GB/T 16270 Q960C quenched and tempered high-strength structural steel plate, 960 MPa yield, SHH STEEL

Q960C QT Carbon Steel Plate GB/T 16270 Supplier

GB/T 16270 Q960C is quenched-and-tempered carbon structural plate with 960 MPa minimum yield and 0°C impact toughness. SHH STEEL supplies Q960C QT plate mill-direct for cranes, mining frames and heavy fabrication.
Keywords
Q960C, Q960C steel plate, GB/T 16270 Q960C, Q960C QT plate, Q960C carbon steel plate, Q960C supplier, S960Q, ASTM A514, GB/T 16270 QT plate
Equivalent Grades:
GB/T 16270 Q960C / EN 10025-6 S960QL / ASTM A514 (over, not direct) / JIS G3128 SHY785 (lower) — Material Specification: GB/T 16270 — Delivery: QT
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
Equivalent Material Grades
QT Structural Service
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Applications
Supply Capability
Global Delivery and Markets
Why Choose SHH STEEL
FAQ
Conclusion

What is Q960C QT Carbon Steel Plate GB/T 16270?

Q960C, also searched as GB/T 16270 Q960C, Q960C QT plate, Q960C carbon steel plate, Q960C steel plate and Q960C quenched and tempered plate, is the 960 MPa quality-grade-C grade in GB/T 16270. That standard covers high-strength structural steel plate delivered quenched and tempered. Q is the yield symbol, 960 is the thin-plate minimum yield in MPa, and C is the quality letter for Charpy impact at 0°C.

Q960C sits above Q890C. About 139 ksi on a US drawing is the same yield number. Equipment builders use it on crane booms, mine-truck bodies and trailer goosenecks that were too heavy in 690 or 890 MPa plate. It is still a QT carbon plate, not a stainless grade and not a pressure-vessel grade. Not every mill will roll 960 MPa on thick plate.

Quality grade C means the impact test is at 0°C. D is −20°C. E is −40°C. F is −60°C. Q960C is the right letter for temperate fabrication and mild outdoor service. If the drawing shows winter design at −40°C, the letter is E, not C.

The closest European name is EN 10025-6 S960Q. Both are about 960 MPa QT plate tested at 0°C. S960QL is −40°C and lines up with Q960E. S960QL1 is −60°C and lines up with Q960F. On the US side, A514 Grade Q is only 100 ksi / 690 MPa. There is no standard ASTM 960 MPa plate grade. Dual mark only when both books are fully met. See EN 10025-6 steel plate.

SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. We source Q960C from first-line QT mills, print heat analysis and product analysis when ordered, and ship plate to fabricators in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Related pages include high strength low alloy plates and structural steel plates.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Plate book GB/T 16270 Q960C Confirmed
Other search names Q960C QT plate, Q960C carbon steel plate Covered
Delivery condition Quenched and tempered Confirmed
Yield, thin plate 960 MPa min Confirmed
Quality grade C, impact at 0°C Confirmed
EN comparison S960Q, 0°C Comparison, not a swap
US comparison A514 is 690 MPa Not a twin
Product analysis GB/T 222 column when ordered Confirmed
Not the same strength Q890C Do not substitute
Supply role Global steel mill sourcing partner SHH STEEL
Certification EN 10204 3.1 or 3.2 As ordered

Nearby pages that buyers compare, but must not swap blindly, include S960Q, S960QL and A514 Gr.Q.

Chemical Composition

Heat analysis is the mill ladle table in GB/T 16270. Product analysis, when ordered, follows GB/T 222. Q960C is a low-alloy QT carbon plate. Mills add Nb, V, Ti or Al for grain refinement, and may add Cr, Ni, Mo or B by thickness. Boron is common on 960 MPa heats. The certificate shows the elements actually used.

