GB/T 16270 Q890E quenched and tempered high-strength structural steel plate, −40 °C impact, SHH STEEL

Q890E QT Carbon Steel Plate GB/T 16270 Supplier

GB/T 16270 Q890E is quenched-and-tempered carbon structural plate with 890 MPa minimum yield and −40°C impact toughness. SHH STEEL supplies Q890E QT plate mill-direct for cranes, mining frames and cold-region fabrication.
Keywords
Q890E, Q890E steel plate, GB/T 16270 Q890E, Q890E QT plate, Q890E carbon steel plate, Q890E supplier, S890QL, ASTM A514, GB/T 16270 QT plate
Equivalent Grades:
GB/T 16270 Q890E / EN 10025-6 S890QL (cold) / ASTM A514 (near) — Material Specification: GB/T 16270 — Delivery: QT; -40℃
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
Equivalent Material Grades
QT Structural Service
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Applications
Supply Capability
Global Delivery and Market
Why Choose SHH STEEL
FAQ
Conclusion

What is GB/T 16270 Q890E Steel Plate?

Q890E, also searched as GB/T 16270 Q890E, Q890E QT plate, Q890E carbon steel plate, Q890E steel plate and Q890E quenched and tempered plate, is the 890 MPa quality-grade-E grade in GB/T 16270. That standard covers high-strength structural steel plate delivered quenched and tempered. Q is the yield symbol, 890 is the thin-plate minimum yield in MPa, and E is the quality letter for Charpy impact at −40°C.

Q890E is the grade most buyers compare with European QL plate at 890 MPa. C is 0°C. D is −20°C. E is −40°C. F is −60°C. About 129 ksi on a US drawing is the same yield number. Cold-region crane and mine-truck builders use Q890E when the member was sized at 890 MPa and the specification names −40°C. A Q890C heat tested only at 0°C cannot be stamped E.

The closest European name is EN 10025-6 S890QL. Both are about 890 MPa QT plate tested at −40°C. S890Q is 0°C and lines up with Q890C. S890QL1 is −60°C and lines up with Q890F. On the US side, A514 Grade Q is only 100 ksi / 690 MPa. There is no standard ASTM 890 MPa plate grade. Dual mark only when both books are fully met. See EN 10025-6 steel plate.

SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. We source Q890E from first-line QT mills, print heat analysis and product analysis when ordered, and ship plate to fabricators in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Related pages include high strength low alloy plates and structural steel plates.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Plate book GB/T 16270 Q890E Confirmed
Other search names Q890E QT plate, Q890E carbon steel plate Covered
Delivery condition Quenched and tempered Confirmed
Yield, thin plate 890 MPa min Confirmed
Quality grade E, impact at −40°C Confirmed
EN comparison S890QL, −40°C Comparison, not a swap
US comparison A514 is 690 MPa Not a twin
Product analysis GB/T 222 column when ordered Confirmed
Not the same letter Q890C or Q890D Do not substitute
Supply role Global steel mill sourcing partner SHH STEEL
Certification EN 10204 3.1 or 3.2 As ordered

Nearby pages that buyers compare, but must not swap blindly, include S890QL, S890Q and A514 Gr.Q.

Chemical Composition

Heat analysis is the mill ladle table in GB/T 16270. Product analysis, when ordered, follows GB/T 222. Grade E is tighter on phosphorus and sulfur than grade C, because the impact test is at −40°C. Mills add Nb, V, Ti or Al for grain refinement, and may add Cr, Ni, Mo or B by thickness. Boron is common on 890 MPa heats. Nickel helps the cold impact. The certificate shows the elements actually used.

Heat Analysis and Product Analysis — GB/T 16270 Q890E

Element Heat analysis (%) Product analysis (%)
Carbon (C), max 0.18 0.20
Silicon (Si), max 0.80 0.85
Manganese (Mn), max 2.00 2.08
Phosphorus (P), max 0.020 0.025
Sulfur (S), max 0.010 0.013
Copper (Cu), max 0.50 0.55
Chromium (Cr), max 1.50 1.55
Nickel (Ni), max 2.00 2.05
Molybdenum (Mo), max 0.70 0.75
Boron (B), max 0.005 0.006
Vanadium (V), max 0.12 0.13
Niobium (Nb), max 0.06 0.07
Titanium (Ti), max 0.05 0.06
Aluminium (Als), min when used 0.015 0.010

If the purchase order writes product analysis, SHH STEEL prints both columns and the thickness band used for the tensile test. Do not treat this chemistry as weathering plate. Do not treat it as S355JR.

Mechanical Properties

Buyers search Q890E mechanical properties, Q890E yield strength, GB/T 16270 Q890E tensile and Q890E impact −40°C.

Tensile and impact — GB/T 16270 Q890E

Thickness Yield min Tensile Elongation min Impact
≤ 50 mm 890 MPa 940–1100 MPa 11% −40°C, grade E
> 50–100 mm 830 MPa 880–1100 MPa 11% −40°C, grade E
> 100–150 mm 780 MPa as standard table 11% −40°C, grade E

Impact energy is the average of three longitudinal Charpy V-notch specimens. One value may fall below the table, but not below 70% of that value. A typical production heat is at or above 27 J to 34 J at −40°C, depending on the ordered edition and thickness. Write the energy on the purchase order if the owner wants a number above the book minimum.

Yield steps down with thickness. An 890 MPa name on 20 mm plate is not the minimum on a 80 mm flange. 890 MPa is about 129 ksi. ASTM A514 is 100 ksi and is not this number. SHH STEEL quotes the thickness band on the offer.

Density is 7.85 g/cm³. Hardness after temper is a mill control, not a design value. Z15, Z25 or Z35 through-thickness tensile is an extra.

Material Comparison

Grade Book Delivery Yield, thin plate Impact Swap?
Q890C GB/T 16270 QT 890 MPa 0°C Warmer sister
Q890D GB/T 16270 QT 890 MPa −20°C Warmer sister
Q890E GB/T 16270 QT 890 MPa −40°C This page
Q890F GB/T 16270 QT 890 MPa −60°C Colder sister
Q800E GB/T 16270 QT 800 MPa −40°C Lower yield
S890Q EN 10025-6 QT 890 MPa 0°C No
S890QL EN 10025-6 QT 890 MPa −40°C Closest comparison
A514 Gr.Q ASTM A514 QT 690 MPa Different Lower yield

Equivalent Material Grades

There is no official one-to-one substitute for Q890E. What buyers compare is an 890 MPa QT plate tested at −40°C.

The usual European pair is S890QL. S890Q is warmer. S890QL1 is colder. S690QL is one strength step lower. In the United States there is no standard 890 MPa plate grade. A514 Grade Q is 100 ksi / 690 MPa. A572 Gr.65 is only 65 ksi. SHH STEEL will not stamp S890QL or A514 on a Q890E certificate unless the purchase order names both books and both tables are met.

Designation Country / region Standard Notes
Q890E China GB/T 16270 Name on this page
Q890C / Q890D / Q890F China GB/T 16270 Other impact letters
Q800E China GB/T 16270 Lower yield sister
A514 Gr.Q USA ASTM A514 100 ksi, lower yield
A572 Gr.65 USA ASTM A572 65 ksi, lower yield
S890QL Europe EN 10025-6 −40°C QT comparison
S890Q Europe EN 10025-6 0°C, closer to Q890C
SM570 Japan JIS G3106 Well below this yield

QT Structural Service

Buyers pick Q890E when a welded frame, boom or chassis wants 890 MPa yield, QT delivery and impact at −40°C. Search phrases such as Q890E steel plate, GB/T 16270 Q890E and Q890E QT plate all point here.

It is the wrong plate for a 0°C file that can use Q890C. It is the wrong plate for a −20°C file that can use Q890D. It is the wrong plate for a −60°C arctic file. That work is Q890F. It is the wrong plate for a 100 ksi US file. That work is A514 Grade Q. It is the wrong plate for a pressure vessel. That work sits on ASTM A516 or pressure vessel steel plates.

SHH STEEL supplies this plate when the drawing names GB/T 16270 and quality grade E at 890 MPa.

Weldability

Q890E is weldable QT carbon plate. The plate has already been quenched and tempered, and the joint must keep −40°C toughness. Many heats use boron. A procedure written for S355JR is not a Q890E procedure.

Typical consumables are matching 890 MPa low-hydrogen electrodes or wires, qualified on a QT 890 MPa family with a −40°C impact coupon. E7018-class electrodes are under-matched if the joint must develop full plate strength. A procedure written for S890QL is the usual starting point. An A514 procedure is a lower-strength reference, not a finished WPS for this grade.

Preheat follows thickness, hydrogen and the approved WPS. Interpass temperature should stay below the mill temper range, or local yield and the −40°C result can drop. After heavy cold forming, a stress relief may be required. The fabricator owns the WPS. SHH STEEL can share mill heat data, product analysis and carbon equivalent for that review.

Heat Treatment and Delivery Condition

Usual delivery from SHH STEEL for Q890E is quenched and tempered. Austenitize typically in the 880–930°C range, quench, then temper in the window that holds 890 MPa yield and the −40°C impact. Exact temperatures stay on the mill process sheet.

Do not order Q890E as as-rolled or TMCP unless the contract leaves GB/T 16270. ASTM A514 is not a delivery instruction for this page. Stress relief after fabrication, if used, must stay below the original temper temperature.

The certificate lists GB/T 16270 Q890E, heat number, heat analysis, product analysis when ordered, tensile by thickness band, and −40°C impact. Certificates may be EN 10204 3.1 or EN 10204 3.2. Dual marking to S890QL is available only when both books are fully met.

Dimensions

Usual supply range from SHH STEEL for Q890E QT carbon steel plate:

  • Thickness: commonly 8 mm – 50 mm, heavier plate to 60 mm by enquiry
  • Width: 1500 mm – 3000 mm
  • Length: 3000 mm – 12000 mm

Cut-to-size webs, flanges and base plates are available. Browse more sizes on structural steel plates and the products index.

Tolerances

Dimensional limits for Q890E follow GB/T 709 unless the purchase order names another table.

Typical thickness tolerance idea for Q890E QT plate

Nominal thickness (mm) Usual minus (mm) Usual plus (mm)
8 – 10 −0.3 +0.8
10 – 20 −0.4 +0.9
20 – 30 −0.4 +1.0
30 – 40 −0.5 +1.1
40 – 50 −0.5 +1.2
50 – 60 −0.6 +1.4

Width on 1500–3000 mm plate is commonly held to about ±20–25 mm unless a tighter extra is named. Length on 3000–12000 mm plate is commonly held to about +50 / 0 mm or ±25 mm by mill practice. Flatness after QT follows the agreed class. SHH STEEL will not assume a zero-minus extra on Q890E unless the order says so.

Supplementary Requirements

Q890E already defines 890 MPa yield, QT delivery and −40°C impact. Extra items still have to be written on the purchase order.

Book name. Write GB/T 16270 Q890E. Do not write only Q890E.

Impact. Grade E is −40°C. Write a higher energy if the owner requires it.

EN or US comparison. Write S890QL or A514 only if dual mark is required and both tables are met.

Product analysis. Write it if the file needs the second chemistry column.

Through-thickness. Z15, Z25 or Z35 when the joint is loaded through the thickness.

NDE. UT to GB/T 2970 or the named class.

Heat-treatment record. QT temperatures when the inspector asks.

Identification. Heat number, Q890E, thickness and mill logo.

Third-party witness. EN 10204 3.2 with SGS, TÜV, BV, ABS or the inspector named.

Applications

Industry Typical components
Construction machinery Q890E QT booms, frames and bases
Mining equipment Q890E chassis and body plate from SHH STEEL
Cranes and port equipment Q890E webs and flanges
Cold-region fabrication Q890E members tested at −40°C
Comparison vs S890QL Q890E next to S890QL
Comparison vs S890Q Q890E next to S890Q
Comparison vs A514 Q890E next to A514 Gr.Q

Q890E is the plate for an 890 MPa QT file tested at −40°C. It is the wrong plate for a painted warehouse that can use S355JR. It is the wrong plate for a 960 MPa member.

Supply Capability

SHH STEEL sources Q890E from first-line Chinese QT mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron and Steel, Baosteel, Xinyu, Xingcheng and other qualified mills when the size requires it.

Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.

Usual rolling thickness: 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 32 mm, 40 mm, 50 mm. Heavier plate is confirmed before order.

Processing: CNC or flame cutting, bevel, flattening, shot blast, UT to the named class.

Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.

Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.

Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.

Global Delivery and Market

SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply GB, ASTM, ASME, EN, DIN and JIS steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.

SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.

Typical lead time: ex-stock 5–7 days when plate is in yard; standard QT rolling about 40–50 days; 3.2 inspection about 50–60 days.

Why Choose SHH STEEL

SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. For Q890E that means mill-direct QT price, not a multi-layer stockist mark-up. We buy from mills that already run the 890 MPa quench-and-temper route, so the heat carries the −40°C impact without a second upgrade charge.

Delivery is short when the size is in rolling range: ex-stock 5–7 days, standard heat about 40–50 days, 3.2 inspection about 50–60 days. Cutting, bevel and UT can run in the same window. FOB Shanghai is the main term. CIF to US West, US Gulf, Rotterdam, Jebel Ali and Singapore is quoted on the same file.

Experience on this grade is simple: print GB/T 16270 Q890E, keep the QT route, and do not ship Q890D or a silent S890QL stamp as Q890E. We will not change E to D to save a cold test, and we will not treat Q890E as S355. If the drawing needs −60°C, we will move the inquiry to Q890F and keep the price on the right grade.

FAQ

What is Q890E steel plate?
Q890E in GB/T 16270 is quenched-and-tempered carbon structural plate with 890 MPa minimum yield on thin plate and Charpy impact at −40°C. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
Is Q890E the same as Q890C?
No. Both yield at 890 MPa. Q890C is tested at 0°C. Q890E is tested at −40°C.
What is the US equivalent of Q890E?
There is no official ASTM twin at 890 MPa. A514 is 100 ksi / 690 MPa, one step lower, and it does not carry a −40°C E letter. SHH STEEL does not dual-mark A514 unless both books are met. Q: Is Q890E the same as S890QL?
Is Q890E the same as S890QL?
They are the usual comparison pair: both are about 890 MPa QT plate tested at −40°C. Dual mark only when both books are fully met. S890Q is warmer. S890QL1 is colder.

Conclusion

Q890E QT carbon steel plate to GB/T 16270 is 890 MPa quenched-and-tempered structural plate with impact at −40°C. The nearest European comparison is S890QL. ASTM A514 is 690 MPa and is not a substitute. Whether the inquiry says Q890E, GB/T 16270 Q890E, Q890E QT plate or Q890E carbon steel plate, SHH STEEL as a global steel mill sourcing partner supplies plate with Q890E chemistry, heat and product analysis as ordered, GB/T 709 tolerances and EN 10204 3.1 or 3.2 certification.

SHH STEEL supplies Q890E QT Carbon Steel Plate to the United States, Europe, the Middle East, Africa, Asia and the Americas for work that actually names this grade.

Contact SHH STEEL for mill rolling, QT route, cutting, UT, 3.2 inspection or a worldwide quotation.

Q890E, Q890E steel plate, GB/T 16270 Q890E, Q890E QT plate, Q890E carbon steel plate, Q890E supplier, SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X