JIS G 3101 SS490 Steel Channel
What is JIS G 3101 SS490 Steel Channel?
JIS G 3101 SS490 steel channel is a hot-rolled channel in rolled steel for general structure, grade SS490. The material standard is JIS G 3101, Rolled steels for general structure. The chemical and mechanical figures on this page are those of the issued JIS G 3101:2015 tables. JIS G 3101:2024 is the current listed edition, issued 20 February 2024; the edition named on the order governs acceptance. Dimensions, mass and tolerances for the section itself are those of JIS G 3192:2024. SHH STEEL supplies these channels to the grade, designation, edition and certificate named on the order.
The number in the grade name is the specified tensile strength in N/mm² (1 N/mm² = 1 MPa), not a yield class. Formal grades in the standard are SS330, SS400, SS490 and SS540. This page is SS490. It is not the JIS G 3101 SS400 steel channel page, not a JIS G 3106 SM490 steel channel, and not a data sheet for SS490 steel plate.
The standard designation is the four-part size H×B×t1×t2, for example 150×75×6.5×10 or 380×100×13×20, where H is the depth, B the flange width, t1 the web thickness and t2 the flange thickness. The standard allows thickness to be shown as t1 only, but this page lists both thicknesses because several depths share the same H and B with more than one t1×t2 combination. The designation is not an American C or MC prefix, and a 200 mm Japanese channel is not a UPN 200, a UPE 200 or a Chinese channel of similar depth.
These channels are filed under JIS G3101 steel channel profiles in the steel channel profiles category of steel structural profiles. The same grade in plate form is listed separately; do not use a plate page as a channel data sheet, and do not copy a plate elongation-reduction rule onto a channel certificate.
SS490 channels are used for building and general industrial framing when the specification names this Japanese general-structure grade. JIS G 3101 does not specify a Charpy test for SS490. The grade is not a pressure-vessel or nuclear safety material, and it is not a substitute for JIS G 3106 SM490 when a welded-structure grade and a defined impact quality are what the order requires.
Material, Dimensions and Tolerances for SS490 Channels
Keep the material specification and the dimensional standard distinct. JIS G 3101 is the material standard. The ladle-analysis and mechanical figures used here are those of the issued JIS G 3101:2015 tables (Table 2 and Table 3). JIS G 3101:2024 is the current listed edition; the edition named on the order governs acceptance. JIS G 3192:2024 is the shape standard for these channels. A documented special combination is valid only if every requirement of each named standard is met. Matching a nominal 200 mm or 8 in depth is not a substitution method. JIS G 3101 does not require a fully killed practice and does not require the product to be normalized. If a heat treatment has been applied, the standard gives sampling rules for that heat-treated lot; it does not turn normalizing into the delivery condition of the grade.
SS490 Channel Sizes: JIS G 3192 Standard Channel Series
The table lists the 16 standard channel sizes in JIS G 3192:2024 Table 12, with designation H×B×t1×t2, the tabulated root and toe radii r1 and r2, theoretical area and theoretical mass. Use the table to identify and estimate, not as a rolling programme for SS490. Mid-range sizes such as 150×75 and 200×90 are the usual enquiry core; the 75×40 row and the 380×100 rows should be confirmed size by size.
The tabulated sizes are the complete standard series in Table 12. They are representative dimensions; other section dimensions may be used by agreement between the parties, but this page does not invent rows that Table 12 does not list.
75×40×5×7 has a 7 mm flange, so the 285 N/mm² yield band applies. 300×90×12×16 has a 16 mm flange and remains in that first band. 380×100×13×16.5 and 380×100×13×20 have 16.5 mm and 20 mm flanges, so the minimum yield is 275 N/mm², not 285 N/mm². The 255 N/mm² and 245 N/mm² bands belong to thicker material and do not appear among these Table 12 flanges. 150×75×6.5×10 and 150×75×9×12.5 share the same depth and flange width but are different sections.
