EN 10025-2 S185 Steel Plate | S185 Structural Steel - SHH STEEL

EN 10025-2 S185 Steel Plate | S185 Structural Steel

EN 10025-2 S185 is a low-strength non-alloy structural steel plate with a minimum yield strength of 185 MPa. It offers excellent weldability, formability and economy for general and light structural applications. SHH STEEL is a China Mill-Direct Exporter supplying S185 steel plate worldwide.
Equivalent Grades:
ASTM A283 Gr A / JIS SS330 / GB Q195 / ISO E185
Specification:
EN 10025-2 — Delivery: As-rolled or normalized rolling (N)
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Tolerances
Weldability
Equivalent Material Grades
Applications
Why Choose SHH STEEL
FAQ
Conclusion

What is EN 10025-2 S185 Steel Plate?

As a professional steel plate supplier and China Mill-Direct Exporter, SHH STEEL is pleased to present EN 10025-2 S185 Steel Plate (Material Number: 1.0035).

S185 is the lowest strength grade of non-alloy structural steel under the European standard EN 10025-2. It provides a minimum yield strength of 185 MPa (for thickness ≤ 16 mm) and is characterized by excellent weldability, formability and cost-effectiveness. This grade is typically used for light structural applications, general fabrication and components where high strength is not required. SHH STEEL sources this material directly from leading Chinese steel mills, ensuring competitive mill-direct pricing, stable quality and reliable delivery.

We supply S185 steel plate in thicknesses from 6 mm to 150 mm (thicker plates available on request), widths up to 3000–4000 mm, and lengths up to 12000–18000 mm. Custom cutting, shot blasting and priming services are available. All plates are delivered with full Mill Test Certificates (EN 10204 3.1).

Material Specification

EN 10025-2 S185 steel plate is produced in accordance with EN 10025-2.

Specification Element Requirement SHH STEEL Compliance
Primary Standard EN 10025-2 Full compliance
Steel Grade S185 (1.0035) Confirmed
Delivery Condition +AR (As-rolled) Available
Product Form Steel Plate Available
Thickness Range 6 mm – 150 mm Custom sizes available
Width / Length Up to 3000–4000 mm / 12000–18000 mm Custom cutting supported
Certification EN 10204 3.1 / 3.2 Available

Chemical Composition

According to EN 10025-2, S185 has relatively loose chemical composition requirements (mainly limits on impurities).

Ladle Analysis (Cast Analysis)

Element Max. Limit (%)
Phosphorus (P) 0.045
Sulfur (S) 0.045
Nitrogen (N) 0.012
Copper (Cu) 0.55

Product Analysis

Element Max. Limit (%)
Phosphorus (P) 0.055
Sulfur (S) 0.055
Nitrogen (N) 0.014
Copper (Cu) 0.60

Note:

  • Carbon, Silicon and Manganese contents are not strictly limited in the standard for S185.
  • The maximum nitrogen content does not apply if the total aluminium content is ≥ 0.020%.
  • Deoxidation method is at the manufacturer’s discretion.

Mechanical Properties

Mechanical properties of EN 10025-2 S185 (typical values):

Thickness (mm) Yield Strength ReH (min) Tensile Strength Rm Elongation A (min)
≤ 16 185 MPa 290 – 510 MPa 18%
> 16 ≤ 40 175 MPa 290 – 510 MPa 18%
> 40 ≤ 63 175 MPa 290 – 510 MPa 17%
> 63 ≤ 100 175 MPa 290 – 510 MPa 16%
> 100 ≤ 150 165 MPa 280 – 500 MPa 15%

Density: 7.85 g/cm³

Note: Impact testing is not mandatory for S185 under EN 10025-2.

Delivery Conditions

SHH STEEL, as a China Mill-Direct Supplier, supplies EN 10025-2 S185 steel plate mainly in the as-rolled (+AR) condition.

Additional options:

  • Shot blasting and shop primer
  • Ultrasonic testing (EN 10160)
  • Third-party inspection (SGS, BV, TUV, etc.)

Tolerances

Dimensional tolerances for S185 steel plate follow EN 10029 (for plates) or EN 10051 (for strips).

  • Thickness, width and length tolerances according to the ordered class.
  • Flatness according to EN 10029.
  • Edge conditions: Mill edge or cut edge (flame / plasma).

Tighter tolerances can be provided upon request.

Weldability

S185 has excellent weldability due to its low strength and low carbon content. It can be welded by all conventional methods (SMAW, SAW, GMAW, FCAW, etc.) without preheating in most cases. It is one of the easiest structural steels to weld and form.

Equivalent Material Grades

Grade Standard Notes
S185 EN 10025-2 —
1.0035 EN Material number
Q195 GB/T 700 Closest Chinese equivalent
A283 Grade A/B ASTM Approximate
St33 DIN (old) Former designation
Fe310 ISO Approximate

Applications

EN 10025-2 S185 is used for light structural and general fabrication applications where high strength is not required. Typical uses include:

Application Area Typical Components / Uses (Keywords)
Light Structures Light frames, supports – S185 Structural Steel
General Fabrication Simple welded structures – S185 Fabrication
Machinery Non-critical base plates and frames – S185 Machinery
Construction Light construction components – S185 Construction
Storage Simple tanks and silos – S185 Storage
Agricultural Equipment Light equipment frames – S185 Agricultural

Why Choose SHH STEEL

SHH STEEL is a China Mill-Direct Exporter. We maintain long-term strategic cooperation with major Chinese steel mills and act as a first-level (primary) agent. This direct mill supply model allows us to offer competitive mill-direct pricing, faster delivery times, stable and traceable quality, and full Mill Test Certificates (EN 10204 3.1 / 3.2) for EN 10025-2 S185 Steel Plate.

Customers benefit from reliable supply, short lead times and cost-effective solutions for structural steel projects worldwide. Our professional export team provides technical support and customized processing services to meet project requirements.

FAQ

What is the main characteristic of S185?
S185 is the lowest strength grade in the EN 10025-2 series, with a minimum yield strength of 185 MPa. It offers excellent weldability and formability at a low cost.
Does S185 require impact testing?
No. Impact testing is not mandatory for S185 under EN 10025-2 (unlike JR, J0 and J2 grades).
What is the closest Chinese equivalent to S185?
Q195 (GB/T 700).

Conclusion

EN 10025-2 S185 (1.0035) Steel Plate from SHH STEEL is an economical low-strength non-alloy structural steel ideal for light fabrication and general applications. As a China Mill-Direct Exporter, we provide competitive pricing, fast delivery and consistent quality backed by full mill certifications. Trust SHH STEEL for your S185 structural steel plate requirements.

Contact SHH STEEL today for stock availability, pricing and technical support. EN 10025-2 S185 Steel Plate, S185 steel plate, S185 structural steel, EN 10025 S185, S185 equivalent, S185 supplier, 1.0035

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X