Q960E QT Carbon Steel Plate GB/T 16270 Supplier
What is Q960E QT Carbon Steel Plate GB/T 16270?
Q960E, also searched as GB/T 16270 Q960E, Q960E QT plate, Q960E carbon steel plate, Q960E steel plate and Q960E quenched and tempered plate, is the 960 MPa quality-grade-E grade in GB/T 16270. That standard covers high-strength structural steel plate delivered quenched and tempered. Q is the yield symbol, 960 is the thin-plate minimum yield in MPa, and E is the quality letter for Charpy impact at −40°C.
Q960E is the grade most buyers compare with European QL plate at 960 MPa. C is 0°C. D is −20°C. E is −40°C. F is −60°C. About 139 ksi on a US drawing is the same yield number. Cold-region crane and mine-truck builders use Q960E when the member was sized at 960 MPa and the specification names −40°C. A Q960C heat tested only at 0°C cannot be stamped E. Not every mill will roll 960 MPa on thick plate.
The closest European name is EN 10025-6 S960QL. Both are about 960 MPa QT plate tested at −40°C. S960Q is 0°C and lines up with Q960C. S960QL1 is −60°C and lines up with Q960F. On the US side, A514 Grade Q is only 100 ksi / 690 MPa. There is no standard ASTM 960 MPa plate grade. Dual mark only when both books are fully met. See EN 10025-6 steel plate.
SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. We source Q960E from first-line QT mills, print heat analysis and product analysis when ordered, and ship plate to fabricators in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Related pages include high strength low alloy plates and structural steel plates.
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Plate book | GB/T 16270 Q960E | Confirmed |
| Other search names | Q960E QT plate, Q960E carbon steel plate | Covered |
| Delivery condition | Quenched and tempered | Confirmed |
| Yield, thin plate | 960 MPa min | Confirmed |
| Quality grade | E, impact at −40°C | Confirmed |
| EN comparison | S960QL, −40°C | Comparison, not a swap |
| US comparison | A514 is 690 MPa | Not a twin |
| Product analysis | GB/T 222 column when ordered | Confirmed |
| Not the same letter | Q960C or Q960D | Do not substitute |
| Supply role | Global steel mill sourcing partner | SHH STEEL |
| Certification | EN 10204 3.1 or 3.2 | As ordered |
Nearby pages that buyers compare, but must not swap blindly, include S960QL, S960Q and A514 Gr.Q.
Chemical Composition
Heat analysis is the mill ladle table in GB/T 16270. Product analysis, when ordered, follows GB/T 222. Grade E is tighter on phosphorus and sulfur than grade C, because the impact test is at −40°C. Mills add Nb, V, Ti or Al for grain refinement, and may add Cr, Ni, Mo or B by thickness. Boron is common on 960 MPa heats. Nickel helps the cold impact. The certificate shows the elements actually used.
Heat Analysis and Product Analysis — GB/T 16270 Q960E
| Element | Heat analysis (%) | Product analysis (%) |
|---|---|---|
| Carbon (C), max | 0.18 | 0.20 |
| Silicon (Si), max | 0.80 | 0.85 |
| Manganese (Mn), max | 2.00 | 2.08 |
| Phosphorus (P), max | 0.020 | 0.025 |
| Sulfur (S), max | 0.010 | 0.013 |
| Copper (Cu), max | 0.50 | 0.55 |
| Chromium (Cr), max | 1.50 | 1.55 |
| Nickel (Ni), max | 2.00 | 2.05 |
| Molybdenum (Mo), max | 0.70 | 0.75 |
| Boron (B), max | 0.005 | 0.006 |
| Vanadium (V), max | 0.12 | 0.13 |
| Niobium (Nb), max | 0.06 | 0.07 |
| Titanium (Ti), max | 0.05 | 0.06 |
| Aluminium (Als), min when used | 0.015 | 0.010 |
If the purchase order writes product analysis, SHH STEEL prints both columns and the thickness band used for the tensile test. Do not treat this chemistry as weathering plate. Do not treat it as S355JR.
Mechanical Properties
Buyers search Q960E mechanical properties, Q960E yield strength, GB/T 16270 Q960E tensile and Q960E impact −40°C.
Tensile and impact — GB/T 16270 Q960E
| Thickness | Yield min | Tensile | Elongation min | Impact |
|---|---|---|---|---|
| ≤ 50 mm | 960 MPa | 980–1150 MPa | 10% | −40°C, grade E |
| > 50–100 mm | 880 MPa | 900–1150 MPa | 10% | −40°C, grade E |
| > 100 mm | as standard table | as standard table | 10% | −40°C, grade E |
Impact energy is the average of three longitudinal Charpy V-notch specimens. One value may fall below the table, but not below 70% of that value. A typical production heat is at or above 27 J to 34 J at −40°C, depending on the ordered edition and thickness. Write the energy on the purchase order if the owner wants a number above the book minimum.
Yield steps down with thickness. A 960 MPa name on 16 mm plate is not the minimum on a 50 mm flange. 960 MPa is about 139 ksi. ASTM A514 is 100 ksi and is not this number. SHH STEEL quotes the thickness band on the offer.
Density is 7.85 g/cm³. Hardness after temper is a mill control, not a design value. Z15, Z25 or Z35 through-thickness tensile is an extra.
Material Comparison
| Grade | Book | Delivery | Yield, thin plate | Impact | Swap? |
|---|---|---|---|---|---|
| Q960C | GB/T 16270 | QT | 960 MPa | 0°C | Warmer sister |
| Q960D | GB/T 16270 | QT | 960 MPa | −20°C | Warmer sister |
| Q960E | GB/T 16270 | QT | 960 MPa | −40°C | This page |
| Q960F | GB/T 16270 | QT | 960 MPa | −60°C | Colder sister |
| Q890E | GB/T 16270 | QT | 890 MPa | −40°C | Lower yield |
| S960Q | EN 10025-6 | QT | 960 MPa | 0°C | No |
| S960QL | EN 10025-6 | QT | 960 MPa | −40°C | Closest comparison |
| A514 Gr.Q | ASTM A514 | QT | 690 MPa | Different | Lower yield |
Equivalent Material Grades
There is no official one-to-one substitute for Q960E. What buyers compare is a 960 MPa QT plate tested at −40°C.
The usual European pair is S960QL. S960Q is warmer. S960QL1 is colder. S890QL is one strength step lower. In the United States there is no standard 960 MPa plate grade. A514 Grade Q is 100 ksi / 690 MPa. A572 Gr.65 is only 65 ksi. SHH STEEL will not stamp S960QL or A514 on a Q960E certificate unless the purchase order names both books and both tables are met.
| Designation | Country / region | Standard | Notes |
|---|---|---|---|
| Q960E | China | GB/T 16270 | Name on this page |
| Q960C / Q960D / Q960F | China | GB/T 16270 | Other impact letters |
| Q890E | China | GB/T 16270 | Lower yield sister |
| A514 Gr.Q | USA | ASTM A514 | 100 ksi, lower yield |
| A572 Gr.65 | USA | ASTM A572 | 65 ksi, lower yield |
| S960QL | Europe | EN 10025-6 | −40°C QT comparison |
| S960Q | Europe | EN 10025-6 | 0°C, closer to Q960C |
| SM570 | Japan | JIS G3106 | Well below this yield |
Q960E QT Structural Service
Buyers pick Q960E when a welded frame, boom or chassis wants 960 MPa yield, QT delivery and impact at −40°C. Search phrases such as Q960E steel plate, GB/T 16270 Q960E and Q960E QT plate all point here.
It is the wrong plate for a 0°C file that can use Q960C. It is the wrong plate for a −20°C file that can use Q960D. It is the wrong plate for a −60°C arctic file. That work is Q960F. It is the wrong plate for a 100 ksi US file. That work is A514 Grade Q. It is the wrong plate for a pressure vessel. That work sits on ASTM A516 or pressure vessel steel plates.
SHH STEEL supplies this plate when the drawing names GB/T 16270 and quality grade E at 960 MPa.
Weldability
Q960E is weldable QT carbon plate. The plate has already been quenched and tempered, and the joint must keep −40°C toughness. Many heats use boron. A procedure written for S355JR is not a Q960E procedure.
Typical consumables are matching 960 MPa low-hydrogen electrodes or wires, qualified on a QT 960 MPa family with a −40°C impact coupon. E7018-class electrodes are under-matched if the joint must develop full plate strength. A procedure written for S960QL is the usual starting point. An A514 procedure is a lower-strength reference, not a finished WPS for this grade.
Preheat follows thickness, hydrogen and the approved WPS. Interpass temperature should stay below the mill temper range, or local yield and the −40°C result can drop. After heavy cold forming, a stress relief may be required. The fabricator owns the WPS. SHH STEEL can share mill heat data, product analysis and carbon equivalent for that review.
Heat Treatment and Delivery Condition
Usual delivery from SHH STEEL for Q960E is quenched and tempered. Austenitize typically in the 880–930°C range, quench, then temper in the window that holds 960 MPa yield and the −40°C impact. Exact temperatures stay on the mill process sheet.
Do not order Q960E as as-rolled or TMCP unless the contract leaves GB/T 16270. ASTM A514 is not a delivery instruction for this page. Stress relief after fabrication, if used, must stay below the original temper temperature.
The certificate lists GB/T 16270 Q960E, heat number, heat analysis, product analysis when ordered, tensile by thickness band, and −40°C impact. Certificates may be EN 10204 3.1 or EN 10204 3.2. Dual marking to S960QL is available only when both books are fully met.
Dimensions
Usual supply range from SHH STEEL for Q960E QT carbon steel plate:
- Thickness: commonly 8 mm – 40 mm, heavier plate to 50 mm by enquiry
- Width: 1500 mm – 2800 mm
- Length: 3000 mm – 12000 mm
Cut-to-size webs, flanges and base plates are available. Browse more sizes on structural steel plates and the products index.
Tolerances
Dimensional limits for Q960E follow GB/T 709 unless the purchase order names another table.
Typical thickness tolerance idea for Q960E QT plate
| Nominal thickness (mm) | Usual minus (mm) | Usual plus (mm) |
|---|---|---|
| 8 – 10 | −0.3 | +0.8 |
| 10 – 20 | −0.4 | +0.9 |
| 20 – 30 | −0.4 | +1.0 |
| 30 – 40 | −0.5 | +1.1 |
| 40 – 50 | −0.5 | +1.2 |
Width on 1500–2800 mm plate is commonly held to about ±20–25 mm unless a tighter extra is named. Length on 3000–12000 mm plate is commonly held to about +50 / 0 mm or ±25 mm by mill practice. Flatness after QT follows the agreed class. SHH STEEL will not assume a zero-minus extra on Q960E unless the order says so.
Supplementary Requirements
Q960E already defines 960 MPa yield, QT delivery and −40°C impact. Extra items still have to be written on the purchase order.
Book name. Write GB/T 16270 Q960E. Do not write only Q960E.
Impact. Grade E is −40°C. Write a higher energy if the owner requires it.
EN or US comparison. Write S960QL or A514 only if dual mark is required and both tables are met.
Product analysis. Write it if the file needs the second chemistry column.
Through-thickness. Z15, Z25 or Z35 when the joint is loaded through the thickness.
NDE. UT to GB/T 2970 or the named class.
Heat-treatment record. QT temperatures when the inspector asks.
Identification. Heat number, Q960E, thickness and mill logo.
Third-party witness. EN 10204 3.2 with SGS, TÜV, BV, ABS or the inspector named.
Applications
| Industry | Typical components |
|---|---|
| Construction machinery | Q960E QT booms, frames and bases |
| Mining equipment | Q960E chassis and body plate from SHH STEEL |
| Cranes and port equipment | Q960E webs and flanges |
| Cold-region fabrication | Q960E members tested at −40°C |
| Comparison vs S960QL | Q960E next to S960QL |
| Comparison vs S960Q | Q960E next to S960Q |
| Comparison vs A514 | Q960E next to A514 Gr.Q |
Q960E is the plate for a 960 MPa QT file tested at −40°C. It is the wrong plate for a painted warehouse that can use S355JR. It is the wrong plate for an 890 MPa member that was already sized.
Supply Capability
SHH STEEL sources Q960E from first-line Chinese QT mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron and Steel, Baosteel, Xinyu, Xingcheng and other qualified mills when the size requires it.
Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.
Usual rolling thickness: 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 40 mm. Heavier plate is confirmed before order.
Processing: CNC or flame cutting, bevel, flattening, shot blast, UT to the named class.
Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.
Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.
Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.
Global Delivery and Markets
SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply GB, ASTM, ASME, EN, DIN and JIS steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.
SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.
Typical lead time: ex-stock 5–7 days when plate is in yard; standard QT rolling about 45–55 days; 3.2 inspection about 55–65 days.
Why Choose SHH STEEL
SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. For Q960E that means mill-direct QT price, not a multi-layer stockist mark-up. We buy from mills that already run the 960 MPa quench-and-temper route, so the heat carries the −40°C impact without a second upgrade charge.
Delivery is short when the size is in rolling range: ex-stock 5–7 days, standard heat about 45–55 days, 3.2 inspection about 55–65 days. Cutting, bevel and UT can run in the same window. FOB Shanghai is the main term. CIF to US West, US Gulf, Rotterdam, Jebel Ali and Singapore is quoted on the same file.
Experience on this grade is simple: print GB/T 16270 Q960E, keep the QT route, and do not ship Q960D or a silent S960QL stamp as Q960E. We will not change E to D to save a cold test, and we will not treat Q960E as S355. If the drawing needs −60°C, we will move the inquiry to Q960F and keep the price on the right grade.
FAQ
-
What is Q960E steel plate?
- Q960E in GB/T 16270 is quenched-and-tempered carbon structural plate with 960 MPa minimum yield on thin plate and Charpy impact at −40°C. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
-
Is Q960E the same as Q960C?
- No. Both yield at 960 MPa. Q960C is tested at 0°C. Q960E is tested at −40°C.
-
What is the US equivalent of Q960E?
- There is no official ASTM twin at 960 MPa. A514 is 100 ksi / 690 MPa, well below this number, and it does not carry a −40°C E letter. SHH STEEL does not dual-mark A514 unless both books are met.
-
Is Q960E the same as S960QL?
- They are the usual comparison pair: both are about 960 MPa QT plate tested at −40°C. Dual mark only when both books are fully met. S960Q is warmer. S960QL1 is colder.
Conclusion
Q960E QT carbon steel plate to GB/T 16270 is 960 MPa quenched-and-tempered structural plate with impact at −40°C. The nearest European comparison is S960QL. ASTM A514 is 690 MPa and is not a substitute. Whether the inquiry says Q960E, GB/T 16270 Q960E, Q960E QT plate or Q960E carbon steel plate, SHH STEEL as a global steel mill sourcing partner supplies plate with Q960E chemistry, heat and product analysis as ordered, GB/T 709 tolerances and EN 10204 3.1 or 3.2 certification.
SHH STEEL supplies Q960E QT Carbon Steel Plate to the United States, Europe, the Middle East, Africa, Asia and the Americas for work that actually names this grade.
Contact SHH STEEL for mill rolling, QT route, cutting, UT, 3.2 inspection or a worldwide quotation.
Q960E, Q960E steel plate, GB/T 16270 Q960E, Q960E QT plate, Q960E carbon steel plate, Q960E supplier, SHH STEEL