EN 10025-2 E355 Steel Plate | E355 Structural Steel
What is EN 10025-2 E355 Steel Plate?
As a professional steel plate supplier and China Mill-Direct Exporter, SHH STEEL is pleased to present EN 10025-2 E355 Steel Plate (Material Number: 1.0060).
E355 is a non-alloy structural steel under the European standard EN 10025-2. It provides a minimum yield strength of 355 MPa (for thickness ≤ 16 mm) and is positioned as a higher-strength option compared with E295. This grade is suitable for general structural and engineering applications where moderate-to-high strength is required. SHH STEEL sources this material directly from leading Chinese steel mills, ensuring competitive mill-direct pricing, stable quality and reliable delivery.
We supply E355 steel plate in thicknesses from 6 mm to 150 mm (thicker plates available on request), widths up to 3000–4000 mm, and lengths up to 12000–18000 mm. Custom cutting, shot blasting and priming services are available. All plates are delivered with full Mill Test Certificates (EN 10204 3.1).
Material Specification
EN 10025-2 E355 steel plate is produced in accordance with EN 10025-2.
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Primary Standard | EN 10025-2 | Full compliance |
| Steel Grade | E355 (1.0060) | Confirmed |
| Delivery Condition | +AR (As-rolled) or +N (Normalized) | Available |
| Product Form | Steel Plate | Available |
| Thickness Range | 6 mm – 150 mm | Custom sizes available |
| Width / Length | Up to 3000–4000 mm / 12000–18000 mm | Custom cutting supported |
| Certification | EN 10204 3.1 / 3.2 | Available |
Chemical Composition
According to EN 10025-2, E355 has relatively simple chemical composition requirements focused on impurity control.
Ladle Analysis (Cast Analysis)
| Element | Max. Limit (%) |
|---|---|
| Phosphorus (P) | 0.045 |
| Sulfur (S) | 0.045 |
| Nitrogen (N) | 0.012 |
Product Analysis
| Element | Max. Limit (%) |
|---|---|
| Phosphorus (P) | 0.055 |
| Sulfur (S) | 0.055 |
| Nitrogen (N) | 0.014 |
Note:
- Carbon, Silicon and Manganese contents are not strictly limited in the standard for E355.
- Rimming steel is not permitted (FN).
- The maximum nitrogen content does not apply if the total aluminium content is ≥ 0.020%.
Mechanical Properties
Mechanical properties of EN 10025-2 E355 (longitudinal direction):
| Thickness (mm) | Yield Strength ReH (min) | Tensile Strength Rm | Elongation A (min) |
|---|---|---|---|
| ≤ 16 | 355 MPa | 490 – 630 MPa | 20% |
| > 16 ≤ 40 | 345 MPa | 490 – 630 MPa | 20% |
| > 40 ≤ 63 | 335 MPa | 490 – 630 MPa | 19% |
| > 63 ≤ 100 | 325 – 315 MPa | 490 – 630 MPa | 18% |
| > 100 ≤ 150 | 295 MPa | 470 – 610 MPa | 16% |
Density: 7.85 g/cm³
Note: Impact testing is not mandatory for E355 under EN 10025-2.
Delivery Conditions
SHH STEEL, as a China Mill-Direct Supplier, supplies EN 10025-2 E355 steel plate mainly in the following conditions:
- +AR (As-rolled) – most common
- +N (Normalized) – available on request
Additional options:
- Shot blasting and shop primer
- Ultrasonic testing (EN 10160)
- Third-party inspection (SGS, BV, TUV, etc.)
Tolerances
Dimensional tolerances for E355 steel plate follow EN 10029 (for plates) or EN 10051 (for strips).
- Thickness, width and length tolerances according to the ordered class.
- Flatness according to EN 10029.
- Edge conditions: Mill edge or cut edge (flame / plasma).
Tighter tolerances can be provided upon request.
Weldability
E355 has good weldability for a higher-strength non-alloy structural steel. It can be welded using conventional methods including SMAW, GMAW (MIG/MAG), FCAW and SAW.
Recommended welding consumables:
| Welding Process | Recommended Consumables |
|---|---|
| SMAW (Stick) | E7018, E7016 |
| GMAW (MIG/MAG) | ER70S-6 |
| FCAW | E71T-1, E71T-1C |
| SAW | EM12K + suitable flux |
Notes:
- Low-hydrogen consumables are recommended.
- Preheating may be required for thicker plates (typically above 25–30 mm) depending on carbon equivalent and joint design.
- Interpass temperature should be controlled.
- Proper cleaning of the weld area is important to avoid defects.
Equivalent Material Grades
| Grade | Standard | Notes |
|---|---|---|
| E355 | EN 10025-2 | — |
| 1.0060 | EN | Material number |
| Q355 (approx.) | GB/T 1591 | Closest Chinese equivalent |
| St52-3 (approx.) | DIN (old) | Similar strength level |
| Fe510 | ISO / Other | Approximate |
Applications
EN 10025-2 E355 is used for structural applications requiring higher strength than E295. Typical uses include:
| Application Area | Typical Components / Uses (Keywords) |
|---|---|
| Building Structures | Beams, columns, frames – E355 Structural Steel |
| Machinery | Base plates, heavy frames – E355 Machinery |
| Construction | High-strength construction components – E355 Construction |
| Industrial Structures | Support structures – E355 Industrial |
| General Fabrication | Welded high-strength structures – E355 Fabrication |
| Heavy Equipment | Equipment frames – E355 Heavy Equipment |
Why Choose SHH STEEL
SHH STEEL is a China Mill-Direct Exporter. We maintain long-term strategic cooperation with major Chinese steel mills and act as a first-level (primary) agent. This direct mill supply model allows us to offer competitive mill-direct pricing, faster delivery times, stable and traceable quality, and full Mill Test Certificates (EN 10204 3.1 / 3.2) for EN 10025-2 E355 Steel Plate.
Customers benefit from reliable supply, short lead times and cost-effective solutions for structural steel projects worldwide. Our professional export team provides technical support and customized processing services to meet project requirements.
FAQ
-
What is the main characteristic of E355?
- E355 is a non-alloy structural steel with a minimum yield strength of 355 MPa, offering higher strength than E295 for more demanding structural applications.
-
Does E355 require impact testing?
- No. Impact testing is not mandatory for E355 under EN 10025-2.
-
What welding wires are recommended for E355?
- Common recommendations include E7018 (SMAW), ER70S-6 (GMAW), E71T-1 (FCAW) and EM12K for SAW.
-
What is the material number of E355?
- 1.0060
Conclusion
EN 10025-2 E355 (1.0060) Steel Plate from SHH STEEL is a reliable higher-strength non-alloy structural steel suitable for general engineering and construction applications. As a China Mill-Direct Exporter, we provide competitive pricing, fast delivery and consistent quality backed by full mill certifications. Trust SHH STEEL for your E355 structural steel plate requirements.
Contact SHH STEEL today for stock availability, pricing and technical support. EN 10025-2 E355 Steel Plate, E355 steel plate, E355 structural steel, EN 10025 E355, E355 equivalent, E355 supplier, 1.0060