DIN 17100 St37-3 Steel Plate | St37-3 Structural Steel
What is DIN 17100 St37-3 Steel Plate?
As a professional steel plate supplier and China Mill-Direct Exporter, SHH STEEL is pleased to present DIN 17100 St37-3 Steel Plate.
St37-3 is a non-alloy structural steel under the former German standard DIN 17100. It provides a minimum yield strength of 235 MPa (for thickness ≤ 16 mm) and a tensile strength range of 360–510 MPa. Compared with St37-2, St37-3 has stricter limits on phosphorus, sulfur and nitrogen, resulting in better toughness and overall quality. Although DIN 17100 has been largely superseded by EN 10025-2, St37-3 remains requested in many markets and is closely equivalent to S235J0.
This grade belongs to the DIN 17100 Steel Plate series. SHH STEEL supplies St37-3 as Mill Direct Supply, sourcing directly from major Chinese steel mills. This ensures competitive mill pricing, consistent quality, shorter lead times and full traceability. We offer thicknesses from 6 mm to 150 mm, widths up to 3000–4000 mm and lengths up to 12000–18000 mm. Custom cutting, shot blasting and priming services are available. All plates are delivered with full Mill Test Certificates (EN 10204 3.1 or equivalent).
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Primary Standard | DIN 17100 | Full compliance |
| Steel Grade | St37-3 (1.0116) | Confirmed |
| Delivery Condition | As-rolled / Normalized | Available |
| Product Form | Steel Plate | Available |
| Thickness Range | 6 mm – 150 mm | Custom sizes available |
| Width / Length | Up to 3000–4000 mm / 12000–18000 mm | Custom cutting supported |
| Certification | EN 10204 3.1 / Mill Certificate | Available |
Chemical Composition
Chemical composition according to DIN 17100:
| Element | Ladle Analysis (Max. %) | Product Analysis (Max. %) |
|---|---|---|
| Carbon (C) | ≤ 0.17 | ≤ 0.19 |
| Silicon (Si) | ≤ 0.35 | ≤ 0.40 |
| Manganese (Mn) | ≤ 1.40 | ≤ 1.50 |
| Phosphorus (P) | ≤ 0.040 | ≤ 0.045 |
| Sulfur (S) | ≤ 0.040 | ≤ 0.045 |
| Nitrogen (N) | ≤ 0.009 | ≤ 0.010 |
Note: Stricter limits on P, S and N compared with St37-2 improve toughness and weldability consistency.
Mechanical Properties
Mechanical properties of DIN 17100 St37-3:
| Thickness (mm) | Yield Strength ReH (min) | Tensile Strength Rm | Elongation A (min) | Impact Energy (typical) |
|---|---|---|---|---|
| ≤ 16 | 235 MPa | 360 – 510 MPa | 26% | 27 J at 0°C / +20°C |
| > 16 ≤ 40 | 225 MPa | 360 – 510 MPa | 25% | 27 J at 0°C / +20°C |
| > 40 ≤ 63 | 215 MPa | 360 – 510 MPa | 24% | 27 J at 0°C / +20°C |
| > 63 ≤ 100 | 215 MPa | 360 – 510 MPa | 23% | 27 J at 0°C / +20°C |
| > 100 ≤ 150 | 195 MPa | 340 – 470 MPa | 22% | By agreement |
Density: 7.85 g/cm³
Delivery Conditions
SHH STEEL supplies DIN 17100 St37-3 steel plate as Mill Direct Supply in as-rolled or normalized condition according to customer requirements.
Additional options available:
- Shot blasting and shop primer
- Ultrasonic testing (EN 10160 or equivalent)
- Z-direction testing (Z15 / Z25 / Z35)
- Third-party inspection (SGS, BV, TUV, etc.)
Tolerances
Dimensional tolerances for St37-3 steel plate follow DIN standards or equivalent international standards (EN 10029 / ASTM A6).
- Thickness, width and length tolerances according to the ordered class.
- Flatness according to applicable standard.
- Edge conditions: Mill edge or cut edge (flame / plasma).
Tighter tolerances can be provided upon request.
Weldability
St37-3 has excellent weldability due to its low carbon content and controlled impurities. It can be welded by all conventional methods (SMAW, GMAW, FCAW, SAW) without special difficulties.
Recommended welding consumables:
| Welding Process | Recommended Consumables |
|---|---|
| SMAW (Stick) | E7018, E7016 |
| GMAW (MIG/MAG) | ER70S-6 |
| FCAW | E71T-1 |
| SAW | EM12K + suitable flux |
Preheating is generally not required for thin and medium thicknesses under normal conditions.
Equivalent Material Grades
| Grade | Standard | Notes |
|---|---|---|
| St37-3 | DIN 17100 | — |
| 1.0116 | DIN / EN | Material number |
| S235J0 | EN 10025-2 | Closest modern European equivalent |
| Q235C / Q235D | GB/T 700 | Closest Chinese equivalents |
| ASTM A36 | ASTM | Approximate American equivalent |
| SS400 | JIS G3101 | Approximate Japanese equivalent |
Applications
DIN 17100 St37-3 is widely used in structural and engineering applications requiring better toughness than basic St37-2. Typical uses include:
| Application Area | Typical Components / Uses (Keywords) |
|---|---|
| Building Structures | Beams, columns, frames – St37-3 Structural Steel |
| Bridges | Secondary members – St37-3 Bridge |
| Machinery | Base frames, supports – St37-3 Machinery |
| Containers & Storage | Tanks, containers – St37-3 Container |
| General Fabrication | Welded structures – St37-3 Fabrication |
| Construction | Structural parts requiring better toughness – St37-3 Construction |
Why Choose SHH STEEL
SHH STEEL provides St37-3 as Mill Direct Supply. We maintain long-term strategic cooperation with major Chinese steel mills and act as a first-level (primary) agent. This direct mill supply model allows us to offer competitive mill-direct pricing, faster delivery times, stable and traceable quality, and full Mill Test Certificates for DIN 17100 St37-3 Steel Plate.
Customers benefit from reliable supply, short lead times and cost-effective solutions for structural steel projects worldwide. Our professional export team provides technical support and customized processing services to meet project requirements.
FAQ
-
What is the difference between St37-2 and St37-3?
- St37-3 has stricter limits on phosphorus, sulfur and nitrogen, resulting in better toughness and overall quality compared with St37-2.
-
Is St37-3 equivalent to S235J0?
- Yes, St37-3 is commonly considered equivalent or very close to EN 10025-2 S235J0.
-
What is the material number of St37-3?
- 1.0116
Conclusion
DIN 17100 St37-3 Steel Plate from SHH STEEL is a higher-quality structural steel offering 235 MPa minimum yield strength, improved toughness and excellent weldability. As Mill Direct Supply, we provide competitive pricing, consistent quality and full technical support. Trust SHH STEEL for your St37-3 steel plate requirements.
Contact SHH STEEL today for stock availability, pricing and technical support. DIN 17100 St37-3 Steel Plate, St37-3 steel plate, St37-3, St37-3 Structural Steel, St37-3 supplier, St37-3 equivalent