ASTM A240 UNS S32906 Stainless Steel Sheet at SHH STEEL warehouse

ASTM A240 UNS S32906 Stainless Steel Sheet

ASTM A240 UNS S32906 Stainless Steel Sheet: super duplex (high chromium) grade to ASTM A240/A240M, sheet in 2B and No.1 finishes from stock in China. SHH STEEL supplies mill-direct material with EN 10204 3.1/3.2 certificates, third-party inspection and cutting to size.
Keywords
A240 UNS S32906 sheet, S32906 sheet, S32906 stainless sheet supplier, ASTM A240/A240M S32906, S32906 sheet stock China
Equivalent Grades:
EN 1.4477 X2CrNiMoN29-7-2
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Performance
Grade Selection
Heat Treatment
Surface Finishes
Tolerances
Stock
Equivalent Grades
Related Grades
Applications and Fabrication
Testing and Inspection
Specification Mistakes
Buyer Concerns
How to Order
FAQ
Conclusion

What is ASTM A240 UNS S32906 Stainless Steel Sheet?

Technical reviewer: Jack · Updated: 2026-10-21

Equivalent grades: UNS S32906 ≈ EN 1.4477 X2CrNiMoN29-7-2.

UNS S32906 is a super duplex (high chromium) grade. S32906 is a 29Cr-6.5Ni-2Mo-0.35N super-duplex grade. Its very high chromium and nitrogen give strong resistance to ammonium carbamate in urea plants and to chloride pitting (PREN about 40), with the highest yield strength of the common duplex grades.

ASTM A240/A240M covers chromium, chromium-nickel and chromium-manganese-nickel stainless steel plate, sheet and strip for pressure vessels and general applications. Under ASTM A480, sheet is flat material under 5.00 mm thick and 600 mm or more wide, so UNS S32906 sheet is a cold-rolled 2B/2D product in thin gauges and a hot-rolled, annealed and pickled No.1 product toward the 4.75 mm end.

This page sets out the ASTM A240/A240M requirements for UNS S32906 sheet: specification summary, chemistry, mechanical properties, corrosion resistance, heat treatment, finishes and tolerances, current stock, equivalents, fabrication and testing. SHH STEEL supplies it mill-direct from China with EN 10204 3.1 certificates, optional third-party inspection and in-house cutting.

UNS S32906 sheet: specification summary

Item UNS S32906 data
Standard ASTM A240/A240M; general requirements ASTM A480/A480M
ASME counterpart SA-240 (ordered for ASME Code construction)
Product form (A480) sheet: under 5.00 mm thick, 600 mm and wider; plate 5.00 mm and over
Typical gauges 0.5–3.0 mm cold-rolled 2B/2D; 3.0–4.75 mm hot-rolled No.1
Widths 1000, 1219, 1250, 1500 mm; slit coil to order
Lengths 2000, 2438, 2500, 3000 mm or cut to size
Finishes No.1, 2D, 2B; BA and No.4 by agreement
Required tests heat analysis, tension test, hardness (and bend where the grade requires it)
Certificates EN 10204 3.1; 3.2 with third-party witness on request
Grade family super duplex

Size range. Sheet is normally cold rolled from about 0.3–0.5 mm up to 3 mm and hot rolled from about 3 mm to just under 5 mm. Coil widths of 1000, 1219, 1250 and 1500 mm are standard; slitting and cut-to-length lines produce narrower strip and exact lengths. Sheets thinner than 0.5 mm or wider than 1500 mm should be confirmed before ordering. UNS S32906 is a specialty grade made by a limited number of mills in campaign rolling. Stock covers the common sizes listed below; for project quantities or unusual sizes, plan for a mill campaign and reserve the heat early.

Chemical composition of UNS S32906 (ASTM A240/A240M)

Element wt %
C 0.030 max
Si 0.80 max
Mn 0.80–1.50
P 0.030 max
S 0.030 max
Cr 28.0–30.0
Ni 5.8–7.5
Mo 1.50–2.60
Cu 0.80 max
N 0.30–0.40

Single values are maximums unless marked min. Ranges are heat (cast) analysis limits.

PREN check (Cr + 3.3 Mo + 16 N): about 37.8 at the specification minimums and about 41.4 at mid-range. Where corrosion resistance is critical, write a minimum PREN on the order and ask for the calculated value from the heat analysis on the certificate.

Mechanical properties of UNS S32906 sheet

Condition / thickness Tensile strength, min Yield strength 0.2 %, min Elongation in 50 mm, min Hardness, max
thickness < 10 mm 800 MPa (116 ksi) 650 MPa (94 ksi) 25 % 310 HBW / 32 HRC
thickness ≥ 10 mm 750 MPa (109 ksi) 550 MPa (80 ksi) 25 % 310 HBW / 32 HRC

The minimum yield strength of 650 MPa is about 3.8 times the 170 MPa minimum of ASTM 316L. Designers use this to reduce thickness, but higher strength also means higher press loads and more springback. Mill values for production heats are usually well above the minimums; use certificate values when you calculate bending forces. Tension tests are taken in the direction stated in the standard; where a hardness limit is given, it is a maximum that confirms correct annealing.

