EN 10297-2 1.4002 Seamless Stainless Steel Tube
What is EN 10297-2 1.4002 Seamless Stainless Steel Tube
EN 10297-2 covers seamless stainless tube for mechanical and general engineering (i.e. not pressure). Within that scope, 1.4002 is the ferritic corrosion-resisting grade X6CrAl13, commercially discussed as 405. Buyers chasing “405 seamless tube” under a European mechanical standard are usually looking for EN 10297-2 1.4002 — not an austenitic pressure page. Duty thread: Al-bearing 13%Cr ferritic seamless tube for annealed mechanical parts that need oxidation resistance without nickel.
Mill path for 1.4002: mechanical OD×wall bands finished +A (annealed), often CFD/HFD descaled. SHH STEEL can make and supply EN 10297-2 1.4002 / X6CrAl13 as seamless general-purpose tube across mechanical OD×wall bands finished +A (annealed), often CFD/HFD descaled, solution annealed or annealed/QT as the grade tables require, documented on EN 10204 3.1 MTCs tied to cast analysis and mechanical results. Use thread: furnace hardware adjacent parts, quenched-and-drawn mechanical sleeves, and general engineering tube where 405-class chemistry is named.
On the shop floor people still say “405 tube,” yet that commercial alias does not select cast chemistry, seamless process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10297-2, 1.4002, the Annex A process/surface symbol, and any Options so the mill applies the correct analysis, piercing/drawing route, heat treatment, mechanical floors, and marking. This number’s job on seamless general-purpose duty is: Al-bearing 13%Cr ferritic seamless tube for annealed mechanical parts that need oxidation resistance without nickel. Typical duties include furnace hardware adjacent parts, quenched-and-drawn mechanical sleeves, and general engineering tube where 405-class chemistry is named. Design caution: elongation floors are modest — do not expect 304-like cold expansion; specify anneal (+A) and verify forming trials. Caution thread: elongation floors are modest — do not expect 304-like cold expansion; specify anneal (+A) and verify forming trials.
EN 10297-2 is seamless product only for this series. When a welded general-purpose twin is required, look to EN 10296-2 rather than forcing a seam into a 10297-2 order. When PED pressure seamless acceptance is mandatory, use EN 10216-5 for the same steel number where it exists. Preferred dimensions commonly reference EN ISO 1127 practice agreed at enquiry. Role reminder for 1.4002: Al-bearing 13%Cr ferritic seamless tube for annealed mechanical parts that need oxidation resistance without nickel. Duty thread: Al-bearing 13%Cr ferritic seamless tube for annealed mechanical parts that need oxidation resistance without nickel.
Inside this seamless general-purpose series, compare EN 10297-2 1.4512, EN 10297-2 1.4016, EN 10297-2 1.4006. Hub: EN 10297-2.
Chemical Composition of EN 10297-2 1.4002
Cast window focus for 1.4002: Buying 405-family seamless tube without locking 1.4002 invites silent chemistry drift. Under EN 10297-2 the cast must satisfy X6CrAl13; highlight elements for this grade include C ≤0.08, Cr 12.0–14.0, Al 0.10–0.30, Si ≤1.00, S ≤0.015. Options for product analysis are agreed at enquiry when the purchaser wants them on the certificate. Commercial alias 405 is body text only. Corrosion thread: aluminium helps scaling resistance in mildly oxidising heat; aqueous chloride resistance remains ferritic-limited.
Below is the BSSA-sourced EN 10297-2 chemistry window for 1.4002 (X6CrAl13). Maxima apply unless a band is printed. SHH STEEL quotes against this window and reports actual cast values on the EN 10204 document — not a rewritten catalogue paraphrase. Duty thread: Al-bearing 13%Cr ferritic seamless tube for annealed mechanical parts that need oxidation resistance without nickel.
| Steel | C | Si | Mn | P | S | Cr | Al |
|---|---|---|---|---|---|---|---|
| 1.4002 / X6CrAl13 | ≤0.08 | ≤1.00 | ≤1.00 | ≤0.040 | ≤0.015 | 12.0–14.0 | 0.10–0.30 |
Mechanical Properties of EN 10297-2 1.4002
Ambient floors focus for 1.4002: Table mechanical floors for 1.4002 / X6CrAl13 are delivery-condition values at room temperature, not elevated-temperature design allowables. Summary: Rp0.2 min 210 MPa, Rp1.0 min 220 MPa, Rm min 400 MPa, longitudinal elongation min 17%. SHH STEEL reports actual tensile results on the EN 10204 3.1 document for the ordered test unit. Family: ferritic corrosion-resisting. Caution thread: elongation floors are modest — do not expect 304-like cold expansion; specify anneal (+A) and verify forming trials.
