ASTM A202 Grade A Steel Plate | A202 Gr.A Cr-Mn-Si Vessel Plate supplier
What is ASTM A202 Grade A Steel ?
ASTM A202 Grade A, also searched as A202 Gr.A, A202GRA, A202GR A, A202GR.A, A202-A and SA202 Grade A, is the lower-strength grade in ASTM A202/A202M. The book is chromium-manganese-silicon alloy plate for welded boilers and pressure vessels. This page is not A202 Grade B. Grade B is 585–760 MPa. This page is not ASME SA204 Grade A. SA-204 is molybdenum plate. This page is not ASME SA203 Grade A. SA-203 is nickel plate. This page is not ASTM A515 Grade 60. A515 is carbon high-temp plate.
Tensile is 75–95 ksi / 515–655 MPa. Yield is 45 ksi / 310 MPa min. Usual practice limits thickness to about 50 mm / 2 in. Delivery is normally as-rolled. Normalized or stress-relieved plate is supplied when ordered. SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). We buy this grade from qualified Chinese mills, check chemistry and tensile against A202 / SA-202, and ship it to fabricators in the USA, Europe, Middle East, Southeast Asia, Africa and South America.
ASTM A202/A202M was later withdrawn. For ASME Boiler and Pressure Vessel Code work the name on the certificate should be SA-202 Grade A. If a drawing says A202 Grade B, we will not ship Grade A and call 515 enough.
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Grade | ASTM A202/A202M Grade A | Confirmed |
| Code counterpart | ASME SA-202 Grade A | Available |
| Other search names | A202 Gr.A, A202GRA, A202GR A, A202GR.A | Covered |
| Steel type | Killed Cr-Mn-Si alloy vessel plate | Confirmed |
| Usual delivery | As-rolled; N or SR when ordered | Confirmed |
| Tensile | 515–655 MPa (75–95 ksi) | Confirmed |
| Yield | 310 MPa (45 ksi) min | Confirmed |
| Usual thickness | About 6–50 mm | Confirmed |
| Supply role | Global steel mill sourcing partner | SHH STEEL |
| Certification | EN 10204 3.1 or 3.2 / third-party | As ordered |
This plate sits in pressure vessel steel plates. Mo sisters belong on ASME SA204. Nickel sisters belong on ASME SA203. Carbon high-temp sisters belong on ASTM A515.
Chemical Composition
Heat analysis and product analysis follow ASTM A202 / ASME SA-202 Table 1.
Heat Analysis and Product Analysis — ASTM A202 Grade A
| Element | Heat Analysis (%) | Product Analysis (%) |
|---|---|---|
| Carbon (C), max | 0.17 | 0.17 |
| Manganese (Mn) | 1.05 – 1.40 | 0.97 – 1.52 |
| Phosphorus (P), max | 0.035 | 0.035 |
| Sulfur (S), max | 0.035 | 0.035 |
| Silicon (Si) | 0.60 – 0.90 | 0.54 – 0.96 |
| Chromium (Cr) | 0.35 – 0.60 | 0.31 – 0.64 |
Grade A and Grade B share the same Mn, Si and Cr windows. The difference on chemistry is carbon: Grade A is 0.17% max, Grade B is 0.25% max. This is not a 0.5Mo heat. If the file wants molybdenum, the book is ASME SA204 Grade A. SHH STEEL prints heat analysis on every certificate and product analysis when ordered. Density is 7.85 g/cm³.
Mechanical Properties
Buyers search A202 Gr.A mechanical properties, A202GRA yield and A202 Grade A tensile.
Tensile and Yield — ASTM A202 Grade A
| Item | Requirement |
|---|---|
| Tensile strength | 75–95 ksi / 515–655 MPa |
| Yield strength, min | 45 ksi / 310 MPa |
| Elongation in 8 in. [200 mm], min | 16% |
| Elongation in 2 in. [50 mm], min | 19% |
| Density | 7.85 g/cm³ |
Do not quote 325 MPa yield on Grade A. That number belongs to Grade B. Do not treat 515–655 MPa as permission to stamp ASTM A515 Grade 70 or EN 10028-2 P265GH without checking both books.
Material Comparison
| Grade | Book | What buyers search | Swap? |
|---|---|---|---|
| ASTM A202 Grade A | A202 | A202 Gr.A / A202GRA | This page |
| ASTM A202 Grade B | A202 | A202 Gr.B | No |
| ASME SA202 Grade A | SA-202 | SA202 Gr.A | Code name |
| ASME SA204 Grade A | SA-204 | SA204 Gr.A | No |
| ASME SA203 Grade A | SA-203 | SA203 Gr.A | No |
| ASTM A515 Grade 60 | A515 | A515 Gr.60 | No |
| EN 10028-2 16Mo3 | EN 10028-2 | 16Mo3 | No |
| EN 10028-2 P265GH | EN 10028-2 | P265GH | No |
Equivalent Material Grades
| Designation | Standard / region | Notes |
|---|---|---|
| ASTM A202 Grade A / A202 Gr.A / A202GRA | A202 | Name on this page |
| ASME SA-202 Grade A | SA-202 | Code counterpart for Section VIII |
| ASTM A202 Grade B | A202 | Higher tensile sister |
| ASME SA204 Grade A | SA-204 | Mo vessel, not Cr-Mn-Si |
| ASME SA203 Grade A | SA-203 | Nickel vessel |
| ASTM A515 Grade 65 | A515 | Carbon high-temp |
| EN 10028-2 P265GH | EN 10028-2 | Carbon comparison only |
| JIS G3103 SB450 | JIS G3103 | Japanese carbon boiler comparison |
Cr-Mn-Si Pressure-Vessel Service
Buyers pick A202 Gr.A when a drawing still names ASTM A202 Grade A. Search phrases such as A202GRA, A202GR A, A202GR.A and SA202 Grade A all point here.
