EN 10025-4 S275ML Steel Plate | S275ML Fine Grain Structural Steel - SHH STEEL

EN 10025-4 S275ML Steel Plate | S275ML Fine Grain Structural Steel

EN 10025-4 S275ML is a thermomechanically rolled fine-grain structural steel plate with a minimum yield strength of 275 MPa and impact tested at –50°C. It offers excellent low-temperature toughness, weldability and formability. SHH STEEL is a China Mill-Direct Exporter supplying S275ML steel plate worldwide.
Equivalent Grades:
ASTM A572 Gr 42 (TMCP, -50℃ CVN) / JIS SN490B (L ref) / GB Q275ME / ISO E275ML
Material Specification:
EN 10025-4 — Delivery: Thermo-Mechanically Rolled (TMCP), -50℃ impact guaranteed
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Tolerances
Weldability
Equivalent Material Grades
Applications
Why Choose SHH STEEL
FAQ
Conclusion

What is EN 10025-4 S275ML Steel Plate?

As a professional steel plate supplier and China Mill-Direct Exporter, SHH STEEL is pleased to present EN 10025-4 S275ML Steel Plate (Material Number: 1.8819).

S275ML is a thermomechanically rolled (TMCP) weldable fine-grain structural steel under the European standard EN 10025-4. It provides a minimum yield strength of 275 MPa (for thickness ≤ 16 mm) and is impact tested at –50°C with a minimum energy of 27 J. Compared with S275M, S275ML offers superior low-temperature toughness, making it suitable for structural applications in colder environments. SHH STEEL sources this material directly from leading Chinese steel mills, ensuring competitive mill-direct pricing, stable quality and reliable delivery.

We supply S275ML steel plate in thicknesses from 6 mm to 120 mm (thicker plates available on request), widths up to 3000–4000 mm, and lengths up to 12000–18000 mm. Custom cutting, shot blasting and priming services are available. All plates are delivered with full Mill Test Certificates (EN 10204 3.1).

Material Specification

EN 10025-4 S275ML steel plate is produced in accordance with EN 10025-4.

Specification Element Requirement SHH STEEL Compliance
Primary Standard EN 10025-4 Full compliance
Steel Grade S275ML (1.8819) Confirmed
Delivery Condition Thermomechanically rolled (M) Confirmed
Product Form Steel Plate Available
Thickness Range 6 mm – 120 mm Custom sizes available
Width / Length Up to 3000–4000 mm / 12000–18000 mm Custom cutting supported
Certification EN 10204 3.1 / 3.2 Available

Chemical Composition

According to EN 10025-4, the chemical composition is specified for both ladle analysis (cast analysis) and product analysis.

Ladle Analysis (Cast Analysis)

Element Max. / Range (%)
Carbon (C) ≤ 0.13
Silicon (Si) ≤ 0.50
Manganese (Mn) ≤ 1.50
Phosphorus (P) ≤ 0.025
Sulfur (S) ≤ 0.020
Niobium (Nb) ≤ 0.05
Vanadium (V) ≤ 0.08
Aluminium (Al total) ≥ 0.020
Titanium (Ti) ≤ 0.05
Chromium (Cr) ≤ 0.30
Nickel (Ni) ≤ 0.30
Molybdenum (Mo) ≤ 0.10
Copper (Cu) ≤ 0.55
Nitrogen (N) ≤ 0.015

Product Analysis

Element Max. / Range (%)
Carbon (C) ≤ 0.15
Silicon (Si) ≤ 0.55
Manganese (Mn) ≤ 1.60
Phosphorus (P) ≤ 0.030
Sulfur (S) ≤ 0.025
Niobium (Nb) ≤ 0.06
Vanadium (V) ≤ 0.10
Aluminium (Al total) ≥ 0.015
Titanium (Ti) ≤ 0.06
Chromium (Cr) ≤ 0.35
Nickel (Ni) ≤ 0.35
Molybdenum (Mo) ≤ 0.13
Copper (Cu) ≤ 0.60
Nitrogen (N) ≤ 0.017

Note:

  • The minimum Al content does not apply if sufficient other nitrogen-binding elements are present.
  • Carbon Equivalent (CEV) is typically limited to ensure excellent weldability.

Mechanical Properties

Mechanical properties of EN 10025-4 S275ML (longitudinal direction):

Thickness (mm) Yield Strength ReH (min) Tensile Strength Rm Elongation A (min) Impact Energy KV (min)
≤ 16 275 MPa 370 – 530 MPa 24% 27 J at –50°C
> 16 ≤ 40 265 MPa 370 – 530 MPa 24% 27 J at –50°C
> 40 ≤ 63 255 MPa 360 – 520 MPa 24% 27 J at –50°C
> 63 ≤ 80 245 MPa 350 – 510 MPa 24% 27 J at –50°C
> 80 ≤ 100 245 MPa 350 – 510 MPa 24% 27 J at –50°C
> 100 ≤ 120 240 MPa 350 – 510 MPa 24% 27 J at –50°C

Density: 7.85 g/cm³

Delivery Conditions

SHH STEEL, as a China Mill-Direct Supplier, supplies EN 10025-4 S275ML steel plate in the thermomechanically rolled (M) condition.

Additional options:

  • Shot blasting and shop primer
  • Ultrasonic testing (EN 10160)
  • Z-direction testing (Z15 / Z25 / Z35)
  • Third-party inspection (SGS, BV, TUV, etc.)

Tolerances

Dimensional tolerances for S275ML steel plate follow EN 10029 (for plates).

  • Thickness, width and length tolerances according to the ordered class.
  • Flatness according to EN 10029.
  • Edge conditions: Mill edge or cut edge (flame / plasma).

Tighter tolerances can be provided upon request.

Weldability

S275ML has excellent weldability due to its low carbon content, low carbon equivalent and fine-grain structure achieved by thermomechanical rolling. It can be welded by all conventional methods (SMAW, GMAW, FCAW, SAW) with minimal preheating requirements.

Recommended welding consumables:

Welding Process Recommended Consumables
SMAW (Stick) E7018, E7016
GMAW (MIG/MAG) ER70S-6
FCAW E71T-1
SAW EM12K + suitable flux

Preheating is generally not required for thin and medium thicknesses. Low-hydrogen consumables are recommended for thicker plates or critical low-temperature applications.

Equivalent Material Grades

Grade Standard Notes
S275ML EN 10025-4 —
1.8819 EN Material number
Q275ML / Q275ME GB/T 1591 Closest Chinese equivalents
A633 / similar TM low-temp ASTM Approximate
TStE 275 TM DIN (old) Former designation

Applications

EN 10025-4 S275ML is widely used in structural applications requiring good strength and excellent low-temperature toughness. Typical uses include:

Application Area Typical Components / Uses (Keywords)
Building Structures Beams, columns in cold regions – S275ML Structural Steel
Bridges Bridge components – S275ML Bridge
Machinery Base plates, frames – S275ML Machinery
Low-Temperature Construction Structures requiring –50°C toughness – S275ML Construction
Industrial Structures Support structures – S275ML Industrial
General Fabrication Welded fine-grain structures – S275ML Fabrication

Why Choose SHH STEEL

SHH STEEL is a China Mill-Direct Exporter. We maintain long-term strategic cooperation with major Chinese steel mills and act as a first-level (primary) agent. This direct mill supply model allows us to offer competitive mill-direct pricing, faster delivery times, stable and traceable quality, and full Mill Test Certificates (EN 10204 3.1 / 3.2) for EN 10025-4 S275ML Steel Plate.

Customers benefit from reliable supply, short lead times and cost-effective solutions for thermomechanically rolled fine-grain low-temperature structural steel projects worldwide. Our professional export team provides technical support and customized processing services to meet project requirements.

FAQ

What does the “ML” in S275ML mean?
“M” indicates thermomechanically rolled condition, and “L” indicates impact tested at –50°C with a minimum of 27 J.
What is the difference between S275M and S275ML?
Both are thermomechanically rolled. S275M is impact tested at –20°C (40 J), while S275ML is impact tested at –50°C (27 J), offering better low-temperature toughness.

Conclusion

EN 10025-4 S275ML (1.8819) Steel Plate from SHH STEEL is a thermomechanically rolled fine-grain structural steel offering good strength, excellent weldability and superior toughness at –50°C. As a China Mill-Direct Exporter, we provide competitive pricing, fast delivery and consistent quality backed by full mill certifications. Trust SHH STEEL for your S275ML fine grain structural steel plate requirements.

Contact SHH STEEL today for stock availability, pricing and technical support. EN 10025-4 S275ML Steel Plate, S275ML steel plate, S275ML fine grain structural steel, EN 10025 S275ML, S275ML equivalent, S275ML supplier, 1.8819

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X