GB/T 3280 12Cr18Mn9Ni5N S35450 Cold Rolled Stainless Steel Plate
What is GB/T 3280 12Cr18Mn9Ni5N S35450 Cold Rolled Stainless Steel Plate?
Equivalent grades: 12Cr18Mn9Ni5N (S35450) ≈ UNS S20200 ≈ EN 1.4373 X12CrMnNiN18-9-5 ≈ JIS SUS202.
12Cr18Mn9Ni5N (S35450) is a Cr-Mn-Ni-N austenitic (200 series) grade. 12Cr18Mn9Ni5N is the Chinese 202 grade. It has more chromium and manganese than 201, slightly better corrosion resistance and a more stable austenite, but it is still for mild indoor service rather than for chlorides.
GB/T 3280-2015 is the Chinese national standard for cold-rolled stainless steel plate, sheet and strip. It is the cold-rolled counterpart of GB/T 4237 (hot rolled) and uses the same grade names and unified numeric codes (ISC) from GB/T 20878. Cold-rolled sheet is the normal product for thin gauges with 2B, BA or polished finishes.
This page sets out the GB/T 3280-2015 requirements for 12Cr18Mn9Ni5N (S35450) sheet: specification summary, chemistry, mechanical properties, corrosion resistance, heat treatment, finishes and tolerances, current stock, equivalents, fabrication and testing. SHH STEEL supplies it mill-direct from China with EN 10204 3.1 certificates, optional third-party inspection and in-house cutting.
12Cr18Mn9Ni5N (S35450) sheet: specification summary
| Item | 12Cr18Mn9Ni5N (S35450) data |
|---|---|
| Standard | GB/T 3280-2015, cold-rolled stainless steel plate, sheet and strip |
| Product form | cold-rolled plate, sheet and strip |
| Typical thickness | 0.3–6.0 mm |
| Widths | 1000, 1219, 1250, 1500 mm; slit coil to order |
| Lengths | 2000, 2438, 2500, 3000 mm or cut to size |
| Finishes | 2D, 2B, BA, No.3, No.4, HL |
| Heat treatment | solution treated (austenitic, duplex) or annealed (ferritic) |
| Tests | chemical analysis, tensile, hardness; bend and intergranular corrosion (GB/T 4334) where specified |
| Certificates | mill certificate to GB/T 18253 (EN 10204 3.1 type); 3.2 on request |
| Grade family | Cr-Mn-Ni-N austenitic (200 series) |
Size range. Sheet is normally cold rolled from about 0.3–0.5 mm up to 3 mm and hot rolled from about 3 mm to just under 5 mm. Coil widths of 1000, 1219, 1250 and 1500 mm are standard; slitting and cut-to-length lines produce narrower strip and exact lengths. Sheets thinner than 0.5 mm or wider than 1500 mm should be confirmed before ordering. 12Cr18Mn9Ni5N (S35450) is produced regularly by several mills; common sizes are held in stock, and other sizes are rolled in the mill’s scheduled campaigns for the grade.
Chemical composition of 12Cr18Mn9Ni5N (S35450) (GB/T 3280-2015)
| Element | wt % |
|---|---|
| C | 0.15 max |
| Si | 1.00 max |
| Mn | 7.50–10.00 |
| P | 0.050 max |
| S | 0.030 max |
| Cr | 17.00–19.00 |
| Ni | 4.00–6.00 |
| N | 0.05–0.25 |
Single values are maximums unless marked min. Ranges are heat (cast) analysis limits.
PREN check (Cr + 3.3 Mo + 16 N): about 17.8 at the specification minimums and about 20.4 at mid-range. Where corrosion resistance is critical, write a minimum PREN on the order and ask for the calculated value from the heat analysis on the certificate.
Mechanical properties of 12Cr18Mn9Ni5N (S35450) sheet
| Rp0.2 min, MPa | Rm min, MPa | A min, % | HBW max | HRB max | HV max |
|---|---|---|---|---|---|
| per GB/T 3280 | per GB/T 3280 | per GB/T 3280 | per GB/T 3280 | per GB/T 3280 | per GB/T 3280 |
The room-temperature mechanical minimums for this grade are as stated in the current edition of the standard and are confirmed by the tensile and hardness results on the mill certificate (EN 10204 3.1) for each heat. Where a hardness limit applies, it is a maximum that confirms correct annealing.
Corrosion resistance of 12Cr18Mn9Ni5N (S35450): PREN and limits
The 200-series grades replace part of the nickel with manganese and nitrogen. Nitrogen raises the annealed strength, and the lower nickel makes the price more stable than 304. The PREN at the specification minimum is about 17.8, lower than 304, so the grades are used for indoor, dry or lightly corrosive service.