Corrosion resistance of UNS S32906: PREN and limits

Super-duplex grades are duplex steels with PREN of about 40 or more. At the specification minimum this grade calculates to about 37.8, and a mid-range heat to about 41.4. That level gives resistance to pitting and crevice corrosion in ambient seawater, strong resistance to chloride stress-corrosion cracking and a yield strength above 500 MPa.

The higher alloy content makes super-duplex more sensitive to intermetallic phases than 2205. The solution-anneal temperature is higher and cooling must be fast, especially for heavy plate. Specify ASTM A923 Methods A, B and C, a ferrite range (commonly 35–55 % by ASTM E562) and, for critical service, an ASTM G48 Method A test at the temperature named in the project specification. Like all duplex grades, the upper service limit is about 250–300 °C.

How UNS S32906 compares with related grades

Grade Cr Ni Mo N PREN (min) YS / Rp0.2 min, MPa
UNS S32906 28.0–30.0 5.8–7.5 1.50–2.60 0.30–0.40 37.8 650
UNS S32760 24.0–26.0 6.0–8.0 3.0–4.0 0.20–0.30 37.1 550
UNS S32550 24.0–27.0 4.5–6.5 2.9–3.9 0.10–0.25 35.2 550
UNS S32520 24.0–26.0 5.5–8.0 3.0–4.0 0.20–0.35 37.1 550

Choose UNS S32906 for ambient seawater, chlorinated brines and high-chloride process water where 2205 is not sufficient, and where its high strength reduces weight. Do not use it above about 250–300 °C, and check that your fabricator has qualified super-duplex welding procedures.

The table uses specification limits, not typical mill values, so it shows the guaranteed position of each grade. Final selection should also consider product availability in the thickness you need, welding consumables, and the inspection requirements of your project.

Heat treatment and delivery condition of UNS S32906

Heat treatment: 1040–1100 °C, rapid cooling.

The higher alloy content gives faster intermetallic precipitation than 2205, so heavy plate must be water quenched. Hot forming is done between about 1000 and 1200 °C and must be followed by a full solution anneal and quench.

Surface finishes for UNS S32906 sheet

No.1 is hot-rolled, annealed and pickled, used for the 3–4.75 mm end of the sheet range. 2D is a dull cold-rolled, annealed and pickled finish that holds lubricant in deep drawing. 2B adds a light skin pass for a smoother, brighter surface and is the normal base for polishing. BA (bright annealed) and No.4 brushed finishes are available for many austenitic and ferritic grades by agreement. For highly alloyed grades, cold-rolled thin gauges are produced by fewer mills, so confirm the finish and gauge range before you fix a design.

Dimensions, tolerances and flatness

Thickness, width, length, flatness and camber tolerances follow ASTM A480/A480M. Cold-rolled sheet has tighter thickness tolerances than hot-rolled No.1 sheet. Higher-strength grades show more residual stress after slitting and laser cutting, so for laser blanks or long panels specify flatness and, where needed, tension-levelled material. Edge condition (mill or slit edge) and PVC film on one side should be stated on the order.

Ordering notes for A240 sheet. A240 refers to ASTM A480 for everything that is not grade-specific: definitions of sheet, strip and plate, dimensional tolerances, finishes, marking, retests and certification. A purchase order that says only “A240 S32906” therefore leaves several choices to the mill. State the finish (2B, 2D or No.1), the thickness tolerance basis, whether coil, slit coil or cut lengths are wanted, and whether the certificate must also show SA-240. If the sheet will be formed into vessel heads or pressure parts, say so, because some grades need specific heat-treatment records and supplementary tests that are only reported when requested. For export, also state the edition year if your specification fixes one; most mills certify to the current edition by default.

UNS S32906 sheet stock in China

Thickness (mm) Width (mm) Length (mm) Finish Approx. quantity Location
0.5 1000 / 1219 2000 / 2438 2B 100+ t China
0.8 1219 2438 2B 100+ t China
1.0 1219 / 1250 2438 / 2500 2B 100+ t China
1.5 1219 / 1500 2438 / 3000 2B 100+ t China
2.0 1219 / 1500 2438 / 3000 2B 100+ t China
3.0 1500 3000 2B / No.1 100+ t China
4.0 1500 3000 / 6000 No.1 100+ t China

Quantities are approximate and stock changes daily. Send your size list for current availability; other thicknesses, widths and cut sizes can be supplied from mill production.

Packing and logistics. Sheet is packed on wooden or steel pallets with interleaving paper or PVC film, edge protectors and waterproof wrapping, typically 2–3 t per pallet. Coil is packed eye-to-wall or eye-to-sky with steel bands. We consolidate mixed grades and sizes into one container and send loading photos with the shipping documents.