16 standard sizes, from 75×40×5×7 to 380×100×13×20.
Swipe horizontally to view all dimensions.
SS490 Chemical Composition for Channels (Table 2)
The ladle analysis shall comply with Table 2 of JIS G 3101, using the issued 2015 figures given below. JIS G 3101:2024 is the current listed edition; the edition named on the order governs. The SS490 row is the same row as SS330 and SS400: only phosphorus and sulfur have maxima. Carbon and manganese are shown as having no tabulated requirement. Silicon is not a tabulated column on that row. This page does not invent carbon or manganese windows from mill catalogues or from the SS540 row.
Elements shown as having no tabulated requirement, and alloying elements not listed in Table 2, may be added as necessary. Table 2 is a ladle-analysis table. The issued 2015 text recovered for this page specifies ladle analysis only and does not give a separate numeric product-analysis table. This page does not invent one.
SS490 Channel Mechanical Properties: Yield, Tensile and Elongation
Mechanical properties of SS490 plates, strip, flats and sections follow Table 3 of the issued JIS G 3101:2015 text, which is a single mechanical table that includes plate, strip, flat, section and bar rows. These channels use the plate, strip, flat and section rows, not the bar rows. The recovered 2015 Table 3 notes do not add an upper-yield or 0.2% proof-stress instruction, and this page does not add one. Thickness for a section is the thickness at the test-piece location; on this page the usual basis for selecting a yield band is the flange thickness t2.
A 2015 Table 3 note reduces the No. 4 elongation on plates thicker than 90 mm; that is a plate rule and is not extended here to invent a section value. This page does not reprint a No. 4 elongation percentage, because that figure was not recovered from the issued 2015 table image. The 255 N/mm² and 245 N/mm² yield bands do not appear among the tabulated G 3192 sizes on this page, all of which have a flange thickness of 20 mm or less. JIS G 3101 does not specify Charpy absorbed-energy values. The bend test may be omitted unless the purchaser specifies it; the steel still has to satisfy the bendability requirement, and the outside of the bend piece must be free of cracks.
Delivery, Inspection and Identification of SS490 Channels
SS490 channels are commonly supplied as-rolled. If not otherwise specified at the time of order, the default inspection document is a JIS G 0415 inspection certificate 3.1. The document should identify JIS G 3101 and its edition, the grade SS490, the G 3192 designation, the heat number, the ladle analysis and the tensile results. An EN 10204 type 3.1 request is usually satisfied by that 3.1 document; type 3.2 or nominated third-party attendance can be added when the order requires it. Length is a matter for the rolling programme and the order, often in the region of 6–12 m; those lengths are enquiry ranges, not a stock list. A SS490 plate certificate does not identify a channel.
Weldability and Surface Condition of SS490 Channels
SS490 is a general structural steel intended to be welded, bolted or otherwise fabricated when the procedure is suitable for the thickness and the joint. JIS G 3101 does not table a carbon-equivalent limit or a Charpy value for this grade. This page does not prescribe a welding procedure or a preheat chart. The as-rolled surface is mill scale. Blast, paint or galvanizing is an order option. Cutting, punching, forming or coating can be reviewed when that specification is sent with the enquiry.
JIS G 3192 Shape Tolerances and Theoretical Mass
Dimensional and mass tolerances for these channels are those of JIS G 3192, not of JIS G 3101 itself. This article does not reproduce the millimetre tolerance tables; acceptance is against the edition of G 3192 named on the order. Root and toe radii in the tables are tabulated standard dimensions in this series. Settlement on theoretical or weighed mass should follow the contract.
Applications and Service Limits
SS490 steel channels are used where a general structural L-section in this tensile class is specified: frames, bracing, towers, shops and fabrications that name JIS G 3101 SS490 rather than SS400, SS540 or a welded-structure grade such as SM490. The grade is not specified here as a pressure-vessel or nuclear-safety material. Durability comes from the coating or fire-protection system named on the order, not from the SS490 designation itself.
