ASTM B265 Grade 37 Titanium Plate | Ti-1.5Al (UNS R52815)

ASTM B265 Grade 37 titanium plate is Ti-1.5Al titanium alloy (UNS R52815) supplied annealed. It is specified for 345 MPa minimum tensile strength, 215–450 MPa yield and 20% minimum elongation. Typical uses include exhaust systems and mufflers. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.
Keywords
ASTM B265 Grade 37 titanium plate, Grade 37 titanium plate, UNS R52815 plate, Ti-1.5Al titanium alloy plate, ASTM B265 titanium sheet
Equivalent Grades:
UNS R52815, ASME SB-265 Gr.37, JIS Class 50 (TAP1500)
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is ASTM B265 Grade 37 titanium plate?

ASTM B265 Grade 37 titanium plate is made to ASTM B265, the ASTM specification for titanium and titanium alloy strip, sheet and plate. It carries the UNS number R52815. Grade 37 is Ti-1.5Al. The aluminium addition improves oxidation resistance and elevated-temperature strength over CP titanium while keeping good formability and weldability.

This is an alpha or near-alpha titanium alloy. Aluminium (and in some grades tin or zirconium) strengthens the alpha phase, while only small amounts of beta stabilisers such as manganese, molybdenum or vanadium are present. Such alloys keep good weldability and creep strength at elevated temperature, are normally used annealed, and respond little to strengthening heat treatment.

Its typical density of about 4.50 g/cm³ is a little over half that of carbon steel, which is one reason titanium plate is chosen where weight matters.

ASTM B265 groups its grades into unalloyed titanium, corrosion-resistant grades with small additions of palladium, ruthenium, nickel or molybdenum, and structural alloys such as Ti-3Al-2.5V and Ti-6Al-4V. Each grade has its own UNS number, and the H grades add a higher guaranteed tensile strength for pressure vessel use.

SHH STEEL handles Grade 37 plate enquiries within its range of titanium alloy plates and sheets, checking the ordered ASTM B265 edition, product form and certificate type before confirming supply. Related designations covered on this site include ASME SB-265 Grade 37, JIS H4600 Class 50 TAP1500.

Material specification for ASTM B265 Grade 37

ASTM B265 classifies flat titanium products by thickness and width. The same chemistry and tensile requirements apply to strip, sheet and plate, but dimensional tolerances and bend testing differ by product form.

Ordering item ASTM B265 basis
Standard ASTM B265, Titanium and Titanium Alloy Strip, Sheet, and Plate; state the edition on the order
Grade / UNS Grade 37, Ti-1.5Al, UNS R52815
Plate Over 0.187 in (4.75 mm) thick and over 10 in (254 mm) wide
Sheet 0.187 in (4.75 mm) and under, 24 in (610 mm) wide or more; state cold or hot rolled
Strip 0.187 in (4.75 mm) and under, less than 24 in (610 mm) wide
Condition Annealed
Certificate Manufacturer’s report with chemical analysis, tensile results and other required tests

Order information listed by the specification includes grade, product limitations, special mechanical properties, marking, finish, packaging, any additional reports and the disposition of rejected material. For ASME Code construction, order to ASME SB-265 Grade 37 and state any dual certification on the purchase order.

Chemical composition of ASTM B265 Grade 37 (UNS R52815)

Single values are maximums; ranges are shown where an element is added. Titanium is determined by difference. Product analysis tolerances cover variation between laboratories and do not broaden the heat analysis limits.

Element Heat analysis, % Permissible variation in product analysis, %
Nitrogen (N) 0.03 +0.02
Carbon (C) 0.08 +0.02
Hydrogen (H) 0.015 +0.002
Iron (Fe) 0.30 +0.15
Oxygen (O) 0.25 +0.03
Aluminium (Al) 1.0–2.0 ±0.20
Other elements, each 0.1 +0.02
Other elements, total 0.4 —
Titanium (Ti) Balance —

Ingot top and bottom are analysed for the listed elements. Hydrogen is tested and reported on at least one final product sample, and a lower hydrogen limit may be negotiated. Other elements need not be reported unless they exceed 0.10% each or 0.40% total, and they may not be added intentionally.

Mechanical properties of ASTM B265 Grade 37

The values below are the requirements for Grade 37 plate in the annealed condition.