Buyers should be aware that low-cost 200-series material sometimes comes with copper or lower chromium than the standard allows. Always check the certificate chemistry, and do not use 200-series in coastal, chloride or acidic environments where 304 or 316 is needed.
How 12Cr18Mn9Ni5N (S35450) compares with related grades
| Grade | Cr | Ni | Mo | N | PREN (min) | YS / Rp0.2 min, MPa |
|---|---|---|---|---|---|---|
| 12Cr18Mn9Ni5N (S35450) | 17.00–19.00 | 4.00–6.00 | — | 0.05–0.25 | 17.8 | per standard |
| 12Cr17Mn6Ni5N (S35350) | 16.00–18.00 | 3.50–5.50 | — | 0.05–0.25 | 16.8 | per standard |
| UNS S20100 (Type 201) | 16.0–18.0 | 3.5–5.5 | — | 0.25 max | 16.0 | 260 |
| UNS S20153 (Type 201LN) | 16.0–17.5 | 4.0–5.0 | — | 0.10–0.25 | 17.6 | 310 |
Choose 12Cr18Mn9Ni5N (S35450) for cost-sensitive indoor products where 304-level corrosion resistance is not required. For outdoor, coastal or food-contact service with salt or acids, use 304 or 316.
The table uses specification limits, not typical mill values, so it shows the guaranteed position of each grade. Final selection should also consider product availability in the thickness you need, welding consumables, and the inspection requirements of your project.
Heat treatment and delivery condition of 12Cr18Mn9Ni5N (S35450)
Heat treatment: 1010–1120 °C, rapid cooling.
200-series grades are solution annealed and cooled rapidly. They work-harden faster than 304, so intermediate anneals may be needed in multi-stage forming.
Surface finishes for 12Cr18Mn9Ni5N (S35450) sheet
GB/T 3280 sheet is supplied in cold-rolled finishes: 2D (dull, for deep drawing), 2B (skin passed, the general-purpose finish), BA (bright annealed), and polished No.3, No.4 or HL (hairline). Decorative finishes and PVC or laser film are available. State the finish and film side on the order.
Dimensions, tolerances and flatness
Thickness, width, length and flatness tolerances are tabulated in GB/T 3280, with normal and higher precision classes. For laser-cut blanks, specify flatness and, if needed, tension-levelled sheet. Coil slit to width keeps edge camber low.
Chinese grade names and codes. GB/T 3280 uses the GB/T 20878 grade names, which spell out the composition (carbon in hundredths of a percent followed by alloying elements), and the unified numeric code (ISC) such as S35450. GB/T 20878-2024 renamed a few grades, so a certificate may show either the 2007 or the 2024 form; the ISC code is the safest identifier. Order with both the grade name and the code, the finish, the thickness tolerance class and the certificate type. Export orders often also ask for the ASTM or JIS designation on the certificate as a reference only.
12Cr18Mn9Ni5N (S35450) sheet stock in China
| Thickness (mm) | Width (mm) | Length (mm) | Finish | Approx. quantity | Location |
|---|---|---|---|---|---|
| 0.5 | 1000 / 1219 | 2000 / 2438 | 2B | 200+ t | China |
| 0.8 | 1219 | 2438 | 2B | 200+ t | China |
| 1.0 | 1219 / 1250 | 2438 / 2500 | 2B | 100+ t | China |
| 1.5 | 1219 / 1500 | 2438 / 3000 | 2B | 100+ t | China |
| 2.0 | 1219 / 1500 | 2438 / 3000 | 2B | 100+ t | China |
| 3.0 | 1500 | 3000 | 2B / No.1 | 100+ t | China |
| 4.0 | 1500 | 3000 / 6000 | No.1 | 100+ t | China |
Quantities are approximate and stock changes daily. Send your size list for current availability; other thicknesses, widths and cut sizes can be supplied from mill production.
Packing and logistics. Sheet is packed on wooden or steel pallets with interleaving paper or PVC film, edge protectors and waterproof wrapping, typically 2–3 t per pallet. Coil is packed eye-to-wall or eye-to-sky with steel bands. We consolidate mixed grades and sizes into one container and send loading photos with the shipping documents.
12Cr18Mn9Ni5N (S35450) equivalents in other standards
| Standard | Designation | Comment |
|---|---|---|
| ASTM / UNS | UNS S20200 | same alloy family and limits closely matched; compare each limit on the certificate |
| EN | 1.4373 X12CrMnNiN18-9-5 | same alloy family and limits closely matched; compare each limit on the certificate |
| JIS | SUS202 | same alloy family and limits closely matched; compare each limit on the certificate |
Equivalents are close, not identical. When a project names one standard, order to that standard or ask for multiple certification and check every limit on the certificate.
Related grades by alloy family
200 series (Cr-Mn-Ni-N)
Lower-nickel 200-series grades: A240 S20100, A240 S30100, A240 S30400.
Austenitic
General-purpose austenitic grades for comparison: A240 S30403, A240 S31600, A240 S31603, A240 S30500, A240 S32100, 1.4301 plate, 1.4307 plate, 1.4404 plate.
Same standard
Other grades in this standard: GB/T 3280 S35350, GB/T 3280 S30408, GB/T 3280 S30403.
Applications, forming and welding of 12Cr18Mn9Ni5N (S35450)
Typical uses: kitchen equipment, decorative panels, appliance parts, and furniture.
200-series sheet work-hardens quickly; allow for higher forming loads than 304. Cut by plasma, laser or waterjet and remove heat tint by pickling or grinding. For welding use an ER308L or ER309L filler; nitrogen-bearing 200-series welds should be kept short and the heat input moderate. Keep the weld area clean and free of carbon-steel contamination, and pickle and passivate after welding where corrosion resistance matters.
Welding practice. 200-series sheet welds like 304 but has a higher work-hardening rate and slightly higher thermal expansion. Use moderate heat input, keep the weld area clean and pickle afterwards. Avoid using 200-series filler in corrosive service; a 308L or 309L filler gives a more corrosion-resistant weld.
Certificates, testing and receiving inspection
Every delivery carries a mill certificate to GB/T 3280-2015 with heat analysis, tensile results and hardness, and the grade and standard as ordered. Supplementary tests we can arrange: chemistry check of Cr, Ni, Mn, Cu and N on every heat, intergranular corrosion test where specified, and PMI. Third-party witness by SGS, BV, TÜV, DNV, ABS or LR is available with EN 10204 3.2 certificates.
On receipt, check marking and heat number against the certificate, measure thickness at several points and confirm the finish and edge condition before cutting.
Common mistakes when specifying 12Cr18Mn9Ni5N (S35450)
- Accepting 200-series material with copper or low chromium outside the standard.
- Using it in coastal or chloride service.
- Not checking the certificate for nitrogen and manganese ranges.
Each of these can be avoided by writing the requirement into the purchase order and checking it on the certificate before the material is cut.
Sourcing 12Cr18Mn9Ni5N (S35450): buyer concerns and SHH STEEL solutions
| Concern | How SHH STEEL handles it |
|---|---|
| Off-spec low-cost 200-series | full heat chemistry including Cu and N checked against the standard |
| Corrosion complaints in service | application reviewed; 304 or 316 recommended where chlorides are present |
| Small quantities across many sizes | mixed thicknesses and grades combined in one shipment |
| Cutting and edge preparation | in-house shearing, plasma, laser and waterjet cutting, bevelling |
| Delivery delays | weekly production and shipping updates with photos |
How to order 12Cr18Mn9Ni5N (S35450) sheet
State the standard and edition (GB/T 3280-2015), the grade (12Cr18Mn9Ni5N (S35450)), thickness, width and length or coil, finish, quantity, tolerance class, any added chemistry limits, the supplementary tests and acceptance values from your specification, the certificate type and inspection agency, and packing. Send the list to SHH STEEL and we will reply with price, available stock and lead time.
FAQ
-
What is the difference between GB/T 3280 and GB/T 4237 12Cr18Mn9Ni5N?
- GB/T 3280 covers cold-rolled plate, sheet and strip; GB/T 4237 covers hot-rolled material. The grade names and chemistry are the same, but thickness ranges, finishes and tolerances differ.
-
Is 12Cr18Mn9Ni5N (S35450) equivalent to UNS S20200?
- They are the same alloy designation in different standards. Limits are closely matched, but always order to the standard named in your specification or ask for multiple certification.
-
Can 12Cr18Mn9Ni5N (S35450) replace 304?
- Only in dry indoor applications. Its corrosion resistance is lower than 304, especially in chloride or acidic environments.
-
Can I order small quantities or cut sizes?
- Yes. We combine mixed thicknesses and grades into one shipment and cut plate and sheet to size in our workshop.
-
Which certificates and tests can you provide?
- Every order ships with a mill certificate (EN 10204 3.1 type) showing heat analysis and mechanical tests. Supplementary tests and 3.2 certificates with SGS, BV, TÜV or another agency are available by agreement.
Conclusion
12Cr18Mn9Ni5N (S35450) sheet should be ordered with the points the standard leaves open written into the contract: finish, tolerance class, any extra chemistry limits and the supplementary tests your application needs. With those fixed, stock material from China is a fast and reliable route.