GB/T 3280 12Cr17Mn6Ni5N S35350 Cold Rolled Stainless Steel Plate at SHH STEEL warehouse

GB/T 3280 12Cr17Mn6Ni5N S35350 Cold Rolled Stainless Steel Plate

GB/T 3280 12Cr17Mn6Ni5N S35350 Cold Rolled Stainless Steel Plate: Cr-Mn-Ni-N austenitic (200 series) grade to GB/T 3280-2015, sheet in 2B and No.1 finishes from stock in China. SHH STEEL supplies mill-direct material with EN 10204 3.1/3.2 certificates, third-party inspection and cutting to size.
Keywords
GB/T 3280 12Cr17Mn6Ni5N sheet, 12Cr17Mn6Ni5N sheet, 12Cr17Mn6Ni5N stainless sheet supplier, GB/T 3280-2015 12Cr17Mn6Ni5N, 12Cr17Mn6Ni5N sheet stock China
Equivalent Grades:
UNS S20100; EN 1.4372 X12CrMnNiN17-7-5; JIS SUS201
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Performance
Grade Selection
Heat Treatment
Surface Finishes
Tolerances
Stock
Equivalent Grades
Related Grades
Applications and Fabrication
Testing and Inspection
Specification Mistakes
Buyer Concerns
How to Order
FAQ
Conclusion

What is GB/T 3280 12Cr17Mn6Ni5N S35350 Cold Rolled Stainless Steel Plate?

Technical reviewer: Jack · Updated: 2026-10-21

Equivalent grades: 12Cr17Mn6Ni5N (S35350) ≈ UNS S20100 ≈ EN 1.4372 X12CrMnNiN17-7-5 ≈ JIS SUS201.

12Cr17Mn6Ni5N (S35350) is a Cr-Mn-Ni-N austenitic (200 series) grade. 12Cr17Mn6Ni5N is the Chinese 201 grade: part of the nickel is replaced by manganese and nitrogen. It is cheaper than 304 and stronger in the annealed condition, but its pitting resistance and its resistance to acids and chlorides are lower, so it suits dry indoor use.

GB/T 3280-2015 is the Chinese national standard for cold-rolled stainless steel plate, sheet and strip. It is the cold-rolled counterpart of GB/T 4237 (hot rolled) and uses the same grade names and unified numeric codes (ISC) from GB/T 20878. Cold-rolled sheet is the normal product for thin gauges with 2B, BA or polished finishes.

This page sets out the GB/T 3280-2015 requirements for 12Cr17Mn6Ni5N (S35350) sheet: specification summary, chemistry, mechanical properties, corrosion resistance, heat treatment, finishes and tolerances, current stock, equivalents, fabrication and testing. SHH STEEL supplies it mill-direct from China with EN 10204 3.1 certificates, optional third-party inspection and in-house cutting.

12Cr17Mn6Ni5N (S35350) sheet: specification summary

Item 12Cr17Mn6Ni5N (S35350) data
Standard GB/T 3280-2015, cold-rolled stainless steel plate, sheet and strip
Product form cold-rolled plate, sheet and strip
Typical thickness 0.3–6.0 mm
Widths 1000, 1219, 1250, 1500 mm; slit coil to order
Lengths 2000, 2438, 2500, 3000 mm or cut to size
Finishes 2D, 2B, BA, No.3, No.4, HL
Heat treatment solution treated (austenitic, duplex) or annealed (ferritic)
Tests chemical analysis, tensile, hardness; bend and intergranular corrosion (GB/T 4334) where specified
Certificates mill certificate to GB/T 18253 (EN 10204 3.1 type); 3.2 on request
Grade family Cr-Mn-Ni-N austenitic (200 series)

Size range. Sheet is normally cold rolled from about 0.3–0.5 mm up to 3 mm and hot rolled from about 3 mm to just under 5 mm. Coil widths of 1000, 1219, 1250 and 1500 mm are standard; slitting and cut-to-length lines produce narrower strip and exact lengths. Sheets thinner than 0.5 mm or wider than 1500 mm should be confirmed before ordering. 12Cr17Mn6Ni5N (S35350) is one of the high-volume grades produced by most Chinese stainless mills, so common sizes are held in stock and non-stock sizes are usually rolled within a normal mill cycle.

Chemical composition of 12Cr17Mn6Ni5N (S35350) (GB/T 3280-2015)

Element wt %
C 0.15 max
Si 1.00 max
Mn 5.50–7.50
P 0.050 max
S 0.030 max
Cr 16.00–18.00
Ni 3.50–5.50
N 0.05–0.25

Single values are maximums unless marked min. Ranges are heat (cast) analysis limits.

PREN check (Cr + 3.3 Mo + 16 N): about 16.8 at the specification minimums and about 19.4 at mid-range. Where corrosion resistance is critical, write a minimum PREN on the order and ask for the calculated value from the heat analysis on the certificate.

Mechanical properties of 12Cr17Mn6Ni5N (S35350) sheet

Rp0.2 min, MPa Rm min, MPa A min, % HBW max HRB max HV max
per GB/T 3280 per GB/T 3280 per GB/T 3280 per GB/T 3280 per GB/T 3280 per GB/T 3280

The room-temperature mechanical minimums for this grade are as stated in the current edition of the standard and are confirmed by the tensile and hardness results on the mill certificate (EN 10204 3.1) for each heat. Where a hardness limit applies, it is a maximum that confirms correct annealing.

Corrosion resistance of 12Cr17Mn6Ni5N (S35350): PREN and limits

The 200-series grades replace part of the nickel with manganese and nitrogen. Nitrogen raises the annealed strength, and the lower nickel makes the price more stable than 304. The PREN at the specification minimum is about 16.8, lower than 304, so the grades are used for indoor, dry or lightly corrosive service.

Buyers should be aware that low-cost 200-series material sometimes comes with copper or lower chromium than the standard allows. Always check the certificate chemistry, and do not use 200-series in coastal, chloride or acidic environments where 304 or 316 is needed.

How 12Cr17Mn6Ni5N (S35350) compares with related grades

Grade Cr Ni Mo N PREN (min) YS / Rp0.2 min, MPa
12Cr17Mn6Ni5N (S35350) 16.00–18.00 3.50–5.50 — 0.05–0.25 16.8 per standard
12Cr18Mn9Ni5N (S35450) 17.00–19.00 4.00–6.00 — 0.05–0.25 17.8 per standard
UNS S20100 (Type 201) 16.0–18.0 3.5–5.5 — 0.25 max 16.0 260
UNS S20153 (Type 201LN) 16.0–17.5 4.0–5.0 — 0.10–0.25 17.6 310

Choose 12Cr17Mn6Ni5N (S35350) for cost-sensitive indoor products where 304-level corrosion resistance is not required. For outdoor, coastal or food-contact service with salt or acids, use 304 or 316.

The table uses specification limits, not typical mill values, so it shows the guaranteed position of each grade. Final selection should also consider product availability in the thickness you need, welding consumables, and the inspection requirements of your project.

Heat treatment and delivery condition of 12Cr17Mn6Ni5N (S35350)

Heat treatment: 1010–1120 °C, rapid cooling.

200-series grades are solution annealed and cooled rapidly. They work-harden faster than 304, so intermediate anneals may be needed in multi-stage forming.

Surface finishes for 12Cr17Mn6Ni5N (S35350) sheet

GB/T 3280 sheet is supplied in cold-rolled finishes: 2D (dull, for deep drawing), 2B (skin passed, the general-purpose finish), BA (bright annealed), and polished No.3, No.4 or HL (hairline). Decorative finishes and PVC or laser film are available. State the finish and film side on the order.

Dimensions, tolerances and flatness

Thickness, width, length and flatness tolerances are tabulated in GB/T 3280, with normal and higher precision classes. For laser-cut blanks, specify flatness and, if needed, tension-levelled sheet. Coil slit to width keeps edge camber low.

Chinese grade names and codes. GB/T 3280 uses the GB/T 20878 grade names, which spell out the composition (carbon in hundredths of a percent followed by alloying elements), and the unified numeric code (ISC) such as S35350. GB/T 20878-2024 renamed a few grades, so a certificate may show either the 2007 or the 2024 form; the ISC code is the safest identifier. Order with both the grade name and the code, the finish, the thickness tolerance class and the certificate type. Export orders often also ask for the ASTM or JIS designation on the certificate as a reference only.

12Cr17Mn6Ni5N (S35350) sheet stock in China

Thickness (mm) Width (mm) Length (mm) Finish Approx. quantity Location
0.5 1000 / 1219 2000 / 2438 2B 300+ t China
0.8 1219 2438 2B 300+ t China
1.0 1219 / 1250 2438 / 2500 2B 300+ t China
1.5 1219 / 1500 2438 / 3000 2B 200+ t China
2.0 1219 / 1500 2438 / 3000 2B 200+ t China
3.0 1500 3000 2B / No.1 100+ t China
4.0 1500 3000 / 6000 No.1 100+ t China

Quantities are approximate and stock changes daily. Send your size list for current availability; other thicknesses, widths and cut sizes can be supplied from mill production.

Packing and logistics. Sheet is packed on wooden or steel pallets with interleaving paper or PVC film, edge protectors and waterproof wrapping, typically 2–3 t per pallet. Coil is packed eye-to-wall or eye-to-sky with steel bands. We consolidate mixed grades and sizes into one container and send loading photos with the shipping documents.

12Cr17Mn6Ni5N (S35350) equivalents in other standards

Standard Designation Comment
ASTM / UNS UNS S20100 same alloy family and limits closely matched; compare each limit on the certificate
EN 1.4372 X12CrMnNiN17-7-5 same alloy family and limits closely matched; compare each limit on the certificate
JIS SUS201 same alloy family and limits closely matched; compare each limit on the certificate

Equivalents are close, not identical. When a project names one standard, order to that standard or ask for multiple certification and check every limit on the certificate.

Related grades by alloy family

200 series (Cr-Mn-Ni-N)

Lower-nickel 200-series grades: A240 S20200, A240 S30100, A240 S30400.

Austenitic

General-purpose austenitic grades for comparison: A240 S30403, A240 S31600, A240 S31603, A240 S30500, A240 S32100, 1.4301 plate, 1.4307 plate.

Same standard

Other grades in this standard: GB/T 3280 S35450, GB/T 3280 S30408, GB/T 3280 S30403.

Applications, forming and welding of 12Cr17Mn6Ni5N (S35350)

Typical uses: kitchenware and sinks, indoor decoration, furniture tubing, appliance panels, and light-duty structural parts.

200-series sheet work-hardens quickly; allow for higher forming loads than 304. Cut by plasma, laser or waterjet and remove heat tint by pickling or grinding. For welding use an ER308L or ER309L filler; nitrogen-bearing 200-series welds should be kept short and the heat input moderate. Keep the weld area clean and free of carbon-steel contamination, and pickle and passivate after welding where corrosion resistance matters.

Welding practice. 200-series sheet welds like 304 but has a higher work-hardening rate and slightly higher thermal expansion. Use moderate heat input, keep the weld area clean and pickle afterwards. Avoid using 200-series filler in corrosive service; a 308L or 309L filler gives a more corrosion-resistant weld.

Certificates, testing and receiving inspection

Every delivery carries a mill certificate to GB/T 3280-2015 with heat analysis, tensile results and hardness, and the grade and standard as ordered. Supplementary tests we can arrange: chemistry check of Cr, Ni, Mn, Cu and N on every heat, intergranular corrosion test where specified, and PMI. Third-party witness by SGS, BV, TÜV, DNV, ABS or LR is available with EN 10204 3.2 certificates.

On receipt, check marking and heat number against the certificate, measure thickness at several points and confirm the finish and edge condition before cutting.

Common mistakes when specifying 12Cr17Mn6Ni5N (S35350)

  • Accepting 200-series material with copper or low chromium outside the standard.
  • Using it in coastal or chloride service.
  • Not checking the certificate for nitrogen and manganese ranges.

Each of these can be avoided by writing the requirement into the purchase order and checking it on the certificate before the material is cut.

Sourcing 12Cr17Mn6Ni5N (S35350): buyer concerns and SHH STEEL solutions

Concern How SHH STEEL handles it
Off-spec low-cost 200-series full heat chemistry including Cu and N checked against the standard
Corrosion complaints in service application reviewed; 304 or 316 recommended where chlorides are present
Small quantities across many sizes mixed thicknesses and grades combined in one shipment
Cutting and edge preparation in-house shearing, plasma, laser and waterjet cutting, bevelling
Delivery delays weekly production and shipping updates with photos

How to order 12Cr17Mn6Ni5N (S35350) sheet

State the standard and edition (GB/T 3280-2015), the grade (12Cr17Mn6Ni5N (S35350)), thickness, width and length or coil, finish, quantity, tolerance class, any added chemistry limits, the supplementary tests and acceptance values from your specification, the certificate type and inspection agency, and packing. Send the list to SHH STEEL and we will reply with price, available stock and lead time.

FAQ

What is the difference between GB/T 3280 and GB/T 4237 12Cr17Mn6Ni5N?
GB/T 3280 covers cold-rolled plate, sheet and strip; GB/T 4237 covers hot-rolled material. The grade names and chemistry are the same, but thickness ranges, finishes and tolerances differ.
Is 12Cr17Mn6Ni5N (S35350) equivalent to UNS S20100?
They are the same alloy designation in different standards. Limits are closely matched, but always order to the standard named in your specification or ask for multiple certification.
Can 12Cr17Mn6Ni5N (S35350) replace 304?
Only in dry indoor applications. Its corrosion resistance is lower than 304, especially in chloride or acidic environments.
Can I order small quantities or cut sizes?
Yes. We combine mixed thicknesses and grades into one shipment and cut plate and sheet to size in our workshop.
Which certificates and tests can you provide?
Every order ships with a mill certificate (EN 10204 3.1 type) showing heat analysis and mechanical tests. Supplementary tests and 3.2 certificates with SGS, BV, TÜV or another agency are available by agreement.

Conclusion

12Cr17Mn6Ni5N (S35350) sheet should be ordered with the points the standard leaves open written into the contract: finish, tolerance class, any extra chemistry limits and the supplementary tests your application needs. With those fixed, stock material from China is a fast and reliable route.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X