EN 10025-6 S500Q is a quenched and tempered high-strength structural steel plate with a minimum yield strength of 500 MPa and impact toughness at –20°C. It offers a strength level between S460 and S550 grades for heavily loaded structures. SHH STEEL supplies this grade as a China Mill-Direct Exporter with full mill certification and competitive pricing.
Equivalent Grades
ASTM A514 Gr Q / JIS SHT70 / GB Q500CF / ISO E500Q
Material Specification:
EN 10025-6 — Delivery: Quenched & Tempered (Q+T)
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Tolerances
Weldability
Equivalent Material Grades
Applications
Why Choose SHH STEEL
FAQ
Conclusion

What is EN 10025-6 S500Q Steel Plate?

SHH STEEL is a professional China Mill-Direct Exporter of high-strength structural steel plates. We are pleased to offer EN 10025-6 S500Q Steel Plate (Material Number 1.8924), a quenched and tempered grade designed for structural applications requiring higher strength than the S460 series while remaining below the S550 level.

S500Q belongs to the family of EN 10025-6 steel plate products covering high-yield-strength steels in the quenched and tempered condition. After quenching and tempering, this grade achieves a minimum yield strength of 500 MPa (up to 50 mm thickness) while maintaining adequate impact toughness at –20°C. The refined tempered microstructure provides a good balance of strength, ductility and weldability for heavily loaded welded structures.

SHH STEEL supplies S500Q plates in thicknesses ranging from 6 mm to 150 mm, widths up to 3000–4000 mm and lengths up to 12000–18000 mm. Custom cutting, ultrasonic testing, surface treatment and third-party inspection services are available. Every plate is delivered with a full EN 10204 3.1 Mill Test Certificate, ensuring complete traceability from the producing mill.

Material Specification

Parameter Requirement / Availability
Governing Standard EN 10025-6
Steel Designation S500Q (1.8924)
Delivery Condition Quenched and Tempered (Q)
Product Form Flat steel plate
Thickness Range 6 mm – 150 mm (thicker plates on request)
Width / Length Up to 3000–4000 mm / 12000–18000 mm
Certification EN 10204 3.1 / 3.2
Additional Testing UT, Z-test, third-party inspection available

Chemical Composition

Chemical composition is controlled in accordance with EN 10025-6 for both ladle (heat) analysis and product analysis.

Ladle Analysis (Cast Analysis)

Element Maximum (%)
Carbon (C) 0.20
Silicon (Si) 0.80
Manganese (Mn) 1.70
Phosphorus (P) 0.025
Sulfur (S) 0.015
Chromium (Cr) 1.50
Nickel (Ni) 2.00
Molybdenum (Mo) 0.70
Copper (Cu) 0.50
Niobium (Nb) 0.06
Vanadium (V) 0.12
Titanium (Ti) 0.05
Boron (B) 0.005
Nitrogen (N) 0.015

Product Analysis

Element Maximum (%)
Carbon (C) 0.22
Silicon (Si) 0.86
Manganese (Mn) 1.80
Phosphorus (P) 0.030
Sulfur (S) 0.017
Chromium (Cr) 1.60
Nickel (Ni) 2.10
Molybdenum (Mo) 0.74
Copper (Cu) 0.55
Niobium (Nb) 0.07
Vanadium (V) 0.14
Titanium (Ti) 0.06
Boron (B) 0.006
Nitrogen (N) 0.016

The alloying design provides sufficient hardenability for quenching while keeping the carbon equivalent at a level that still permits satisfactory welding after tempering.

Mechanical Properties

Nominal Thickness (mm) Min. Yield Strength ReH Tensile Strength Rm Min. Elongation A Impact Energy (longitudinal)
≤ 50 500 MPa 590 – 770 MPa 17 % 30 J at –20 °C
50 < t ≤ 100 480 MPa 590 – 770 MPa 17 % 30 J at –20 °C
100 < t ≤ 150 440 MPa 540 – 720 MPa 17 % 30 J at –20 °C

Density is approximately 7.85 g/cm³.

Delivery Conditions

All S500Q plates are supplied in the quenched and tempered condition as required by EN 10025-6. The quenching and tempering heat treatment produces the required high strength and toughness combination.

Additional processing options available from SHH STEEL:

  • Shot blasting and shop primer application
  • Ultrasonic testing in accordance with EN 10160
  • Through-thickness (Z-direction) testing to Z15, Z25 or Z35
  • Independent third-party inspection (SGS, BV, TUV, Lloyd’s Register, etc.)
  • Precision cutting (flame, plasma or water-jet)

Tolerances

EN 10025-6 S500Q Steel Plate dimensional tolerances are supplied in accordance with EN 10029. For S500Q QT High Structural Steel, customers may select the required class for thickness, width, length and flatness according to project needs. Both mill edges and cut edges (flame or plasma) are available for S500Q steel plate. Tighter tolerances for EN 10025-6 S500Q can be arranged by special agreement when required.

Weldability

S500Q is a high-strength quenched and tempered steel. Successful welding requires careful attention to preheating, heat input and the use of low-hydrogen consumables to maintain toughness in the heat-affected zone.

Recommended welding consumables:

Welding Process Suggested Consumables
SMAW (Stick) E8018-G, E9018-G
GMAW / MAG ER80S-G, ER90S-G
FCAW E81T1-Ni1, E91T1-G
SAW Matching high-strength wire and flux combinations

Preheating is generally required, especially for thicker plates. Interpass temperature control is important, and post-weld heat treatment may be considered for critical applications.

Equivalent Material Grades

Grade Standard Remarks
S500Q EN 10025-6 Primary designation
1.8924 EN Material number
Q500D / Q500E GB/T 1591 Closest Chinese equivalents
Selected A514 / A517 grades ASTM Similar quenched & tempered concept
StE 500 V Former DIN Historical related grade

Applications

EN 10025-6 S500Q is selected when a strength level between S460 and S550 is required. Typical applications include:

Application Area Typical Components / Keywords
Heavy Construction Crane booms, heavy frames, high-load columns – S500Q Structural Steel
Bridge Engineering Main girders, support structures – S500Q Bridge
Mining & Earthmoving Equipment Chassis, boom structures – S500Q Mining
Offshore & Marine Platform components, lifting equipment – S500Q Offshore
Energy & Power Wind turbine components, heavy fabrications – S500Q Energy
General Heavy Fabrication High-strength welded assemblies – S500Q Fabrication

Why Choose SHH STEEL

SHH STEEL is a China Mill-Direct Exporter. We maintain long-term strategic cooperation with major Chinese steel mills and act as a first-level agent. This direct supply model allows us to offer competitive mill-direct pricing, shorter lead times, consistent quality and full Mill Test Certificates (EN 10204 3.1 / 3.2) for EN 10025-6 S500Q Steel Plate.

Our experienced export and technical teams provide support on material selection, welding procedures, cutting and processing. Customers benefit from reliable supply and professional service for high-strength quenched and tempered steel projects worldwide.

FAQ

What does “Q” mean in S500Q?
“Q” indicates the quenched and tempered condition and impact testing at –20°C.
What is the difference between S500Q and S500QL?
Both grades have the same strength level. S500Q is impact tested at –20°C, while S500QL is tested at –40°C and offers higher toughness for colder service.
Can SHH STEEL supply S500Q with Z-direction testing?
Yes. Z15, Z25 and Z35 testing can be arranged according to project requirements.

Conclusion

EN 10025-6 S500Q (1.8924) quenched and tempered steel plate from SHH STEEL provides a high yield strength of 500 MPa combined with reliable toughness at –20°C. As a China Mill-Direct Exporter, we offer competitive pricing, consistent quality and full technical support. Contact SHH STEEL today for stock availability, pricing or processing services.

EN 10025-6 S500Q Steel Plate, S500Q steel plate, S500Q QT, EN 10025 S500Q, S500Q equivalent, S500Q supplier, 1.8924

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X