EN 10025-4 S275M Steel Plate | S275M Fine Grain Structural Steel - SHH STEEL

EN 10025-4 S275M Steel Plate | S275M Fine Grain Structural Steel

EN 10025-4 S275M is a thermomechanically rolled fine-grain structural steel plate with a minimum yield strength of 275 MPa and impact tested at –20°C. It offers excellent weldability, toughness and formability. SHH STEEL is a China Mill-Direct Exporter supplying S275M steel plate worldwide.
Equivalent Grades:
ASTM A572 Gr 42 (TMCP ref) / JIS SN490B / GB Q275MD / ISO E275M
Material Specification:
EN 10025-4 — Delivery: Thermo-Mechanically Rolled (TMCP), -20℃ impact guaranteed
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Tolerances
Weldability
Equivalent Material Grades
Applications
Why Choose SHH STEEL
FAQ
Conclusion

What is EN 10025-4 S275M Steel Plate?

As a professional steel plate supplier and China Mill-Direct Exporter, SHH STEEL is pleased to present EN 10025-4 S275M Steel Plate (Material Number: 1.8818).

S275M is a thermomechanically rolled (TMCP) weldable fine-grain structural steel under the European standard EN 10025-4. It provides a minimum yield strength of 275 MPa (for thickness ≤ 16 mm) and is impact tested at –20°C with a minimum energy of 40 J. Compared with normalized grades, S275M offers lower carbon equivalent, better weldability and good toughness. SHH STEEL sources this material directly from leading Chinese steel mills, ensuring competitive mill-direct pricing, stable quality and reliable delivery.

We supply S275M steel plate in thicknesses from 6 mm to 120 mm (thicker plates available on request), widths up to 3000–4000 mm, and lengths up to 12000–18000 mm. Custom cutting, shot blasting and priming services are available. All plates are delivered with full Mill Test Certificates (EN 10204 3.1).

Material Specification

EN 10025-4 S275M steel plate is produced in accordance with EN 10025-4.

Specification Element Requirement SHH STEEL Compliance
Primary Standard EN 10025-4 Full compliance
Steel Grade S275M (1.8818) Confirmed
Delivery Condition Thermomechanically rolled (M) Confirmed
Product Form Steel Plate Available
Thickness Range 6 mm – 120 mm Custom sizes available
Width / Length Up to 3000–4000 mm / 12000–18000 mm Custom cutting supported
Certification EN 10204 3.1 / 3.2 Available

Chemical Composition

According to EN 10025-4, the chemical composition is specified for both ladle analysis (cast analysis) and product analysis.

Ladle Analysis (Cast Analysis)

Element Max. / Range (%)
Carbon (C) ≤ 0.13
Silicon (Si) ≤ 0.50
Manganese (Mn) ≤ 1.50
Phosphorus (P) ≤ 0.030
Sulfur (S) ≤ 0.025
Niobium (Nb) ≤ 0.05
Vanadium (V) ≤ 0.08
Aluminium (Al total) ≥ 0.020
Titanium (Ti) ≤ 0.05
Chromium (Cr) ≤ 0.30
Nickel (Ni) ≤ 0.30
Molybdenum (Mo) ≤ 0.10
Copper (Cu) ≤ 0.55
Nitrogen (N) ≤ 0.015

Product Analysis

Element Max. / Range (%)
Carbon (C) ≤ 0.15
Silicon (Si) ≤ 0.55
Manganese (Mn) ≤ 1.60
Phosphorus (P) ≤ 0.035
Sulfur (S) ≤ 0.030
Niobium (Nb) ≤ 0.06
Vanadium (V) ≤ 0.10
Aluminium (Al total) ≥ 0.015
Titanium (Ti) ≤ 0.06
Chromium (Cr) ≤ 0.35
Nickel (Ni) ≤ 0.35
Molybdenum (Mo) ≤ 0.13
Copper (Cu) ≤ 0.60
Nitrogen (N) ≤ 0.017

Note:

  • The minimum Al content does not apply if sufficient other nitrogen-binding elements are present.
  • Carbon Equivalent (CEV) is typically limited to ensure excellent weldability.

Mechanical Properties

Mechanical properties of EN 10025-4 S275M (longitudinal direction):

Thickness (mm) Yield Strength ReH (min) Tensile Strength Rm Elongation A (min) Impact Energy KV (min)
≤ 16 275 MPa 370 – 530 MPa 24% 40 J at –20°C
> 16 ≤ 40 265 MPa 370 – 530 MPa 24% 40 J at –20°C
> 40 ≤ 63 255 MPa 360 – 520 MPa 24% 40 J at –20°C
> 63 ≤ 80 245 MPa 350 – 510 MPa 24% 40 J at –20°C
> 80 ≤ 100 245 MPa 350 – 510 MPa 24% 40 J at –20°C
> 100 ≤ 120 240 MPa 350 – 510 MPa 24% 40 J at –20°C

Density: 7.85 g/cm³

Delivery Conditions

SHH STEEL, as a China Mill-Direct Supplier, supplies EN 10025-4 S275M steel plate in the thermomechanically rolled (M) condition.

Additional options:

  • Shot blasting and shop primer
  • Ultrasonic testing (EN 10160)
  • Z-direction testing (Z15 / Z25 / Z35)
  • Third-party inspection (SGS, BV, TUV, etc.)

Tolerances

Dimensional tolerances for S275M steel plate follow EN 10029 (for plates).

  • Thickness, width and length tolerances according to the ordered class.
  • Flatness according to EN 10029.
  • Edge conditions: Mill edge or cut edge (flame / plasma).

Tighter tolerances can be provided upon request.

Weldability

S275M has excellent weldability due to its low carbon content, low carbon equivalent and fine-grain structure achieved by thermomechanical rolling. It can be welded by all conventional methods (SMAW, GMAW, FCAW, SAW) with minimal preheating requirements.

Recommended welding consumables:

Welding Process Recommended Consumables
SMAW (Stick) E7018, E7016
GMAW (MIG/MAG) ER70S-6
FCAW E71T-1
SAW EM12K + suitable flux

Preheating is generally not required for thin and medium thicknesses. Low-hydrogen consumables are recommended for thicker plates or critical applications.

Equivalent Material Grades

Grade Standard Notes
S275M EN 10025-4 —
1.8818 EN Material number
Q275M / Q275MD GB/T 1591 Closest Chinese equivalents
A633 / similar TM ASTM Approximate
StE 275 TM DIN (old) Former designation

Applications

EN 10025-4 S275M is widely used in structural applications requiring good strength and weldability. Typical uses include:

Application Area Typical Components / Uses (Keywords)
Building Structures Beams, columns, frames – S275M Structural Steel
Bridges Bridge components – S275M Bridge
Machinery Base plates, frames – S275M Machinery
Construction General construction – S275M Construction
Industrial Structures Support structures – S275M Industrial
General Fabrication Welded fine-grain structures – S275M Fabrication

Why Choose SHH STEEL

SHH STEEL is a China Mill-Direct Exporter. We maintain long-term strategic cooperation with major Chinese steel mills and act as a first-level (primary) agent. This direct mill supply model allows us to offer competitive mill-direct pricing, faster delivery times, stable and traceable quality, and full Mill Test Certificates (EN 10204 3.1 / 3.2) for EN 10025-4 S275M Steel Plate.

Customers benefit from reliable supply, short lead times and cost-effective solutions for thermomechanically rolled fine-grain structural steel projects worldwide. Our professional export team provides technical support and customized processing services to meet project requirements.

FAQ

What does the “M” in S275M mean?
“M” indicates that the steel is supplied in the thermomechanically rolled condition and meets impact requirements of minimum 40 J at –20°C.
What is the difference between S275M and S275ML?
Both are thermomechanically rolled. S275M is impact tested at –20°C (40 J), while S275ML is impact tested at –50°C (27 J), offering better low-temperature toughness.
What is the advantage of S275M compared with S275N?
S275M (TMCP) generally has lower carbon equivalent and better weldability than the normalized grade S275N.

Conclusion

EN 10025-4 S275M (1.8818) Steel Plate from SHH STEEL is a thermomechanically rolled fine-grain structural steel offering good strength, excellent weldability and reliable toughness at –20°C. As a China Mill-Direct Exporter, we provide competitive pricing, fast delivery and consistent quality backed by full mill certifications. Trust SHH STEEL for your S275M fine grain structural steel plate requirements.

Contact SHH STEEL today for stock availability, pricing and technical support. EN 10025-4 S275M Steel Plate, S275M steel plate, S275M fine grain structural steel, EN 10025 S275M, S275M equivalent, S275M supplier, 1.8818

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *