JIS G3101 Steel Structural Profiles
SHH STEEL supplies JIS G 3101 rolled-steel channels for general structures, most often SS400, with other G 3101 grades when specified. Dimensions typically follow JIS G 3192 and are designated in millimetres, for example 150×75, 200×80, 250×90, or 300×90. These JIS channels are not equivalent to ASTM C, UPN, or GB/T 706 channels by depth alone. Sizes and certificates are confirmed per inquiry.
-
JIS G 3101 SS540 Steel Channel
JIS G 3101 SS540 steel channel is a general-structure section named for a 540 N/mm² tensile minimum, not for a 540 N/mm² yield. Yield is 400 N/mm² up to 16 mm and 390 N/mm² between 16 mm and 40 mm, based on flange thickness t2. Mechanical properties stop at 40 mm. Dimensions follow the JIS G 3192 Table 12 channel series. This page is SS540 only, not SS400, SS490 or SM490. SHH STEEL reviews grade, designation, edition and certificate requirements before quoting.View More -
JIS G 3101 SS490 Steel Channel
JIS G 3101 SS490 steel channel is a general-structure section named for a 490–610 N/mm² tensile range, not for a 490 N/mm² yield. Minimum yield is 285 N/mm² up to 16 mm and 275 N/mm² between 16 mm and 40 mm, based on flange thickness t2. Dimensions follow the JIS G 3192 Table 12 channel series. This page is SS490 only, not SS400, SS540 or SM490. SHH STEEL reviews grade, designation, edition and certificate requirements before quoting.View More -
JIS G 3101 SS400 Steel Channel
JIS G 3101 SS400 steel channel is a general-structure channel named for a 400–510 N/mm² tensile range, not a 400 N/mm² yield. Minimum yield is 245 N/mm² up to 16 mm. Dimensions follow the JIS G 3192 standard channel series. The ordered edition governs. SHH STEEL reviews grade, designation, edition and certificate requirements before quoting.View More
JIS G3101 Steel Structural Profiles
C Channels and U Channels
SHH STEEL supplies hot-rolled steel channel profiles for frames, bracing, and equipment support. Material is specified to the project standard—for example ASTM A36, A572, or A529; ASME SA-36; EN 10025-2; GB/T 700 or GB/T 1591; JIS G 3101; ISO 630-1; or GOST 8240 practice. Dimensional series are stated separately and may include ASTM A6 C and MC channels (for example C6×8.2, C8×11.5, or C12×20.7); EN 10365 UPN and UPE (for example UPN 200 or UPE 200) with tolerances to EN 10279; GB/T 706 channels such as 16a and 20a; and JIS G 3192 channels such as 150×75 or 200×80. A grade such as ASTM A36 may be furnished as UPN or UPE when so specified and certified; C, UPN, and GB/JIS designations are not interchangeable by depth alone. Sizes and certificates are confirmed per inquiry.
Customers typically search this category as C channel, U channel, steel channel, C channel steel or U channel steel, and by series names such as MC channel, UPN, UPE, PFC (parallel flange channel) and taper flange channel. This category covers ASTM A6 C and MC channels, EN 10365 UPN and UPE, British-practice PFC, GB/T 706 channels and JIS G 3192 channels, furnished to the material standard named on the order. C, MC, UPN, UPE, PFC, GB/T 706 and JIS designations are not interchangeable by depth alone.