UNS S32906 equivalents in other standards

Standard Designation Comment
EN 1.4477 X2CrNiMoN29-7-2 same alloy family and limits closely matched; compare each limit on the certificate

Equivalents are close, not identical. When a project names one standard, order to that standard or ask for multiple certification and check every limit on the certificate.

Related grades by alloy family

Super duplex

PREN 40+ duplex grades for seawater and severe chlorides: A240 S32750, 1.4410 plate, 1.4501 plate, 1.4507 plate, A240 S32760, A240 S32520, A240 S32550.

Duplex and lean duplex

Duplex grades with about twice the yield strength of 316L: A240 S32205, A240 S32304, A240 S32101, 1.4462 plate, 1.4362 plate.

Super austenitic

6Mo and 7Mo grades for seawater and chloride service; upgrade path from 316L and 904L: A240 N08904, A240 S31726.

Same grade, other specification

SA-240 S32906.

Applications, forming and welding of UNS S32906

Typical uses: urea strippers and carbamate condensers, offshore hydraulic and umbilical components, seawater systems and high-strength structural parts.

Super-duplex plate needs more press force than 2205 and careful control of cutting heat. Cut by plasma, laser or waterjet and remove heat tint by pickling or grinding. For welding use a super-duplex filler such as ER2594 (AWS A5.9) or a nickel-base filler where the specification allows it. Keep the weld area clean and free of carbon-steel contamination, and pickle and passivate after welding where corrosion resistance matters.

Welding practice. Super duplex has a narrower heat-input window than 2205, typically about 0.5–1.5 kJ/mm with interpass below 100–150 °C. Use a nitrogen-bearing shielding and backing gas, and qualify with ferrite counts in weld metal and HAZ, G48 testing and Charpy tests as the project specification requires. Avoid repair welding in the same spot more than once.

Certificates, testing and receiving inspection

Every delivery carries a mill certificate to ASTM A480/A480M with heat analysis, tensile results and hardness, and the grade and standard as ordered. Supplementary tests we can arrange: ASTM A923 Methods A, B and C, ferrite count to ASTM E562, ASTM G48 Method A at the specified temperature, Charpy impact, and PMI on each plate. Third-party witness by SGS, BV, TÜV, DNV, ABS or LR is available with EN 10204 3.2 certificates.

On receipt, check marking and heat number against the certificate, measure thickness at several points and confirm the finish and edge condition before cutting.

Common mistakes when specifying UNS S32906

  • Not stating whether PREN includes tungsten.
  • Accepting heavy plate without A923 results; intermetallics are invisible on the surface.
  • Using a 2205 welding procedure for super duplex.

Each of these can be avoided by writing the requirement into the purchase order and checking it on the certificate before the material is cut.

Sourcing UNS S32906: buyer concerns and SHH STEEL solutions

Concern How SHH STEEL handles it
Sigma phase in heavy plate A923 A/B/C and G48 results reviewed per heat before cutting
PREN definition (with or without W) formula and minimum fixed in the purchase order
Small quantities across many sizes mixed thicknesses and grades combined in one shipment
Cutting and edge preparation in-house shearing, plasma, laser and waterjet cutting, bevelling
Delivery delays weekly production and shipping updates with photos

How to order UNS S32906 sheet

State the standard and edition (ASTM A240/A240M), the grade (UNS S32906), thickness, width and length or coil, finish, quantity, tolerance class, any added chemistry limits, the supplementary tests and acceptance values from your specification, the certificate type and inspection agency, and packing. Send the list to SHH STEEL and we will reply with price, available stock and lead time.

FAQ

Can I use A240 S32906 sheet for ASME Code equipment?
Only if it is certified to SA-240 as well. Most mills dual-certify A240/SA-240; tell us when the sheet is for Code construction and we will supply dual-marked material with the certificate stating both.
Is UNS S32906 equivalent to EN 1.4477 X2CrNiMoN29-7-2?
They are the same alloy designation in different standards. Limits are closely matched, but always order to the standard named in your specification or ask for multiple certification.
Should PREN include tungsten?
Only if your specification says so. Some specifications use Cr + 3.3 Mo + 16 N, others Cr + 3.3 (Mo + 0.5 W) + 16 N; write the formula and the minimum on the order.
Can I order small quantities or cut sizes?
Yes. We combine mixed thicknesses and grades into one shipment and cut plate and sheet to size in our workshop.
Which certificates and tests can you provide?
Every order ships with a mill certificate (EN 10204 3.1 type) showing heat analysis and mechanical tests. Supplementary tests and 3.2 certificates with SGS, BV, TÜV or another agency are available by agreement.

Conclusion

UNS S32906 sheet should be ordered with the points the standard leaves open written into the contract: finish, tolerance class, any extra chemistry limits and the supplementary tests your application needs. With those fixed, stock material from China is a fast and reliable route.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *