Q890D QT Carbon Steel Plate GB/T 16270 Supplier
What is GB/T 16270 Q890D QT steel?
Q890D, also searched as GB/T 16270 Q890D, Q890D QT plate, Q890D carbon steel plate, Q890D steel plate and Q890D quenched and tempered plate, is the 890 MPa quality-grade-D grade in GB/T 16270. That standard covers high-strength structural steel plate delivered quenched and tempered. Q is the yield symbol, 890 is the thin-plate minimum yield in MPa, and D is the quality letter for Charpy impact at −20°C.
Q890D is the middle impact letter in the 890 MPa family. C is 0°C. D is −20°C. E is −40°C. F is −60°C. About 129 ksi on a US drawing is the same yield number. Equipment builders use it when the frame needs 890 MPa and the site sees sub-zero nights, but the specification does not call for −40°C. It is not a substitute for Q890C, and it is not a substitute for Q890E.
EN 10025-6 does not have a −20°C letter. S890Q is tested at 0°C. S890QL is tested at −40°C and lines up more closely with Q890E. Q890D sits between those two. On the US side, A514 Grade Q is only 100 ksi / 690 MPa. There is no standard ASTM 890 MPa plate grade. Dual mark only when both books are fully met. See EN 10025-6 steel plate.
SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. We source Q890D from first-line QT mills, print heat analysis and product analysis when ordered, and ship plate to fabricators in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Related pages include high strength low alloy plates and structural steel plates.
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Plate book | GB/T 16270 Q890D | Confirmed |
| Other search names | Q890D QT plate, Q890D carbon steel plate | Covered |
| Delivery condition | Quenched and tempered | Confirmed |
| Yield, thin plate | 890 MPa min | Confirmed |
| Quality grade | D, impact at −20°C | Confirmed |
| EN comparison | S890Q warmer, S890QL colder | Not a twin |
| US comparison | A514 is 690 MPa | Not a twin |
| Product analysis | GB/T 222 column when ordered | Confirmed |
| Not the same letter | Q890C or Q890E | Do not substitute |
| Supply role | Global steel mill sourcing partner | SHH STEEL |
| Certification | EN 10204 3.1 or 3.2 | As ordered |
Nearby pages that buyers compare, but must not swap blindly, include S890Q, S890QL and A514 Gr.Q.
Chemical Composition
Heat analysis is the mill ladle table in GB/T 16270. Product analysis, when ordered, follows GB/T 222. Grade D is tighter on phosphorus and sulfur than grade C, because the impact test is colder. Mills add Nb, V, Ti or Al for grain refinement, and may add Cr, Ni, Mo or B by thickness. Boron is common on 890 MPa heats. The certificate shows the elements actually used.
Heat Analysis and Product Analysis — GB/T 16270 Q890D
| Element | Heat analysis (%) | Product analysis (%) |
|---|---|---|
| Carbon (C), max | 0.18 | 0.20 |
| Silicon (Si), max | 0.80 | 0.85 |
| Manganese (Mn), max | 2.00 | 2.08 |
| Phosphorus (P), max | 0.020 | 0.025 |
| Sulfur (S), max | 0.010 | 0.013 |
| Copper (Cu), max | 0.50 | 0.55 |
| Chromium (Cr), max | 1.50 | 1.55 |
| Nickel (Ni), max | 2.00 | 2.05 |
| Molybdenum (Mo), max | 0.70 | 0.75 |
| Boron (B), max | 0.005 | 0.006 |
| Vanadium (V), max | 0.12 | 0.13 |
| Niobium (Nb), max | 0.06 | 0.07 |
| Titanium (Ti), max | 0.05 | 0.06 |
| Aluminium (Als), min when used | 0.015 | 0.010 |
If the purchase order writes product analysis, SHH STEEL prints both columns and the thickness band used for the tensile test. Do not treat this chemistry as weathering plate. Do not treat it as S355JR.
