ASME SA-36 Wide Flange H Beam
What is an ASME SA-36 Wide Flange H Beam?
An ASME SA-36 wide flange H beam is a rolled W-shape certified to SA-36/SA-36M as adopted in a named edition of the ASME Boiler and Pressure Vessel Code, Section II, Part A, whose dimensions, shape and tolerances conform to ASTM A6/A6M. In the 2023 Section II, Part A book, SA-36/SA-36M is identical with ASTM A36/A36M-19: 36 ksi [250 MPa] minimum yield and 58–80 ksi [400–550 MPa] tensile strength for shapes. The designation “W” is the American wide-flange series. It is not a translation of a Chinese HW section or of a European HEA of a similar nominal depth, and it is not an S shape.
This page covers the rolled wide-flange shape under an SA-36 certificate, not plate and not an S-shape I-beam. The same ASME listing in plate form is discussed on ASME SA-36 steel plate. Ordinary ASTM coverage is ASTM A36 Wide Flange Beam for W-shapes, ASTM A36 S Shape I Beams for S shapes, and ASTM A36 steel plate for plate. An ordinary A36 certificate is not SA-36. The plate yield reduction to 32 ksi [220 MPa] over 8 in [200 mm] does not apply to shapes.
These beams are filed under ASME SA-36 in H Beams and Wide Flange Beams, in the steel structural profiles category. Sister higher-strength American W-shape pages include ASTM A572 Grade 50 and ASTM A992 listings. Those are different specifications and different certificates.
SA-36 W-shapes are used where the order requires the ASME mark on a 36 ksi carbon wide-flange beam. They are not a 50 ksi grade, not a weathering steel, and not themselves a pressure-vessel part merely because the material is listed in Section II. If the enquiry only says “SA-36 beam,” the shape series (W, S or another A6 form), the Code edition and the designation still need to be confirmed.
ASME SA-36 Code Edition, Certification and What SA-36 Is Not
Ordering “SA-36” means ordering the ASME adopted specification as it appears in Section II, Part A of a named Boiler and Pressure Vessel Code edition. This article follows the 2023 Section II, Part A text, which states that SA-36/SA-36M is identical with ASTM A36/A36M-19. If the construction project is under a different Code year, the SA-36 text in that year’s Section II, Part A is the one that applies. A later ASTM A36 revision is not, by itself, the SA specification in a 2023 book.
An ordinary ASTM A36 certificate does not make the piece SA-36. Material made and documented only to ASTM A36/A36M can be used where the contract calls for A36; it is not SA-36 until it is produced and certified to SA-36/SA-36M as adopted in the named Code edition. Dual marking or a combined A36/SA-36 certificate is legitimate only when every requirement of each named specification is met and the inspection document actually says so. The names are not interchangeable, and a shop should not restamp A36 as SA-36 after the fact.
Listing in Section II, Part A makes the specification available for use where a construction Code — for example Section I, Section III or Section VIII, as the project requires — permits SA-36 for the part in question. That listing is not a blanket approval for every pressure part, every temperature, or every service. SA-36 is a carbon structural steel specification. It is not a pressure-vessel plate specification such as SA-516, and it is not a nuclear-safety default material. Whether an SA-36 beam may be used around a vessel, in a support, or in any other Code-stamped item is decided by the applicable construction Code, the part, the design temperature and the permitted material tables — not by this product page.
The steel shall be killed. Supplementary requirements printed with SA-36/SA-36M — S5 Charpy V-notch, S30 Charpy V-notch for structural shapes with alternate core location, and S32 single-heat bundles — apply only when they are named on the order. They are not default tests for every SA-36 beam.
Material, Dimensions and Tolerances for ASME SA-36 W-Shapes
Three identifications should appear, separately, on the purchase order and on the certificate:
- SA-36/SA-36M is the ASME Section II, Part A material listing. This article uses the 2023 book, in which the text is identical with ASTM A36/A36M-19. The Code edition named on the order governs acceptance.
- ASTM A36/A36M is the ASTM specification referenced by that identical text. It is not, by itself, an SA-36 certificate.
- ASTM A6/A6M is the general-requirements standard for the W-shape designation system, dimensions, tolerances, marking and the heat-analysis and tension-test rules. SA-36 does not itself contain the W-shape size tables.
Do not treat “SA-36 beam” as if it automatically meant a W12×50, and do not substitute ASTM A36 S Shape I Beams, an HEA or a Chinese HW by matching a nominal depth. A mill may certify SA-36 on a non-W shape only when that product form is actually in the listing and is fully documented; this page is the W-shape listing.
ASME SA-36 W-Shape Sizes and Reference Dimensions (ASTM A6/A6M)
The tables list nominal W-shape reference dimensions: designation, nominal depth, mass in lb/ft and kg/m, and actual depth, width, web thickness and flange thickness in both inch and millimetre units. There are 283 designations, grouped by depth so the tables stay readable. They are reference dimensions for identification and estimating, not a rolling list, and not a claim of guaranteed availability or that every W-shape is produced in SA-36. Dimensional acceptance, including shape and mass tolerances, follows the edition of ASTM A6/A6M named on the order. Mid-range W12 to W30 beams and the common W8–W14 column sizes are the usual enquiry core; the lightest W4–W6 rows, jumbo column sections, and the deepest W40–W44 rows should be confirmed size by size.
A designation such as W16×26 is a series call: the first number is the nominal depth in inches and the second is the nominal mass in pounds per foot. The actual depth of a W16×26 is slightly less than 16 in. That is normal. Root radius is omitted because a single fillet radius is not published as a delivery dimension for these shapes, and a radius is not invented here.
Theoretical mass is the tabulated reference value. Settlement should follow the contract — tabulated theoretical mass or weighed mass — and the ordered A6 edition for mass tolerance. These W-shape rows are not interchangeable with HW, HM, HN or HEA/HEB/IPE rows of a similar nominal depth, and they are not S shapes.
W4 to W10
The lighter W-shapes, often used as small beams, lintels and miscellaneous members. 41 designations in this group, from W4×13 to the W10 series.
Swipe horizontally to view all dimensions.
W12 and W14
The mid-depth column and beam group, including many of the heavier W12 and W14 column sections. 67 designations.
Swipe horizontally to view all dimensions.
W16 to W21
Common building-beam depths. 55 designations.
Swipe horizontally to view all dimensions.
W24 to W30
Deeper building and industrial beams. 54 designations.
Swipe horizontally to view all dimensions.
W33 to W44
The deepest W-shapes in these reference tables, through W44. 66 designations. Heavier and deeper rows should be confirmed size by size against the mill programme.
Swipe horizontally to view all dimensions.
Chinese HW/HM/HN sizes belong to GB/T 11263. European HEA/HEB/IPE sizes are listed on the S235JR H-beam page for that material system, not as SA-36 dimensions. S-shape dimensions belong on the ASTM A36 S Shape I Beams page, not in this table. The live ASTM listing that uses the same W series is ASTM A36 Wide Flange Beam; that page is not an SA-36 certificate.
ASME SA-36 Chemical Composition for Shapes (Heat Analysis)
The figures below are heat-analysis limits for SA-36 shapes from Table 3 of SA-36/SA-36M as printed in ASME BPVC Section II, Part A, 2023 (identical with ASTM A36/A36M-19). They are the shapes column for all thicknesses, not a plate-width column, and they are limits, not typical heat results. Product analysis shall conform to the same Table 3 limits, subject to the numeric permitted variations below, taken from Table A of ASTM A6/A6M-19, the general-requirements edition identified with A36/A36M-19 and with this SA-36/SA-36M printing. The A6/A6M edition named on the order governs. Where Table A shows no under-minimum or over-maximum figure, none is applied on this page.
The following product-analysis variations apply to the shapes-column heat-analysis limits above. Manganese has no specified heat-analysis requirement in that column, so no manganese product-analysis limit is invented here.
Do not copy a plate-width chemistry column onto a beam. The plate columns in the same table use different carbon, manganese, phosphorus, sulfur and silicon limits, and they are written for plates, not for W-shape shapes.
ASME SA-36 W-Shape Mechanical Properties: Yield, Tensile and Elongation
Tensile properties of SA-36 beams follow the shapes requirements in Table 2 of SA-36/SA-36M as printed in ASME BPVC Section II, Part A, 2023 (identical with ASTM A36/A36M-19), not the plates-and-bars elongation column. The 32 ksi [220 MPa] yield that applies to plates over 8 in does not apply to these sections. The footnote that removes the 80 ksi tensile maximum and lowers the 2 in elongation to 19% applies only to wide-flange shapes with flange thickness over 3 in, not to C or MC shapes.
For shapes with a cross-sectional area less than 1 in² [645 mm²], clause 8.2 of the specification provides that the manufacturer need not tension-test the product if the chemistry used is appropriate for obtaining the tensile properties in Table 2. Clause 8.2 is about cross-sectional area, not about a copied angle size list. Confirm it against the actual C or MC designation and its tabulated area. For reference, the following angle sizes are the ones listed in the sister SA-36 beam article and are not used as a beam list: L 2×2×1/8, L 2×2×3/16, L 2×2×1/4, L 2-1/2×1-1/2×3/16, L 2-1/2×1-1/2×1/4, L 2-1/2×2×3/16, L 2-1/2×2-1/2×3/16 and L 3×2×3/16. Larger beams in the tables remain subject to the ordinary tensile test. The rule does not replace Table 2, and this page does not invent a substitute test method.
Charpy V-notch testing is not a default SA-36 requirement. S5 or S30 applies only when it is named on the order. Bearing-plate rules in Section 5 of the specification concern plates, not these C or MC shapes.
Delivery, Inspection and Identification of ASME SA-36 W-Shapes
SA-36 W-shapes are commonly delivered in the as-rolled condition unless the order names a different condition. The certificate should identify SA-36/SA-36M, the Code edition (for example the 2023 Section II, Part A book), the W designation, and the heat. Marking should follow the ordered product standards so the piece can be matched to the documents.
An ASTM A36 mill test report, even on the same W-shape series, is not an SA-36 certificate. If the project only needs ASTM A36, use the ASTM A36 Wide Flange Beam page instead of this one.
Weldability and Surface Condition of ASME SA-36 W-Shapes
SA-36, as identical with A36-19 in the 2023 book, is a readily welded carbon structural steel in ordinary thicknesses. This page is not a welding procedure. Procedure qualification, consumables and preheat remain the fabricator’s responsibility. A Charpy test is not required unless it is specified on the order.
Surface condition and any special finish for painting or galvanizing should be named when they matter. Jumbo W-shapes and thick-flange sections need thickness-specific review; they are not assumed from a mid-range W12 enquiry.
ASTM A6/A6M Shape Tolerances and Theoretical Mass for ASME SA-36 W-Shapes
Dimensional, straightness, camber, sweep, out-of-square and mass tolerances for these W-shapes are those of ASTM A6/A6M, not of SA-36/SA-36M itself. This article does not reproduce the A6 tolerance tables; acceptance is against the edition named on the order.
The size tables above are nominal W-shape reference dimensions. A delivered W16×26 will measure close to the tabulated depth, width and thicknesses within those tolerances, not as a set of exact advertised inches. The lb/ft and kg/m columns are published theoretical masses. Settlement should follow the contract.
Applications and Service Limits for ASME SA-36 Wide Flange H Beams
SA-36 W-shapes are used where a 36 ksi carbon wide-flange beam must carry an ASME SA-36/SA-36M certificate tied to a named Code edition. Listing in Section II, Part A does not, by itself, make the beam a pressure-vessel part or a nuclear safety material. They are not a 50 ksi, weathering, or quenched-and-self-tempered product.
If the order does not actually require the ASME mark, the ASTM A36 Wide Flange Beam page is the ASTM listing for the same W series. If the shape is an S beam, use ASTM A36 S Shape I Beams.
ASME SA-36 Wide Flange Compared with A36 W-Shapes, SA-36 Plate and Grade 50
The same W series certified only to ASTM A36/A36M is ASTM A36 Wide Flange Beam. The mechanical and chemistry figures can match because the 2023 SA-36 text is identical with A36-19, but the certificates are not the same. ASME SA-36 steel plate is the same SA-36 listing in a different product form, with plate-thickness rules that do not apply to these W-shapes.
ASTM A36 S Shape I Beams are A36 (or, if so ordered, a separately documented SA-36 path) on the S series, not on W-shapes. A572 Grade 50 and A992 wide-flange pages are 50 ksi American grades with their own chemistry and, for A992, shape-specific rules. Dual certification is possible only when the delivered piece meets every requirement of each named standard, including the ASME mark when SA-36 is required.
Near-Equivalents for ASME SA-36 Wide Flange H Beams: Not Automatic Substitutes
The comparisons below are for orientation. They are not a licence to substitute one grade, one certificate or one shape for another on a contract or an inspection document.
Published sister pages for the comparison grades in beam form include GB/T 706 Q235B, JIS G 3101 SS400 and EN 10025-2 S235JR. Use those pages for their own standards; do not treat them as SA-36 equivalents.
Sourcing ASME SA-36 Wide Flange H Beams from SHH STEEL
SHH STEEL reviews enquiries for ASME SA-36 W-shapes against a named A6 designation list, a named Section II, Part A edition, and a named certificate path. We distinguish an ordinary A36 W-shape from an SA-36 certificate, and a W-shape from an S shape, before quoting. We do not treat an HEA, a Chinese HW or an S beam of similar depth as the same item.
Send the W designation list, the Code edition, the inspection document type and delivery notes. Images on this page stay empty; photographs can be provided with a quotation when they are available.
SA-36 Wide Flange H Beam FAQs
-
Is an ASTM A36 wide-flange certificate the same as SA-36?
- No. In the 2023 ASME Section II, Part A book, SA-36/SA-36M is identical with ASTM A36/A36M-19, but an ordinary A36 mill test report is not an SA-36 certificate. The order and the documents have to carry the ASME listing and the Code edition.
-
Which Code edition is used on this page?
- The 2023 Section II, Part A book, in which SA-36/SA-36M is identical with ASTM A36/A36M-19. If the order names a different Code edition, that edition governs; this page does not invent an identity year for an edition that has not been checked here.
-
Do these W-shapes use the 32 ksi yield reduction listed for thick A36 plate?
- No. That 32 ksi [220 MPa] reduction applies to plates over 8 in [200 mm] thick. It does not apply to shapes.
-
Is this page also the S-shape listing?
- No. This article tabulates ASTM A6 W-shapes. American Standard S shapes are a different series and are covered on the ASTM A36 S Shape I Beams page. An S12 is not a W12.
-
Does an SA-36 certificate make the beam a pressure-vessel part?
- No. Section II, Part A is a material listing. It does not, by itself, make a wide-flange beam a Code-stamped pressure-vessel part or a nuclear safety material.
Request a Quotation for ASME SA-36 Wide Flange H Beams
ASME SA-36 wide flange H beams are carbon structural W-shapes certified to SA-36/SA-36M as adopted in a named ASME BPVC Section II, Part A edition. In the 2023 book the text is identical with ASTM A36/A36M-19 (36 ksi [250 MPa] minimum yield). Nominate the W-shape to ASTM A6/A6M and the material to SA-36/SA-36M in the ordered Code edition. The tables are reference dimensions, not a rolling list. An ordinary A36 certificate is not SA-36. Send the designation list, Code edition, certificate type and any processing notes; SHH STEEL will review them before quoting.