EN 10025-6 S960QL quenched and tempered high-yield structural steel plate, 960 MPa, −40 °C, material number 1.8933, SHH STEEL

EN 10025-6 S960QL High Structural Steel Plate Supplier

EN 10025-6 S960QL is quenched-and-tempered structural plate with 960 MPa minimum yield and −40°C impact toughness. SHH STEEL supplies S960QL plate mill-direct for cranes, mining frames and cold-region fabrication.
Keywords
S960QL, S960QL steel plate, EN 10025-6 S960QL, S960QL QT plate, S960QL high strength plate, S960QL supplier, Q960E, S960Q, GB/T 16270
Equivalent Grades:
EN 10025-6 S960QL / GB/T 16270 Q960E (near) / ASTM A514 (over, not direct) / JIS G3128 SHY785 (lower) — Material Specification: EN 10025-6 — Delivery: Quenched + Tempered (QT); -40℃ impact
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
Equivalent Material Grades
QT Structural Service
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Applications
Supply Capability
Global Delivery and Markets
Why Choose SHH STEEL
FAQ
Conclusion

What is S960QL steel?

S960QL, also searched as EN 10025-6 S960QL, S960QL steel plate, S960QL QT plate, S960 QL and S960QL high strength plate, is the 960 MPa QL grade in EN 10025-6. That standard covers flat products of high-yield-strength structural steels in the quenched and tempered condition. S is structural steel, 960 is the thin-plate minimum yield in MPa, Q means quenched and tempered, and L means Charpy impact at −40°C.

S960QL is the European name most crane and mining buyers use when a boom or chassis was sized at 960 MPa and the site design temperature is −40°C. It sits above S890QL and is the cold letter of the S960 family. Q is 0°C. QL is −40°C. QL1 is −60°C. A heat tested only at 0°C cannot be stamped QL. Not every mill will roll 960 MPa on thick plate.

The closest Chinese name is GB/T 16270 Q960E. Both are about 960 MPa QT plate tested at −40°C. S960Q is the 0°C sister. S960QL1 is the −60°C sister. On the US side, A514 Grade Q is only 100 ksi / 690 MPa. There is no standard ASTM 960 MPa plate grade. Dual mark only when both books are fully met. See EN 10025-6 steel plate.

SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. We source S960QL from first-line QT mills, print heat analysis and product analysis when ordered, and ship plate to fabricators in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Related pages include high strength low alloy plates and structural steel plates.

S960QL Material Specification

Specification Element Requirement SHH STEEL Compliance
Plate book EN 10025-6 S960QL Confirmed
Other search names S960QL steel plate, S960 QL Covered
Delivery condition Quenched and tempered Confirmed
Yield, ≤ 50 mm 960 MPa min Confirmed
Impact QL, −40°C Confirmed
Chinese comparison Q960E, −40°C Comparison, not a swap
US comparison A514 is 690 MPa Not a twin
Product analysis EN 10025-6 column when ordered Confirmed
Not the same letter S960Q or S960QL1 Do not substitute
Supply role Global steel mill sourcing partner SHH STEEL
Certification EN 10204 3.1 or 3.2 As ordered

Nearby pages that buyers compare, but must not swap blindly, include S960Q, S960QL1 and S890QL.

Chemical Composition

Heat analysis is the ladle table in EN 10025-6. Product analysis, when ordered, follows the permitted deviation in the same standard. S960QL is a low-alloy QT carbon plate. Mills add Nb, V, Ti or Al for grain refinement, and may add Cr, Ni, Mo or B by thickness. Boron is common on 960 MPa heats. Nickel helps the −40°C result. The certificate shows the elements actually used.

Ladle Analysis and Product Analysis — EN 10025-6 S960QL

Element Ladle analysis (%) Product analysis (%)
Carbon (C), max 0.20 0.22
Silicon (Si), max 0.80 0.85
Manganese (Mn), max 1.70 1.80
Phosphorus (P), max 0.020 0.025
Sulfur (S), max 0.010 0.012
Nitrogen (N), max 0.015 0.016
Boron (B), max 0.0050 0.0060
Chromium (Cr), max 1.50 1.55
Copper (Cu), max 0.50 0.55
Molybdenum (Mo), max 0.70 0.75
Niobium (Nb), max 0.06 0.07
Nickel (Ni), max 2.0 2.1
Titanium (Ti), max 0.05 0.06
Vanadium (V), max 0.12 0.13
Zirconium (Zr), max 0.15 0.16

If the purchase order writes product analysis, SHH STEEL prints both columns and the thickness band used for the tensile test. Do not treat this chemistry as weathering plate. Do not treat it as S355JR.

Mechanical Properties

Buyers search S960QL mechanical properties, S960QL yield strength, EN 10025-6 S960QL tensile and S960QL impact −40°C.

Tensile and impact — EN 10025-6 S960QL

Thickness Yield min Tensile Elongation min Impact
3 – 50 mm 960 MPa 980–1150 MPa 10% −40°C, 30 J min
> 50 – 100 mm 850 MPa 880–1100 MPa 10% −40°C, 30 J min
> 100 – 150 mm as standard table as standard table 10% −40°C, 27 J min

Impact energy is the average of three longitudinal Charpy V-notch specimens. One value may fall below the table, but not below 70% of that value. Write a higher energy on the order if the owner requires it.

Yield steps down with thickness. A 960 MPa name on 20 mm plate is not the minimum on an 80 mm flange. 960 MPa is about 139 ksi. ASTM A514 is 100 ksi and is not this number. SHH STEEL quotes the thickness band on the offer.

Density is 7.85 g/cm³. Hardness after temper is a mill control, not a design value. Z15, Z25 or Z35 through-thickness tensile is an extra under EN 10164.

Material Comparison

Grade Book Delivery Yield, thin plate Impact Swap?
S890QL EN 10025-6 QT 890 MPa −40°C Lower sister
S960Q EN 10025-6 QT 960 MPa 0°C Warmer sister
S960QL EN 10025-6 QT 960 MPa −40°C This page
S960QL1 EN 10025-6 QT 960 MPa −60°C Colder sister
Q960E GB/T 16270 QT 960 MPa −40°C Closest comparison
Q960C GB/T 16270 QT 960 MPa 0°C No
A514 Gr.Q ASTM A514 QT 690 MPa Different Lower yield

Equivalent Material Grades

There is no official one-to-one substitute for S960QL. What buyers compare is a 960 MPa QT plate tested at −40°C.

The usual Chinese pair is GB/T 16270 Q960E. Q960C is warmer. Q960F is colder. S890QL is one strength step lower in the same book. In the United States there is no standard 960 MPa plate grade. A514 Grade Q is 100 ksi / 690 MPa. A572 Gr.65 is only 65 ksi. SHH STEEL will not stamp Q960E or A514 on an S960QL certificate unless the purchase order names both books and both tables are met.

Designation Country / region Standard Notes
S960QL Europe EN 10025-6 Name on this page
S960Q Europe EN 10025-6 0°C sister
S960QL1 Europe EN 10025-6 −60°C sister
Q960E China GB/T 16270 −40°C comparison
Q960C China GB/T 16270 0°C, closer to S960Q
A514 Gr.Q USA ASTM A514 100 ksi, lower yield
A572 Gr.65 USA ASTM A572 65 ksi, lower yield
SM570 Japan JIS G3106 Well below this yield

QT Structural Service

Buyers pick S960QL when a welded frame, boom or chassis wants 960 MPa yield, QT delivery and impact at −40°C. Search phrases such as S960QL steel plate, EN 10025-6 S960QL and S960QL QT plate all point here.

It is the wrong plate for a 0°C file that can use S960Q. It is the wrong plate for a −60°C arctic file. That work is S960QL1. It is the wrong plate for an 890 MPa file that was sized on S890QL. Raising the grade without a design check can change weld procedure and deflection. It is the wrong plate for a 100 ksi US file. That work is A514 Grade Q. It is the wrong plate for a pressure vessel. That work sits on ASTM A516 or pressure vessel steel plates.

SHH STEEL supplies this plate when the drawing names EN 10025-6 and the QL letter at 960 MPa.

Weldability

S960QL is weldable QT carbon plate. The plate has already been quenched and tempered, and the joint must keep −40°C toughness. Many heats use boron. A procedure written for S355JR is not an S960QL procedure.

Typical consumables are matching 960 MPa low-hydrogen electrodes or wires, qualified on a QT 960 MPa family with a −40°C impact coupon. E7018-class electrodes are under-matched if the joint must develop full plate strength. A procedure written for S890QL is a lower-strength reference. An A514 procedure is also a lower-strength reference. Neither is a finished WPS for this grade.

Preheat follows thickness, hydrogen and the approved WPS. Interpass temperature should stay below the mill temper range, or local yield and the −40°C result can drop. After heavy cold forming, a stress relief may be required. The fabricator owns the WPS. SHH STEEL can share mill heat data, product analysis and carbon equivalent for that review.

Heat Treatment and Delivery Condition

Usual delivery from SHH STEEL for S960QL is quenched and tempered to EN 10025-6. Austenitize typically in the 880–930°C range, quench, then temper in the window that holds 960 MPa yield and the −40°C impact. Exact temperatures stay on the mill process sheet.

Do not order S960QL as as-rolled, normalized or TMCP unless the contract leaves EN 10025-6. ASTM A514 is not a delivery instruction for this page. Stress relief after fabrication, if used, must stay below the original temper temperature.

The certificate lists EN 10025-6 S960QL, heat number, ladle analysis, product analysis when ordered, tensile by thickness band, and −40°C impact. Certificates may be EN 10204 3.1 or EN 10204 3.2. Dual marking to Q960E is available only when both books are fully met.

Dimensions

Usual supply range from SHH STEEL for S960QL high structural steel plate:

  • Thickness: commonly 8 mm – 40 mm, heavier plate to 50 mm by enquiry
  • Width: 1500 mm – 2800 mm
  • Length: 3000 mm – 12000 mm

Cut-to-size webs, flanges and base plates are available. Browse more sizes on structural steel plates and the products index.

Tolerances

Dimensional limits for S960QL follow EN 10029 Class A unless the purchase order names Class B, C or D, or a GB/T 709 table.

Typical thickness tolerance idea for S960QL QT plate, EN 10029 Class A

Nominal thickness (mm) Usual minus (mm) Usual plus (mm)
8 – 10 −0.3 +0.8
10 – 20 −0.3 +1.0
20 – 30 −0.3 +1.1
30 – 40 −0.3 +1.2
40 – 50 −0.3 +1.3

Width on 1500–2800 mm plate is commonly held to about +20 / 0 mm unless a tighter extra is named. Length on 3000–12000 mm plate is commonly held to about +50 / 0 mm by mill practice. Flatness after QT follows the agreed class. SHH STEEL will not assume Class B or a zero-minus extra on S960QL unless the order says so.

Supplementary Requirements

S960QL already defines 960 MPa yield, QT delivery and −40°C impact. Extra items still have to be written on the purchase order.

Book name. Write EN 10025-6 S960QL. Do not write only S960.

Impact. QL is −40°C, minimum 30 J up to 100 mm in the usual table. Write a higher energy if the owner requires it.

Chinese or US comparison. Write Q960E or A514 only if dual mark is required and both tables are met.

Product analysis. Write it if the file needs the second chemistry column.

Through-thickness. Z15, Z25 or Z35 to EN 10164 when the joint is loaded through the thickness.

NDE. UT to EN 10160 class S1 E1, or the named class.

Heat-treatment record. QT temperatures when the inspector asks.

Identification. Heat number, S960QL, thickness and mill logo.

Third-party witness. EN 10204 3.2 with SGS, TÜV, BV, ABS or the inspector named.

