JIS G3118 SGV450 Steel Plate | SGV450 Carbon Vessel Plate | JIS G3118 Steel - SHH STEEL

JIS G3118 SGV450 Steel Plate | SGV450 Carbon Vessel Plate

JIS G3118 SGV450 is a hot-rolled carbon steel plate for pressure vessels for intermediate and moderate temperature service, to JIS G 3118:2024. It has 450–540 N/mm² tensile strength and 245 N/mm² minimum yield, in thicknesses from 6 mm to 200 mm. SHH STEEL produces and exports this plate to the ordered heat treatment and tests.
Equivalent Grades:
Near: ASTM A516 Grade 65, EN 10028-2 P295GH. Not automatic substitutes.
Heat Treatment
As-rolled up to 38 mm (N optional); normalized over 38 mm; TMC by agreement.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is JIS G3118 SGV450 steel plate?

JIS G3118 SGV450 is a hot-rolled carbon steel plate for pressure vessels for intermediate and moderate temperature service, to JIS G 3118:2024. The standard is written for plates used in pressure vessels operating mainly from moderate to ordinary temperatures. SGV450 has a tensile strength of 450–540 N/mm² and a minimum yield point or proof stress of 245 N/mm².

JIS G 3118:2024 was revised and gazetted on 20 November 2024 and replaced JIS G 3118:2020. It is based on ISO 9328-1:2018 and ISO 9328-2:2018 with technical modifications (MOD). The current edition has three grades only: SGV410, SGV450 and SGV480, applicable from 6 mm to 200 mm thickness. The 2024 revision clarified the heat-treatment designation rules, defined yield point or proof stress, removed the elongation relaxation for plates over 90 mm and added an ordering-information clause.

SHH STEEL produces and exports JIS G3118 SGV450 plate as a producer, exporter and mill agent, to the thickness, heat-treatment symbol and inspection document written on the enquiry. The grade sits in our JIS G3118 range under Nuclear-Grade Steel Plates. The sibling grades are JIS G3118 SGV410, JIS G3118 SGV480.

Material specification for JIS G3118 SGV450

The table summarises the standard items for this grade. Sizes are agreed per order; no stock range is implied.

Parameter Detail
Standard JIS G 3118:2024, Carbon steel plates for pressure vessels for intermediate and moderate temperature services
Grade SGV450
Applicable thickness 6 mm to 200 mm (standard scope)
Steelmaking Fine-grain killed steel
Heat treatment As-rolled up to 38 mm (normalizing optional or on request); normalized over 38 mm; see Delivery Conditions
Austenitic grain size No. 5 or finer
General delivery JIS G 0404; inspection document JIS G 0415 3.1 unless otherwise specified
Dimensions JIS G 3193 with the thickness tolerance of this standard
Our supply We produce and export JIS G3118 SGV450 plate to the order

Chemical composition of JIS G3118 SGV450

Heat analysis shall meet Table 3 of JIS G 3118:2024; product analysis (Table 4) applies when the purchaser requests it. Carbon limits depend on thickness.

Thickness, mm C max, heat % Si, heat % Mn, heat % P max, % S max, %
6 to 12.5 0.24 0.15–0.40 0.85–1.20 0.020 0.020
over 12.5 to 50 0.26 0.15–0.40 0.85–1.20 0.020 0.020
over 50 to 100 0.28 0.15–0.40 0.85–1.20 0.020 0.020
over 100 to 200 0.29 0.15–0.40 0.85–1.20 0.020 0.020

Product analysis: C as above, Si 0.13–0.45 %, Mn 0.80–1.25 %, P and S 0.020 % max. For each 0.01 % reduction below the carbon maximum, the manganese maximum may be raised by 0.06 %, up to 1.60 %. Alloying elements not listed may be added where necessary and must then be reported.

Weldability (Clause 7): for thermo-mechanically controlled (TMC) plate the carbon equivalent Ceq = C + Mn/6 + Si/24 + Ni/40 + Cr/5 + Mo/4 + V/14 applies, or by agreement the weld cracking parameter PCM.

TMC plate thickness, mm Ceq max, % PCM max, % (by agreement)
6 to 50 0.38 0.23
over 50 to 100 0.40 0.25

Mechanical properties of JIS G3118 SGV450

Tensile and bend properties shall meet Table 7 of JIS G 3118:2024. Test pieces are transverse to the final rolling direction. Unless otherwise specified, the yield point is the upper yield point ReH; where no yield point appears, the 0.2 % proof stress is measured.

Property Requirement
Yield point or proof stress, min 245 N/mm²
Tensile strength 450–540 N/mm²
Elongation, 6 to 40 mm, No. 1A test piece 19 % min
Elongation, over 40 to 50 mm 19 % min (No. 1A) or 23 % min (No. 10)
Elongation, over 50 to 200 mm, No. 10 test piece 23 % min

For No. 1A pieces, elongation is reduced by 1 for each 1 mm under 8 mm thickness, and by 0.5 for each 3 mm over 20 mm, to a maximum reduction of 3.

Bend test thickness, mm Inside radius (180°)
6 to 25 0.75 × t
over 25 to 50 1.0 × t
over 50 to 100 1.0 × t
over 100 to 200 1.25 × t

The bend test may be omitted at the manufacturer’s discretion, but the plate must still meet it, and it is performed when the purchaser specifies it. Charpy impact, ultrasonic and sulphur-print tests are not base requirements; they are agreed separately when needed.

Heat treatment and delivery condition of JIS G3118 SGV450

Heat treatment follows Table 2 of JIS G 3118:2024.

Thickness, mm Plate heat treatment
6 to 38 As-rolled; the manufacturer may normalize, and the purchaser may specify normalizing; thermo-mechanical control processing by agreement
over 38 to 100 Normalized
over 100 to 200 Normalized

By agreement, accelerated cooling after normalizing followed by tempering may be applied. Where the purchaser will carry out a heat treatment in place of normalizing, the plate may be supplied as-rolled or with the treatment the purchaser specifies, and the purchaser states the test-piece heat treatment. Symbols are added after the grade: N (normalized plate), TN (normalized test piece), TMC (thermo-mechanically controlled), SR (test piece given a PWHT-equivalent treatment), for example SGV450N or SGV450NSR.

Welding JIS G3118 SGV450 plate

JIS G3118 SGV450 is a fine-grain killed carbon-manganese steel and is readily weldable with a qualified procedure. Carbon rises with thickness, so preheat should be set for the actual thickness, restraint and consumables.

For TMC plate the Ceq or PCM limits in Chemical Composition apply and are reported on the certificate.

Weld repair of surface defects requires the purchaser’s prior approval.

Dimensions and thickness tolerance

Shape, dimensions and mass follow JIS G 3193, with the thickness tolerance of JIS G 3118:2024 Table 8. The minus tolerance is 0.25 mm; where 0 mm minus is agreed, 0.25 mm is added to the plus tolerance. Widths of 5000 mm and over are by agreement.

Thickness, mm Plus tolerance, width under 1600 mm Plus tolerance, width 2500 to under 3150 mm
6.00 to under 6.30 +0.75 +1.25
16.0 to under 25.0 +1.05 +1.65
40.0 to under 63.0 +1.35 +1.95
100 to under 160 +2.35 +3.15
160 to 200 +2.95 +3.55

Width tolerance is cut-edge tolerance A and length tolerance A of JIS G 3193 unless otherwise specified.

Applications and standard limits

JIS G3118 SGV450 plate is used for boiler drums, pressure vessels, heat-exchanger shells and similar welded pressure equipment working at moderate and intermediate temperatures.

Listing this specification in our JIS G3118 range under the Nuclear-Grade Steel Plates family is a catalogue grouping only. It is not a nuclear qualification, an RCC-M qualification or an ASME Section III certification of SHH STEEL, of the mill or of any heat. Where plate is intended for nuclear construction, the Code edition, material organisation and quality-system rules, fracture-toughness testing and project chemistry limits must be written on the purchase order and confirmed before acceptance.

  • Thickness: 6 mm to 200 mm per the standard
  • Low-temperature service needs impact testing agreed separately; this standard has no base impact requirement
  • Allowable stresses come from the code named on the order

Compare JIS G3118 SGV450 with related plates

Within JIS G3118 the grade is set by tensile strength level. SGV450 must not be replaced by a lower grade, and a higher grade changes carbon limits and welding behaviour. Related JIS plates are written to other standards.

Grade Tensile strength, N/mm² Yield, min, N/mm² Relation
JIS G3118 SGV450 450–540 245 This page
JIS G3118 SGV410 410–490 225 Same standard, different strength
JIS G3118 SGV480 480–590 265 Same standard, different strength
JIS G3115 SPV410 Per JIS G3115 Per JIS G3115 Higher-yield vessel plate, different standard
JIS G3103 SB450 Per JIS G3103 Per JIS G3103 Boiler plate, different standard

Equivalent and related grades for JIS G3118 SGV450

Equivalents below are engineering judgement only and are not automatic substitutes. Chemistry, heat treatment and test rules differ; any equivalence must be approved by the designer or code authority.

Region Grade Note
USA ASTM A516 Grade 65 Similar tensile class carbon vessel plate; engineering judgement only
Europe EN 10028-2 P295GH Elevated-temperature carbon vessel plate; different test basis; engineering judgement only
Japan JIS G3103 SB450 Boiler and pressure vessel plate; different standard; engineering judgement only

Why choose SHH STEEL for JIS G3118 SGV450

  • SHH STEEL produces and exports JIS G3118 SGV450 plate as a producer, exporter and mill agent
  • We check carbon by thickness, heat-treatment symbol and Table 7 properties against JIS G 3118:2024
  • We state the heat-treatment symbol on the certificate and marking
  • We do not present the Nuclear-Grade Steel Plates listing as a nuclear qualification
  • We match the inspection document to the order

How to enquire for JIS G3118 SGV450

Item What to state
Standard JIS G 3118:2024, SGV450
Heat treatment Symbol required, for example N, TN, TMC, SR
Size Thickness, width, length and quantity
Extra tests Impact, ultrasonic or other tests by agreement
Documentation JIS G 0415 3.1 by default, or as specified

Cutting and processing can be added when written on the order.

FAQ

What is JIS G3118 SGV450?
A carbon steel plate for pressure vessels for intermediate and moderate temperature service to JIS G 3118:2024, with 450–540 N/mm² tensile strength and 245 N/mm² minimum yield.
What is the current edition?
JIS G 3118:2024, gazetted on 20 November 2024, replacing JIS G 3118:2020. It has three grades: SGV410, SGV450 and SGV480.
How is it heat treated?
Up to 38 mm as-rolled, with normalizing optional or on request; over 38 mm normalized. TMC by agreement. The symbol, such as N or SR, follows the grade.
What thickness does the standard cover?
6 mm to 200 mm. Actual sizes are agreed per order.
Is impact testing required?
No base impact requirement exists in JIS G 3118. Charpy or other tests are agreed between purchaser and manufacturer when needed.

Request a quotation

Contact SHH STEEL for a quotation for JIS G3118 SGV450 carbon steel pressure vessel plate. Please send the specification and edition, grade, thickness, width, length, quantity, delivery destination and preferred delivery schedule so we can review your production and export requirements.

State the heat-treatment symbol, for example SGV450N or SGV450NSR, and any agreed impact or ultrasonic tests.

State any supplementary requirements, simulated post-weld heat treatment, impact testing, ultrasonic examination and the inspection document required, so they are agreed before the order is placed.

For a detailed quotation, email your material specification, drawing, quantity and delivery requirements to our team.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *