JIS G 3106 SM490 H-Beam
What is JIS G 3106 SM490 H-Beam?
JIS G 3106 SM490 H-beam is a hot-rolled H-section in rolled steel for welded structure, in the SM490 tensile class (490–610 N/mm²). The material standard is JIS G 3106. Dimensions, mass and tolerances for the section are those of JIS G 3192. There is no single suffixless grade in the standard called only “SM490”. The designation on the order must be one of SM490A, SM490B, SM490C, SM490YA or SM490YB. Those symbols share a tensile class, but they do not share a yield table, a carbon table, an applicable-thickness limit or an impact requirement.
This page covers the rolled H-section in that family. The same symbols in plate form are listed separately as SM490A, SM490B, SM490C, SM490YA and SM490YB steel plate. Do not use a plate page as a beam data sheet, and do not apply the plate-only thickness extensions in JIS G 3106 to an H-section unless that extension is actually agreed for the product form on the order.
These beams will be filed under a JIS G 3106 beam-profiles term once that category exists; they belong in the steel beam profiles category of steel structural profiles. The dimensional standard is identified under JIS G 3192. The usual product is the standard H-section series. This page is not a JIS G 3101 SS400 article, and it is not an EN 10025-5 weathering grade.
SM490 H-beams are used for welded building and industrial frames when a Japanese welded-structure grade in this tensile class is specified. The quality letter still has to be named. The family is not a pressure-vessel or nuclear safety material.
Material, Dimensions and Tolerances for SM490 Sections
The order and the inspection certificate should keep material, dimensions, tolerances and the quality symbol distinct:
- JIS G 3106 is the material standard. This article uses heat-analysis and tensile values for SM490A, SM490B, SM490C, SM490YA and SM490YB from JIS G 3106:2020. The edition named on the order governs acceptance.
- JIS G 3192 is the dimensional standard for hot-rolled sections. The size table below lists the 53 standard H-sections in JIS G 3192 Table 15. Those rows are reference dimensions, not a mill rolling list, and they do not by themselves select A, B, C, YA or YB.
Under the standard scope for sections, SM490A and SM490B run to 200 mm, while SM490C, SM490YA and SM490YB run to 100 mm. A special combination of one of these grades with a non-Japanese shape is valid only when it is documented against every named requirement.
SM490 H-Beam Sizes: JIS G 3192 Standard H-Sections
The same 53 standard H-sections of JIS G 3192 Table 15, from H 100×50×5×7 to H 918×303×19×37, are used for this family. The designation is written H × flange width × web thickness × flange thickness, in millimetres. Availability is a mill-programme question for the named quality, not a property of the size table. Mid-range square and narrow sections are the usual enquiry core; rows marked * are identified as other than general-purpose and should be confirmed size by size, especially in SM490C or the YA/YB qualities.
The flange thickness decides the yield band, and the band is not the same for A/B/C as for YA/YB. H 200×200×8×12, with a 12 mm flange, is 325 N/mm² in SM490A, B or C and 365 N/mm² in SM490YA or YB. H 400×400×13×21, with a 21 mm flange, steps down to 315 N/mm² or 355 N/mm² respectively. H 148×100×6×9 is a 150×100-series section whose actual depth is 148 mm, not a 150 mm square H-section.
For SM490C, SM490YA and SM490YB, the standard section scope stops at 100 mm. Heavier 400×400 rows with flanges above 100 mm are not filled from those qualities under the ordinary Table 1 limits; they would have to be an agreed departure, which this page does not invent.
Swipe horizontally to view all dimensions.
Rows marked * are the 20 sizes that Table 15 identifies as other than general-purpose. Constant outside-dimension H-sections and I-beams can be reviewed when named. Chinese HW, HM and HN names belong to GB/T 11263; European series belong to EN 10025-2 practice.
SM490A, SM490B, SM490C, SM490YA and SM490YB Are Different Qualities
An enquiry that only says “SM490 H-beam” is incomplete. The five symbols below are the designations JIS G 3106:2020 actually tables in this tensile class. SM490A is not a quieter way of writing SM490B. SM490C is not SM490B with a different letter for the same 27 J test. SM490YA and SM490YB use a higher yield table, and only YB carries a standard impact test.
SM490 Chemical Composition by Quality (Heat Analysis)
The figures below are heat-analysis maxima from Table 2 of JIS G 3106:2020. Thickness for sections is t2 of the H-section in JIS G 3192. Carbon is tighter for SM490B than for SM490A in both thickness bands, and SM490C is limited to 0.18% through its 100 mm scope. SM490YA and SM490YB share one carbon table, 0.20% through 100 mm, which is not the same as SM490A above 50 mm. Phosphorus and sulphur are 0.035% for all five symbols. Elements with no tabulated limit, and elements not listed, may be added as necessary and shall be reported if they are.
SM490 Mechanical Properties: Two Yield Tables and Three Impact Cases
Tensile properties follow Table 7 of JIS G 3106:2020. Thickness is that at the test-piece location. SM490A, SM490B and SM490C share one yield and tensile table through 100 mm; only A and B continue, under the standard scope, through 200 mm. SM490YA and SM490YB share a higher yield table through 100 mm, with the same 490–610 N/mm² tensile range. Annex JB (leg length under 40 mm) does not apply to the standard H-sections tabulated above.
Yield and tensile — SM490A, SM490B and SM490C:
Yield and tensile — SM490YA and SM490YB:
Elongation uses different minima for the two yield groups:
For No. 4 test pieces on products thicker than 100 mm, the standard reduces the tabulated elongation by 1 for each 25 mm or fraction of thickness, with a maximum reduction of 3. That rule is relevant only where a quality is actually supplied above 100 mm (SM490A or SM490B in the standard section scope).
Charpy testing in clause 8.2 applies to the symbols listed in Table 8 when the thickness is over 12 mm. The result is the mean of three V-notch test pieces in the rolling direction. SM490A and SM490YA are not in that table.
A lower test temperature than the one tabulated may be applied by agreement. A warmer-quality or A-quality certificate does not demonstrate a B, C or YB test.
Delivery Conditions, Inspection and Identification
SM490 sections are commonly supplied as-rolled. Heat treatment, including normalizing or a thermo-mechanical control process, is used when agreed; any agreed heat-treatment symbol is suffixed to the grade (for example SM490CN). The inspection document should show JIS G 3106 and its edition, the full quality symbol (SM490A, B, C, YA or YB), the JIS G 3192 size designation, the delivery condition, the heat number, the heat analysis, the tensile results by thickness, and, for B, C or YB, the Table 8 impact result. An A or YA certificate does not demonstrate a 0 °C test.
If not otherwise specified, inspection documents for JIS structural steels are commonly requested as JIS G 0415 type 3.1; type 3.2 or nominated third-party attendance can be added when the specification requires it. Identification follows the mill’s marking practice. Standard lengths in JIS G 3192 are in the region of 6–13 m; other lengths are a matter for the rolling programme and the order.
Weldability of SM490 H-Beams
The SM family is specified as rolled steel for welded structure. That does not replace a welding procedure. In JIS G 3106:2020, the tabulated carbon-equivalent and crack-sensitivity limits in clause 7.1 apply to SM570, and the SM490 carbon-equivalent figures in clause 7.2 apply to plates and sheets made by a thermo-mechanical control process. This page does not treat those plate TMCP figures as a default CEV for as-rolled H-sections, and it does not invent a substitute limit. If a carbon equivalent or PCM value is required on a section order, it should be agreed and verified on that order.
The as-rolled surface is mill scale. Blast, paint or galvanizing is an order option and should be reviewed against the actual silicon and the coating specification. Cutting, weld-end preparation, forming or coating can be reviewed when that specification is sent with the enquiry.
JIS G 3192 Shape Tolerances and Theoretical Mass
Dimensional and mass tolerances for these H-sections are those of JIS G 3192, not of JIS G 3106. This article does not reproduce the millimetre tolerance tables; acceptance is against the edition named on the order.
A delivered H 300×300×10×15 will measure close to 300 × 300 × 10 × 15 mm within those tolerances, not as a set of exact advertised millimetres. Out-of-square and web off-centre matter for end-plate connections. Settlement on theoretical or weighed mass should follow the contract.
Applications and Service Limits
SM490 H-beams are used where a Japanese welded-structure grade in the 490 N/mm² tensile class is specified:
- Welded building and industrial frames that name SM490A, SM490B, SM490C, SM490YA or SM490YB, rather than SS400 or a European S355 quality.
- Members that need a 0 °C test at 27 J (B or YB) or at 47 J (C), or a higher yield table (YA or YB), provided the matching symbol is the one actually ordered.
- Export packages that compare a named quality with Q355B H-beam or with S355JR H-beam, provided each line keeps its own standard, quality letter and shape system.
It is not specified here for pressure equipment, for nuclear safety-related components, or for structures that actually require a weathering grade or a European −20 °C quality. Durability comes from the coating or fire-protection system, not from the SM490 tensile class.
SM490 Compared with SS400, Q355B and S355JR
SS400 can use the same JIS H-section series, but it is a JIS G 3101 general-structure grade with a lower tensile range and no Charpy table. It does not fulfil an SM490B or SM490C order. Q355B and S355JR are useful 355 MPa comparisons only if the impact test, chemistry and shape standard are also satisfied. S355J0 and S355J2 are different European qualities, not automatic stand-ins for SM490B, C or YB.
Dual certification requires every requirement of each named standard and quality to be met on the delivered piece. Naming “SM490” without A, B, C, YA or YB is not a complete specification.
Near-Equivalents: Not Automatic Substitutes
The comparisons below are for orientation. They are not a licence to substitute one grade or one quality letter for another on a contract or an inspection certificate.
The SS400 H-beam page in this series will be linked here once it is published. Until then, use the live category, plate, Q355B and S355JR links above.
Sourcing SM490 H-Beams from SHH STEEL
SHH STEEL supplies SM490 H-beams as an export trading house, coordinating mill production and project procurement. For this family the useful work is to keep the quality letter on the order (A, B, C, YA or YB), to keep a 27 J certificate from being treated as a 47 J SM490C result, to distinguish the higher YA/YB yield table from A/B/C, and to align the JIS G 3192 designation and the inspection document with the edition named on the order before a rolling programme is committed.
Sections can be sourced from mills that SHH STEEL buys from, including Masteel, Rizhao Steel, Laiwu (Shandong Steel Laiwu) and Tung Ho Steel, among others when the programme matches the order. Those mills do not each roll every JIS H-section in every SM490 quality. Mid-range sizes in SM490A or SM490B are the usual core; C, YA, YB, asterisked Table 15 rows and heavy 400×400 variants are confirmed per line.
The same enquiry can also cover Chinese, American or European designations, provided each line states its material standard, quality letter, shape standard and size. If cutting, weld-end preparation, forming or a coating system is required, include that specification for review. Export packing and container loading can be arranged to the packing list agreed for the shipment.
SM490 H-Beam FAQs
-
Is there a single grade called only SM490?
- No. JIS G 3106 tables SM490A, SM490B, SM490C, SM490YA and SM490YB as separate symbols in the same tensile class. The order and the inspection document should use one of those five designations. A suffixless “SM490” is not a complete specification.
-
Is SM490C the same as SM490B?
- No. Both are tested at 0 °C when thickness exceeds 12 mm, but SM490C requires 47 J rather than 27 J, has a tighter carbon maximum (0.18% through 100 mm), and has a standard section scope of 100 mm rather than 200 mm. A B result does not meet C.
-
Do SM490A and SM490YA have an impact test?
- Not in Table 8 of JIS G 3106:2020. Clause 8.2 applies the Charpy test to the symbols listed in that table. A and YA are not listed. A toughness guarantee must not be inferred from the 490 tensile class or from the higher YA yield table.
-
What is the difference between SM490A and SM490YA?
- Both lack a standard Table 8 impact test, but they do not share a yield table or a thickness scope. Up to 16 mm, A has a minimum yield of 325 N/mm² and YA 365 N/mm². YA (and YB) is limited to 100 mm in the standard section scope; A may run to 200 mm.
-
Which standards should appear on the inspection document?
- At least JIS G 3106 and its edition, the full quality symbol (SM490A, B, C, YA or YB), the JIS G 3192 designation, the delivery condition, heat analysis, tensile results by thickness, and, for B, C or YB, the specified 0 °C impact result.
Request a Quotation for JIS G 3106 SM490 H-Beam
JIS G 3106 SM490 H-beam is ordered as SM490A, SM490B, SM490C, SM490YA or SM490YB — not as a suffixless grade. Nominate the quality letter, the JIS G 3192 H-section size, and the material to JIS G 3106:2020 (or the edition on the order). The size table is a reference series, not a rolling list. Send the quality, size list, edition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.