EN 10025-6 S890QL Steel Plate | S890QL QT High Structural Steel - SHH STEEL

EN 10025-6 S890QL Steel Plate | S890QL QT High Structural Steel

EN 10025-6 S890QL is a quenched and tempered ultra-high-strength structural steel plate with a minimum yield strength of 890 MPa and enhanced impact toughness at –40°C. It is designed for extremely heavily loaded structures operating in low-temperature environments where weight reduction is critical. SHH STEEL supplies this grade as a China Mill-Direct Exporter with full mill certification and competitive pricing.
Equivalent Grades
ASTM A514 Gr S (-40℃) / JIS SHT100 (L ref) / GB Q890CF-D / ISO E890QL
Material Specification:
EN 10025-6 — Delivery: Quenched & Tempered (Q+T)
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Tolerances
Weldability
Equivalent Material Grades
Applications
Why Choose SHH STEEL
FAQ
Conclusion

What is EN 10025-6 S890QL Steel Plate?

SHH STEEL is a professional China Mill-Direct Exporter of high-strength structural steel plates. We are pleased to offer EN 10025-6 S890QL Steel Plate (Material Number 1.8983), a quenched and tempered ultra-high-strength grade engineered for structural applications that require both maximum strength and improved low-temperature toughness.

S890QL belongs to the family of EN 10025-6 steel plate products covering high-yield-strength steels in the quenched and tempered condition. Compared with S890Q, the “QL” designation indicates a more stringent impact requirement at –40°C, making this grade particularly suitable for structures exposed to colder service temperatures. After quenching and tempering, the steel develops a fine-grained tempered microstructure that delivers a minimum yield strength of 890 MPa (up to 50 mm thickness) together with reliable Charpy-V toughness at low temperature. This combination allows significant weight reduction in mobile cranes, heavy lifting equipment and other demanding structures.

SHH STEEL supplies S890QL plates in thicknesses ranging from 6 mm to 100 mm (thicker plates available on request), widths up to 3000–4000 mm and lengths up to 12000–18000 mm. Custom cutting, ultrasonic testing, surface treatment and third-party inspection services are available. Every plate is delivered with a full EN 10204 3.1 Mill Test Certificate, ensuring complete traceability from the producing mill.

Material Specification

Parameter Requirement / Availability
Governing Standard EN 10025-6
Steel Designation S890QL (1.8983)
Delivery Condition Quenched and Tempered (Q)
Product Form Flat steel plate
Thickness Range 6 mm – 100 mm (thicker plates on request)
Width / Length Up to 3000–4000 mm / 12000–18000 mm
Certification EN 10204 3.1 / 3.2
Additional Testing UT, Z-test, third-party inspection available

Chemical Composition

Chemical composition is controlled in accordance with EN 10025-6 for both ladle (heat) analysis and product analysis. The QL grade features tighter limits on phosphorus and sulphur to support improved low-temperature toughness.

Ladle Analysis (Cast Analysis)

Element Maximum (%)
Carbon (C) 0.20
Silicon (Si) 0.80
Manganese (Mn) 1.70
Phosphorus (P) 0.020
Sulfur (S) 0.010
Chromium (Cr) 1.50
Nickel (Ni) 2.00
Molybdenum (Mo) 0.70
Copper (Cu) 0.50
Niobium (Nb) 0.06
Vanadium (V) 0.12
Titanium (Ti) 0.05
Boron (B) 0.005
Nitrogen (N) 0.015

Product Analysis

Element Maximum (%)
Carbon (C) 0.22
Silicon (Si) 0.86
Manganese (Mn) 1.80
Phosphorus (P) 0.025
Sulfur (S) 0.012
Chromium (Cr) 1.60
Nickel (Ni) 2.10
Molybdenum (Mo) 0.74
Copper (Cu) 0.55
Niobium (Nb) 0.07
Vanadium (V) 0.14
Titanium (Ti) 0.06
Boron (B) 0.006
Nitrogen (N) 0.016

The restricted impurity levels and controlled alloying contribute to reliable toughness performance at –40°C while maintaining acceptable weldability after quenching and tempering.

Mechanical Properties

Nominal Thickness (mm) Min. Yield Strength ReH Tensile Strength Rm Min. Elongation A Impact Energy (longitudinal)
≤ 50 890 MPa 940 – 1100 MPa 11 % 40 J at –40 °C
50 < t ≤ 100 830 MPa 880 – 1100 MPa 11 % 40 J at –40 °C

Density is approximately 7.85 g/cm³. Transverse impact values are also specified in the standard and can be provided when required by the project.

