х18Н9. Email the size list to start. SHH STEEL can produce trial lengths of 10Х23Н18 for procedure qualification before the bulk release when the project calendar needs it.
FAQ
-
What is GOST 9941 10Х23Н18 seamless stainless steel pipe used for?
- GOST 9941 10Х23Н18 is cold-/warm-deformed seamless stainless pipe for corrosion-resistant and heat-resistant CIS fluid service — reformer outlets, furnace coils, and high-temperature CIS process pipe short of true nickel alloys. Role summary: 25-20 class heat-resisting austenitic seamless pipe for furnace and hot-gas lines. It is a GOST product standard grade (chemistry from GOST 5632), not an automatic ASTM A312 certificate.
-
Is GOST 9941 10Х23Н18 seamless only, or does it cover welded pipe?
- Seamless only — and specifically cold- and warm-deformed. Hot-deformed pipe of related marks belongs under GOST 9940-81. SHH STEEL can produce and supply the cold-/warm-deformed seamless route for 10Х23Н18 when the mill can meet the ordered size and tests. Welded pipe is outside both 9940 and 9941.
-
Is heat treatment mandatory for 10Х23Н18 under GOST 9941?
- By default yes. Clause 2.3 requires heat treatment; without HT only when the purchaser orders it (mech then by agreement). Guidance for this mark: Solution anneal / family HT mandatory by default (GOST 9941 clause 2.3); without HT only when purchaser orders it — then mech by agreement. Certificate wording should match the treatment actually performed — or explicitly state without heat treatment. Delivery: heat-treated by default (clause 2.3); without HT only by purchaser request.
-
How does 10Х23Н18 compare with sister grades 08Х20Н14С2, 12Х18Н12Т, 17Х18Н9?
- 10Х23Н18 is filed as austenitic heat-resisting 25-20 class. Typical sisters on the same RFQ are 08Х20Н14С2, 12Х18Н12Т, 17Х18Н9. Design caution: sulphur-bearing atmospheres attack chromium films — check the gas analysis before copying a 310S note Pick the sister when the medium or diameter cap outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 10Х23Н18?
- Expect GOST 5632 cast analysis (from the billet document), room-temperature tensile results (Table 3 Rm and δ5), dimensions, and every optional hydro, UT, flattening, IGC, or yield test actually ordered. Documents follow GOST 10692 or EN 10204 3.1 style when specified. Party size max 300 pieces.
-
Is 310 / UNS S31000 family (approx) the same as ordering 10Х23Н18?
- No. 310 / UNS S31000 family (approx) is a commercial cross-walk for body text. The purchase order should lock GOST 9941 and Cyrillic 10Х23Н18 so cast limits, cold-/warm-deformed tensile floors, and optional HT are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GOST 9941 10Х23Н18?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 10Х23Н18 within Table 1 practice, respecting the mark’s diameter cap (cold/warm Table 1 practice). Size context: cold-/warm heat-resisting sizes — thinner wall than cold-/warm-deformed 9940 sister. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Random length typically 1.5–12.5 m by wall band.
-
How should 10Х23Н18 be welded on site?
- Shop guidance: 310-class fillers; control ferrite and hot cracking on thick wall. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, sulphur ≤0.020%, or anneal practice as applicable. Caution: sulphur-bearing atmospheres attack chromium films — check the gas analysis before copying a 310S note
-
When should I choose a Mo-bearing or duplex grade instead of 10Х23Н18?
- Move when chloride pitting, crevice attack, reducing-acid risk, or strength demand exceeds what austenitic heat-resisting 25-20 class practice can defend for the temperature and stress state. Caution for this mark: sulphur-bearing atmospheres attack chromium films — check the gas analysis before copying a 310S note Sister pointers: 08Х20Н14С2, 12Х18Н12Т, 17Х18Н9. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GOST 9941 10Х23Н18 with ASTM A312?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GOST 9941 10Х23Н18 does not clear ASTM A312 acceptance by default. State both standards, sizes, and test scopes before melt.
-
How does GOST 9941 10Х23Н18 differ from GOST 9940 of the same mark?
- GOST 9941 is cold-/warm-deformed (smaller OD, thinner wall, HT mandatory by default); GOST 9940 is hot-deformed (larger OD/wall, HT optional) with different Rm/δ5 pairs for most marks. SHH STEEL can produce and supply either standard when the PO names it clearly — do not mix certificates for 10Х23Н18.
Conclusion
GOST 9941 10Х23Н18 is cold-/warm-deformed seamless stainless steel pipe for CIS corrosion-resistant service — 25-20 class heat-resisting austenitic seamless pipe for furnace and hot-gas lines. SHH STEEL can produce and supply it in the cold-/warm-deformed seamless route with the heat-treatment choice, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 08Х20Н14С2, 12Х18Н12Т, 17Х18Н9. Related ASTM A312 pages share chemistry families but not GOST acceptance text. Email admin@steelspecs.com with OD × wall, precision class, HT yes/no, and medium notes to start the quote.