Property Requirement
Tensile strength, min 50 ksi (345 MPa)
Yield strength, 0.2% offset 31–65 ksi (215–450 MPa)
Elongation in 2 in or 50 mm, min 20%
Bend test, under 0.070 in (1.8 mm) Mandrel radius 2T, bent 105° without outside fracture
Bend test, 0.070–0.187 in (1.8–4.75 mm) Mandrel radius 2.5T
Bend test, over 0.187 in (4.75 mm) Not applicable to material over 4.75 mm

Tensile tests are made at room temperature. The yield range has an upper limit as well as a lower one. That cap protects formability, so a plate with very high yield can fail the grade even if it is strong. Bend tests apply to sheet and strip up to 0.187 in (4.75 mm); plate over that thickness is not bend tested under the specification.

Elevated-temperature design values are not part of the plate specification. They come from the design code, such as ASME Section II, Part D where the grade is listed.

Delivery condition, finish and marking

ASTM B265 covers material in the annealed condition. Plate must be free of injurious external and internal imperfections. Annealed product may be furnished descaled, sandblasted, ground, or sandblasted and ground; state the finish on the order.

  • Condition: Annealed
  • Surface: descaled, sandblasted or ground, as ordered; minor spot grinding is permitted within the thickness tolerance
  • Marking: specification, grade, heat number, manufacturer’s identification and nominal thickness, in rows that can be removed with hot alkaline cleaning
  • Packaging: boxed, crated, boarded or as the manufacturer’s standard practice unless the order states otherwise

The alloy is supplied annealed; stress relieving after forming or welding is agreed with the purchaser. If the plate will be formed or welded in your shop, say so at enquiry so the finish and protective packing suit the next process.

Welding and fabrication of Grade 37 titanium plate

Grade 37 is weldable by gas tungsten arc, plasma arc, electron beam and laser processes, provided the weld zone is fully shielded from air.

  • Use trailing shields and back purging until the weld cools below about 400 °C
  • Use matching or engineer-approved filler metal and qualified procedures
  • Clean joints and filler wire; remove oil, moisture and iron contamination
  • Consider post-weld stress relief for highly restrained or precision parts, as agreed in the procedure

Room-temperature formability is lower than for CP titanium. Moderate bends can be cold formed with generous radii, but severe shapes are normally hot formed or creep formed.

Machining needs sharp carbide tools, rigid set-ups, low cutting speeds and generous coolant, because titanium alloys conduct heat poorly and the heat stays at the cutting edge. Avoid dwelling, which work-hardens the surface, and keep fine chips away from ignition sources.

These are general practices, not a qualified procedure. The fabricator must qualify the welding procedure, filler metal and inspection to the applicable code.

Dimensional tolerances and flatness

Dimensional tolerances are set in the specification’s tables for thickness, width, length, weight and flatness. Plate flatness has its own table for annealed plate. For sheet, cold-rolled tolerances apply unless hot-rolled sheet is ordered.

State the nominal thickness, width, length, quantity and any cutting drawing at enquiry. If a project needs tighter flatness, a specific edge condition or cut-to-size pieces, write it on the order rather than relying on the default tables. No stock sizes are implied by this page.

Titanium plate can be cut by waterjet, abrasive saw, plasma or machining. Thermal cutting leaves an oxygen-enriched edge that should be removed by machining or grinding before welding or forming, so agree the cut-edge condition and any machining allowance on the order.

Applications and service limits of Grade 37 titanium plate

Typical uses of Grade 37 plate include:

  • Exhaust systems and mufflers
  • Heat-exposed sheet parts
  • Welded ducting
  • Parts needing CP-like forming with better high-temperature performance

As with all titanium, the alloy is not suited to hydrofluoric acid, fluoride-bearing media, dry chlorine or red fuming nitric acid. High-aluminium alloys can be sensitive to hot-salt stress corrosion, and maximum service temperatures depend on the alloy and design code. The design engineer must confirm suitability for the actual service.

When selecting Grade 37, compare it with Grade 6, Grade 32, Grade 39. The choice usually turns on the balance of strength, formability, corrosion behaviour in the actual medium and cost, and on which standard the drawing or design code names.

Compare Grade 37 with other ASTM B265 grades

The grades below are the closest neighbours of Grade 37 in ASTM B265. Values are tensile strength, 0.2% yield or proof strength and minimum elongation, as set by the standard.

Grade Tensile strength Yield / proof strength Elongation, min Typical role
Grade 6 (R54520) 120 ksi (828 MPa) 115 ksi (793 MPa) min 10% Weldable alpha alloy for elevated temperature
Grade 32 (R55111) 100 ksi (689 MPa) 85 ksi (586 MPa) min 10% Ti-5111 near-alpha alloy
Grade 37 (R52815) 50 ksi (345 MPa) 31–65 ksi (215–450 MPa) 20% Ti-1.5Al, oxidation-resistant
Grade 39 (R53390) 75 ksi (515 MPa) 60–90 ksi (410–620 MPa) 20% Ti-0.25Fe-0.4Si heat-resistant

Alpha and near-alpha alloys trade formability for strength and elevated-temperature performance. Compare the full requirements, not only tensile strength, before changing grade.

ASTM B265 Grade 37 equivalent grades

The designations below are commonly compared with ASTM B265 Grade 37. They are close in composition and role, but limits, tests and product forms are set by each standard, so they are not automatically interchangeable.

Standard / system Designation Relationship to ASTM B265 Grade 37
ASME SB-265 Grade 37 ASME Code adoption of B265; ordered for pressure equipment
JIS H4600 Class 50 (TAP1500) Close equivalent; JIS strength range and tests differ
UNS R52815 Same unified number as ASTM Grade 37

Where a drawing names one designation and the supplier offers another, agree in writing which standard governs chemistry, tensile values, testing and marking. Dual or multiple certification is possible only when the material meets every cited standard in full, and the certificate must show the results against each one.

Why choose SHH STEEL for Grade 37 titanium plate

SHH STEEL supports specification-led purchasing of titanium plate and sheet.

  • We quote to the ASTM B265 edition, grade and product form you name, and keep B265 and SB-265 requirements distinct
  • Certificates are checked against the Grade 37 chemistry and tensile limits, including the yield upper limit
  • Sizes, quantities, testing and delivery are confirmed in the quotation, not assumed
  • Finish, marking and packing are agreed before production

Questions on equivalents, dual certification or edition changes are answered before an order is placed.

How to enquire for ASTM B265 Grade 37 plate

Send the material schedule with the details below. We review the enquiry and raise any open points before confirming the supply route.

Enquiry item Information required
Material ASTM B265 Grade 37 (UNS R52815), edition; add ASME SB-265 if Code use
Product form Plate, sheet or strip; for sheet, cold or hot rolled
Dimensions Thickness, width, length, quantity and any cutting drawing
Finish Descaled, sandblasted, ground or other agreed surface
Testing Any special mechanical properties, extra analysis or reports
Documents Certificate type and any third-party inspection
Destination Delivery place and packing requirements

FAQ

Is ASTM B265 Grade 37 the same as ASME SB-265 Grade 37?
SB-265 is the ASME Code adoption of B265, so Grade 37 requirements normally match. They are separate documents, and ASME may adopt a different edition. For Code work, order SB-265 Grade 37 or dual certification.
What is the tensile strength of ASTM B265 Grade 37 titanium plate?
The requirement is 50 ksi (345 MPa) minimum. The 0.2% proof or yield strength is 31–65 ksi (215–450 MPa). Minimum elongation is 20%. Values apply to the condition and thickness range stated in the standard.
What is Grade 37 mainly used for?
Typical uses include exhaust systems and mufflers, heat-exposed sheet parts and welded ducting. The design engineer should confirm the grade for the actual service.
When is a titanium product classed as plate under B265?
Plate is over 0.187 in (4.75 mm) thick and over 10 in (254 mm) wide. Thinner product is sheet if 24 in (610 mm) wide or more, otherwise strip.
What should I send for a quotation?
Send ASTM B265 Grade 37, the edition, product form, thickness, width, length and quantity, the finish, any special testing, the certificate type and the destination. Add ASME SB-265 if the plate is for Code construction.

Request a quotation for ASTM B265 Grade 37 titanium plate

ASTM B265 Grade 37 is Ti-1.5Al titanium alloy, UNS R52815, specified for 50 ksi (345 MPa) minimum tensile strength, 31–65 ksi (215–450 MPa) yield or proof strength and 20% minimum elongation in the annealed condition. Typical uses include exhaust systems and mufflers and heat-exposed sheet parts.

Send the product form, sizes, quantity, finish, certificate type and destination to SHH STEEL. Compare other grades on the ASTM B265 page or browse all titanium alloy plates and sheets. Availability, testing and delivery are confirmed against each enquiry.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *