Q800C QT Carbon Steel Plate GB/T 16270 Supplier
What is Q800C QT Carbon Steel Plate GB/T 16270?
Q800C, also searched as GB/T 16270 Q800C, Q800C QT plate, Q800C carbon steel plate, Q800C steel plate and Q800C quenched and tempered plate, is the 800 MPa quality-grade-C grade in GB/T 16270. That standard covers high-strength structural steel plate delivered quenched and tempered. Q is the yield symbol, 800 is the thin-plate minimum yield in MPa, and C is the quality letter for Charpy impact at 0°C.
Q800C sits above Q690C and below Q890C. About 116 ksi on a US drawing is the same yield number. Equipment builders use it when a boom or chassis was too heavy in 690 MPa plate and does not yet need 890 MPa. It is still a QT carbon plate, not a stainless grade and not a pressure-vessel grade.
Quality grade C means the impact test is at 0°C. D is −20°C. E is −40°C. F is −60°C. Q800C is the right letter for temperate fabrication. If the drawing shows winter design at −40°C, the letter is E, not C.
EN 10025-6 has no S800 grade. S690Q is 690 MPa and is one step lower. S890Q is 890 MPa and is one step higher. On the US side, A514 Grade Q is 100 ksi / 690 MPa, also one step lower. There is no standard ASTM 800 MPa plate grade. Dual mark only when both books are fully met. See EN 10025-6 steel plate.
SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. We source Q800C from first-line QT mills, print heat analysis and product analysis when ordered, and ship plate to fabricators in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Related pages include high strength low alloy plates and structural steel plates.
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Plate book | GB/T 16270 Q800C | Confirmed |
| Other search names | Q800C QT plate, Q800C carbon steel plate | Covered |
| Delivery condition | Quenched and tempered | Confirmed |
| Yield, thin plate | 800 MPa min | Confirmed |
| Quality grade | C, impact at 0°C | Confirmed |
| EN comparison | S690Q lower, S890Q higher | Not a twin |
| US comparison | A514 is 690 MPa | Not a twin |
| Product analysis | GB/T 222 column when ordered | Confirmed |
| Not the same strength | Q690C or Q890C | Do not substitute |
| Supply role | Global steel mill sourcing partner | SHH STEEL |
| Certification | EN 10204 3.1 or 3.2 | As ordered |
Nearby pages that buyers compare, but must not swap blindly, include S690Q, S890Q and A514 Gr.Q.
Chemical Composition
Heat analysis is the mill ladle table in GB/T 16270. Product analysis, when ordered, follows GB/T 222. Q800C is a low-alloy QT carbon plate. Mills add Nb, V, Ti or Al for grain refinement, and may add Cr, Ni, Mo or B by thickness. Boron is common on 800 MPa heats. The certificate shows the elements actually used.
Heat Analysis and Product Analysis — GB/T 16270 Q800C
| Element | Heat analysis (%) | Product analysis (%) |
|---|---|---|
| Carbon (C), max | 0.20 | 0.22 |
| Silicon (Si), max | 0.80 | 0.85 |
| Manganese (Mn), max | 2.00 | 2.08 |
| Phosphorus (P), max | 0.025 | 0.030 |
| Sulfur (S), max | 0.015 | 0.018 |
| Copper (Cu), max | 0.50 | 0.55 |
| Chromium (Cr), max | 1.50 | 1.55 |
| Nickel (Ni), max | 2.00 | 2.05 |
| Molybdenum (Mo), max | 0.70 | 0.75 |
| Boron (B), max | 0.005 | 0.006 |
| Vanadium (V), max | 0.12 | 0.13 |
| Niobium (Nb), max | 0.06 | 0.07 |
| Titanium (Ti), max | 0.05 | 0.06 |
| Aluminium (Als), min when used | 0.015 | 0.010 |
Grade C allows a slightly wider phosphorus and sulfur window than grade E or F. That is acceptable at 0°C. It is not a reason to use Q800C on a −40°C drawing. If the file needs product analysis, SHH STEEL prints both columns and the thickness band used for the mechanical test.
Do not treat this chemistry as weathering plate. Do not treat it as S355JR.
Mechanical Properties
Buyers search Q800C mechanical properties, Q800C yield strength, GB/T 16270 Q800C tensile and Q800C impact 0°C.
Tensile and impact — GB/T 16270 Q800C
| Thickness | Yield min | Tensile | Elongation min | Impact |
|---|---|---|---|---|
| ≤ 50 mm | 800 MPa | 840–1000 MPa | 13% | 0°C, grade C |
| > 50–100 mm | 780 MPa | 840–1000 MPa | 13% | 0°C, grade C |
| > 100–150 mm | 720 MPa | as standard table | 13% | 0°C, grade C |
Impact energy is the average of three longitudinal Charpy V-notch specimens. One value may fall below the table, but not below 70% of that value. A typical production heat is at or above 34 J at 0°C. Write a higher energy on the order if the owner requires it.
Yield steps down with thickness. An 800 MPa name on 20 mm plate is not the minimum on a 120 mm flange. 800 MPa is about 116 ksi. ASTM A514 is 100 ksi and is not this number. SHH STEEL quotes the thickness band on the offer.
Density is 7.85 g/cm³. Hardness after temper is a mill control, not a design value. Z15, Z25 or Z35 through-thickness tensile is an extra.
Material Comparison
| Grade | Book | Delivery | Yield, thin plate | Impact | Swap? |
|---|---|---|---|---|---|
| Q690C | GB/T 16270 | QT | 690 MPa | 0°C | Lower sister |
| Q800C | GB/T 16270 | QT | 800 MPa | 0°C | This page |
| Q800D | GB/T 16270 | QT | 800 MPa | −20°C | Colder sister |
| Q800E | GB/T 16270 | QT | 800 MPa | −40°C | Colder sister |
| Q890C | GB/T 16270 | QT | 890 MPa | 0°C | Higher sister |
| S690Q | EN 10025-6 | QT | 690 MPa | 0°C | Lower comparison |
| S890Q | EN 10025-6 | QT | 890 MPa | 0°C | Higher comparison |
| A514 Gr.Q | ASTM A514 | QT | 690 MPa | Different | Lower yield |
Equivalent Material Grades
There is no official one-to-one substitute for Q800C. EN 10025-6 jumps from 690 MPa to 890 MPa. ASTM A514 stops at 100 ksi.
S690Q is the lower European neighbour. S890Q is the higher neighbour. A514 Grade Q is 100 ksi / 690 MPa. A572 Gr.65 is only 65 ksi. SHH STEEL will not stamp S890Q or A514 on a Q800C certificate unless the purchase order names both books and both tables are met.
| Designation | Country / region | Standard | Notes |
|---|---|---|---|
| Q800C | China | GB/T 16270 | Name on this page |
| Q800D / Q800E / Q800F | China | GB/T 16270 | Colder quality letters |
| Q690C | China | GB/T 16270 | Lower yield sister |
| A514 Gr.Q | USA | ASTM A514 | 100 ksi, lower yield |
| A572 Gr.65 | USA | ASTM A572 | 65 ksi, lower yield |
| S690Q | Europe | EN 10025-6 | 690 MPa, lower comparison |
| S890Q | Europe | EN 10025-6 | 890 MPa, higher comparison |
| SM570 | Japan | JIS G3106 | Well below this yield |
QT Structural Service
Buyers pick Q800C when a welded frame, boom or chassis wants 800 MPa yield, QT delivery and impact at 0°C. Search phrases such as Q800C steel plate, GB/T 16270 Q800C and Q800C QT plate all point here.
It is the wrong plate for a −40°C mine site. That work is Q800E. It is the wrong plate for a 690 MPa file that was sized on Q690C. Raising the grade without a design check can change weld procedure and deflection. It is the wrong plate for a 100 ksi US file. That work is A514 Grade Q. It is the wrong plate for a pressure vessel. That work sits on ASTM A516 or pressure vessel steel plates.
SHH STEEL supplies this plate when the drawing names GB/T 16270 and quality grade C at 800 MPa.
Weldability
Q800C is weldable QT carbon plate. Carbon is controlled, but the plate has already been quenched and tempered, and many heats use boron. A procedure written for S355JR is not a Q800C procedure. A procedure qualified only on Q690C may be under-matched.
Typical consumables are matching 800 MPa low-hydrogen electrodes or wires, qualified on a QT 800 MPa family. E7018-class electrodes are under-matched if the joint must develop full plate strength. A procedure written for S890Q is a higher-strength reference. An A514 procedure is a lower-strength reference. Neither is a finished WPS for this grade.
Preheat follows thickness, hydrogen and the approved WPS. Interpass temperature should stay below the mill temper range, or local yield can drop. After heavy cold forming, a stress relief may be required. The fabricator owns the WPS. SHH STEEL can share mill heat data, product analysis and carbon equivalent for that review.
Heat Treatment and Delivery Condition
Usual delivery from SHH STEEL for Q800C is quenched and tempered. Austenitize typically in the 880–930°C range, quench, then temper in the window that holds 800 MPa yield and the 0°C impact. Exact temperatures stay on the mill process sheet.
Do not order Q800C as as-rolled or TMCP unless the contract leaves GB/T 16270. ASTM A514 is not a delivery instruction for this page. Stress relief after fabrication, if used, must stay below the original temper temperature.
The certificate lists GB/T 16270 Q800C, heat number, heat analysis, product analysis when ordered, tensile by thickness band, and 0°C impact. Certificates may be EN 10204 3.1 or EN 10204 3.2. Dual marking to S690Q or S890Q is available only when both books are fully met.
Dimensions
Usual supply range from SHH STEEL for Q800C QT carbon steel plate:
- Thickness: commonly 8 mm – 60 mm, heavier plate to 80 mm by enquiry
- Width: 1500 mm – 3200 mm
- Length: 3000 mm – 12000 mm
Cut-to-size webs, flanges and base plates are available. Browse more sizes on structural steel plates and the products index.
Tolerances
Dimensional limits for Q800C follow GB/T 709 unless the purchase order names another table.
Typical thickness tolerance idea for Q800C QT plate
| Nominal thickness (mm) | Usual minus (mm) | Usual plus (mm) |
|---|---|---|
| 8 – 10 | −0.3 | +0.8 |
| 10 – 20 | −0.4 | +0.9 |
| 20 – 30 | −0.4 | +1.0 |
| 30 – 40 | −0.5 | +1.1 |
| 40 – 50 | −0.5 | +1.2 |
| 50 – 80 | −0.6 | +1.4 |
Width on 1500–3200 mm plate is commonly held to about ±20–25 mm unless a tighter extra is named. Length on 3000–12000 mm plate is commonly held to about +50 / 0 mm or ±25 mm by mill practice. Flatness after QT follows the agreed class. SHH STEEL will not assume a zero-minus extra on Q800C unless the order says so.
Supplementary Requirements
Q800C already defines 800 MPa yield, QT delivery and 0°C impact. Extra items still have to be written on the purchase order.
Book name. Write GB/T 16270 Q800C. Do not write only Q800C.
Impact. Grade C is 0°C. Write a higher energy if the owner requires it.
EN or US comparison. Write S690Q, S890Q or A514 only if dual mark is required and both tables are met.
Product analysis. Write it if the file needs the second chemistry column.
Through-thickness. Z15, Z25 or Z35 when the joint is loaded through the thickness.
NDE. UT to GB/T 2970 or the named class.
Heat-treatment record. QT temperatures when the inspector asks.
Identification. Heat number, Q800C, thickness and mill logo.
Third-party witness. EN 10204 3.2 with SGS, TÜV, BV, ABS or the inspector named.
Applications
| Industry | Typical components |
|---|---|
| Construction machinery | Q800C QT booms, frames and bases |
| Mining equipment | Q800C chassis and body plate from SHH STEEL |
| Cranes and port equipment | Q800C webs and flanges |
| Heavy trailers | Q800C goosenecks |
| Comparison vs S690Q | Q800C next to S690Q |
| Comparison vs S890Q | Q800C next to S890Q |
| Comparison vs A514 | Q800C next to A514 Gr.Q |
Q800C is the plate for an 800 MPa QT file tested at 0°C. It is the wrong plate for a painted warehouse that can use S355JR. It is the wrong plate for an 890 MPa member.
Supply Capability
SHH STEEL sources Q800C from first-line Chinese QT mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron and Steel, Baosteel, Xinyu, Xingcheng and other qualified mills when the size requires it.
Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.
Usual rolling thickness: 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 32 mm, 40 mm, 50 mm, 60 mm. Heavier plate is confirmed before order.
Processing: CNC or flame cutting, bevel, flattening, shot blast, UT to the named class.
Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.
Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.
Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.
Global Delivery and Markets
SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply GB, ASTM, ASME, EN, DIN and JIS steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.
SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.
Typical lead time: ex-stock 5–7 days when plate is in yard; standard QT rolling about 35–45 days; 3.2 inspection about 45–60 days.
Why Choose SHH STEEL
SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. For Q800C that means mill-direct QT price, not a multi-layer stockist mark-up. We buy from mills that already run the 800 MPa quench-and-temper route, so the heat carries the 0°C impact without a second upgrade charge.
Delivery is short when the size is in rolling range: ex-stock 5–7 days, standard heat about 35–45 days, 3.2 inspection about 45–60 days. Cutting, bevel and UT can run in the same window. FOB Shanghai is the main term. CIF to US West, US Gulf, Rotterdam, Jebel Ali and Singapore is quoted on the same file.
Experience on this grade is simple: print GB/T 16270 Q800C, keep the QT route, and do not ship Q690C or S890Q as Q800C. We will not change C to E on the certificate to win an order, and we will not treat Q800C as S355. If the drawing needs −40°C, we will move the inquiry to Q800E and keep the price on the right grade.
FAQ
-
What is Q800C steel plate?
- Q800C in GB/T 16270 is quenched-and-tempered carbon structural plate with 800 MPa minimum yield on thin plate and Charpy impact at 0°C. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
-
Is Q800C the same as Q690C?
- No. Both are QT plate tested at 0°C. Q800C yields at 800 MPa. Q690C yields at 690 MPa.
-
What is the US equivalent of Q800C?
- There is no official ASTM twin at 800 MPa. A514 is 100 ksi / 690 MPa, one step lower. SHH STEEL does not dual-mark A514 unless both books are met.
-
Is Q800C the same as S690Q or S890Q?
- Neither. EN 10025-6 has no S800 grade. S690Q is lower. S890Q is higher. Dual mark only when both books are fully met.
Conclusion
Q800C QT carbon steel plate to GB/T 16270 is 800 MPa quenched-and-tempered structural plate with impact at 0°C. S690Q is lower, S890Q is higher, and ASTM A514 is 690 MPa. None of those is a silent substitute. Whether the inquiry says Q800C, GB/T 16270 Q800C, Q800C QT plate or Q800C carbon steel plate, SHH STEEL as a global steel mill sourcing partner supplies plate with Q800C chemistry, heat and product analysis as ordered, GB/T 709 tolerances and EN 10204 3.1 or 3.2 certification.
SHH STEEL supplies Q800C QT Carbon Steel Plate to the United States, Europe, the Middle East, Africa, Asia and the Americas for work that actually names this grade.
Contact SHH STEEL for mill rolling, QT route, cutting, UT, 3.2 inspection or a worldwide quotation.
Q800C, Q800C steel plate, GB/T 16270 Q800C, Q800C QT plate, Q800C carbon steel plate, Q800C supplier, SHH STEEL