GB/T 16270 Q800E quenched and tempered high-strength structural steel plate, −40 °C impact, SHH STEEL

Q800E QT Carbon Steel Plate GB/T 16270 Supplier

GB/T 16270 Q800E is quenched-and-tempered carbon structural plate with 800 MPa minimum yield and −40°C impact toughness. SHH STEEL supplies Q800E QT plate mill-direct for cranes, mining frames and cold-region fabrication.
Keywords
Q800E, Q800E steel plate, GB/T 16270 Q800E, Q800E QT plate, Q800E carbon steel plate, Q800E supplier, S690QL, S890QL, GB/T 16270 QT plate
Equivalent Grades
GB/T 16270 Q800E / EN 10025-6 S700QL (cold) / JIS G3128 SHY785 — Material Specification: GB/T 16270 — Delivery: QT; -40℃
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
Equivalent Material Grades
QT Structural Service
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Applications
Supply Capability
Global Delivery and Markets
Why Choose SHH STEEL
FAQ
Conclusion

What is Q800E QT Carbon Steel Plate GB/T 16270 ?

Q800E, also searched as GB/T 16270 Q800E, Q800E QT plate, Q800E carbon steel plate, Q800E steel plate and Q800E quenched and tempered plate, is the 800 MPa quality-grade-E grade in GB/T 16270. That standard covers high-strength structural steel plate delivered quenched and tempered. Q is the yield symbol, 800 is the thin-plate minimum yield in MPa, and E is the quality letter for Charpy impact at −40°C.

Q800E is the grade cold-region crane and mine-truck builders use when the member was sized at 800 MPa and the specification names −40°C. C is 0°C. D is −20°C. E is −40°C. F is −60°C. About 116 ksi on a US drawing is the same yield number. A Q800C heat tested only at 0°C cannot be stamped E.

EN 10025-6 has no S800 grade. S690QL is 690 MPa at −40°C, one step lower. S890QL is 890 MPa at −40°C, one step higher. S890Q is 890 MPa at 0°C and is warmer. On the US side, A514 Grade Q is 100 ksi / 690 MPa, also one step lower, and it does not carry an E letter. Dual mark only when both books are fully met. See EN 10025-6 steel plate.

SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. We source Q800E from first-line QT mills, print heat analysis and product analysis when ordered, and ship plate to fabricators in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Related pages include high strength low alloy plates and structural steel plates.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Plate book GB/T 16270 Q800E Confirmed
Other search names Q800E QT plate, Q800E carbon steel plate Covered
Delivery condition Quenched and tempered Confirmed
Yield, thin plate 800 MPa min Confirmed
Quality grade E, impact at −40°C Confirmed
EN comparison S690QL lower, S890QL higher Not a twin
US comparison A514 is 690 MPa Not a twin
Product analysis GB/T 222 column when ordered Confirmed
Not the same letter Q800C or Q800D Do not substitute
Supply role Global steel mill sourcing partner SHH STEEL
Certification EN 10204 3.1 or 3.2 As ordered

Nearby pages that buyers compare, but must not swap blindly, include S690QL, S890QL and A514 Gr.Q.

Chemical Composition

Heat analysis is the mill ladle table in GB/T 16270. Product analysis, when ordered, follows GB/T 222. Grade E is tighter on phosphorus and sulfur than grade C, because the impact test is at −40°C. Mills add Nb, V, Ti or Al for grain refinement, and may add Cr, Ni, Mo or B by thickness. Boron is common on 800 MPa heats. Nickel helps the cold impact. The certificate shows the elements actually used.

Heat Analysis and Product Analysis — GB/T 16270 Q800E

Element Heat analysis (%) Product analysis (%)
Carbon (C), max 0.18 0.20
Silicon (Si), max 0.80 0.85
Manganese (Mn), max 2.00 2.08
Phosphorus (P), max 0.020 0.025
Sulfur (S), max 0.010 0.013
Copper (Cu), max 0.50 0.55
Chromium (Cr), max 1.50 1.55
Nickel (Ni), max 2.00 2.05
Molybdenum (Mo), max 0.70 0.75
Boron (B), max 0.005 0.006
Vanadium (V), max 0.12 0.13
Niobium (Nb), max 0.06 0.07
Titanium (Ti), max 0.05 0.06
Aluminium (Als), min when used 0.015 0.010

If the purchase order writes product analysis, SHH STEEL prints both columns and the thickness band used for the tensile test. Do not treat this chemistry as weathering plate. Do not treat it as S355JR.

Mechanical Properties

Buyers search Q800E mechanical properties, Q800E yield strength, GB/T 16270 Q800E tensile and Q800E impact −40°C.

Tensile and impact — GB/T 16270 Q800E

Thickness Yield min Tensile Elongation min Impact
≤ 50 mm 800 MPa 840–1000 MPa 13% −40°C, grade E
> 50–100 mm 780 MPa 840–1000 MPa 13% −40°C, grade E
> 100–150 mm 720 MPa as standard table 13% −40°C, grade E

Impact energy is the average of three longitudinal Charpy V-notch specimens. One value may fall below the table, but not below 70% of that value. A typical production heat is at or above 27 J to 34 J at −40°C, depending on the ordered edition and thickness. Write the energy on the purchase order if the owner wants a number above the book minimum.

Yield steps down with thickness. An 800 MPa name on 20 mm plate is not the minimum on a 100 mm flange. 800 MPa is about 116 ksi. ASTM A514 is 100 ksi and is not this number. SHH STEEL quotes the thickness band on the offer.

Density is 7.85 g/cm³. Hardness after temper is a mill control, not a design value. Z15, Z25 or Z35 through-thickness tensile is an extra.

Material Comparison

Grade Book Delivery Yield, thin plate Impact Swap?
Q800C GB/T 16270 QT 800 MPa 0°C Warmer sister
Q800D GB/T 16270 QT 800 MPa −20°C Warmer sister
Q800E GB/T 16270 QT 800 MPa −40°C This page
Q800F GB/T 16270 QT 800 MPa −60°C Colder sister
Q690E GB/T 16270 QT 690 MPa −40°C Lower yield
S690QL EN 10025-6 QT 690 MPa −40°C Lower comparison
S890QL EN 10025-6 QT 890 MPa −40°C Higher comparison
A514 Gr.Q ASTM A514 QT 690 MPa Different Lower yield

Equivalent Material Grades

There is no official one-to-one substitute for Q800E. EN 10025-6 jumps from 690 MPa to 890 MPa. ASTM A514 stops at 100 ksi.

The usual European neighbours at −40°C are S690QL and S890QL. S890Q is warmer. A514 Grade Q is 100 ksi / 690 MPa. A572 Gr.65 is only 65 ksi. SHH STEEL will not stamp S890QL or A514 on a Q800E certificate unless the purchase order names both books and both tables are met.

Designation Country / region Standard Notes
Q800E China GB/T 16270 Name on this page
Q800C / Q800D / Q800F China GB/T 16270 Other impact letters
Q690E China GB/T 16270 Lower yield sister
A514 Gr.Q USA ASTM A514 100 ksi, lower yield
A572 Gr.65 USA ASTM A572 65 ksi, lower yield
S690QL Europe EN 10025-6 690 MPa at −40°C
S890QL Europe EN 10025-6 890 MPa at −40°C
SM570 Japan JIS G3106 Well below this yield

QT Structural Service

Buyers pick Q800E when a welded frame, boom or chassis wants 800 MPa yield, QT delivery and impact at −40°C. Search phrases such as Q800E steel plate, GB/T 16270 Q800E and Q800E QT plate all point here.

It is the wrong plate for a 0°C file that can use Q800C. It is the wrong plate for a −20°C file that can use Q800D. It is the wrong plate for a −60°C arctic file. That work is Q800F. It is the wrong plate for a 100 ksi US file. That work is A514 Grade Q. It is the wrong plate for a pressure vessel. That work sits on ASTM A516 or pressure vessel steel plates.

SHH STEEL supplies this plate when the drawing names GB/T 16270 and quality grade E at 800 MPa.

Weldability

Q800E is weldable QT carbon plate. The plate has already been quenched and tempered, and the joint must keep −40°C toughness. Many heats use boron. A procedure written for S355JR is not a Q800E procedure.

Typical consumables are matching 800 MPa low-hydrogen electrodes or wires, qualified on a QT 800 MPa family with a −40°C impact coupon. E7018-class electrodes are under-matched if the joint must develop full plate strength. A procedure written for S890QL is a higher-strength reference. An A514 procedure is a lower-strength reference. Neither is a finished WPS for this grade.

Preheat follows thickness, hydrogen and the approved WPS. Interpass temperature should stay below the mill temper range, or local yield and the −40°C result can drop. After heavy cold forming, a stress relief may be required. The fabricator owns the WPS. SHH STEEL can share mill heat data, product analysis and carbon equivalent for that review.

Heat Treatment and Delivery Condition

Usual delivery from SHH STEEL for Q800E is quenched and tempered. Austenitize typically in the 880–930°C range, quench, then temper in the window that holds 800 MPa yield and the −40°C impact. Exact temperatures stay on the mill process sheet.

Do not order Q800E as as-rolled or TMCP unless the contract leaves GB/T 16270. ASTM A514 is not a delivery instruction for this page. Stress relief after fabrication, if used, must stay below the original temper temperature.

The certificate lists GB/T 16270 Q800E, heat number, heat analysis, product analysis when ordered, tensile by thickness band, and −40°C impact. Certificates may be EN 10204 3.1 or EN 10204 3.2. Dual marking to S690QL or S890QL is available only when both books are fully met.

Dimensions

Usual supply range from SHH STEEL for Q800E QT carbon steel plate:

  • Thickness: commonly 8 mm – 50 mm, heavier plate to 80 mm by enquiry
  • Width: 1500 mm – 3200 mm
  • Length: 3000 mm – 12000 mm

Cut-to-size webs, flanges and base plates are available. Browse more sizes on structural steel plates and the products index.

Tolerances

Dimensional limits for Q800E follow GB/T 709 unless the purchase order names another table.

Typical thickness tolerance idea for Q800E QT plate

Nominal thickness (mm) Usual minus (mm) Usual plus (mm)
8 – 10 −0.3 +0.8
10 – 20 −0.4 +0.9
20 – 30 −0.4 +1.0
30 – 40 −0.5 +1.1
40 – 50 −0.5 +1.2
50 – 80 −0.6 +1.4

Width on 1500–3200 mm plate is commonly held to about ±20–25 mm unless a tighter extra is named. Length on 3000–12000 mm plate is commonly held to about +50 / 0 mm or ±25 mm by mill practice. Flatness after QT follows the agreed class. SHH STEEL will not assume a zero-minus extra on Q800E unless the order says so.

Supplementary Requirements

Q800E already defines 800 MPa yield, QT delivery and −40°C impact. Extra items still have to be written on the purchase order.

Book name. Write GB/T 16270 Q800E. Do not write only Q800E.

Impact. Grade E is −40°C. Write a higher energy if the owner requires it.

EN or US comparison. Write S690QL, S890QL or A514 only if dual mark is required and both tables are met.

Product analysis. Write it if the file needs the second chemistry column.

Through-thickness. Z15, Z25 or Z35 when the joint is loaded through the thickness.

NDE. UT to GB/T 2970 or the named class.

Heat-treatment record. QT temperatures when the inspector asks.

Identification. Heat number, Q800E, thickness and mill logo.

Third-party witness. EN 10204 3.2 with SGS, TÜV, BV, ABS or the inspector named.

