GB/T 3280 022Cr23Ni5Mo3N S22053 Cold Rolled Stainless Steel Plate at SHH STEEL warehouse

GB/T 3280 022Cr23Ni5Mo3N S22053 Cold Rolled Stainless Steel Plate

GB/T 3280 022Cr23Ni5Mo3N S22053 Cold Rolled Stainless Steel Plate: duplex grade to GB/T 3280-2015, sheet in 2B and No.1 finishes from stock in China. SHH STEEL supplies mill-direct material with EN 10204 3.1/3.2 certificates, third-party inspection and cutting to size.
Keywords
GB/T 3280 022Cr23Ni5Mo3N sheet, 022Cr23Ni5Mo3N sheet, 022Cr23Ni5Mo3N stainless sheet supplier, GB/T 3280-2015 022Cr23Ni5Mo3N, 022Cr23Ni5Mo3N sheet stock China
Equivalent Grades:
UNS S32205; EN 1.4462 X2CrNiMoN22-5-3; JIS SUS329J3L
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Performance
Grade Selection
Heat Treatment
Surface Finishes
Tolerances
Stock
Equivalent Grades
Related Grades
Applications and Fabrication
Testing and Inspection
Specification Mistakes
Buyer Concerns
How to Order
FAQ
Conclusion

What is GB/T 3280 022Cr23Ni5Mo3N S22053 Cold Rolled Stainless Steel Plate?

Technical reviewer: Jack · Updated: 2026-10-21

Equivalent grades: 022Cr23Ni5Mo3N (S22053) ≈ UNS S32205 ≈ EN 1.4462 X2CrNiMoN22-5-3 ≈ JIS SUS329J3L.

022Cr23Ni5Mo3N (S22053) is a duplex grade. 022Cr23Ni5Mo3N is the Chinese 2205 duplex grade with Cr 22.0–23.0 % and N 0.14–0.20 %, matching UNS S32205.

GB/T 3280-2015 is the Chinese national standard for cold-rolled stainless steel plate, sheet and strip. It is the cold-rolled counterpart of GB/T 4237 (hot rolled) and uses the same grade names and unified numeric codes (ISC) from GB/T 20878. Cold-rolled sheet is the normal product for thin gauges with 2B, BA or polished finishes.

This page sets out the GB/T 3280-2015 requirements for 022Cr23Ni5Mo3N (S22053) sheet: specification summary, chemistry, mechanical properties, corrosion resistance, heat treatment, finishes and tolerances, current stock, equivalents, fabrication and testing. SHH STEEL supplies it mill-direct from China with EN 10204 3.1 certificates, optional third-party inspection and in-house cutting.

022Cr23Ni5Mo3N (S22053) sheet: specification summary

Item 022Cr23Ni5Mo3N (S22053) data
Standard GB/T 3280-2015, cold-rolled stainless steel plate, sheet and strip
Product form cold-rolled plate, sheet and strip
Typical thickness 0.3–6.0 mm
Widths 1000, 1219, 1250, 1500 mm; slit coil to order
Lengths 2000, 2438, 2500, 3000 mm or cut to size
Finishes 2D, 2B, BA, No.3, No.4, HL
Heat treatment solution treated (austenitic, duplex) or annealed (ferritic)
Tests chemical analysis, tensile, hardness; bend and intergranular corrosion (GB/T 4334) where specified
Certificates mill certificate to GB/T 18253 (EN 10204 3.1 type); 3.2 on request
Grade family duplex

Size range. Sheet is normally cold rolled from about 0.3–0.5 mm up to 3 mm and hot rolled from about 3 mm to just under 5 mm. Coil widths of 1000, 1219, 1250 and 1500 mm are standard; slitting and cut-to-length lines produce narrower strip and exact lengths. Sheets thinner than 0.5 mm or wider than 1500 mm should be confirmed before ordering. 022Cr23Ni5Mo3N (S22053) is produced regularly by several mills; common sizes are held in stock, and other sizes are rolled in the mill’s scheduled campaigns for the grade.

Chemical composition of 022Cr23Ni5Mo3N (S22053) (GB/T 3280-2015)

Element wt %
C 0.03 max
Si 1 max
Mn 2 max
P 0.03 max
S 0.02 max
Cr 22–23
Ni 4.5–6.5
Mo 3–3.5
N 0.14–0.2

Single values are maximums unless marked min. Ranges are heat (cast) analysis limits.

PREN check (Cr + 3.3 Mo + 16 N): about 34.1 at the specification minimums and about 35.9 at mid-range. Where corrosion resistance is critical, write a minimum PREN on the order and ask for the calculated value from the heat analysis on the certificate.

Mechanical properties of 022Cr23Ni5Mo3N (S22053) sheet

Rp0.2 min, MPa Rm min, MPa A min, % HBW max HRC max HV max
450 655 25 293 31 —

The minimum yield strength of 450 MPa is about 2.6 times the 170 MPa minimum of ASTM 316L. Designers use this to reduce thickness, but higher strength also means higher press loads and more springback. Mill values for production heats are usually well above the minimums; use certificate values when you calculate bending forces. Tension tests are taken in the direction stated in the standard; where a hardness limit is given, it is a maximum that confirms correct annealing.

Corrosion resistance of 022Cr23Ni5Mo3N (S22053): PREN and limits

Duplex steels combine about half ferrite and half austenite after solution annealing. The structure gives about twice the yield strength of 304L/316L and much better resistance to chloride stress-corrosion cracking. The PREN (Cr + 3.3 Mo + 16 N) at the specification minimum is about 34.1; a mid-range heat is about 35.9, which places the grade relative to 304L (about 18), 316L (about 24) and 2205 (about 34).

The phase balance depends on correct solution annealing and fast cooling. Too low an annealing temperature or slow cooling can precipitate sigma, chi or chromium nitrides, which cut toughness and corrosion resistance without any visible sign. That is why project specifications add ASTM A923 Method A/B/C tests and a ferrite range. Duplex grades are not recommended for long service above about 300 °C, where 475 °C embrittlement of the ferrite begins.

How 022Cr23Ni5Mo3N (S22053) compares with related grades

Grade Cr Ni Mo N PREN (min) YS / Rp0.2 min, MPa
022Cr23Ni5Mo3N (S22053) 22–23 4.5–6.5 3–3.5 0.14–0.2 34.1 450
UNS S82441 23.0–25.0 3.0–4.5 1.00–2.00 0.20–0.30 29.5 540
UNS S32003 19.5–22.5 3.0–4.0 1.50–2.00 0.14–0.20 26.7 485
UNS S32202 21.5–24.0 1.00–2.80 0.45 max 0.18–0.26 24.4 450
UNS S32900 23.0–28.0 2.0–5.0 1.00–2.00 — 26.3 485

Choose 022Cr23Ni5Mo3N (S22053) when you need more strength and chloride stress-corrosion resistance than 316L at lower cost than super-austenitic or super-duplex grades. Do not use it for long-term service above about 300 °C or where full non-magnetic behaviour is required.

The table uses specification limits, not typical mill values, so it shows the guaranteed position of each grade. Final selection should also consider product availability in the thickness you need, welding consumables, and the inspection requirements of your project.

Heat treatment and delivery condition of 022Cr23Ni5Mo3N (S22053)

Heat treatment: 1 040 – 1 100 °C, water quench (or rapid cooling for thin sections).

Rapid cooling from the solution-anneal temperature is essential to avoid sigma, chi and chromium nitrides in the 700–1000 °C range. Stress relieving in that range is not allowed; any hot forming must be followed by a full solution anneal and quench.

Surface finishes for 022Cr23Ni5Mo3N (S22053) sheet

GB/T 3280 sheet is supplied in cold-rolled finishes: 2D (dull, for deep drawing), 2B (skin passed, the general-purpose finish), BA (bright annealed), and polished No.3, No.4 or HL (hairline). Decorative finishes and PVC or laser film are available. State the finish and film side on the order.

Dimensions, tolerances and flatness

Thickness, width, length and flatness tolerances are tabulated in GB/T 3280, with normal and higher precision classes. For laser-cut blanks, specify flatness and, if needed, tension-levelled sheet. Coil slit to width keeps edge camber low.

Chinese grade names and codes. GB/T 3280 uses the GB/T 20878 grade names, which spell out the composition (carbon in hundredths of a percent followed by alloying elements), and the unified numeric code (ISC) such as S22053. GB/T 20878-2024 renamed a few grades, so a certificate may show either the 2007 or the 2024 form; the ISC code is the safest identifier. Order with both the grade name and the code, the finish, the thickness tolerance class and the certificate type. Export orders often also ask for the ASTM or JIS designation on the certificate as a reference only.

022Cr23Ni5Mo3N (S22053) sheet stock in China

Thickness (mm) Width (mm) Length (mm) Finish Approx. quantity Location
0.5 1000 / 1219 2000 / 2438 2B 200+ t China
0.8 1219 2438 2B 200+ t China
1.0 1219 / 1250 2438 / 2500 2B 100+ t China
1.5 1219 / 1500 2438 / 3000 2B 100+ t China
2.0 1219 / 1500 2438 / 3000 2B 100+ t China
3.0 1500 3000 2B / No.1 100+ t China
4.0 1500 3000 / 6000 No.1 100+ t China

Quantities are approximate and stock changes daily. Send your size list for current availability; other thicknesses, widths and cut sizes can be supplied from mill production.

Packing and logistics. Sheet is packed on wooden or steel pallets with interleaving paper or PVC film, edge protectors and waterproof wrapping, typically 2–3 t per pallet. Coil is packed eye-to-wall or eye-to-sky with steel bands. We consolidate mixed grades and sizes into one container and send loading photos with the shipping documents.

022Cr23Ni5Mo3N (S22053) equivalents in other standards

Standard Designation Comment
ASTM / UNS UNS S32205 same alloy family and limits closely matched; compare each limit on the certificate
EN 1.4462 X2CrNiMoN22-5-3 same alloy family and limits closely matched; compare each limit on the certificate
JIS SUS329J3L same alloy family and limits closely matched; compare each limit on the certificate

Equivalents are close, not identical. When a project names one standard, order to that standard or ask for multiple certification and check every limit on the certificate.

Related grades by alloy family

Duplex and lean duplex

Duplex grades with about twice the yield strength of 316L: A240 S32304, A240 S32101, 1.4362 plate.

Super duplex

PREN 40+ duplex grades for seawater and severe chlorides: A240 S32750, 1.4410 plate, 1.4501 plate, 1.4507 plate.

Austenitic

General-purpose austenitic grades for comparison: A240 S30400.

Same standard

Other grades in this standard: GB/T 3280 S35350, GB/T 3280 S35450, GB/T 3280 S30408.

Same grade, other specification

GB/T 4237 S22053.

Applications, forming and welding of 022Cr23Ni5Mo3N (S22053)

Typical uses: chemical tankers, heat exchangers, FGD ducts, desalination, and offshore equipment.

Duplex sheet and plate need about 1.5–2 times the press force of 316L and show more springback. Cut by plasma, laser or waterjet and remove heat tint by pickling or grinding. For welding use a nickel-enriched duplex filler such as ER2209 (AWS A5.9), never an autogenous weld without filler. Keep the weld area clean and free of carbon-steel contamination, and pickle and passivate after welding where corrosion resistance matters.

Welding practice. Keep heat input in the range of about 0.5–2.5 kJ/mm and interpass temperature below about 150 °C. Too low a heat input gives a highly ferritic weld and HAZ; too high a heat input or slow cooling forms intermetallics. Use argon with 1–2 % nitrogen for GTAW where the specification allows, and back-purge root runs. Qualify the procedure with ferrite measurement and, where specified, A923 tests on the weld.

Certificates, testing and receiving inspection

Every delivery carries a mill certificate to GB/T 3280-2015 with heat analysis, tensile results and hardness, and the grade and standard as ordered. Supplementary tests we can arrange: ASTM A923 Methods A, B and C, ferrite count to ASTM E562, ASTM G48 pitting test, Charpy impact at the project temperature, and PMI on each plate. Third-party witness by SGS, BV, TÜV, DNV, ABS or LR is available with EN 10204 3.2 certificates.

On receipt, check marking and heat number against the certificate, measure thickness at several points and confirm the finish and edge condition before cutting.

Common mistakes when specifying 022Cr23Ni5Mo3N (S22053)

  • Ordering by UNS number only, without minimum N or PREN, and receiving a heat at the bottom of the range.
  • Assuming impact or ferrite requirements from one project apply to all; they come from the project specification, not the product standard.
  • Using 2205 design data for a lean duplex grade, or the reverse; strength and PREN differ.

Each of these can be avoided by writing the requirement into the purchase order and checking it on the certificate before the material is cut.

Sourcing 022Cr23Ni5Mo3N (S22053): buyer concerns and SHH STEEL solutions

Concern How SHH STEEL handles it
Phase balance and intermetallics solution-anneal records checked; A923 and ferrite tests agreed before production
Low nitrogen at the bottom of the range minimum N and PREN written into the order and confirmed from the heat analysis
Small quantities across many sizes mixed thicknesses and grades combined in one shipment
Cutting and edge preparation in-house shearing, plasma, laser and waterjet cutting, bevelling
Delivery delays weekly production and shipping updates with photos

How to order 022Cr23Ni5Mo3N (S22053) sheet

State the standard and edition (GB/T 3280-2015), the grade (022Cr23Ni5Mo3N (S22053)), thickness, width and length or coil, finish, quantity, tolerance class, any added chemistry limits, the supplementary tests and acceptance values from your specification, the certificate type and inspection agency, and packing. Send the list to SHH STEEL and we will reply with price, available stock and lead time.

FAQ

What is the difference between GB/T 3280 and GB/T 4237 022Cr23Ni5Mo3N?
GB/T 3280 covers cold-rolled plate, sheet and strip; GB/T 4237 covers hot-rolled material. The grade names and chemistry are the same, but thickness ranges, finishes and tolerances differ.
Is 022Cr23Ni5Mo3N (S22053) equivalent to UNS S32205?
They are the same alloy designation in different standards. Limits are closely matched, but always order to the standard named in your specification or ask for multiple certification.
What ferrite range should I specify for 022Cr23Ni5Mo3N (S22053)?
Use your project specification. Many specifications ask for 35–55 % ferrite measured to ASTM E562; the product standard itself does not set a range.
Can I order small quantities or cut sizes?
Yes. We combine mixed thicknesses and grades into one shipment and cut plate and sheet to size in our workshop.
Which certificates and tests can you provide?
Every order ships with a mill certificate (EN 10204 3.1 type) showing heat analysis and mechanical tests. Supplementary tests and 3.2 certificates with SGS, BV, TÜV or another agency are available by agreement.

Conclusion

022Cr23Ni5Mo3N (S22053) sheet should be ordered with the points the standard leaves open written into the contract: finish, tolerance class, any extra chemistry limits and the supplementary tests your application needs. With those fixed, stock material from China is a fast and reliable route.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X