| Delivery condition | Rp0.2 min (MPa) | Rp1.0 min (MPa) | Rm (MPa) | A long. min (%) | A trans. min (%) | IGC |
|---|---|---|---|---|---|---|
| +A | 210 | 220 | 400 min | 17 | 17 | No |
Ambient values from EN 10297-2:2005 Tables 6–9 for 1.4002 / X6CrAl13. Guideline solution/anneal band (Annex B): 750–850 °C; cooling: air, water or gas.
Seamless Tube Manufacture for EN 10297-2 1.4002
Seamless route narrative for 1.4002: Ferritic seamless 1.4002 (X6CrAl13) is produced from pierced or extruded hollows, then annealed (+A) to restore ductility after hot or cold finishing. Grain-growth control during anneal matters for toughness and forming. Order EN 10297-2 1.4002 with an Annex A surface/process symbol — HFD or CFD for metallically clean descaled tube, CFA when bright-annealed OD is required, CFG/CFP when ground or polished roughness is written into the purchase order. Weld thread: ferritic practice with controlled heat input; grain growth risk rises with overheating — anneal after heavy weld cycles when ductility matters.
Ferritic 1.4002 ships annealed (+A). Annex B points at roughly 750–850 °C with air, water or gas cooling. Do not expect austenitic elongation floors after cold expansion without a forming trial. Forming and expansion trials should respect ferritic elongation floors rather than austenitic shop habits. Duty thread: Al-bearing 13%Cr ferritic seamless tube for annealed mechanical parts that need oxidation resistance without nickel.
State leak-tightness, hydrostatic, eddy-current, or ultrasonic Options explicitly for 1.4002. General-purpose seamless acceptance is not identical to EN 10216-5 TC1/TC2 pressure regimes; copy the Options list you need onto the EN 10297-2 order. Size context for 1.4002: mechanical OD×wall bands finished +A (annealed), often CFD/HFD descaled. Use thread: furnace hardware adjacent parts, quenched-and-drawn mechanical sleeves, and general engineering tube where 405-class chemistry is named.
Dimensions and Tolerances for EN 10297-2 1.4002
Dimensional order line for 1.4002: Dimensional orders for 1.4002 name OD × wall, length tolerance, and the Annex A finish symbol. Exact cut lengths and special end preparations are by agreement. Mechanical od×wall bands finished +a (annealed), often cfd/hfd descaled. Use thread: furnace hardware adjacent parts, quenched-and-drawn mechanical sleeves, and general engineering tube where 405-class chemistry is named.
Length supply for 1.4002 may be mill random, fixed, or multiple cut lengths. Bundle make-up and end protection are confirmed against the packaging clause so bright or polished finishes are not marked in transit. Size hint for 1.4002: mechanical OD×wall bands finished +A (annealed), often CFD/HFD descaled. Duty thread: Al-bearing 13%Cr ferritic seamless tube for annealed mechanical parts that need oxidation resistance without nickel.
Equivalent Grades for EN 10297-2 1.4002
Equivalence talk for 1.4002 starts with X6CrAl13: 1.4002 / X6CrAl13 is the EN 10297-2 designation for this chemistry as seamless general-purpose tube. Commercial alias 405 appears in body text only — not in the H1. ASTM/ASME pages that share a related chemistry are different product standards with different wall bases, mechanical tables, and tests. Confirm before treating them as interchangeable. Inside this seamless general-purpose series, compare sisters 1.4512, 1.4016, 1.4006. Hook for buyers still using only the 405 alias: lock EN 10297-2 1.4002 on the order line. Caution thread: elongation floors are modest — do not expect 304-like cold expansion; specify anneal (+A) and verify forming trials.
Heat Treatment and Delivery Condition for EN 10297-2 1.4002
Ferritic 1.4002 ships annealed (+A). Annex B points at roughly 750–850 °C with air, water or gas cooling. Do not expect austenitic elongation floors after cold expansion without a forming trial. Weld thread: ferritic practice with controlled heat input; grain growth risk rises with overheating — anneal after heavy weld cycles when ductility matters.
Fabrication HT reminder for 1.4002 (+A): Hot-working temperature bands in Annex B for X6CrAl13 are guidance during further processing (for example hot bending). Cooling type matters — chase the rapid cool required for austenitic and duplex solution anneal; ferritic anneal practice differs. Delivery framing on the certificate for 1.4002 should match +A. Duty thread: Al-bearing 13%Cr ferritic seamless tube for annealed mechanical parts that need oxidation resistance without nickel.
Corrosion Resistance of EN 10297-2 1.4002
Corrosion behaviour of EN 10297-2 1.4002 tracks its ferritic corrosion-resisting balance: aluminium helps scaling resistance in mildly oxidising heat; aqueous chloride resistance remains ferritic-limited. This standard’s IGC column (where present) refers to EN ISO 3651-2 testing under the tabulated conditions — it is not a blanket warranty for every process medium. Design caution remains: elongation floors are modest — do not expect 304-like cold expansion; specify anneal (+A) and verify forming trials Corrosion thread: aluminium helps scaling resistance in mildly oxidising heat; aqueous chloride resistance remains ferritic-limited.
Chloride pitting, crevice attack, and stress-corrosion cracking limits depend on temperature, concentration, and tensile stress — move across sisters 1.4512, 1.4016, 1.4006 when the medium outgrows this number rather than hoping surface finish alone will hold. Family filing for 1.4002 is ferritic corrosion-resisting. Caution thread: elongation floors are modest — do not expect 304-like cold expansion; specify anneal (+A) and verify forming trials.
Applications of EN 10297-2 1.4002 Tube
Applications of EN 10297-2 1.4002 tube centre on mechanical and general engineering rather than PED pressure shells: furnace hardware adjacent parts, quenched-and-drawn mechanical sleeves, and general engineering tube where 405-class chemistry is named. Role summary: Al-bearing 13%Cr ferritic seamless tube for annealed mechanical parts that need oxidation resistance without nickel. When the same chemistry is required as pressure seamless tube, open the EN 10216-5 sister page where that steel number exists. Use thread: furnace hardware adjacent parts, quenched-and-drawn mechanical sleeves, and general engineering tube where 405-class chemistry is named.
It is the wrong first choice when a welded product form is mandatory (use EN 10296-2 or EN 10217-7 as applicable), when PED pressure seamless acceptance is locked to EN 10216-5 alone, or when the medium clearly needs a sister such as 1.4512. Primary application sketch: furnace hardware adjacent parts, quenched-and-drawn mechanical sleeves, and general engineering tube where 405-class chemistry is named. Duty thread: Al-bearing 13%Cr ferritic seamless tube for annealed mechanical parts that need oxidation resistance without nickel.
Weldability of EN 10297-2 1.4002
1.4002 / X6CrAl13 is welded as a fabricator joint on mechanical assemblies even though the tube product itself is seamless under EN 10297-2. Shop guidance: ferritic practice with controlled heat input; grain growth risk rises with overheating — anneal after heavy weld cycles when ductility matters. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Weld thread: ferritic practice with controlled heat input; grain growth risk rises with overheating — anneal after heavy weld cycles when ductility matters.
For corrosive service after welding, confirm whether stabilisation, low carbon, duplex ferrite control, or post-weld solution anneal is required. Caution for this number: elongation floors are modest — do not expect 304-like cold expansion; specify anneal (+A) and verify forming trials Filler/shop note for 1.4002: ferritic practice with controlled heat input; grain growth risk rises with overheating — anneal after heavy weld cycles when ductility matters. Caution thread: elongation floors are modest — do not expect 304-like cold expansion; specify anneal (+A) and verify forming trials.
Surface Finishes for EN 10297-2 1.4002
Finish selection for 1.4002 on Annex A: Interior Ra limits, electropolish, or special protection for X6CrAl13 fall under explicit order text. SHH STEEL can produce and supply pickled/descaled, bright-annealed, and polished 1.4002 when the mill can measure and report the finish. Alias reminder: commercial talk may say 405, but the finish symbol still belongs on the EN 10297-2 line. Use thread: furnace hardware adjacent parts, quenched-and-drawn mechanical sleeves, and general engineering tube where 405-class chemistry is named.
Storage guidance for 1.4002: keep bundles off bare concrete in coastal yards, avoid chloride-bearing tarps against CFA OD, and leave end caps fitted until fabrication. Special export crate liners are available when the packing note asks for them. Duty thread: Al-bearing 13%Cr ferritic seamless tube for annealed mechanical parts that need oxidation resistance without nickel.
Inspection and Testing for EN 10297-2 1.4002
Inspection lot framing for 1.4002 in ferritic corrosion-resisting: SHH STEEL EN 10204 3.1 documents for 1.4002 report cast chemistry, tensile results, delivery condition, dimensions, and the Optional tests actually performed. We do not print a hydrostatic or eddy-current line unless that Option was executed. Keep 1.4002 heat identity intact from cast through bundle tag. Weld thread: ferritic practice with controlled heat input; grain growth risk rises with overheating — anneal after heavy weld cycles when ductility matters.
Technological tests on 1.4002 follow the order matrix — they are not assumed. IGC, when required, cites EN ISO 3651-2. Stencil or inkjet marking stays light on polished OD so the finish remains acceptable after receipt inspection. Use thread: furnace hardware adjacent parts, quenched-and-drawn mechanical sleeves, and general engineering tube where 405-class chemistry is named.
Packaging and Shipping for EN 10297-2 1.4002
Dispatch note for 1.4002 (405 body alias only): Export packing for 1.4002 / X6CrAl13 keeps heat identities intact: tags and bundle cards carry the cast/code that matches the EN 10204 3.1 document. Polished and bright tubes are sleeved; heavy HFD bundles use spacers to stop fretting in transit. Duty thread: Al-bearing 13%Cr ferritic seamless tube for annealed mechanical parts that need oxidation resistance without nickel.
Marking and identity for 1.4002: For 1.4002, inland trucking may use lighter wrap than ocean freight, but end protection and heat-identity tags remain mandatory. Chloride-bearing road salt exposure on open flats is avoided for bright finishes. Finish-sensitive packing for 1.4002 follows the Annex A symbol on the order. Use thread: furnace hardware adjacent parts, quenched-and-drawn mechanical sleeves, and general engineering tube where 405-class chemistry is named.
Packing lists for 1.4002 map bundle IDs to heats and sizes so receiving inspection can clear documents without unpacking every crate. Damaged wrap discovered at destination is reported with photos before the material is issued to fabrication. Caution thread: elongation floors are modest — do not expect 304-like cold expansion; specify anneal (+A) and verify forming trials.
Why Choose SHH STEEL
SHH STEEL can produce and supply EN 10297-2 1.4002 seamless stainless steel tube. Why 1.4002 with SHH STEEL — role: Al-bearing 13%Cr ferritic seamless tube for annealed mechanical parts that need oxidation resistance without nickel. Choose SHH STEEL for EN 10297-2 1.4002 when you need a mill partner who will not blur EN 10297-2 with EN 10216-5 or EN 10217-7 on the certificate. We can produce and supply the ordered Annex A finish, delivery condition, and Optional tests — and we say so in plain language on the quote. Duty thread: Al-bearing 13%Cr ferritic seamless tube for annealed mechanical parts that need oxidation resistance without nickel.
Grade advice stays practical for 1.4002. If the duty needs a sister chemistry, we point to 1.4512, 1.4016, 1.4006. Design caution for this number: elongation floors are modest — do not expect 304-like cold expansion; specify anneal (+A) and verify forming trials Quotes state scope boundaries in plain language so purchasing and engineering share the same acceptance standard. Contact the engineering desk with OD × wall, delivery condition, and medium notes before the cast is locked. Caution thread: elongation floors are modest — do not expect 304-like cold expansion; specify anneal (+A) and verify forming trials.