Applications

Industry Typical components
Construction machinery Q800E QT booms, frames and bases
Mining equipment Q800E chassis and body plate from SHH STEEL
Cranes and port equipment Q800E webs and flanges
Cold-region fabrication Q800E members tested at −40°C
Comparison vs S690QL Q800E next to S690QL
Comparison vs S890QL Q800E next to S890QL
Comparison vs A514 Q800E next to A514 Gr.Q

Q800E is the plate for an 800 MPa QT file tested at −40°C. It is the wrong plate for a painted warehouse that can use S355JR. It is the wrong plate for an 890 MPa member.

Supply Capability

SHH STEEL sources Q800E from first-line Chinese QT mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron and Steel, Baosteel, Xinyu, Xingcheng and other qualified mills when the size requires it.

Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.

Usual rolling thickness: 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 32 mm, 40 mm, 50 mm. Heavier plate is confirmed before order.

Processing: CNC or flame cutting, bevel, flattening, shot blast, UT to the named class.

Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.

Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.

Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.

Global Delivery and Markets

SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply GB, ASTM, ASME, EN, DIN and JIS steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.

SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.

Typical lead time: ex-stock 5–7 days when plate is in yard; standard QT rolling about 40–50 days; 3.2 inspection about 50–60 days.

Why Choose SHH STEEL

SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. For Q800E that means mill-direct QT price, not a multi-layer stockist mark-up. We buy from mills that already run the 800 MPa quench-and-temper route, so the heat carries the −40°C impact without a second upgrade charge.

Delivery is short when the size is in rolling range: ex-stock 5–7 days, standard heat about 40–50 days, 3.2 inspection about 50–60 days. Cutting, bevel and UT can run in the same window. FOB Shanghai is the main term. CIF to US West, US Gulf, Rotterdam, Jebel Ali and Singapore is quoted on the same file.

Experience on this grade is simple: print GB/T 16270 Q800E, keep the QT route, and do not ship Q800D or A514 as Q800E. We will not change E to D to save a cold test, and we will not treat Q800E as S355. If the drawing needs −60°C, we will move the inquiry to Q800F and keep the price on the right grade.

FAQ

What is Q800E steel plate?
Q800E in GB/T 16270 is quenched-and-tempered carbon structural plate with 800 MPa minimum yield on thin plate and Charpy impact at −40°C. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
Is Q800E the same as Q800C?
No. Both yield at 800 MPa. Q800C is tested at 0°C. Q800E is tested at −40°C.
What is the US equivalent of Q800E?
There is no official ASTM twin at 800 MPa. A514 is 100 ksi / 690 MPa, one step lower, and it does not carry a −40°C E letter. SHH STEEL does not dual-mark A514 unless both books are met.
Is Q800E the same as S690QL or S890QL?
Neither. EN 10025-6 has no S800 grade. S690QL is lower at the same test temperature. S890QL is higher. Dual mark only when both books are fully met.

Conclusion

Q800E QT carbon steel plate to GB/T 16270 is 800 MPa quenched-and-tempered structural plate with impact at −40°C. S690QL is lower, S890QL is higher, and ASTM A514 is 690 MPa. None of those is a silent substitute. Whether the inquiry says Q800E, GB/T 16270 Q800E, Q800E QT plate or Q800E carbon steel plate, SHH STEEL as a global steel mill sourcing partner supplies plate with Q800E chemistry, heat and product analysis as ordered, GB/T 709 tolerances and EN 10204 3.1 or 3.2 certification.

SHH STEEL supplies Q800E QT Carbon Steel Plate to the United States, Europe, the Middle East, Africa, Asia and the Americas for work that actually names this grade.

Contact SHH STEEL for mill rolling, QT route, cutting, UT, 3.2 inspection or a worldwide quotation.

Q800E, Q800E steel plate, GB/T 16270 Q800E, Q800E QT plate, Q800E carbon steel plate, Q800E supplier, SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X