Heat Analysis and Product Analysis — GB/T 16270 Q960C

Element Heat analysis (%) Product analysis (%)
Carbon (C), max 0.20 0.22
Silicon (Si), max 0.80 0.85
Manganese (Mn), max 2.00 2.08
Phosphorus (P), max 0.025 0.030
Sulfur (S), max 0.015 0.018
Copper (Cu), max 0.50 0.55
Chromium (Cr), max 1.50 1.55
Nickel (Ni), max 2.00 2.05
Molybdenum (Mo), max 0.70 0.75
Boron (B), max 0.005 0.006
Vanadium (V), max 0.12 0.13
Niobium (Nb), max 0.06 0.07
Titanium (Ti), max 0.05 0.06
Aluminium (Als), min when used 0.015 0.010

Grade C allows a slightly wider phosphorus and sulfur window than grade E or F. That is acceptable at 0°C. It is not a reason to use Q960C on a −40°C drawing. If the file needs product analysis, SHH STEEL prints both columns and the thickness band used for the mechanical test.

Do not treat this chemistry as weathering plate. Do not treat it as S355JR.

Mechanical Properties

Buyers search Q960C mechanical properties, Q960C yield strength, GB/T 16270 Q960C tensile and Q960C impact 0°C.

Tensile and impact — GB/T 16270 Q960C

Thickness Yield min Tensile Elongation min Impact
≤ 50 mm 960 MPa 980–1150 MPa 10% 0°C, grade C
> 50–100 mm 880 MPa 900–1150 MPa 10% 0°C, grade C
> 100 mm as standard table as standard table 10% 0°C, grade C

Impact energy is the average of three longitudinal Charpy V-notch specimens. One value may fall below the table, but not below 70% of that value. A typical production heat is at or above 34 J at 0°C. Write a higher energy on the order if the owner requires it.

Yield steps down with thickness. A 960 MPa name on 16 mm plate is not the minimum on a 60 mm flange. 960 MPa is about 139 ksi. ASTM A514 is 100 ksi and is not this number. SHH STEEL quotes the thickness band on the offer.

Density is 7.85 g/cm³. Hardness after temper is a mill control, not a design value. Z15, Z25 or Z35 through-thickness tensile is an extra.

Material Comparison

Grade Book Delivery Yield, thin plate Impact Swap?
Q890C GB/T 16270 QT 890 MPa 0°C Lower sister
Q960C GB/T 16270 QT 960 MPa 0°C This page
Q960D GB/T 16270 QT 960 MPa −20°C Colder sister
Q960E GB/T 16270 QT 960 MPa −40°C Colder sister
Q960F GB/T 16270 QT 960 MPa −60°C Colder sister
S960Q EN 10025-6 QT 960 MPa 0°C Closest comparison
S960QL EN 10025-6 QT 960 MPa −40°C No, unless E
A514 Gr.Q ASTM A514 QT 690 MPa Different Lower yield

Equivalent Material Grades

There is no official one-to-one substitute for Q960C. What buyers compare is a 960 MPa QT plate tested at 0°C.

The usual European pair is S960Q. S960QL is colder and closer to Q960E. S890Q is one strength step lower. In the United States there is no standard 960 MPa plate grade. A514 Grade Q is 100 ksi / 690 MPa. A572 Gr.65 is only 65 ksi. SHH STEEL will not stamp S960Q or A514 on a Q960C certificate unless the purchase order names both books and both tables are met.

Designation Country / region Standard Notes
Q960C China GB/T 16270 Name on this page
Q960D / Q960E / Q960F China GB/T 16270 Colder quality letters
Q890C China GB/T 16270 Lower yield sister
A514 Gr.Q USA ASTM A514 100 ksi, lower yield
A572 Gr.65 USA ASTM A572 65 ksi, lower yield
S960Q Europe EN 10025-6 0°C QT comparison
S960QL Europe EN 10025-6 −40°C, closer to Q960E
SM570 Japan JIS G3106 Well below this yield

QT Structural Service

Buyers pick Q960C when a welded frame, boom or chassis wants 960 MPa yield, QT delivery and impact at 0°C. Search phrases such as Q960C steel plate, GB/T 16270 Q960C and Q960C QT plate all point here.