It is not a substitute for ASME SA204 Grade A. That grade is molybdenum. It is not a substitute for ASME SA203 Grade A. That grade is nickel. For current ASME Code work, specify SA-202 Grade A. Dual marking is possible only when both books are met.
SHH STEEL supplies this plate to fabricators in the United States, Mexico, South America, Europe, the Middle East, Africa and Asia.
Weldability
A202 Grade A is killed Cr-Mn-Si alloy vessel plate. Treat welding as production welding, and as ASME Section VIII / PED welding when the equipment is a vessel.
Qualify to the applicable code. Consumables must match the 515–655 MPa band and the Cr-Mn-Si chemistry. A carbon procedure written for ASTM A516 Grade 70 is a comparison only. A Mo procedure written for ASME SA204 Grade B is the wrong family. Preheat and interpass must stay inside the qualified WPS. The fabricator owns the WPS. SHH STEEL can share mill heat data for that review.
Heat Treatment and Delivery Condition
Usual delivery from SHH STEEL is as-rolled ASTM A202 Grade A. The specification allows the plate to be ordered normalized, stress-relieved, or both.
This is not QT from EN 10028-6 P355Q. This is not the 50 mm normalizing rule from JIS G3103 carbon grades.
If the vessel will see PWHT, say so. Simulated PWHT on test coupons is worth naming. Extra simulation, 3.2 hold points or special NDE add time. Plan about two months when those extras are on the order.
The certificate lists ASTM A202 Grade A and, when ordered, ASME SA-202 Grade A; heat number; heat analysis; product analysis when ordered; tensile; delivery condition. Certificates may be EN 10204 3.1 or EN 10204 3.2.
Dimensions
Usual supply range from SHH STEEL for A202 Gr.A Cr-Mn-Si vessel plate:
- Thickness: commonly 6 mm – 50 mm, thicker only by mill agreement
- Width: 1500 mm – 4000 mm
- Length: 3000 mm – 12000 mm
Current practice in the specification normally limits thickness to about 2 in. [50 mm]. Mo plate belongs on ASME SA204 Grade A. Nickel plate belongs on ASME SA203 Grade A.
Tolerances
Dimensional limits for ASTM A202 Grade A follow ASTM A20 / ASME SA-20 unless the purchase order names another table. Do not apply ASTM A36 structural tolerances to a Cr-Mn-Si vessel plate without writing them.
Typical thickness tolerance idea for A202 Gr.A (A20 / SA-20 reference)
| Nominal thickness (mm) | Usual minus (mm) | Usual plus (mm) |
|---|---|---|
| 6 – 16 | −0.3 | +0.8 |
| 16 – 25 | −0.4 | +0.9 |
| 25 – 40 | −0.5 | +1.0 |
| 40 – 50 | −0.8 | +1.2 |
Width on 1500–4000 mm plate is commonly held to about ±20–25 mm unless the mill quote names a tighter extra. Length on 3000–12000 mm plate is commonly held to about +50 / 0 mm or ±25 mm by mill practice. Flatness follows A20 / SA-20 unless a tighter class is written. Edge condition is mill edge or cut edge as ordered. If the vessel calculation used minimum thickness after corrosion, write the allowed minus on the RFQ. SHH STEEL will not assume a zero-minus extra on A202 Gr.A unless the order says so.
Supplementary Requirements
ASTM A202 Grade A already defines chemistry and tensile. Extra items still have to be written on the purchase order. SHH STEEL will not assume them from the grade name alone.
Code name. Write SA-202 Grade A when the equipment is ASME Code work.
Heat treatment extras. Write normalized, stress-relieved, or both when as-rolled is not enough.
Charpy details. A202 Grade A does not assume a default impact temperature. Write temperature, joules, location and orientation if impact is required.
Simulated PWHT. When the vessel will be stress-relieved, name hold temperature, hold time and cooling rate on the coupon.
Product analysis. Especially C, Mn, Si and Cr. Grade A carbon must stay at 0.17% max.
Through-thickness / Z-test. Name Z15, Z25 or Z35 when the plate will be welded in the thickness direction.
NDE. A20 / SA-20 ultrasonic extras, ASTM A435 or ASTM A578 as named. Write scanning extent and acceptance class.
Hardness. If the destination file caps hardness after rolling or after simulated PWHT, write the max HB and the test location.
HIC / SSC / NACE. Only when the equipment is sour service. A202 Grade A is not automatically NACE MR0175 / ISO 15156.
Third-party witness. EN 10204 3.2 with SGS, TÜV, BV, ABS, CCS, DNV or the inspector named. Hold points for chemistry, tensile and UT should be listed on the ITP.
Identification and stamping. Heat number, grade A202 Grade A / A202 Gr.A, SA-202 Grade A when ordered, thickness and mill logo on each plate.
Applications
| Industry | Typical components |
|---|---|
| Legacy A202 drawings | A202 Gr.A / A202GRA shells and drums |
| Welded pressure vessels | A202 Grade A courses from SHH STEEL |
| ASME Code dual-name | A202 Gr.A / SA-202 Grade A when both books fit |
| Comparison vs Mo plate | A202GRA next to ASME SA204 Grade A |
A202 Grade A is the plate for a file that still names ASTM A202 at 515–655 MPa. It is the wrong plate for 0.5Mo service. That work is ASME SA204 Grade A. It is the wrong plate for nickel low-temp service. That work is ASME SA203 Grade A.
Supply Capability
SHH STEEL sources ASTM A202 Grade A from first-line Chinese mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron & Steel, Baosteel, Xinyu, Xingcheng, Yongjin, Tsingshan, TISCO (Taiyuan), Jiuquan (JISCO), Lianzhong, Zhangpu and Baoxin, plus other qualified mills when the size or heat-treatment route requires it.
Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.
Usual stock and rolling thickness: 8 mm, 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 32 mm, 36 mm, 40 mm, 50 mm, thicker by mill agreement.
Processing: CNC or flame cutting, bevel, flattening, UT to the named class.
Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.
Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.
Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.
Global Delivery & Markets
SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN, DIN, JIS and GB steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.
SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.
Typical lead time: ex-stock 5–7 days; standard rolling about 45–60 days; normalizing / simulated PWHT / 3.2 about 2 months.
Why Choose SHH STEEL
Experience on this grade is simple: keep Grade A and Grade B apart, keep A202 away from SA-203 and SA-204, and put SA-202 Grade A on Code certificates. SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) prices A202 Gr.A from first-line mills, reports Cr-Mn-Si chemistry, records as-rolled or ordered heat treatment, and issues 3.1 as standard or 3.2 when specified.
We keep the grade on the order. A202 Grade A is not A202 Grade B. A202GRA is not ASME SA204 Grade A. A202GR A is not ASTM A515 Grade 60. If the drawing says Grade B, we will not ship Grade A and call 515 close.
FAQ
-
What is A202 Grade A steel plate?
- ASTM A202 Grade A, also searched as A202 Gr.A, A202GRA, A202GR A, A202GR.A and SA202 Grade A, is a Cr-Mn-Si alloy pressure-vessel plate. Tensile is 515–655 MPa and yield is 310 MPa min. Usual supply is as-rolled, commonly up to about 50 mm. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
-
Is ASTM A202 still valid?
- ASTM A202/A202M was later withdrawn. Old drawings still search A202 Grade A. For ASME Code work, specify SA-202 Grade A. SHH STEEL can dual-name when the heat meets both books.
-
What is the equivalent of A202 Gr.A?
- The Code counterpart is SA-202 Grade A. Related comparisons are A202 Grade B, SA-515 and P265GH. Dual marking is possible only when both books are fully met.
-
How is A202 Grade A different from Grade B?
- Grade A is 515–655 MPa with 0.17% C max. Grade B is 585–760 MPa with 0.25% C max. Same Mn, Si and Cr windows.
-
How is A202GRA different from SA204 Grade A?
- SA-204 is molybdenum vessel plate. A202 is Cr-Mn-Si vessel plate. Do not ship one against the other.
-
an SHH STEEL issue EN 10204 3.2 for A202GRA?
- Yes. EN 10204 3.1 is standard. EN 10204 3.2 is arranged with SGS, TÜV, BV, ABS, CCS, DNV or the inspector named on the order.
Conclusion
ASTM A202 Grade A Steel Plate is Cr-Mn-Si alloy pressure-vessel plate at 515–655 MPa tensile and 310 MPa yield. Whether the inquiry says ASTM A202 Grade A, A202 Gr.A, A202GRA, A202GR A, A202GR.A, A202-A or SA202 Grade A, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplies plate with A202 Grade A chemistry, recorded delivery condition, and EN 10204 3.1 or 3.2 certification.
SHH STEEL supplies ASTM A202 Grade A / A202 Gr.A Cr-Mn-Si Vessel Plate to the USA, Mexico, South America, Europe, the Middle East, Africa and Asia for work that actually names this grade.
Contact SHH STEEL for mill rolling, stock inquiry, cutting, bevel, 3.2 inspection or a worldwide quotation.
ASTM A202 Grade A Steel Plate, A202 Gr.A, A202GRA, A202GR A, Cr-Mn-Si vessel plate, A202 Gr.A supplier, SHH STEEL