ASTM A572 Grade 60 Wide Flange H Beam
What is ASTM A572 Grade 60 Steel Beam?
ASTM A572 Grade 60 steel beam is a high-strength low-alloy structural shape certified to ASTM A572/A572M Grade 60 [415], with dimensions and tolerances to ASTM A6/A6M. Grade 60 has a minimum yield point of 60 ksi [415 MPa] and a minimum tensile strength of 75 ksi [520 MPa]. For structural shapes, the specification caps flange or leg thickness at 2 in [50 mm].
This page covers rolled W-shapes in Grade 60, not plate and not Grade 50. The usual Grade 50 beam is listed separately as ASTM A572 Grade 50 steel beam. The same grade family in plate form is listed as ASTM A572 Grade 50 plate; that plate page is not a substitute data sheet for Grade 60 beams, and the plate thickness limit for Grade 60 is a different table.
These beams are filed under steel beam profiles in the steel structural profiles category. A W12×26 in Grade 60 is not a Grade 50 bar of the same designation, and it is not an IPE, HEA, or GB/T 11263 H-section of similar depth. Grade 42, 55 and 65 are different A572 grades and are not this product.
Material, Dimensions and Tolerances for A572 Grade 60 Shapes
The purchase order and the inspection document should name, separately:
- ASTM A572/A572M (or the equivalent SA-572/SA-572M edition on the order) and Grade 60 [415];
- the A6/A6M W designation (for example W12×26 or W14×22);
- killed steel (required by the specification), the alloy type actually used, copper steel if it is required, and any supplementary requirements such as a Charpy test.
Grade 60 structural shapes are limited to a flange or leg thickness of 2 in [50 mm]. A designation whose published flange is thicker than that limit is not a Grade 60 shape under Table 1, even if the same designation can be certified Grade 50.
A572 Grade 60 W-Shape Sizes and Reference Dimensions
The tables below are the ASTM A6/A6M W-shape series used on the live A36 and Grade 50 beam pages, restricted to the 225 designations whose published flange thickness is 50 mm [2 in] or less. The full A6 list contains 283 W-shapes; 58 heavier designations (for example W12×230 and heavier W14, W36 and W40 rows) have flanges thicker than 50 mm and are omitted here. This is not a special “thin-flange” production series and not an invented size table.
Values are reference dimensions for identification and estimating, not a rolling list for any one mill. Root radius is omitted because the AISC tables used here do not print a single r.
W4 to W10 (41 designations with tf ≤ 50 mm)
Swipe horizontally to view all dimensions.
W12 and W14 (48 designations with tf ≤ 50 mm)
Swipe horizontally to view all dimensions.
W16 to W21 (49 designations with tf ≤ 50 mm)
Swipe horizontally to view all dimensions.
W24 to W30 (43 designations with tf ≤ 50 mm)
Swipe horizontally to view all dimensions.
W33 to W44 (44 designations with tf ≤ 50 mm)
Swipe horizontally to view all dimensions.
A572 Grade 60 Chemical Composition for Shapes
The figures below are heat-analysis limits from ASTM A572/A572M Table 2 for Grade 60 shapes. The steel shall be killed. Product analysis, where required, follows the specification. These are not the plate columns of the same table.
A572 Grade 60 Mechanical Properties for Shapes
Table 4 of ASTM A572/A572M gives the following tensile requirements for Grade 60 [415]. There is no published maximum yield, and no Charpy requirement unless a supplementary requirement such as S5 or S30 is specified on the order.
Footnote C of Table 4 (19% elongation in 2 in for wide-flange shapes over 426 lb/ft [634 kg/m]) is part of the specification; none of the Grade 60-eligible W-shapes in the A6 list used here reach that mass. The plate-width elongation reduction in footnote D applies to plates, not to these shapes.
Delivery Conditions, Inspection and Identification
The inspection document should identify ASTM A572/A572M or SA-572/SA-572M and its edition, Grade 60 [415], the A6 designation, killed steel, the alloy type, heat analysis, and the tensile results. Supplementary requirements appear only when they were ordered. A Grade 50 certificate, a plate certificate, or an A992 certificate does not, by itself, identify a Grade 60 beam.
Weldability and Surface Condition of A572 Grade 60 Beams
Grade 60 is a weldable high-strength low-alloy structural steel. Welding procedure, preheat and consumable choice should follow the certified heat analysis, the actual flange and web thickness, and the joint design. Surface quality and repair practice belong to the ordered edition of ASTM A6/A6M. This page does not reproduce those limits.
ASTM A6/A6M Shape Tolerances and Theoretical Mass
Shape, straightness, length, camber and theoretical mass belong to the ordered edition of ASTM A6/A6M. Mass in the size table is the published A6/AISC figure. Millimetre and inch tolerance tables are not reproduced here.
Applications and Service Limits
A572 Grade 60 beams are used where a 60 ksi [415 MPa] yield is specified for building or industrial frames and the flange thickness is within the 2 in [50 mm] cap. They are not a silent substitute for Grade 50, A992, or a weathering or pressure-vessel grade. A W-shape is not a drop-in substitute for an IPE, HEA, or GB/T 11263 H-section of similar mass.
A572 Grade 60 Compared with Grade 50, A992 and A36
The comparisons below are an orientation only; they are not automatic substitutes.
Near-Equivalents: Not Automatic Substitutes
A near-equivalent is a starting point for a discussion, not a licence to swap certificates. ASTM A572 Grade 50 steel beam and ASTM A992 steel beam are different specifications. If a project names Grade 60, keep that grade, the A6 designation, and any supplementary tests on the order.
Sourcing A572 Grade 60 Beams from SHH STEEL
SHH STEEL supplies ASTM A572 Grade 60 steel beams against a named W-shape list, the specification edition and the inspection document type. Enquiries should state the designations, cut lengths or mill lengths, any processing, and whether ASTM A572 Grade 50 steel beam is acceptable on part of the list. Every designation should be checked against the 2 in [50 mm] flange-thickness limit.
The size tables are the A6 series within that limit, not a claim that every designation is rolled in every heat. Once the list is clear, a quotation can be prepared against the stated edition and certificate.
A572 Grade 60 Steel Beam FAQs
-
Can every W-shape in the A6 list be certified Grade 60?
- No. Table 1 of A572/A572M limits Grade 60 structural shapes to a flange or leg thickness of 2 in [50 mm]. This page lists the 225 W designations at or under that limit. Heavier designations with thicker flanges are omitted; they may still be available in Grade 50 or another grade, but they are not Grade 60 under that table.
-
How does Grade 60 differ from Grade 50?
- Grade 60 has a higher minimum yield (60 ksi vs 50 ksi) and tensile strength (75 ksi vs 65 ksi), a different carbon maximum, and a 2 in flange-thickness cap that Grade 50 shapes do not have. A Grade 50 certificate is not a Grade 60 certificate.
-
Is a Charpy test required?
- Not by the default Table 4. A Charpy test applies only when a supplementary requirement such as S5 or S30 is specified on the order.
-
Which standards should appear on the inspection document?
- At least ASTM A572/A572M or SA-572/SA-572M and its edition, Grade 60 [415], the A6 W designation, killed steel, the alloy type, heat analysis, and tensile results against the specification. Supplementary requirements appear only when ordered.
Request a Quotation for ASTM A572 Grade 60 Wide Flange H Beam
ASTM A572 Grade 60 steel beam is a high-strength low-alloy W-shape with a 60 ksi [415 MPa] minimum yield and a 2 in [50 mm] maximum flange thickness. Nominate the A6 designations (for example W12×26 or W14×22), A572/A572M or SA-572/SA-572M in the ordered edition, and the inspection document type. Send the size list, edition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.