Supply Capability
Supply capability for EN 10297-2 1.4002 / X6CrAl13 starts with your OD × wall list and delivery-condition choice. SHH STEEL can produce and supply against that list with EN 10204 3.1 documents; the Stock / Available sizes block frames enquiry sizes rather than a public warehouse catalogue. Use thread: furnace hardware adjacent parts, quenched-and-drawn mechanical sleeves, and general engineering tube where 405-class chemistry is named.
| Item | Capability |
|---|---|
| Standard | EN 10297-2:2005 seamless general-purpose |
| Steel | 1.4002 / X6CrAl13 |
| Product form | Seamless tube (HFD / CFD / CFA / CFG / CFP) |
| Delivery condition | +A |
| Documents | EN 10204 3.1 (Options as ordered) |
| Typical enquiry OD | ~6–219 mm (other by agreement) |
| Typical enquiry wall | ~0.5–20 mm within family practice (other by agreement) |
Stock / Available sizes
Available sizes conversation for 1.4002 starts with your OD × wall matrix. Typical note: mechanical OD×wall bands finished +A (annealed), often CFD/HFD descaled. Send preferred delivery condition (+A / +AT / +QT as applicable) and any eddy-current or hydrostatic Options with the size list. Duty thread: Al-bearing 13%Cr ferritic seamless tube for annealed mechanical parts that need oxidation resistance without nickel.
On 1.4002, Options and sister duals (1.4512, 1.4016, 1.4006) belong on the same enquiry as the size list. SHH STEEL can produce and supply production heats after a short pilot when forming or polish trials are required. Weld thread: ferritic practice with controlled heat input; grain growth risk rises with overheating — anneal after heavy weld cycles when ductility matters.
FAQ
-
What is EN 10297-2 1.4002 seamless stainless steel tube used for?
- EN 10297-2 1.4002 (X6CrAl13) is seamless tube for mechanical and general engineering — furnace hardware adjacent parts, quenched-and-drawn mechanical sleeves, and general engineering tube where 405-class chemistry is named. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed. Role summary: Al-bearing 13%Cr ferritic seamless tube for annealed mechanical parts that need oxidation resistance without nickel.
-
Is EN 10297-2 1.4002 the same as EN 10216-5 1.4002?
- Chemistry families may overlap, but acceptance differs. EN 10297-2 is seamless general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10297-2 MTC for 1.4002 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
-
What delivery condition applies to 1.4002 / X6CrAl13?
- Delivery framing for 1.4002 is +A under the EN 10297-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 750–850 °C with air, water or gas cooling. State the delivery condition on the purchase order so marking and the MTC match.
-
What Annex A finishes can SHH STEEL supply for 1.4002?
- SHH STEEL can produce and supply HFD, CFD, CFA, CFG, and CFP routes for EN 10297-2 1.4002 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
-
How does 1.4002 compare with sister grades 1.4512, 1.4016, 1.4006?
- 1.4002 / X6CrAl13 is filed as ferritic corrosion-resisting. Typical sisters discussed on the same RFQ are 1.4512, 1.4016, 1.4006. Design caution: elongation floors are modest — do not expect 304-like cold expansion; specify anneal (+A) and verify forming trials Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
-
Can 1.4002 be welded even though the tube is seamless?
- Yes — fabricator joints are common on mechanical assemblies. Shop guidance: ferritic practice with controlled heat input; grain growth risk rises with overheating — anneal after heavy weld cycles when ductility matters. Mill heat treatment of the seamless tube does not replace a qualified WPS on site welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
-
What tests should appear on the EN 10204 3.1 document for 1.4002?
- Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10297-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
-
What size range can SHH STEEL quote for EN 10297-2 1.4002?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4002 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: mechanical OD×wall bands finished +A (annealed), often CFD/HFD descaled. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
Does commercial alias 405 belong in the purchase-order H1?
- No. On steelspecs.com product pages the H1 is the steel number only. Use 405 in body text and BOM notes, but lock EN 10297-2 and 1.4002 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
When should I choose duplex or Mo austenitic instead of 1.4002?
- Move when chloride pitting, crevice attack, or SCC risk exceeds what ferritic corrosion-resisting practice can defend for the temperature and stress state. Caution for this number: elongation floors are modest — do not expect 304-like cold expansion; specify anneal (+A) and verify forming trials Sister pointers: 1.4512, 1.4016, 1.4006. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
-
Is EN 10297-2 1.4002 suitable for heat-resisting furnace duty?
- Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4002 is filed as ferritic corrosion-resisting. If you need oxidising heat service, confirm whether 1.4749 / 1.4833 / 1.4845 / 1.4835 / 1.4876 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.
Conclusion
EN 10297-2 1.4002 (X6CrAl13) is seamless stainless tube for mechanical and general engineering — Al-bearing 13%Cr ferritic seamless tube for annealed mechanical parts that need oxidation resistance without nickel. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4512, 1.4016, 1.4006. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.