DIN 17100 St60-2 Steel Plate | St60-2 Structural Steel - SHH STEEL

DIN 17100 St60-2 Steel Plate | St60-2 Structural Steel

DIN 17100 St60-2 is a high-strength structural steel plate with a minimum yield strength of 335 MPa and tensile strength of 590–770 MPa. It offers higher strength than St50 and St52 grades while maintaining acceptable weldability. SHH STEEL supplies St60-2 as Mill Direct Supply with competitive pricing and full mill certification.
Equivalent Grades:
ASTM A572 Gr 60 / EN E335 (1.0060) / JIS SM490A / GB Q345A
Specification:
DIN 17100 — Delivery: As-rolled
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Tolerances
Weldability
Equivalent Material Grades
Applications
Why Choose SHH STEEL
FAQ
Conclusion

What is DIN 17100 St60-2 Steel Plate?

As a professional steel plate supplier and China Mill-Direct Exporter, SHH STEEL is pleased to present DIN 17100 St60-2 Steel Plate.

St60-2 is a high-strength non-alloy structural steel under the former German standard DIN 17100. It provides a minimum yield strength of 335 MPa (for thickness ≤ 16 mm) and a tensile strength range of 590–770 MPa. This grade offers higher strength than St50-2 and St52-3 and is used in applications requiring elevated load-bearing capacity. Although DIN 17100 has been largely replaced by EN 10025, St60-2 is still requested in certain markets.

This grade belongs to the DIN 17100 Steel Plate series. SHH STEEL supplies St60-2 as Mill Direct Supply, sourcing directly from major Chinese steel mills. This ensures competitive mill pricing, consistent quality, shorter lead times and full traceability. We offer thicknesses from 6 mm to 100 mm (subject to mill capability), widths up to 3000–4000 mm and lengths up to 12000–18000 mm. Custom cutting, shot blasting and priming services are available. All plates are delivered with full Mill Test Certificates (EN 10204 3.1 or equivalent).

Material Specification

Specification Element Requirement SHH STEEL Compliance
Primary Standard DIN 17100 Full compliance
Steel Grade St60-2 (1.0060) Confirmed
Delivery Condition As-rolled / Normalized Available
Product Form Steel Plate Available
Thickness Range 6 mm – 100 mm (typical) Custom sizes available
Width / Length Up to 3000–4000 mm / 12000–18000 mm Custom cutting supported
Certification EN 10204 3.1 / Mill Certificate Available

Chemical Composition

Chemical composition according to DIN 17100 (typical values):

Element Ladle Analysis (Max. %) Product Analysis (Max. %)
Carbon (C) ≤ 0.20 ≤ 0.22
Silicon (Si) ≤ 0.55 ≤ 0.60
Manganese (Mn) ≤ 1.60 ≤ 1.70
Phosphorus (P) ≤ 0.045 – 0.050 ≤ 0.055
Sulfur (S) ≤ 0.045 – 0.050 ≤ 0.055
Nitrogen (N) ≤ 0.009 ≤ 0.010

Note: Controlled carbon content is important to maintain weldability at this higher strength level.

Mechanical Properties

Mechanical properties of DIN 17100 St60-2:

Thickness (mm) Yield Strength ReH (min) Tensile Strength Rm Elongation A (min)
≤ 16 335 MPa 590 – 770 MPa 16%
> 16 ≤ 40 325 MPa 590 – 770 MPa 15%
> 40 ≤ 63 315 MPa 590 – 770 MPa 14%
> 63 ≤ 100 305 MPa 590 – 770 MPa 13%

Density: 7.85 g/cm³ Impact Test: Typically 27 J at +20°C (when required).

Delivery Conditions

SHH STEEL supplies DIN 17100 St60-2 steel plate as Mill Direct Supply in as-rolled or normalized condition according to customer requirements.

Additional options available:

  • Shot blasting and shop primer
  • Ultrasonic testing (EN 10160 or equivalent)
  • Z-direction testing (Z15 / Z25 / Z35)
  • Third-party inspection (SGS, BV, TUV, etc.)

Tolerances

Dimensional tolerances for St60-2 steel plate follow DIN standards or equivalent international standards (EN 10029 / ASTM A6).

  • Thickness, width and length tolerances according to the ordered class.
  • Flatness according to applicable standard.
  • Edge conditions: Mill edge or cut edge (flame / plasma).

Tighter tolerances can be provided upon request.

Weldability

St60-2 is a higher-strength structural steel. Successful welding requires proper procedures, including preheating for thicker plates and the use of low-hydrogen consumables.

Recommended welding consumables:

Welding Process Recommended Consumables
SMAW (Stick) E8018, E9018
GMAW (MIG/MAG) ER80S-D2, ER90S-D2
FCAW E81T1, E91T1
SAW EH14 / matching high-strength flux

Preheating is generally recommended for thicker sections. Interpass temperature control is important.

Equivalent Material Grades

Grade Standard Notes
St60-2 DIN 17100 —
1.0060 DIN / EN Material number
S355J2 / S420N EN 10025-2 / EN 10025-3 Approximate modern equivalents
Q390B / Q420B GB/T 1591 Closest Chinese equivalents
ASTM A572 Grade 55/60 ASTM Approximate American grades
SM520B JIS G3106 Approximate Japanese grade

Applications

DIN 17100 St60-2 is used in higher-strength structural and engineering applications. Typical uses include:

Application Area Typical Components / Uses (Keywords)
Building Structures Heavy beams, columns, frames – St60-2 Structural Steel
Bridges Main girders, high-load components – St60-2 Bridge
Machinery Heavy frames, supports – St60-2 Machinery
Crane & Lifting Equipment Structural parts – St60-2 Crane
General Fabrication High-strength welded structures – St60-2 Fabrication
Construction Structural parts – St60-2 Construction

Why Choose SHH STEEL

SHH STEEL provides St60-2 as Mill Direct Supply. We maintain long-term strategic cooperation with major Chinese steel mills and act as a first-level (primary) agent. This direct mill supply model allows us to offer competitive mill-direct pricing, faster delivery times, stable and traceable quality, and full Mill Test Certificates for DIN 17100 St60-2 Steel Plate.

Customers benefit from reliable supply, short lead times and cost-effective solutions for high-strength structural steel projects worldwide. Our professional export team provides technical support and customized processing services to meet project requirements.

FAQ

What is the strength level of St60-2?
St60-2 has a minimum yield strength of 335 MPa (≤16 mm) and tensile strength of 590–770 MPa, higher than St50-2 and St52-3.
Is St60-2 still commonly used?
Although DIN 17100 is an old standard, St60-2 is still requested in some markets, particularly where higher strength than St52-3 is needed under the traditional designation.

Conclusion

DIN 17100 St60-2 Steel Plate from SHH STEEL is a high-strength structural steel offering 335 MPa minimum yield strength and 590–770 MPa tensile strength. As Mill Direct Supply, we provide competitive pricing, consistent quality and full technical support. Trust SHH STEEL for your St60-2 steel plate requirements.

Contact SHH STEEL today for stock availability, pricing and technical support. DIN 17100 St60-2 Steel Plate, St60-2 steel plate, St60-2, St60-2 Structural Steel, St60-2 supplier, St60-2 equivalent

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X