EN 10025-2 E295 Steel Plate | E295 Structural Steel
What is EN 10025-2 E295 Steel Plate?
As a professional steel plate supplier and China Mill-Direct Exporter, SHH STEEL is pleased to present EN 10025-2 E295 Steel Plate (Material Number: 1.0050).
E295 is a non-alloy structural steel under the European standard EN 10025-2. It provides a minimum yield strength of 295 MPa (for thickness ≤ 16 mm) and is positioned between the lower-strength S185 and the higher S355 series in terms of mechanical properties. This grade is suitable for general structural applications where moderate strength is required. SHH STEEL sources this material directly from leading Chinese steel mills, ensuring competitive mill-direct pricing, stable quality and reliable delivery.
We supply E295 steel plate in thicknesses from 6 mm to 150 mm (thicker plates available on request), widths up to 3000–4000 mm, and lengths up to 12000–18000 mm. Custom cutting, shot blasting and priming services are available. All plates are delivered with full Mill Test Certificates (EN 10204 3.1).
Material Specification
EN 10025-2 E295 steel plate is produced in accordance with EN 10025-2.
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Primary Standard | EN 10025-2 | Full compliance |
| Steel Grade | E295 (1.0050) | Confirmed |
| Delivery Condition | +AR (As-rolled) or +N (Normalized) | Available |
| Product Form | Steel Plate | Available |
| Thickness Range | 6 mm – 150 mm | Custom sizes available |
| Width / Length | Up to 3000–4000 mm / 12000–18000 mm | Custom cutting supported |
| Certification | EN 10204 3.1 / 3.2 | Available |
Chemical Composition
According to EN 10025-2, E295 has relatively simple chemical composition requirements focused on impurity control.
Ladle Analysis (Cast Analysis)
| Element | Max. Limit (%) |
|---|---|
| Phosphorus (P) | 0.045 |
| Sulfur (S) | 0.045 |
| Nitrogen (N) | 0.012 |
Product Analysis
| Element | Max. Limit (%) |
|---|---|
| Phosphorus (P) | 0.055 |
| Sulfur (S) | 0.055 |
| Nitrogen (N) | 0.014 |
Note:
- Carbon, Silicon and Manganese contents are not strictly limited in the standard for E295.
- Rimming steel is not permitted (FN).
- The maximum nitrogen content does not apply if the total aluminium content is ≥ 0.020%.
Mechanical Properties
Mechanical properties of EN 10025-2 E295 (longitudinal direction):
| Thickness (mm) | Yield Strength ReH (min) | Tensile Strength Rm | Elongation A (min) |
|---|---|---|---|
| ≤ 16 | 295 MPa | 470 – 610 MPa | 20% |
| > 16 ≤ 40 | 285 MPa | 470 – 610 MPa | 20% |
| > 40 ≤ 63 | 275 MPa | 470 – 610 MPa | 19% |
| > 63 ≤ 80 | 265 MPa | 470 – 610 MPa | 18% |
| > 80 ≤ 100 | 255 MPa | 470 – 610 MPa | 18% |
| > 100 ≤ 150 | 245 MPa | 450 – 610 MPa | 16% |
Density: 7.85 g/cm³
Note: Impact testing is not mandatory for E295 under EN 10025-2.
Delivery Conditions
SHH STEEL, as a China Mill-Direct Supplier, supplies EN 10025-2 E295 steel plate mainly in the following conditions:
- +AR (As-rolled) – most common
- +N (Normalized) – available on request
Additional options:
- Shot blasting and shop primer
- Ultrasonic testing (EN 10160)
- Third-party inspection (SGS, BV, TUV, etc.)
Tolerances
Dimensional tolerances for E295 steel plate follow EN 10029 (for plates) or EN 10051 (for strips).
- Thickness, width and length tolerances according to the ordered class.
- Flatness according to EN 10029.
- Edge conditions: Mill edge or cut edge (flame / plasma).
Tighter tolerances can be provided upon request.
Weldability
E295 has good weldability. It can be welded by conventional methods (SMAW, SAW, GMAW, FCAW, etc.). Preheating is generally not required for thinner plates. Low-hydrogen consumables are recommended for thicker sections or critical applications.
Equivalent Material Grades
| Grade | Standard | Notes |
|---|---|---|
| E295 | EN 10025-2 | — |
| 1.0050 | EN | Material number |
| Q295 (approx.) | GB/T 1591 / GB/T 700 | Closest Chinese equivalent |
| St50-2 | DIN (old) | Former designation |
| Fe490 | ISO / Other | Approximate |
Applications
EN 10025-2 E295 is used for general structural applications requiring moderate strength. Typical uses include:
| Application Area | Typical Components / Uses (Keywords) |
|---|---|
| Building Structures | Beams, columns, frames – E295 Structural Steel |
| Machinery | Base plates, frames – E295 Machinery |
| Construction | General construction components – E295 Construction |
| Industrial Structures | Support structures – E295 Industrial |
| General Fabrication | Welded structures – E295 Fabrication |
| Agricultural & Equipment | Equipment frames – E295 Agricultural |
Why Choose SHH STEEL
SHH STEEL is a China Mill-Direct Exporter. We maintain long-term strategic cooperation with major Chinese steel mills and act as a first-level (primary) agent. This direct mill supply model allows us to offer competitive mill-direct pricing, faster delivery times, stable and traceable quality, and full Mill Test Certificates (EN 10204 3.1 / 3.2) for EN 10025-2 E295 Steel Plate.
Customers benefit from reliable supply, short lead times and cost-effective solutions for structural steel projects worldwide. Our professional export team provides technical support and customized processing services to meet project requirements.
FAQ
-
What is the main characteristic of E295?
- E295 is a non-alloy structural steel with a minimum yield strength of 295 MPa. It sits between S185 and S355 in terms of strength level.
-
What is the closest Chinese equivalent to E295?
- Approximately Q295.
Conclusion
EN 10025-2 E295 (1.0050) Steel Plate from SHH STEEL is a reliable non-alloy structural steel with moderate strength for general engineering and construction applications. As a China Mill-Direct Exporter, we provide competitive pricing, fast delivery and consistent quality backed by full mill certifications. Trust SHH STEEL for your E295 structural steel plate requirements.
Contact SHH STEEL today for stock availability, pricing and technical support. EN 10025-2 E295 Steel Plate, E295 steel plate, E295 structural steel, EN 10025 E295, E295 equivalent, E295 supplier, 1.0050