DIN 17100 St44-2 Steel Plate | St44-2 Structural Steel
What is DIN 17100 St44-2 Steel Plate?
As a professional steel plate supplier and China Mill-Direct Exporter, SHH STEEL is pleased to present DIN 17100 St44-2 Steel Plate.
St44-2 is a non-alloy structural steel under the former German standard DIN 17100. It provides a minimum yield strength of 275 MPa (for thickness ≤ 16 mm) and a tensile strength range of 430–580 MPa. This grade offers higher strength than the St37 series while retaining good weldability and formability. Although DIN 17100 has been largely superseded by EN 10025-2, St44-2 remains widely requested and is essentially equivalent to modern S275JR.
This grade belongs to the DIN 17100 Steel Plate series. SHH STEEL supplies St44-2 as Mill Direct Supply, sourcing directly from major Chinese steel mills. This ensures competitive mill pricing, consistent quality, shorter lead times and full traceability. We offer thicknesses from 6 mm to 150 mm, widths up to 3000–4000 mm and lengths up to 12000–18000 mm. Custom cutting, shot blasting and priming services are available. All plates are delivered with full Mill Test Certificates (EN 10204 3.1 or equivalent).
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Primary Standard | DIN 17100 | Full compliance |
| Steel Grade | St44-2 (1.0044) | Confirmed |
| Delivery Condition | As-rolled / Normalized | Available |
| Product Form | Steel Plate | Available |
| Thickness Range | 6 mm – 150 mm | Custom sizes available |
| Width / Length | Up to 3000–4000 mm / 12000–18000 mm | Custom cutting supported |
| Certification | EN 10204 3.1 / Mill Certificate | Available |
Chemical Composition
| Element | Ladle Analysis (Max. %) | Product Analysis (Max. %) |
|---|---|---|
| Carbon (C) | ≤ 0.21 | ≤ 0.23 |
| Silicon (Si) | ≤ 0.35 | ≤ 0.40 |
| Manganese (Mn) | ≤ 1.50 | ≤ 1.60 |
| Phosphorus (P) | ≤ 0.045 – 0.050 | ≤ 0.055 |
| Sulfur (S) | ≤ 0.045 – 0.050 | ≤ 0.055 |
| Nitrogen (N) | ≤ 0.009 | ≤ 0.010 |
Note: Controlled carbon content ensures a good balance of strength and weldability.
Mechanical Properties
Mechanical properties of DIN 17100 St44-2:
| Thickness (mm) | Yield Strength ReH (min) | Tensile Strength Rm | Elongation A (min) |
|---|---|---|---|
| ≤ 16 | 275 MPa | 430 – 580 MPa | 22% |
| > 16 ≤ 40 | 265 MPa | 430 – 580 MPa | 21% |
| > 40 ≤ 63 | 255 MPa | 430 – 580 MPa | 20% |
| > 63 ≤ 100 | 245 MPa | 430 – 580 MPa | 19% |
| > 100 ≤ 150 | 235 MPa | 410 – 540 MPa | 18% |
Density: 7.85 g/cm³ Impact Test: Typically 27 J at +20°C (when required).
Delivery Conditions
SHH STEEL supplies DIN 17100 St44-2 steel plate as Mill Direct Supply in as-rolled or normalized condition according to customer requirements.
Additional options available:
- Shot blasting and shop primer
- Ultrasonic testing (EN 10160 or equivalent)
- Z-direction testing (Z15 / Z25 / Z35)
- Third-party inspection (SGS, BV, TUV, etc.)
Tolerances
Dimensional tolerances for St44-2 steel plate follow DIN standards or equivalent international standards (EN 10029 / ASTM A6).
- Thickness, width and length tolerances according to the ordered class.
- Flatness according to applicable standard.
- Edge conditions: Mill edge or cut edge (flame / plasma).
Tighter tolerances can be provided upon request.
Weldability
St44-2 has good weldability. It can be welded by all conventional methods (SMAW, GMAW, FCAW, SAW) when proper procedures are followed.
Recommended welding consumables:
| Welding Process | Recommended Consumables |
|---|---|
| SMAW (Stick) | E7018, E7016 |
| GMAW (MIG/MAG) | ER70S-6 |
| FCAW | E71T-1 |
| SAW | EM12K + suitable flux |
Preheating is generally not required for thin and medium thicknesses under normal conditions.
Equivalent Material Grades
| Grade | Standard | Notes |
|---|---|---|
| St44-2 | DIN 17100 | — |
| 1.0044 | DIN / EN | Material number |
| S275JR | EN 10025-2 | Modern European equivalent |
| Q275B | GB/T 700 | Closest Chinese equivalent |
| ASTM A36 / A572 Gr.42 | ASTM | Approximate American equivalents |
| SS400 / SM400A | JIS | Approximate Japanese grades |
Applications
DIN 17100 St44-2 is widely used in general structural and engineering applications requiring moderate strength. Typical uses include:
| Application Area | Typical Components / Uses (Keywords) |
|---|---|
| Building Structures | Beams, columns, frames – St44-2 Structural Steel |
| Bridges | Secondary members – St44-2 Bridge |
| Machinery | Base frames, supports – St44-2 Machinery |
| Containers & Storage | Tanks, containers – St44-2 Container |
| General Fabrication | Welded structures – St44-2 Fabrication |
| Construction | Structural parts – St44-2 Construction |
Why Choose SHH STEEL
SHH STEEL provides St44-2 as Mill Direct Supply. We maintain long-term strategic cooperation with major Chinese steel mills and act as a first-level (primary) agent. This direct mill supply model allows us to offer competitive mill-direct pricing, faster delivery times, stable and traceable quality, and full Mill Test Certificates for DIN 17100 St44-2 Steel Plate.
Customers benefit from reliable supply, short lead times and cost-effective solutions for structural steel projects worldwide. Our professional export team provides technical support and customized processing services to meet project requirements.
FAQ
-
What is the strength level of St44-2?
- St44-2 has a minimum yield strength of 275 MPa (≤16 mm) and tensile strength of 430–580 MPa, higher than the St37 series.
-
Is St44-2 equivalent to S275JR?
- Yes, St44-2 is commonly considered equivalent to EN 10025-2 S275JR.
-
What is the material number of St44-2?
- 1.0044
Conclusion
DIN 17100 St44-2 Steel Plate from SHH STEEL is a reliable structural steel offering 275 MPa minimum yield strength, good weldability and formability. As Mill Direct Supply, we provide competitive pricing, consistent quality and full technical support. Trust SHH STEEL for your St44-2 steel plate requirements.
Contact SHH STEEL today for stock availability, pricing and technical support. DIN 17100 St44-2 Steel Plate, St44-2 steel plate, St44-2, St44-2 Structural Steel, St44-2 supplier, St44-2 equivalent