It is the wrong plate for a −40°C mine site. That work is Q960E. It is the wrong plate for an 890 MPa file that was sized on Q890C. Raising the grade without a design check can change weld procedure and deflection. It is the wrong plate for a 100 ksi US file. That work is A514 Grade Q. It is the wrong plate for a pressure vessel. That work sits on ASTM A516 or pressure vessel steel plates.

SHH STEEL supplies this plate when the drawing names GB/T 16270 and quality grade C at 960 MPa.

Weldability

Q960C is weldable QT carbon plate. Carbon is controlled, but the plate has already been quenched and tempered, and many heats use boron. A procedure written for S355JR is not a Q960C procedure. A procedure qualified only on Q690C or Q890C may be under-matched.

Typical consumables are matching 960 MPa low-hydrogen electrodes or wires, qualified on a QT 960 MPa family. E7018-class electrodes are under-matched if the joint must develop full plate strength. A procedure written for S960Q is the usual starting point. An A514 procedure is a lower-strength reference, not a finished WPS for this grade.

Preheat follows thickness, hydrogen and the approved WPS. Interpass temperature should stay below the mill temper range, or local yield can drop. After heavy cold forming, a stress relief may be required. The fabricator owns the WPS. SHH STEEL can share mill heat data, product analysis and carbon equivalent for that review.

Heat Treatment and Delivery Condition

Usual delivery from SHH STEEL for Q960C is quenched and tempered. Austenitize typically in the 880–930°C range, quench, then temper in the window that holds 960 MPa yield and the 0°C impact. Exact temperatures stay on the mill process sheet.

Do not order Q960C as as-rolled or TMCP unless the contract leaves GB/T 16270. ASTM A514 is not a delivery instruction for this page. Stress relief after fabrication, if used, must stay below the original temper temperature.

The certificate lists GB/T 16270 Q960C, heat number, heat analysis, product analysis when ordered, tensile by thickness band, and 0°C impact. Certificates may be EN 10204 3.1 or EN 10204 3.2. Dual marking to S960Q is available only when both books are fully met.

Dimensions

Usual supply range from SHH STEEL for Q960C QT carbon steel plate:

  • Thickness: commonly 8 mm – 40 mm, heavier plate to 50 mm by enquiry
  • Width: 1500 mm – 2800 mm
  • Length: 3000 mm – 12000 mm

Cut-to-size webs, flanges and base plates are available. Browse more sizes on structural steel plates and the products index.

Tolerances

Dimensional limits for Q960C follow GB/T 709 unless the purchase order names another table.

Typical thickness tolerance idea for Q960C QT plate

Nominal thickness (mm) Usual minus (mm) Usual plus (mm)
8 – 10 −0.3 +0.8
10 – 20 −0.4 +0.9
20 – 30 −0.4 +1.0
30 – 40 −0.5 +1.1
40 – 50 −0.5 +1.2

Width on 1500–2800 mm plate is commonly held to about ±20–25 mm unless a tighter extra is named. Length on 3000–12000 mm plate is commonly held to about +50 / 0 mm or ±25 mm by mill practice. Flatness after QT follows the agreed class. SHH STEEL will not assume a zero-minus extra on Q960C unless the order says so.

Supplementary Requirements

Q960C already defines 960 MPa yield, QT delivery and 0°C impact. Extra items still have to be written on the purchase order.

Book name. Write GB/T 16270 Q960C. Do not write only Q960C.

Impact. Grade C is 0°C. Write a higher energy if the owner requires it.

EN or US comparison. Write S960Q or A514 only if dual mark is required and both tables are met.

Product analysis. Write it if the file needs the second chemistry column.

Through-thickness. Z15, Z25 or Z35 when the joint is loaded through the thickness.

NDE. UT to GB/T 2970 or the named class.

Heat-treatment record. QT temperatures when the inspector asks.

Identification. Heat number, Q960C, thickness and mill logo.

Third-party witness. EN 10204 3.2 with SGS, TÜV, BV, ABS or the inspector named.

Applications

Industry Typical components
Construction machinery Q960C QT booms, frames and bases
Mining equipment Q960C chassis and body plate from SHH STEEL
Cranes and port equipment Q960C webs and flanges
Heavy trailers Q960C goosenecks
Comparison vs S960Q Q960C next to S960Q
Comparison vs S960QL Q960C next to S960QL
Comparison vs A514 Q960C next to A514 Gr.Q

Q960C is the plate for a 960 MPa QT file tested at 0°C. It is the wrong plate for a painted warehouse that can use S355JR. It is the wrong plate for an 890 MPa member that was already sized.

Supply Capability

SHH STEEL sources Q960C from first-line Chinese QT mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron and Steel, Baosteel, Xinyu, Xingcheng and other qualified mills when the size requires it.

Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.

Usual rolling thickness: 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 40 mm. Heavier plate is confirmed before order.

Processing: CNC or flame cutting, bevel, flattening, shot blast, UT to the named class.

Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.

Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.

Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.

Global Delivery and Markets

SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply GB, ASTM, ASME, EN, DIN and JIS steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.

SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.

Typical lead time: ex-stock 5–7 days when plate is in yard; standard QT rolling about 40–50 days; 3.2 inspection about 50–60 days.

Why Choose SHH STEEL

SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. For Q960C that means mill-direct QT price, not a multi-layer stockist mark-up. We buy from mills that already run the 960 MPa quench-and-temper route, so the heat carries the 0°C impact without a second upgrade charge.

Delivery is short when the size is in rolling range: ex-stock 5–7 days, standard heat about 40–50 days, 3.2 inspection about 50–60 days. Cutting, bevel and UT can run in the same window. FOB Shanghai is the main term. CIF to US West, US Gulf, Rotterdam, Jebel Ali and Singapore is quoted on the same file.

Experience on this grade is simple: print GB/T 16270 Q960C, keep the QT route, and do not ship Q890C or a silent S960Q stamp as Q960C. We will not change C to E on the certificate to win an order, and we will not treat Q960C as S355. If the drawing needs −40°C, we will move the inquiry to Q960E and keep the price on the right grade.

FAQ

What is Q960C steel plate?
Q960C in GB/T 16270 is quenched-and-tempered carbon structural plate with 960 MPa minimum yield on thin plate and Charpy impact at 0°C. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
Is Q960C the same as Q890C?
No. Both are QT plate tested at 0°C. Q960C yields at 960 MPa. Q890C yields at 890 MPa.
What is the US equivalent of Q960C?
There is no official ASTM twin at 960 MPa. A514 is 100 ksi / 690 MPa, well below this number. SHH STEEL does not dual-mark A514 unless both books are met.
Is Q960C the same as S960Q?
They are the usual comparison pair: both are about 960 MPa QT plate tested at 0°C. Dual mark only when both books are fully met. S960QL is colder and closer to Q960E.
What thickness can SHH STEEL supply?
Common rolling is 8 mm to 40 mm. Plate to 50 mm is quoted by enquiry. Yield on plate over 50 mm is lower than the 960 MPa thin-plate number.
What is the delivery time for Q960C?
Ex-stock about 5–7 days when plate is in yard. Standard QT rolling about 40–50 days. 3.2 inspection about 50–60 days.

Conclusion

Q960C QT carbon steel plate to GB/T 16270 is 960 MPa quenched-and-tempered structural plate with impact at 0°C. The nearest European comparison is S960Q. ASTM A514 is 690 MPa and is not a substitute. Whether the inquiry says Q960C, GB/T 16270 Q960C, Q960C QT plate or Q960C carbon steel plate, SHH STEEL as a global steel mill sourcing partner supplies plate with Q960C chemistry, heat and product analysis as ordered, GB/T 709 tolerances and EN 10204 3.1 or 3.2 certification.

SHH STEEL supplies Q960C QT Carbon Steel Plate to the United States, Europe, the Middle East, Africa, Asia and the Americas for work that actually names this grade.

Contact SHH STEEL for mill rolling, QT route, cutting, UT, 3.2 inspection or a worldwide quotation.

Q960C, Q960C steel plate, GB/T 16270 Q960C, Q960C QT plate, Q960C carbon steel plate, Q960C supplier, SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X