Delivery Conditions

All S890QL plates are supplied in the quenched and tempered condition as required by EN 10025-6. The quenching and tempering heat treatment is carefully controlled to achieve the ultra-high strength and required low-temperature toughness.

Additional processing options available from SHH STEEL:

  • Shot blasting and shop primer application
  • Ultrasonic testing in accordance with EN 10160
  • Through-thickness (Z-direction) testing to Z15, Z25 or Z35
  • Independent third-party inspection (SGS, BV, TUV, Lloyd’s Register, etc.)
  • Precision cutting (flame, plasma or water-jet)

Tolerances

EN 10025-6 S890QL Steel Plate dimensional tolerances are supplied in accordance with EN 10029. For S890QL QT High Structural Steel, customers may select the required class for thickness, width, length and flatness according to project needs. Both mill edges and cut edges (flame or plasma) are available for S890QL steel plate. Tighter tolerances for EN 10025-6 S890QL can be arranged by special agreement when required.

Weldability

S890QL is an ultra-high-strength quenched and tempered steel. Welding requires strict control of preheating, heat input and the exclusive use of matching low-hydrogen high-strength consumables to maintain toughness in the heat-affected zone, especially for low-temperature service.

Recommended welding consumables:

Welding Process Suggested Consumables
SMAW (Stick) E11018-G, E12018-G
GMAW / MAG ER110S-G, ER120S-G
FCAW E111T1-G, E121T1-G
SAW Matching ultra-high-strength wire and flux combinations

Preheating is mandatory for most thicknesses. Interpass temperature must be carefully controlled, and post-weld heat treatment is frequently required for critical or highly stressed components.

Equivalent Material Grades

Grade Standard Remarks
S890QL EN 10025-6 Primary designation
1.8983 EN Material number
Q890E / Q890F GB/T 1591 Closest Chinese equivalents
A514 / Weldox 900 ASTM / SSAB Similar ultra-high-strength QT concept
TStE 890 V Former DIN Historical related grade

Applications

EN 10025-6 S890QL is selected when maximum strength, weight reduction and reliable low-temperature performance are required. Typical applications include:

Application Area Typical Components / Keywords
Mobile Cranes & Lifting Boom structures, telescopic arms – S890QL Crane
Heavy Construction High-load frames, columns – S890QL Structural Steel
Mining & Earthmoving Equipment Chassis, boom structures – S890QL Mining
Offshore & Marine Lifting equipment, platform components – S890QL Offshore
Low-Temperature Structures Structures requiring –40°C toughness – S890QL Low Temperature
Energy & Power Heavy fabrications, special structures – S890QL Energy
General Heavy Fabrication Ultra-high-strength welded assemblies – S890QL Fabrication

Why Choose SHH STEEL

SHH STEEL is a China Mill-Direct Exporter. We maintain long-term strategic cooperation with major Chinese steel mills and act as a first-level agent. This direct supply model allows us to offer competitive mill-direct pricing, shorter lead times, consistent quality and full Mill Test Certificates (EN 10204 3.1 / 3.2) for EN 10025-6 S890QL Steel Plate.

Our experienced export and technical teams provide support on material selection, welding procedures, cutting and processing. Customers benefit from reliable supply and professional service for ultra-high-strength quenched and tempered steel projects requiring improved low-temperature performance.

FAQ

What does “QL” mean in S890QL?
“Q” indicates the quenched and tempered condition, while “L” means the steel meets higher impact energy requirements at –40°C.
What is the difference between S890Q and S890QL?
Both grades have the same strength level. S890Q is impact tested at –20°C, whereas S890QL is tested at –40°C and provides higher toughness values for colder service conditions.
Can SHH STEEL supply S890QL with Z-direction testing?
Yes. Z15, Z25 and Z35 testing can be arranged according to project requirements.

Conclusion

EN 10025-6 S890QL (1.8983) quenched and tempered steel plate from SHH STEEL combines an ultra-high yield strength of 890 MPa with excellent toughness at –40°C. As a China Mill-Direct Exporter, we provide competitive pricing, reliable quality and full technical support. Contact SHH STEEL today for stock availability, pricing or processing services.

EN 10025-6 S890QL Steel Plate, S890QL steel plate, S890QL QT, EN 10025 S890QL, S890QL equivalent, S890QL supplier, 1.8983

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X