Mechanical Properties
Buyers search Q890D mechanical properties, Q890D yield strength, GB/T 16270 Q890D tensile and Q890D impact −20°C.
Tensile and impact — GB/T 16270 Q890D
| Thickness | Yield min | Tensile | Elongation min | Impact |
|---|---|---|---|---|
| ≤ 50 mm | 890 MPa | 940–1100 MPa | 11% | −20°C, grade D |
| > 50–100 mm | 830 MPa | 880–1100 MPa | 11% | −20°C, grade D |
| > 100–150 mm | 780 MPa | as standard table | 11% | −20°C, grade D |
Impact energy is the average of three longitudinal Charpy V-notch specimens. One value may fall below the table, but not below 70% of that value. A typical production heat is at or above 34 J at −20°C. Write a higher energy on the order if the owner requires it.
Yield steps down with thickness. An 890 MPa name on 20 mm plate is not the minimum on a 100 mm flange. 890 MPa is about 129 ksi. ASTM A514 is 100 ksi and is not this number. SHH STEEL quotes the thickness band on the offer.
Density is 7.85 g/cm³. Hardness after temper is a mill control, not a design value. Z15, Z25 or Z35 through-thickness tensile is an extra.
Material Comparison
| Grade | Book | Delivery | Yield, thin plate | Impact | Swap? |
|---|---|---|---|---|---|
| Q890C | GB/T 16270 | QT | 890 MPa | 0°C | Warmer sister |
| Q890D | GB/T 16270 | QT | 890 MPa | −20°C | This page |
| Q890E | GB/T 16270 | QT | 890 MPa | −40°C | Colder sister |
| Q800D | GB/T 16270 | QT | 800 MPa | −20°C | Lower yield |
| Q960D | GB/T 16270 | QT | 960 MPa | −20°C | Higher yield |
| S890Q | EN 10025-6 | QT | 890 MPa | 0°C | Warmer comparison |
| S890QL | EN 10025-6 | QT | 890 MPa | −40°C | Colder comparison |
| A514 Gr.Q | ASTM A514 | QT | 690 MPa | Different | Lower yield |
Equivalent Material Grades
There is no official one-to-one substitute for Q890D. What buyers compare is an 890 MPa QT plate tested at −20°C.
EN 10025-6 jumps from 0°C on S890Q to −40°C on S890QL. Q890D sits in the gap. Some files accept S890Q if an extra −20°C test is written. Others step up to S890QL. S690QL is one strength step lower. In the United States there is no standard 890 MPa plate grade. A514 Grade Q is 100 ksi / 690 MPa. A572 Gr.65 is only 65 ksi. SHH STEEL will not stamp S890Q or A514 on a Q890D certificate unless the purchase order names both books and both tables are met.
| Designation | Country / region | Standard | Notes |
|---|---|---|---|
| Q890D | China | GB/T 16270 | Name on this page |
| Q890C / Q890E / Q890F | China | GB/T 16270 | Other impact letters |
| Q800D | China | GB/T 16270 | Lower yield sister |
| A514 Gr.Q | USA | ASTM A514 | 100 ksi, lower yield |
| A572 Gr.65 | USA | ASTM A572 | 65 ksi, lower yield |
| S890Q | Europe | EN 10025-6 | 0°C QT comparison |
| S890QL | Europe | EN 10025-6 | −40°C, closer to Q890E |
| SM570 | Japan | JIS G3106 | Well below this yield |
QT Structural Service
Buyers pick Q890D when a welded frame, boom or chassis wants 890 MPa yield, QT delivery and impact at −20°C. Search phrases such as Q890D steel plate, GB/T 16270 Q890D and Q890D QT plate all point here.
It is the wrong plate for a 0°C-only file that can use Q890C. It is the wrong plate for a −40°C mine site. That work is Q890E. It is the wrong plate for an 800 MPa file that was sized on Q800D. It is the wrong plate for a 100 ksi US file. That work is A514 Grade Q. It is the wrong plate for a pressure vessel. That work sits on ASTM A516 or pressure vessel steel plates.
SHH STEEL supplies this plate when the drawing names GB/T 16270 and quality grade D at 890 MPa.
Weldability
Q890D is weldable QT carbon plate. The plate has already been quenched and tempered, and many heats use boron. A procedure written for S355JR is not a Q890D procedure. A procedure qualified only on Q890C at 0°C may miss the −20°C coupon.
Typical consumables are matching 890 MPa low-hydrogen electrodes or wires, qualified on a QT 890 MPa family. E7018-class electrodes are under-matched if the joint must develop full plate strength. A procedure written for S890QL is a useful starting point after the −20°C test temperature is checked. An A514 procedure is a lower-strength reference, not a finished WPS for this grade.
Preheat follows thickness, hydrogen and the approved WPS. Interpass temperature should stay below the mill temper range, or local yield can drop. After heavy cold forming, a stress relief may be required. The fabricator owns the WPS. SHH STEEL can share mill heat data, product analysis and carbon equivalent for that review.
Heat Treatment and Delivery Condition
Usual delivery from SHH STEEL for Q890D is quenched and tempered. Austenitize typically in the 880–930°C range, quench, then temper in the window that holds 890 MPa yield and the −20°C impact. Exact temperatures stay on the mill process sheet.
Do not order Q890D as as-rolled or TMCP unless the contract leaves GB/T 16270. ASTM A514 is not a delivery instruction for this page. Stress relief after fabrication, if used, must stay below the original temper temperature.
The certificate lists GB/T 16270 Q890D, heat number, heat analysis, product analysis when ordered, tensile by thickness band, and −20°C impact. Certificates may be EN 10204 3.1 or EN 10204 3.2. Dual marking to S890Q or S890QL is available only when both books are fully met.
Dimensions
Usual supply range from SHH STEEL for Q890D QT carbon steel plate:
- Thickness: commonly 8 mm – 50 mm, heavier plate to 80 mm by enquiry
- Width: 1500 mm – 3000 mm
- Length: 3000 mm – 12000 mm
Cut-to-size webs, flanges and base plates are available. Browse more sizes on structural steel plates and the products index.
Tolerances
Dimensional limits for Q890D follow GB/T 709 unless the purchase order names another table.
Typical thickness tolerance idea for Q890D QT plate
| Nominal thickness (mm) | Usual minus (mm) | Usual plus (mm) |
|---|---|---|
| 8 – 10 | −0.3 | +0.8 |
| 10 – 20 | −0.4 | +0.9 |
| 20 – 30 | −0.4 | +1.0 |
| 30 – 40 | −0.5 | +1.1 |
| 40 – 50 | −0.5 | +1.2 |
| 50 – 80 | −0.6 | +1.4 |
Width on 1500–3000 mm plate is commonly held to about ±20–25 mm unless a tighter extra is named. Length on 3000–12000 mm plate is commonly held to about +50 / 0 mm or ±25 mm by mill practice. Flatness after QT follows the agreed class. SHH STEEL will not assume a zero-minus extra on Q890D unless the order says so.
Supplementary Requirements
Q890D already defines 890 MPa yield, QT delivery and −20°C impact. Extra items still have to be written on the purchase order.
Book name. Write GB/T 16270 Q890D. Do not write only Q890D.
Impact. Grade D is −20°C. Write a higher energy if the owner requires it.
EN or US comparison. Write S890Q, S890QL or A514 only if dual mark is required and both tables are met.
Product analysis. Write it if the file needs the second chemistry column.
Through-thickness. Z15, Z25 or Z35 when the joint is loaded through the thickness.
NDE. UT to GB/T 2970 or the named class.
Heat-treatment record. QT temperatures when the inspector asks.
Identification. Heat number, Q890D, thickness and mill logo.
Third-party witness. EN 10204 3.2 with SGS, TÜV, BV, ABS or the inspector named.
Applications
| Industry | Typical components |
|---|---|
| Construction machinery | Q890D QT booms, frames and bases |
| Mining equipment | Q890D chassis and body plate from SHH STEEL |
| Cranes and port equipment | Q890D webs and flanges |
| Cold-region fabrication | Q890D members tested at −20°C |
| Comparison vs S890Q | Q890D next to S890Q |
| Comparison vs S890QL | Q890D next to S890QL |
| Comparison vs A514 | Q890D next to A514 Gr.Q |
Q890D is the plate for an 890 MPa QT file tested at −20°C. It is the wrong plate for a painted warehouse that can use S355JR. It is the wrong plate for a 960 MPa member.
Supply Capability
SHH STEEL sources Q890D from first-line Chinese QT mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron and Steel, Baosteel, Xinyu, Xingcheng and other qualified mills when the size requires it.
Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.
Usual rolling thickness: 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 32 mm, 40 mm, 50 mm. Heavier plate is confirmed before order.
Processing: CNC or flame cutting, bevel, flattening, shot blast, UT to the named class.
Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.
Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.
Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.
Global Delivery and Markets
SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply GB, ASTM, ASME, EN, DIN and JIS steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.
SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.
Typical lead time: ex-stock 5–7 days when plate is in yard; standard QT rolling about 40–50 days; 3.2 inspection about 50–60 days.
Why Choose SHH STEEL
SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. For Q890D that means mill-direct QT price, not a multi-layer stockist mark-up. We buy from mills that already run the 890 MPa quench-and-temper route, so the heat carries the −20°C impact without a second upgrade charge.
Delivery is short when the size is in rolling range: ex-stock 5–7 days, standard heat about 40–50 days, 3.2 inspection about 50–60 days. Cutting, bevel and UT can run in the same window. FOB Shanghai is the main term. CIF to US West, US Gulf, Rotterdam, Jebel Ali and Singapore is quoted on the same file.
Experience on this grade is simple: print GB/T 16270 Q890D, keep the QT route, and do not ship Q890C or A514 as Q890D. We will not change D to C to save a cold test, and we will not treat Q890D as S355. If the drawing needs −40°C, we will move the inquiry to Q890E and keep the price on the right grade.
FAQ
-
What is Q890D steel plate?
- Q890D in GB/T 16270 is quenched-and-tempered carbon structural plate with 890 MPa minimum yield on thin plate and Charpy impact at −20°C. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
-
Is Q890D the same as Q890C?
- No. Both yield at 890 MPa. Q890C is tested at 0°C. Q890D is tested at −20°C.
-
What is the US equivalent of Q890D?
- There is no official ASTM twin at 890 MPa. A514 is 100 ksi / 690 MPa, one step lower, and it does not carry a −20°C D letter. SHH STEEL does not dual-mark A514 unless both books are met.
-
Is Q890D the same as S890Q or S890QL?
- Neither letter matches exactly. S890Q is 0°C. S890QL is −40°C. Q890D is −20°C. Dual mark only when both books are fully met.
Conclusion
Q890D QT carbon steel plate to GB/T 16270 is 890 MPa quenched-and-tempered structural plate with impact at −20°C. S890Q is warmer, S890QL is colder, and ASTM A514 is 690 MPa. None of those is a silent substitute. Whether the inquiry says Q890D, GB/T 16270 Q890D, Q890D QT plate or Q890D carbon steel plate, SHH STEEL as a global steel mill sourcing partner supplies plate with Q890D chemistry, heat and product analysis as ordered, GB/T 709 tolerances and EN 10204 3.1 or 3.2 certification.
SHH STEEL supplies Q890D QT Carbon Steel Plate to the United States, Europe, the Middle East, Africa, Asia and the Americas for work that actually names this grade.
Contact SHH STEEL for mill rolling, QT route, cutting, UT, 3.2 inspection or a worldwide quotation.
Q890D, Q890D steel plate, GB/T 16270 Q890D, Q890D QT plate, Q890D carbon steel plate, Q890D supplier, SHH STEEL