EN 10025-2 S355J0 Steel Plate | S355J0 Structural Steel
What is EN 10025-2 S355J0 Steel Plate?
As a professional steel plate supplier and China Mill-Direct Exporter, SHH STEEL is pleased to present EN 10025-2 S355J0 Steel Plate (Material Number: 1.0553).
S355J0 is a high-strength non-alloy structural steel under the European standard EN 10025-2. It provides a minimum yield strength of 355 MPa (for thickness ≤ 16 mm) and is impact tested at 0°C with a minimum energy of 27 J. Compared with S355JR, the lower impact test temperature makes S355J0 more suitable for structural applications requiring better toughness in colder environments. SHH STEEL sources this material directly from leading Chinese steel mills, ensuring competitive mill-direct pricing, stable quality and reliable delivery.
We supply S355J0 steel plate in thicknesses from 6 mm to 150 mm (thicker plates available on request), widths up to 3000–4000 mm, and lengths up to 12000–18000 mm. Custom cutting, shot blasting and priming services are available. All plates are delivered with full Mill Test Certificates (EN 10204 3.1).
Material Specification
EN 10025-2 S355J0 steel plate is produced in accordance with EN 10025-2.
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Primary Standard | EN 10025-2 | Full compliance |
| Steel Grade | S355J0 (1.0553) | Confirmed |
| Delivery Condition | +AR (As-rolled) or +N (Normalized) | Available |
| Product Form | Steel Plate | Available |
| Thickness Range | 6 mm – 150 mm | Custom sizes available |
| Width / Length | Up to 3000–4000 mm / 12000–18000 mm | Custom cutting supported |
| Certification | EN 10204 3.1 / 3.2 | Available |
Chemical Composition
According to EN 10025-2, the chemical composition is specified for both ladle analysis (cast analysis) and product analysis.
Ladle Analysis (Cast Analysis)
| Element | Max. Limit (%) |
|---|---|
| Carbon (C) | 0.20 |
| Silicon (Si) | 0.55 |
| Manganese (Mn) | 1.60 |
| Phosphorus (P) | 0.030 |
| Sulfur (S) | 0.030 |
| Nitrogen (N) | 0.012 |
| Copper (Cu) | 0.55 |
Product Analysis
| Element | Max. Limit (%) |
|---|---|
| Carbon (C) | 0.23 |
| Silicon (Si) | 0.60 |
| Manganese (Mn) | 1.70 |
| Phosphorus (P) | 0.040 |
| Sulfur (S) | 0.040 |
| Nitrogen (N) | 0.014 |
| Copper (Cu) | 0.60 |
Note:
- The maximum nitrogen content does not apply if the total aluminium content is ≥ 0.020%.
- Carbon Equivalent (CEV) is controlled to ensure good weldability.
Mechanical Properties
Mechanical properties of EN 10025-2 S355J0 (longitudinal direction):
| Thickness (mm) | Yield Strength ReH (min) | Tensile Strength Rm | Elongation A (min) | Impact Energy KV (min) |
|---|---|---|---|---|
| ≤ 16 | 355 MPa | 470 – 630 MPa | 22% | 27 J at 0°C |
| > 16 ≤ 40 | 345 MPa | 470 – 630 MPa | 22% | 27 J at 0°C |
| > 40 ≤ 63 | 335 MPa | 470 – 630 MPa | 21% | 27 J at 0°C |
| > 63 ≤ 100 | 325 MPa | 470 – 630 MPa | 20% | 27 J at 0°C |
| > 100 ≤ 150 | 295 – 285 MPa | 450 – 600 MPa | 18% | 27 J at 0°C |
Delivery Conditions
SHH STEEL, as a China Mill-Direct Supplier, supplies EN 10025-2 S355J0 steel plate mainly in the following conditions:
- +AR (As-rolled) – most common
- +N (Normalized) – available on request
Additional options:
- Shot blasting and shop primer
- Ultrasonic testing (EN 10160)
- Z-direction testing (Z15 / Z25 / Z35)
- Third-party inspection (SGS, BV, TUV, etc.)
Tolerances
Dimensional tolerances for S355J0 steel plate follow EN 10029 (for plates) or EN 10051 (for strips).
- Thickness, width and length tolerances according to the ordered class.
- Flatness according to EN 10029.
- Edge conditions: Mill edge or cut edge (flame / plasma).
Tighter tolerances can be provided upon request.
Weldability
S355J0 has good weldability. It can be welded by conventional methods (SMAW, SAW, GMAW, FCAW, etc.). Due to the higher strength and carbon equivalent, preheating is often recommended for thicker plates. Low-hydrogen consumables are advised for critical applications.
Equivalent Material Grades
| Grade | Standard | Notes |
|---|---|---|
| S355J0 | EN 10025-2 | — |
| 1.0553 | EN | Material number |
| Q355C | GB/T 1591 | Closest Chinese equivalent |
| A572 Grade 50 (approx.) | ASTM | Similar strength level |
| St52-3U | DIN (old) | Former designation |
Applications
EN 10025-2 S355J0 is widely used in structural applications requiring high strength and better toughness at 0°C. Typical uses include:
| Application Area | Typical Components / Uses (Keywords) |
|---|---|
| Building Structures | Beams, columns, heavy frames – S355J0 Structural Steel |
| Bridges | Bridge components – S355J0 Bridge |
| Machinery | Heavy equipment frames – S355J0 Machinery |
| Construction | High-strength construction in colder regions – S355J0 Construction |
| Offshore & Industrial | Structural components – S355J0 Industrial |
| General Fabrication | Welded high-strength structures – S355J0 Fabrication |
Why Choose SHH STEEL
SHH STEEL is a China Mill-Direct Exporter. We maintain long-term strategic cooperation with major Chinese steel mills and act as a first-level (primary) agent. This direct mill supply model allows us to offer competitive mill-direct pricing, faster delivery times, stable and traceable quality, and full Mill Test Certificates (EN 10204 3.1 / 3.2) for EN 10025-2 S355J0 Steel Plate.
Customers benefit from reliable supply, short lead times and cost-effective solutions for structural steel projects worldwide. Our professional export team provides technical support and customized processing services to meet project requirements.
FAQ
-
What does the “J0” in S355J0 mean?
- “J0” indicates that the steel meets the impact energy requirement of minimum 27 J at 0°C.
-
What is the difference between S355JR, S355J0 and S355J2?
- The difference is the impact test temperature: JR: +20°C J0: 0°C J2: –20°C
-
What is the material number of S355J0?
- 1.0553
Conclusion
EN 10025-2 S355J0 (1.0553) Steel Plate from SHH STEEL offers high strength combined with improved toughness at 0°C, making it suitable for demanding structural applications. As a China Mill-Direct Exporter, we provide competitive pricing, fast delivery and consistent quality backed by full mill certifications. Trust SHH STEEL for your S355J0 structural steel plate requirements.
Contact SHH STEEL today for stock availability, pricing and technical support.
EN 10025-2 S355J0 Steel Plate, S355J0 steel plate, S355J0 structural steel, EN 10025 S355J0, S355J0 equivalent, S355J0 supplier, 1.0553