Applications

Industry Typical components
Construction machinery S960QL QT booms, frames and bases
Mining equipment S960QL chassis and body plate from SHH STEEL
Cranes and port equipment S960QL webs and flanges
Cold-region fabrication S960QL members tested at −40°C
Comparison vs S960Q S960QL next to S960Q
Comparison vs S890QL S960QL next to S890QL
Comparison vs A514 S960QL next to A514 Gr.Q

S960QL is the plate for a 960 MPa QT file tested at −40°C. It is the wrong plate for a painted warehouse that can use S355JR. It is the wrong plate for an 890 MPa member that was already sized.

Supply Capability

SHH STEEL sources S960QL from first-line Chinese QT mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron and Steel, Baosteel, Xinyu, Xingcheng and other qualified mills when the size requires it.

Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.

Usual rolling thickness: 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 40 mm. Heavier plate is confirmed before order.

Processing: CNC or flame cutting, bevel, flattening, shot blast, UT to the named class.

Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.

Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.

Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.

Global Delivery and Markets

SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply EN, GB, ASTM, ASME, DIN and JIS steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.

SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.

Typical lead time: ex-stock 5–7 days when plate is in yard; standard QT rolling about 45–55 days; 3.2 inspection about 55–65 days.

Why Choose SHH STEEL

SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. For S960QL that means mill-direct QT price, not a multi-layer stockist mark-up. We buy from mills that already run the 960 MPa quench-and-temper route, so the heat carries the −40°C impact without a second upgrade charge.

Delivery is short when the size is in rolling range: ex-stock 5–7 days, standard heat about 45–55 days, 3.2 inspection about 55–65 days. Cutting, bevel and UT can run in the same window. FOB Shanghai is the main term. CIF to US West, US Gulf, Rotterdam, Jebel Ali and Singapore is quoted on the same file.

Experience on this grade is simple: print EN 10025-6 S960QL, keep the QT route, and do not ship S960Q or a silent Q960C stamp as QL. We will not change QL to Q to save a cold test, and we will not treat S960QL as S355. If the drawing needs −60°C, we will move the inquiry to S960QL1 and keep the price on the right grade.

FAQ

What is S960QL steel plate?
S960QL in EN 10025-6 is quenched-and-tempered structural plate with 960 MPa minimum yield up to 50 mm and Charpy impact at −40°C. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
Is S960QL the same as S960Q?
No. Both yield at 960 MPa. S960Q is tested at 0°C. S960QL is tested at −40°C.
What is the Chinese equivalent of S960QL?
The nearest comparison is GB/T 16270 Q960E, also 960 MPa at −40°C. The books are not identical. SHH STEEL does not dual-mark Q960E unless both books are met.
What is the US equivalent of S960QL?
There is no official ASTM twin at 960 MPa. A514 is 100 ksi / 690 MPa, well below this number. SHH STEEL does not dual-mark A514 unless both books are met.
Can SHH STEEL issue EN 10204 3.2 for S960QL?
Yes. EN 10204 3.1 is standard. EN 10204 3.2 is arranged with SGS, TÜV, BV, ABS or the inspector named on the order.

Conclusion

S960QL high structural steel plate to EN 10025-6 is 960 MPa quenched-and-tempered plate with impact at −40°C. The nearest Chinese comparison is gt/t 16270 Q960E. ASTM A514 is 690 MPa and is not a substitute. Whether the inquiry says S960QL, EN 10025-6 S960QL, S960QL steel plate or S960QL QT plate, SHH STEEL as a global steel mill sourcing partner supplies plate with S960QL chemistry, ladle and product analysis as ordered, EN 10029 tolerances and EN 10204 3.1 or 3.2 certification.

SHH STEEL supplies EN 10025-6 S960QL High Structural Steel Plate to the United States, Europe, the Middle East, Africa, Asia and the Americas for work that actually names this grade.

Contact SHH STEEL for mill rolling, QT route, cutting, UT, 3.2 inspection or a worldwide quotation.

S960QL, S960QL steel plate, EN 10025-6 S960QL, S960QL QT plate, S960QL high strength plate, S960QL supplier, SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *