EN 10025-2 E360 Steel Plate | E360 Structural Steel - SHH STEEL

EN 10025-2 E360 Steel Plate | E360 Structural Steel

EN 10025-2 E360 is a high-strength non-alloy structural steel plate with a minimum yield strength of 360 MPa. It offers higher strength than E355 with good weldability for demanding structural applications. SHH STEEL is a China Mill-Direct Exporter supplying E360 steel plate worldwide.
Equivalent Grades:
ASTM A572 Gr 65 / JIS SM520C / GB Q420A / ISO E420A
Specification:
EN 10025-2 — Delivery: As-rolled or normalized rolling (N)
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Tolerances
Weldability
Equivalent Material Grades
Applications
Why Choose SHH STEEL
FAQ
Conclusion

What is EN 10025-2 E360 Steel Plate?

As a professional steel plate supplier and China Mill-Direct Exporter, SHH STEEL is pleased to present EN 10025-2 E360 Steel Plate (Material Number: 1.0070).

E360 is a high-strength non-alloy structural steel under the European standard EN 10025-2. It provides a minimum yield strength of 360 MPa (for thickness ≤ 16 mm) and is the highest strength grade among the E-series steels (E295, E355, E360) that do not have mandatory impact requirements. This grade is suitable for structural and engineering applications requiring higher load-bearing capacity. SHH STEEL sources this material directly from leading Chinese steel mills, ensuring competitive mill-direct pricing, stable quality and reliable delivery.

We supply E360 steel plate in thicknesses from 6 mm to 150 mm (thicker plates available on request), widths up to 3000–4000 mm, and lengths up to 12000–18000 mm. Custom cutting, shot blasting and priming services are available. All plates are delivered with full Mill Test Certificates (EN 10204 3.1).

Material Specification

EN 10025-2 E360 steel plate is produced in accordance with EN 10025-2.

Specification Element Requirement SHH STEEL Compliance
Primary Standard EN 10025-2 Full compliance
Steel Grade E360 (1.0070) Confirmed
Delivery Condition +AR (As-rolled) or +N (Normalized) Available
Product Form Steel Plate Available
Thickness Range 6 mm – 150 mm Custom sizes available
Width / Length Up to 3000–4000 mm / 12000–18000 mm Custom cutting supported
Certification EN 10204 3.1 / 3.2 Available

Chemical Composition

According to EN 10025-2, E360 has relatively simple chemical composition requirements focused on impurity control.

Ladle Analysis (Cast Analysis)

Element Max. Limit (%)
Phosphorus (P) 0.045
Sulfur (S) 0.045
Nitrogen (N) 0.012

Product Analysis

Element Max. Limit (%)
Phosphorus (P) 0.055
Sulfur (S) 0.055
Nitrogen (N) 0.014

Note:

  • Carbon, Silicon and Manganese contents are not strictly limited in the standard for E360.
  • Rimming steel is not permitted (FN).
  • The maximum nitrogen content does not apply if the total aluminium content is ≥ 0.020%.

Mechanical Properties

Mechanical properties of EN 10025-2 E360 (longitudinal direction):

Thickness (mm) Yield Strength ReH (min) Tensile Strength Rm Elongation A (min)
≤ 16 360 MPa 510 – 660 MPa 19%
> 16 ≤ 40 350 MPa 510 – 660 MPa 19%
> 40 ≤ 63 340 MPa 510 – 660 MPa 18%
> 63 ≤ 100 330 – 320 MPa 510 – 660 MPa 17%
> 100 ≤ 150 300 MPa 490 – 640 MPa 15%

Density: 7.85 g/cm³

Note: Impact testing is not mandatory for E360 under EN 10025-2.

Delivery Conditions

SHH STEEL, as a China Mill-Direct Supplier, supplies EN 10025-2 E360 steel plate mainly in the following conditions:

  • +AR (As-rolled) – most common
  • +N (Normalized) – available on request

Additional options:

  • Shot blasting and shop primer
  • Ultrasonic testing (EN 10160)
  • Third-party inspection (SGS, BV, TUV, etc.)

Tolerances

Dimensional tolerances for E360 steel plate follow EN 10029 (for plates) or EN 10051 (for strips).

  • Thickness, width and length tolerances according to the ordered class.
  • Flatness according to EN 10029.
  • Edge conditions: Mill edge or cut edge (flame / plasma).

Tighter tolerances can be provided upon request.

Weldability

E360 has moderate-to-good weldability for a higher-strength non-alloy structural steel. It can be welded using conventional methods including SMAW, GMAW (MIG/MAG), FCAW and SAW.

Recommended welding consumables:

Welding Process Recommended Consumables
SMAW (Stick) E7018, E7016, E8018
GMAW (MIG/MAG) ER70S-6, ER80S-D2
FCAW E71T-1, E81T1
SAW EM12K / EH14 + suitable flux

Notes:

  • Low-hydrogen consumables are strongly recommended.
  • Preheating is generally required for thicker plates (typically above 20–25 mm) depending on carbon equivalent and joint restraint.
  • Interpass temperature should be carefully controlled.
  • Proper cleaning of the joint area is essential to avoid weld defects.

Equivalent Material Grades

Grade Standard Notes
E360 EN 10025-2 —
1.0070 EN Material number
Q355 / Q390 (approx.) GB/T 1591 Closest Chinese equivalents
St60-2 (approx.) DIN (old) Similar strength level
Fe590 ISO / Other Approximate

Applications

EN 10025-2 E360 is used for structural applications requiring higher strength. Typical uses include:

Application Area Typical Components / Uses (Keywords)
Building Structures Heavy beams, columns, high-load frames – E360 Structural Steel
Machinery Heavy base plates and frames – E360 Machinery
Construction High-strength construction components – E360 Construction
Industrial Structures Heavy support structures – E360 Industrial
General Fabrication High-strength welded structures – E360 Fabrication
Heavy Equipment Equipment frames and chassis – E360 Heavy Equipment

Why Choose SHH STEEL

SHH STEEL is a China Mill-Direct Exporter. We maintain long-term strategic cooperation with major Chinese steel mills and act as a first-level (primary) agent. This direct mill supply model allows us to offer competitive mill-direct pricing, faster delivery times, stable and traceable quality, and full Mill Test Certificates (EN 10204 3.1 / 3.2) for EN 10025-2 E360 Steel Plate.

Customers benefit from reliable supply, short lead times and cost-effective solutions for high-strength structural steel projects worldwide. Our professional export team provides technical support and customized processing services to meet project requirements.

FAQ

What is the main characteristic of E360?
E360 is a high-strength non-alloy structural steel with a minimum yield strength of 360 MPa, the highest among the E-series grades (E295, E355, E360) in EN 10025-2.
Does E360 require impact testing?
No. Impact testing is not mandatory for E360 under EN 10025-2.
What welding wires are recommended for E360?
Common recommendations include E7018 / E8018 (SMAW), ER70S-6 / ER80S-D2 (GMAW), E71T-1 / E81T1 (FCAW) and EM12K or EH14 for SAW.
What is the material number of E360?
1.0070

Conclusion

EN 10025-2 E360 (1.0070) Steel Plate from SHH STEEL is a high-strength non-alloy structural steel suitable for demanding engineering and construction applications. As a China Mill-Direct Exporter, we provide competitive pricing, fast delivery and consistent quality backed by full mill certifications. Trust SHH STEEL for your E360 structural steel plate requirements.

Contact SHH STEEL today for stock availability, pricing and technical support.

EN 10025-2 E360 Steel Plate, E360 steel plate, E360 structural steel, EN 10025 E360, E360 equivalent, E360 supplier, 1.0070

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X