EN 10025-6 S960Q Steel Plate | S960Q QT High Structural Steel - SHH STEEL

EN 10025-6 S960Q Steel Plate | S960Q QT High Structural Steel

EN 10025-6 S960Q is a quenched and tempered ultra-high-strength structural steel plate with a minimum yield strength of 960 MPa and impact toughness at –20°C. It is the highest strength grade in the EN 10025-6 series, designed for extreme weight reduction in heavily loaded structures. SHH STEEL supplies this grade as a China Mill-Direct Exporter with full mill certification and competitive pricing.
Equivalent Grades:
ASTM A514 Gr X (approx) / JIS SHT110 / GB Q960CF / ISO E960Q
Material Specification:
EN 10025-6 — Delivery: Quenched & Tempered (Q+T)
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Tolerances
Weldability
Equivalent Material Grades
Applications
Why Choose SHH STEEL
FAQ
Conclusion

General Description

SHH STEEL is a professional China Mill-Direct Exporter of high-strength structural steel plates. We are pleased to offer EN 10025-6 S960Q Steel Plate (Material Number 1.8941), the highest strength quenched and tempered grade in the EN 10025-6 series.

S960Q belongs to the family of EN 10025-6 steel plate products covering high-yield-strength steels in the quenched and tempered condition. After quenching and tempering, this grade achieves a minimum yield strength of 960 MPa (up to 50 mm thickness) while maintaining adequate impact toughness at –20°C. The refined tempered microstructure delivers exceptional strength, enabling maximum weight reduction in mobile cranes, telescopic booms, heavy lifting equipment and other structures where every kilogram counts.

SHH STEEL supplies S960Q plates in thicknesses ranging from 6 mm to 100 mm (availability of thicker plates is limited and subject to mill capability), widths up to 3000–4000 mm and lengths up to 12000–18000 mm. Custom cutting, ultrasonic testing, surface treatment and third-party inspection services are available. Every plate is delivered with a full EN 10204 3.1 Mill Test Certificate, ensuring complete traceability from the producing mill.

Material Specification

Parameter Requirement / Availability
Governing Standard EN 10025-6
Steel Designation S960Q (1.8941)
Delivery Condition Quenched and Tempered (Q)
Product Form Flat steel plate
Thickness Range 6 mm – 100 mm (thicker plates limited)
Width / Length Up to 3000–4000 mm / 12000–18000 mm
Certification EN 10204 3.1 / 3.2
Additional Testing UT, Z-test, third-party inspection available

Chemical Composition

Chemical composition is controlled in accordance with EN 10025-6 for both ladle (heat) analysis and product analysis.

Ladle Analysis (Cast Analysis)

Element Maximum (%)
Carbon (C) 0.20
Silicon (Si) 0.80
Manganese (Mn) 1.70
Phosphorus (P) 0.025
Sulfur (S) 0.015
Chromium (Cr) 1.50
Nickel (Ni) 2.00
Molybdenum (Mo) 0.70
Copper (Cu) 0.50
Niobium (Nb) 0.06
Vanadium (V) 0.12
Titanium (Ti) 0.05
Boron (B) 0.005
Nitrogen (N) 0.015

Product Analysis

Element Maximum (%)
Carbon (C) 0.22
Silicon (Si) 0.86
Manganese (Mn) 1.80
Phosphorus (P) 0.030
Sulfur (S) 0.017
Chromium (Cr) 1.60
Nickel (Ni) 2.10
Molybdenum (Mo) 0.74
Copper (Cu) 0.55
Niobium (Nb) 0.07
Vanadium (V) 0.14
Titanium (Ti) 0.06
Boron (B) 0.006
Nitrogen (N) 0.016

The carefully balanced alloying system ensures the high hardenability required to achieve 960 MPa yield strength while keeping the carbon equivalent at a level that still permits controlled welding after quenching and tempering.

Mechanical Properties

Nominal Thickness (mm) Min. Yield Strength ReH Tensile Strength Rm Min. Elongation A Impact Energy (longitudinal)
≤ 50 960 MPa 980 – 1150 MPa 10 % 30 J at –20 °C
50 < t ≤ 100 900 MPa 940 – 1100 MPa 10 % 30 J at –20 °C

Density is approximately 7.85 g/cm³.

Delivery Conditions

All S960Q plates are supplied in the quenched and tempered condition as required by EN 10025-6. The quenching and tempering heat treatment is precisely controlled to achieve the ultra-high strength and required toughness.

Additional processing options available from SHH STEEL:

  • Shot blasting and shop primer application
  • Ultrasonic testing in accordance with EN 10160
  • Through-thickness (Z-direction) testing to Z15, Z25 or Z35
  • Independent third-party inspection (SGS, BV, TUV, Lloyd’s Register, etc.)
  • Precision cutting (flame, plasma or water-jet)

Tolerances

EN 10025-6 S960Q Steel Plate dimensional tolerances are supplied in accordance with EN 10029. For S960Q QT High Structural Steel, customers may select the required class for thickness, width, length and flatness according to project needs. Both mill edges and cut edges (flame or plasma) are available for S960Q steel plate. Tighter tolerances for EN 10025-6 S960Q can be arranged by special agreement when required.

Weldability

S960Q is an ultra-high-strength quenched and tempered steel. Welding requires extremely strict control of preheating, heat input and the exclusive use of matching low-hydrogen ultra-high-strength consumables to maintain toughness in the heat-affected zone.

Recommended welding consumables:

Welding Process Suggested Consumables
SMAW (Stick) E12018-G, E13018-G
GMAW / MAG ER120S-G, ER130S-G
FCAW E121T1-G, E131T1-G
SAW Matching ultra-high-strength wire and flux combinations

Preheating is mandatory. Interpass temperature must be tightly controlled, and post-weld heat treatment is frequently required for critical or highly stressed components. Welding procedures should be carefully qualified.

Equivalent Material Grades

Grade Standard Remarks
S960Q EN 10025-6 Primary designation
1.8941 EN Material number
Q960D / Q960E GB/T 1591 Closest Chinese equivalents
Weldox 960 / Strenx 960 SSAB Similar ultra-high-strength QT concept
StE 960 V Former DIN Historical related grade

Applications

EN 10025-6 S960Q is selected when the absolute maximum strength and maximum weight reduction are required. Typical applications include:

Application Area Typical Components / Keywords
Mobile Cranes & Lifting Boom structures, telescopic arms – S960Q Crane
Heavy Construction Ultra-high-load frames – S960Q Structural Steel
Mining & Earthmoving Equipment Chassis, boom structures – S960Q Mining
Offshore & Marine Lifting equipment – S960Q Offshore
Energy & Power Special high-strength fabrications – S960Q Energy
General Heavy Fabrication Ultra-high-strength welded assemblies – S960Q Fabrication

Why Choose SHH STEEL

SHH STEEL is a China Mill-Direct Exporter. We maintain long-term strategic cooperation with major Chinese steel mills and act as a first-level agent. This direct supply model allows us to offer competitive mill-direct pricing, shorter lead times, consistent quality and full Mill Test Certificates (EN 10204 3.1 / 3.2) for EN 10025-6 S960Q Steel Plate.

Our experienced export and technical teams provide support on material selection, welding procedures, cutting and processing. Customers benefit from reliable supply and professional service for the highest strength quenched and tempered steel projects worldwide.

FAQ

What does “Q” mean in S960Q?
“Q” indicates the quenched and tempered condition and impact testing at –20°C.
What is the difference between S960Q and S960QL?
Both grades have the same strength level. S960Q is impact tested at –20°C, while S960QL is tested at –40°C and offers higher toughness for colder service.

Conclusion

EN 10025-6 S960Q (1.8941) quenched and tempered steel plate from SHH STEEL provides the highest yield strength of 960 MPa in the EN 10025-6 series combined with reliable toughness at –20°C. As a China Mill-Direct Exporter, we offer competitive pricing, consistent quality and full technical support. Contact SHH STEEL today for stock availability, pricing or processing services.

EN 10025-6 S960Q Steel Plate, S960Q steel plate, S960Q QT, EN 10025 S960Q, S960Q equivalent, S960Q supplier, 1.8941

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *