DIN 17100 St52-3 is a high-strength structural steel plate with a minimum yield strength of 355 MPa and tensile strength of 510–680 MPa. It offers good toughness and excellent weldability for demanding structural applications. SHH STEEL supplies St52-3 as Mill Direct Supply with competitive pricing and full mill
Equivalent Grades:
ASTM A572 Gr 50 / EN S355J0 (1.0553) / JIS SM490YA / GB Q355C
Specification:
DIN 17100 — Delivery: As-rolled
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Tolerances
Weldability
Equivalent Material Grades
Applications
Why Choose SHH STEEL
FAQ
Conclusion

What is DIN 17100 St52-3 Steel Plate?

As a professional steel plate supplier and China Mill-Direct Exporter, SHH STEEL is pleased to present DIN 17100 St52-3 Steel Plate.

St52-3 is a high-strength non-alloy structural steel under the former German standard DIN 17100. It provides a minimum yield strength of 355 MPa (for thickness ≤ 16 mm) and a tensile strength range of 510–680 MPa. This grade is one of the most widely used high-strength structural steels from the old DIN series and is essentially equivalent to modern EN 10025-2 S355J2 / S355J0. It offers a good combination of strength, toughness and weldability.

This grade belongs to the DIN 17100 Steel Plate series. SHH STEEL supplies St52-3 as Mill Direct Supply, sourcing directly from major Chinese steel mills. This ensures competitive mill pricing, consistent quality, shorter lead times and full traceability. We offer thicknesses from 6 mm to 150 mm, widths up to 3000–4000 mm and lengths up to 12000–18000 mm. Custom cutting, shot blasting and priming services are available. All plates are delivered with full Mill Test Certificates (EN 10204 3.1 or equivalent).

Material Specification

Specification Element Requirement SHH STEEL Compliance
Primary Standard DIN 17100 Full compliance
Steel Grade St52-3 (1.0570) Confirmed
Delivery Condition As-rolled / Normalized Available
Product Form Steel Plate Available
Thickness Range 6 mm – 150 mm Custom sizes available
Width / Length Up to 3000–4000 mm / 12000–18000 mm Custom cutting supported
Certification EN 10204 3.1 / Mill Certificate Available

Chemical Composition

Chemical composition according to DIN 17100:

Element Ladle Analysis (Max. %) Product Analysis (Max. %)
Carbon (C) ≤ 0.20 ≤ 0.22
Silicon (Si) ≤ 0.55 ≤ 0.60
Manganese (Mn) ≤ 1.60 ≤ 1.70
Phosphorus (P) ≤ 0.040 ≤ 0.045
Sulfur (S) ≤ 0.040 ≤ 0.045
Nitrogen (N) ≤ 0.009 ≤ 0.010

Note: Controlled carbon and manganese contents provide a good balance of high strength and weldability.

Mechanical Properties

Mechanical properties of DIN 17100 St52-3:

Thickness (mm) Yield Strength ReH (min) Tensile Strength Rm Elongation A (min) Impact Energy (typical)
≤ 16 355 MPa 510 – 680 MPa 22% 27 J at 0°C / -20°C
> 16 ≤ 40 345 MPa 510 – 680 MPa 21% 27 J at 0°C / -20°C
> 40 ≤ 63 335 MPa 510 – 680 MPa 20% 27 J at 0°C / -20°C
> 63 ≤ 100 325 MPa 510 – 680 MPa 18% 27 J at 0°C / -20°C
> 100 ≤ 150 315 MPa 490 – 630 MPa 18% By agreement

Density: 7.85 g/cm³

Delivery Conditions

SHH STEEL supplies DIN 17100 St52-3 steel plate as Mill Direct Supply in as-rolled or normalized condition according to customer requirements.

Additional options available:

  • Shot blasting and shop primer
  • Ultrasonic testing (EN 10160 or equivalent)
  • Z-direction testing (Z15 / Z25 / Z35)
  • Third-party inspection (SGS, BV, TUV, etc.)

Tolerances

Dimensional tolerances for St52-3 steel plate follow DIN standards or equivalent international standards (EN 10029 / ASTM A6).

  • Thickness, width and length tolerances according to the ordered class.
  • Flatness according to applicable standard.
  • Edge conditions: Mill edge or cut edge (flame / plasma).

Tighter tolerances can be provided upon request.

Weldability

St52-3 has good weldability for a high-strength structural steel. It can be welded by all conventional methods (SMAW, GMAW, FCAW, SAW) when proper procedures are followed.

Recommended welding consumables:

Welding Process Recommended Consumables
SMAW (Stick) E7018, E8018
GMAW (MIG/MAG) ER70S-6, ER80S-D2
FCAW E71T-1, E81T1
SAW EM12K / EH14 + suitable flux

Preheating may be required for thicker plates. Low-hydrogen consumables are recommended.

Equivalent Material Grades

Grade Standard Notes
St52-3 DIN 17100 —
1.0570 DIN / EN Material number
S355J2 / S355J0 EN 10025-2 Closest modern European equivalents
Q355B / Q355C GB/T 1591 Closest Chinese equivalents
ASTM A572 Grade 50 ASTM Approximate American equivalent
SM490B / SM490C JIS G3106 Approximate Japanese grades

Applications

DIN 17100 St52-3 is widely used in high-strength structural and engineering applications. Typical uses include:

Application Area Typical Components / Uses (Keywords)
Building Structures Beams, columns, frames – St52-3 Structural Steel
Bridges Main girders, components – St52-3 Bridge
Machinery Heavy frames, supports – St52-3 Machinery
Containers & Storage Tanks, containers – St52-3 Container
General Fabrication High-strength welded structures – St52-3 Fabrication
Construction Structural parts – St52-3 Construction

Why Choose SHH STEEL

SHH STEEL provides St52-3 as Mill Direct Supply. We maintain long-term strategic cooperation with major Chinese steel mills and act as a first-level (primary) agent. This direct mill supply model allows us to offer competitive mill-direct pricing, faster delivery times, stable and traceable quality, and full Mill Test Certificates for DIN 17100 St52-3 Steel Plate.

Customers benefit from reliable supply, short lead times and cost-effective solutions for high-strength structural steel projects worldwide. Our professional export team provides technical support and customized processing services to meet project requirements.

FAQ

What is the strength level of St52-3?
St52-3 has a minimum yield strength of 355 MPa (≤16 mm) and tensile strength of 510–680 MPa, significantly higher than St37 and St44 grades.
Is St52-3 equivalent to S355J2?
Yes, St52-3 is commonly considered equivalent to EN 10025-2 S355J2 (or S355J0 depending on impact test temperature).
What is the material number of St52-3?
1.0570

Conclusion

DIN 17100 St52-3 Steel Plate from SHH STEEL is a high-strength structural steel offering 355 MPa minimum yield strength, good toughness and excellent weldability. As Mill Direct Supply, we provide competitive pricing, consistent quality and full technical support. Trust SHH STEEL for your St52-3 steel plate requirements.

Contact SHH STEEL today for stock availability, pricing and technical support. DIN 17100 St52-3 Steel Plate, St52-3 steel plate, St52-3, St52-3 Structural Steel, St52-3 supplier, St52-3 equivalent

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X