GB/T 16270 Q960F quenched and tempered high-strength structural steel plate, −60 °C impact, SHH STEEL

Q960F QT Carbon Steel Plate GB/T 16270 Supplier

GB/T 16270 Q960F is quenched-and-tempered carbon structural plate with 960 MPa minimum yield and −60°C impact toughness. SHH STEEL supplies Q960F QT plate mill-direct for arctic frames, mining equipment and cold-region fabrication.
Keywords
Q960F, Q960F steel plate, GB/T 16270 Q960F, Q960F QT plate, Q960F carbon steel plate, Q960F supplier, S960QL1, ASTM A514, GB/T 16270 QT plate
quivalent Grades
GB/T 16270 Q960F / EN 10025-6 S960QL1 (colder) / ASTM A514 (near) — Material Specification: GB/T 16270 — Delivery: QT; -60℃
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
Equivalent Material Grades
QT Structural Service
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Applications
Supply Capability
Global Delivery and Markets
Why Choose SHH STEEL
FAQ
Conclusion

What is Q960F QT Carbon Steel Plate GB/T 16270?

Q960F, also searched as GB/T 16270 Q960F, Q960F QT plate, Q960F carbon steel plate, Q960F steel plate and Q960F quenched and tempered plate, is the 960 MPa quality-grade-F grade in GB/T 16270. That standard covers high-strength structural steel plate delivered quenched and tempered. Q is the yield symbol, 960 is the thin-plate minimum yield in MPa, and F is the quality letter for Charpy impact at −60°C.

Q960F is the coldest letter in the Q960 family. C is 0°C. D is −20°C. E is −40°C. F is −60°C. About 139 ksi on a US drawing is the same yield number. Buyers use it on arctic frames and any drawing that names −60°C at 960 MPa. A mill that only tested at −40°C cannot stamp F. Not every QT mill will accept F at this strength, and thickness is usually limited.

The closest European name is EN 10025-6 S960QL1. Both are about 960 MPa QT plate tested at −60°C. S960QL is −40°C and lines up with Q960E. S960Q is 0°C and lines up with Q960C. On the US side, A514 Grade Q is only 100 ksi / 690 MPa. There is no standard ASTM 960 MPa plate grade. Dual mark only when both books are fully met. See EN 10025-6 steel plate.

SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. We source Q960F from first-line QT mills that can run a −60°C route, print heat analysis and product analysis when ordered, and ship plate to fabricators in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Related pages include high strength low alloy plates and structural steel plates.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Plate book GB/T 16270 Q960F Confirmed
Other search names Q960F QT plate, Q960F carbon steel plate Covered
Delivery condition Quenched and tempered Confirmed
Yield, thin plate 960 MPa min Confirmed
Quality grade F, impact at −60°C Confirmed
EN comparison S960QL1, −60°C Comparison, not a swap
US comparison A514 is 690 MPa Not a twin
Product analysis GB/T 222 column when ordered Confirmed
Not the same letter Q960E or Q960D Do not substitute
Supply role Global steel mill sourcing partner SHH STEEL
Certification EN 10204 3.1 or 3.2 As ordered

Nearby pages that buyers compare, but must not swap blindly, include S960QL1, S960QL and A514 Gr.Q.

Chemical Composition

Heat analysis is the mill ladle table in GB/T 16270. Product analysis, when ordered, follows GB/T 222. Grade F is the tightest cleanliness letter in the Q960 family, because the impact test is at −60°C. Mills add Nb, V, Ti or Al for grain refinement, and may add Ni, Cr, Mo or B by thickness. Nickel is often used on F heats to hold the cold impact. Boron is common on 960 MPa heats. The certificate shows the elements actually used.

Heat Analysis and Product Analysis — GB/T 16270 Q960F

Element Heat analysis (%) Product analysis (%)
Carbon (C), max 0.18 0.20
Silicon (Si), max 0.80 0.85
Manganese (Mn), max 2.00 2.08
Phosphorus (P), max 0.015 0.020
Sulfur (S), max 0.005 0.008
Copper (Cu), max 0.50 0.55
Chromium (Cr), max 1.50 1.55
Nickel (Ni), max 2.00 2.05
Molybdenum (Mo), max 0.70 0.75
Boron (B), max 0.005 0.006
Vanadium (V), max 0.12 0.13
Niobium (Nb), max 0.06 0.07
Titanium (Ti), max 0.05 0.06
Aluminium (Als), min when used 0.015 0.010

If the purchase order writes product analysis, SHH STEEL prints both columns and the thickness band used for the tensile test. Do not treat this chemistry as weathering plate. Do not treat it as S355JR.

Mechanical Properties

Buyers search Q960F mechanical properties, Q960F yield strength, GB/T 16270 Q960F tensile and Q960F impact −60°C.

Tensile and impact — GB/T 16270 Q960F

Thickness Yield min Tensile Elongation min Impact
≤ 50 mm 960 MPa 980–1150 MPa 10% −60°C, grade F
> 50 mm as standard table as standard table 10% −60°C, grade F

Impact energy is the average of three longitudinal Charpy V-notch specimens. One value may fall below the table, but not below 70% of that value. A −60°C test at 960 MPa is harder to hold than a −40°C test. Write the energy on the purchase order if the owner wants a number above the book minimum. Not every QT mill will accept F on plate over 30 mm. SHH STEEL confirms the thickness before promising the letter.

Yield steps down with thickness. A 960 MPa name on 12 mm plate is not the minimum on a 40 mm flange. 960 MPa is about 139 ksi. ASTM A514 is 100 ksi and is not this number. Density is 7.85 g/cm³. Hardness after temper is a mill control, not a design value. Z15, Z25 or Z35 through-thickness tensile is an extra.

Material Comparison

Grade Book Delivery Yield, thin plate Impact Swap?
Q960C GB/T 16270 QT 960 MPa 0°C No
Q960D GB/T 16270 QT 960 MPa −20°C No
Q960E GB/T 16270 QT 960 MPa −40°C Warmer sister
Q960F GB/T 16270 QT 960 MPa −60°C This page
Q890F GB/T 16270 QT 890 MPa −60°C Lower yield
S960QL EN 10025-6 QT 960 MPa −40°C No
S960QL1 EN 10025-6 QT 960 MPa −60°C Closest comparison
A514 Gr.Q ASTM A514 QT 690 MPa Different Lower yield

Equivalent Material Grades

There is no official one-to-one substitute for Q960F. What buyers compare is a 960 MPa QT plate tested at −60°C.

The usual European pair is S960QL1. S960QL is warmer. S960Q is only 0°C. S890QL1 is one strength step lower. In the United States there is no standard 960 MPa plate grade. A514 Grade Q is 100 ksi / 690 MPa. A572 Gr.65 is only 65 ksi. SHH STEEL will not stamp S960QL1 or A514 on a Q960F certificate unless the purchase order names both books and both tables are met.

Designation Country / region Standard Notes
Q960F China GB/T 16270 Name on this page
Q960C / Q960D / Q960E China GB/T 16270 Warmer impact letters
Q890F China GB/T 16270 Lower yield sister
A514 Gr.Q USA ASTM A514 100 ksi, lower yield
A572 Gr.65 USA ASTM A572 65 ksi, lower yield
S960QL1 Europe EN 10025-6 −60°C QT comparison
S960QL Europe EN 10025-6 −40°C, closer to Q960E
SM570 Japan JIS G3106 Well below this yield

QT Structural Service

Buyers pick Q960F when a welded frame, boom or chassis wants 960 MPa yield, QT delivery and impact at −60°C. Search phrases such as Q960F steel plate, GB/T 16270 Q960F and Q960F QT plate all point here.