SS490 Channel Compared with SS400, SM490 and Other 50 ksi-Class Grades
JIS G 3101 SS400 steel channel uses the same G 3192 Table 12 series at a lower tensile range (400–510 N/mm²) and a lower yield band (245 N/mm² up to 16 mm). An SS400 certificate is not an SS490 certificate.
SS540, also in JIS G 3101, is a higher-tensile grade (540 N/mm² minimum) with a 40 mm thickness cap and a tighter chemistry row (carbon and manganese maxima). It is not this data sheet.
JIS G 3106 SM490 steel channel also uses the G 3192 channel series, but SM490 is a welded-structure grade under a different standard, with its own chemistry and impact-quality family. The “490” in SM490 is not a licence to substitute it for SS490, or the other way around.
Near-Equivalents: Not Automatic Substitutes
The comparisons above are for orientation. They are not a licence to substitute one grade, one certificate or one shape system for another. SS490 chemistry is only P and S have maxima. Use the sister pages for their own standards.
Stock and Supply of SS490 Steel Channels from SHH STEEL
SHH STEEL supplies JIS G 3101 SS490 steel channels as an export trading house, coordinating mill production and project procurement. The useful work on this product is to keep the tensile-named SS490 designation from being read as a 490 N/mm² yield, to keep SS490 distinct from SS400, SS540 and from JIS G 3106 SM490, to apply the yield band to the flange thickness rather than the channel depth, and to align the inspection document with the edition named on the order before a rolling programme is committed.
Sizes, lengths and certificates are confirmed per enquiry. The table is the standard G 3192 Table 12 series, not a list of pieces on the floor. Mid-range 150×75 and 200×90 sizes are the usual core; the 75×40 row and the 380×100 rows are confirmed per line.
Sections can be sourced from mills that SHH STEEL buys from, including Masteel, Rizhao Steel, Laiwu (Shandong Steel Laiwu) and Tung Ho Steel, among others when the programme matches the order. Those mills do not each roll every Table 12 size in SS490. If cutting, punching, forming or a coating system is required, include that specification for review. Export packing and container loading can be arranged to the packing list agreed for the shipment.
SS490 Steel Channel FAQs
-
Is SS490 a 490 N/mm² yield grade?
- No. The 490 in the grade name is the lower end of the specified tensile range, 490–610 N/mm². Minimum yield is 285 N/mm² for flange thickness up to 16 mm, and 275 N/mm² between 16 mm and 40 mm. Do not read the grade number as a yield class.
-
Is an SS400 channel automatically acceptable as SS490?
- No. SS400 and SS490 share the same G 3192 Table 12 series, but they are different grades with different tensile and yield bands. An SS400 certificate is not an SS490 certificate.
-
Is SS490 the same as SM490?
- No. SM490 is a JIS G 3106 welded-structure grade, not a JIS G 3101 general-structure grade. The shared “490” tensile class does not make the certificates interchangeable.
-
Which thickness is used to pick the yield band?
- Thickness for a section is the thickness at the test-piece location. On this page the usual basis for selecting a yield band is the flange thickness t2, not the channel depth H. A 380×100 channel with a 16.5 mm or 20 mm flange uses the 275 N/mm² band, not the 285 N/mm² band.
-
Does JIS G 3101 require a Charpy test for SS490?
- No. JIS G 3101 does not specify Charpy absorbed-energy values for SS490. If an impact test is required, it has to be named on the order; it is not implied by the grade name.
Request a Quotation for JIS G 3101 SS490 Steel Channel
JIS G 3101 SS490 steel channel is a general-structure section with a 490–610 N/mm² tensile range and 285 N/mm² minimum yield up to 16 mm (275 N/mm² between 16 mm and 40 mm, based on flange thickness). Nominate the JIS G 3192 channel size (H×B×t1×t2) and the material to JIS G 3101:2024 (or the edition on the order). The table is the standard Table 12 series, used as reference dimensions, not a rolling list. Send the size list, edition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.