It is the wrong plate for a 0°C file that can use Q960C. It is the wrong plate for a −40°C file that can use Q960E. It is the wrong plate for an 890 MPa arctic boom. That work is Q890F. It is the wrong plate for a 100 ksi US file. That work is A514 Grade Q. It is the wrong plate for a pressure vessel. That work sits on ASTM A516 or pressure vessel steel plates.

SHH STEEL supplies this plate when the drawing names GB/T 16270 and quality grade F at 960 MPa.

Weldability

Q960F is weldable QT carbon plate, but the joint must keep −60°C toughness at 960 MPa. Many heats use boron. A procedure written for S355JR is not a Q960F procedure. A procedure qualified only at −20°C is not enough either.

Typical consumables are matching 960 MPa low-hydrogen electrodes or wires, qualified on a QT 960 MPa family with a −60°C impact coupon. Nickel-bearing wires are common on F-grade joints. E7018-class electrodes are under-matched if the joint must develop full plate strength. A procedure written for S960QL1 is the usual starting point. An A514 procedure is a lower-strength reference, not a finished WPS for this grade.

Preheat follows thickness, hydrogen and the approved WPS. Interpass temperature should stay below the mill temper range, or local yield and the −60°C result can drop. After heavy cold forming, a stress relief may be required. The fabricator owns the WPS. SHH STEEL can share mill heat data, product analysis and carbon equivalent for that review.

Heat Treatment and Delivery Condition

Usual delivery from SHH STEEL for Q960F is quenched and tempered. Austenitize typically in the 880–930°C range, quench, then temper in the window that holds 960 MPa yield and the −60°C impact. Exact temperatures stay on the mill process sheet. F-grade heats at 960 MPa are not every mill’s standard route.

Do not order Q960F as as-rolled or TMCP unless the contract leaves GB/T 16270. ASTM A514 is not a delivery instruction for this page. Stress relief after fabrication, if used, must stay below the original temper temperature.

The certificate lists GB/T 16270 Q960F, heat number, heat analysis, product analysis when ordered, tensile by thickness band, and −60°C impact. Certificates may be EN 10204 3.1 or EN 10204 3.2. Dual marking to S960QL1 is available only when both books are fully met.

Dimensions

Usual supply range from SHH STEEL for Q960F QT carbon steel plate:

  • Thickness: commonly 8 mm – 30 mm, heavier plate to 40 mm by mill confirmation
  • Width: 1500 mm – 2500 mm
  • Length: 3000 mm – 12000 mm

Cut-to-size webs, flanges and base plates are available. Browse more sizes on structural steel plates and the products index.

Tolerances

Dimensional limits for Q960F follow GB/T 709 unless the purchase order names another table.

Typical thickness tolerance idea for Q960F QT plate

Nominal thickness (mm) Usual minus (mm) Usual plus (mm)
8 – 10 −0.3 +0.8
10 – 20 −0.4 +0.9
20 – 30 −0.4 +1.0
30 – 40 −0.5 +1.1

Width on 1500–2500 mm plate is commonly held to about ±20–25 mm unless a tighter extra is named. Length on 3000–12000 mm plate is commonly held to about +50 / 0 mm or ±25 mm by mill practice. Flatness after QT follows the agreed class. SHH STEEL will not assume a zero-minus extra on Q960F unless the order says so.

Supplementary Requirements

Q960F already defines 960 MPa yield, QT delivery and −60°C impact. Extra items still have to be written on the purchase order.

Book name. Write GB/T 16270 Q960F. Do not write only Q960F.

Impact. Grade F is −60°C. Write a higher energy if the owner requires it.

EN or US comparison. Write S960QL1 or A514 only if dual mark is required and both tables are met.

Product analysis. Write it if the file needs the second chemistry column.

Through-thickness. Z15, Z25 or Z35 when the joint is loaded through the thickness.

NDE. UT to GB/T 2970 or the named class.

Heat-treatment record. QT temperatures when the inspector asks.

Identification. Heat number, Q960F, thickness and mill logo.

Third-party witness. EN 10204 3.2 with SGS, TÜV, BV, ABS or the inspector named.

Applications

Industry Typical components
Arctic equipment Q960F QT frames tested at −60°C
Mining equipment Q960F chassis plate from SHH STEEL
Cranes in cold regions Q960F webs and flanges
High-altitude winter work Q960F base plates
Comparison vs S960QL1 Q960F next to S960QL1
Comparison vs S960QL Q960F next to S960QL
Comparison vs A514 Q960F next to A514 Gr.Q

Q960F is the plate for a 960 MPa QT file tested at −60°C. It is the wrong plate for a painted warehouse that can use S355JR. It is the wrong plate for an 890 MPa member unless the drawing names that grade.

Supply Capability

SHH STEEL sources Q960F from first-line Chinese QT mills that can run a −60°C route and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron and Steel, Baosteel, Xinyu, Xingcheng and other qualified mills when the size requires it.

Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.

Usual rolling thickness: 8 mm, 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm. Heavier plate is confirmed before order.

Processing: CNC or flame cutting, bevel, flattening, shot blast, UT to the named class.

Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.

Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.

Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.

Global Delivery and Markets

SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply GB, ASTM, ASME, EN, DIN and JIS steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.

SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.

Typical lead time: ex-stock 5–7 days when an F heat is in yard; standard QT rolling with −60°C test about 50–60 days; 3.2 inspection about 60–70 days.

Why Choose SHH STEEL

SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. For Q960F that means mill-direct QT price, not a multi-layer stockist mark-up on a cold-impact heat. We buy from mills that can actually test at −60°C, so the letter F is on the certificate and not only in the enquiry.

Delivery is short when the size is in rolling range: ex-stock 5–7 days, standard F heat about 50–60 days, 3.2 inspection about 60–70 days. Cutting, bevel and UT can run in the same window. FOB Shanghai is the main term. CIF to US West, US Gulf, Rotterdam, Jebel Ali and Singapore is quoted on the same file.

Experience on this grade is simple: print GB/T 16270 Q960F, keep the QT route, and do not ship Q960E or A514 as F. We will not change F to E to save a cold test, and we will not treat Q960F as S355. If the drawing only needs −40°C, we will move the inquiry to Q960E and keep the price on the right grade.

FAQ

What is Q960F steel plate?
Q960F in GB/T 16270 is quenched-and-tempered carbon structural plate with 960 MPa minimum yield on thin plate and Charpy impact at −60°C. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
Is Q960F the same as Q960E?
No. Both yield at 960 MPa. Q960E is tested at −40°C. Q960F is tested at −60°C.
What is the US equivalent of Q960F?
There is no official ASTM twin at 960 MPa. A514 is 100 ksi / 690 MPa, well below this number, and it does not carry a −60°C F letter. SHH STEEL does not dual-mark A514 unless both books are met.
Is Q960F the same as S960QL1?
They are the usual comparison pair: both are about 960 MPa QT plate tested at −60°C. Dual mark only when both books are fully met. S960QL is warmer.

Conclusion

Q960F QT carbon steel plate to GB/T 16270 is 960 MPa quenched-and-tempered structural plate with impact at −60°C. The nearest European comparison is S960QL1. ASTM A514 is 690 MPa and is not a substitute. Whether the inquiry says Q960F, GB/T 16270 Q960F, Q960F QT plate or Q960F carbon steel plate, SHH STEEL as a global steel mill sourcing partner supplies plate with Q960F chemistry, heat and product analysis as ordered, GB/T 709 tolerances and EN 10204 3.1 or 3.2 certification.

SHH STEEL supplies Q960F QT Carbon Steel Plate to the United States, Europe, the Middle East, Africa, Asia and the Americas for work that actually names this grade.

Contact SHH STEEL for mill rolling, −60°C impact, cutting, UT, 3.2 inspection or a worldwide quotation.

Q960F, Q960F steel plate, GB/T 16270 Q960F, Q960F QT plate, Q960F carbon steel plate, Q960F supplier, SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response