Close view of BV EH32 hull structural steel plate, Bureau Veritas (BV) rules

BV EH32 Shipbuilding Steel Plate

BV BV EH32 (EH32) higher-strength hull structural steel plate, yield 315 N/mm², tensile 440–590 N/mm², Charpy at −40 °C, stamped BV EH32 / BV EH32 with Bureau Veritas–endorsed certificates. SHH STEEL supplies stock and mill-roll plate in China with cutting, multi-class and 3.2 inspection.
Keywords
BV EH32 steel plate, BV EH32 shipbuilding steel plate, BV EH32 marine plate, EH32 hull steel, Bureau Veritas EH32 plate, AH/DH/EH/FH 32 marine plate
Equivalent Grades:
ASTM A131 Grade EH32; ABS EH32; DNV NV E32; LR EH32; CCS EH32; NK KE32; KR RE32; RINA Grade EH32; GB 712 Grade EH32
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Impact Test and Condition of Supply
Thickness Tolerance
Stock
Equivalent Grades
Grade Selection
Applications and Fabrication
Testing and Inspection
Specification Mistakes
Buyer Concerns
How to Order
FAQ
Conclusion

BV EH32 / BV EH32 shipbuilding steel plate — overview

Technical Reviewer: Jack | SHH STEEL Material Solutions Department · Updated: 2026-10-27

For cold-route and special-category scantlings, Bureau Veritas specifies BV EH32 (BV EH32) — higher-strength plate with −40 °C Charpy under NR216 / UR W11. Strength level 32 means minimum yield 315 N/mm², tensile 440–590 N/mm² and elongation 22 % min. (A5). The letter EH fixes Charpy V-notch testing at −40 °C. In commercial enquiries it is called BV EH32 or BV EH32 shipbuilding steel plate.

Equivalent grades: BV EH32 ≈ ASTM A131 Grade EH32 ≈ ABS EH32 ≈ DNV NV E32 ≈ LR EH32 ≈ CCS E32 / EH32 ≈ NK KE32 ≈ KR RE32 ≈ RINA EH32 ≈ GB 712 Grade EH32 (all class-approved, stamped by the issuing society).

BV EH32 is selected when scantlings need the higher yield of the 32 band and the material class assigns −40 °C toughness. Ordinary-strength BV Grade A–E stay at 235 N/mm² yield and cannot replace EH32 without a drawing change. Within the 32 band, letter choice is toughness: AH 0 °C → DH −20 °C → EH −40 °C → FH −60 °C; within the EH letter, strength steps 32 → 36 → 40 raise yield from 315 to 355 to 390 N/mm².

Plates that pass mill tests under Bureau Veritas survey are die-stamped or stencilled BV EH32 or BV EH32 (plus Z or U where through-thickness or ultrasonic requirements apply) and are supplied with a mill certificate the BV Surveyor endorses. SHH STEEL supplies BV EH32 from Chinese mills that hold Bureau Veritas works approval for the grade, from stock in common sizes or from a mill rolling cycle, with BV survey arranged at the mill.

BV BV EH32 plate: specification summary

ItemBV BV EH32 / EH32 data
Rule basisBureau Veritas NR216 Materials; IACS UR W11 higher-strength Grade EH32 (NR216 paragraph cross-refs UNCERTAIN without local BV PDF)
Strength levelhigher strength 32, yield 315 N/mm² min., tensile 440–590 N/mm²
Toughness classEH → Charpy at −40 °C
Plate thickness primarily coveredup to 100 mm under IACS UR W11 scope for plates; greater thickness by special consideration (see UNCERTAIN)
Deoxidationkilled, fine grain practice (UR W11)
Impact testCharpy V at −40 °C; frequency and supply condition per UR W11 / NR216 tables
MarkingBV EH32 / BV EH32; plus Z / U / TM where ordered and qualified
TMCP Ceq (indicative UR W11 / industry practice)≤ 0.36 % for t ≤ 50 mm; ≤ 0.38 % for 50 < t ≤ 100 mm (TM steels) — confirm on mill approval / PO
Thickness toleranceIACS UR W13 as adopted by BV (minus tolerance commonly 0.3 mm class — confirm on PO; see UNCERTAIN)
Certificatemill certificate endorsed by the BV Surveyor; EN 10204 3.1 / 3.2 on request

Size range. Common market thicknesses for EH32 are about 6–80 mm (heavier plates available as per mill approval), widths 1500–3500 mm. Exact maximum thickness for a given delivery condition is as per standard and mill certificate / BV works approval. Ask for confirmation above 100 mm.

BV EH32 / BV EH32 chemical composition (heat and product analysis)

ElementHeat (ladle) analysis, %Product (check) analysis, %Note
C0.18 max.numeric tolerance not tabulated in BV NR216 – agree on order / mill certificateAH/DH/EH group
Mn0.90–1.60 (AH ≤12.5 mm may be 0.70 min.)numeric tolerance not tabulated in BV NR216 – agree on order / mill certificateAH ≤12.5 mm may use 0.70 % Mn min.
Si0.10–0.50numeric tolerance not tabulated in BV NR216 – agree on order / mill certificatemin. waived if acid-soluble Al ≥ 0.015 %
P0.035 max.numeric tolerance not tabulated in BV NR216 – agree on order / mill certificate
S0.035 max.numeric tolerance not tabulated in BV NR216 – agree on order / mill certificate
Al (acid soluble) min.0.015 min. acid-soluble (or total Al per UR W11 fine-grain practice)numeric tolerance not tabulated in BV NR216 – agree on order / mill certificategrain refining
Nb0.02–0.05 when used singlynumeric tolerance not tabulated in BV NR216 – agree on order / mill certificatewhen used singly; combined minima in UR W11
V0.05–0.10 when used singlynumeric tolerance not tabulated in BV NR216 – agree on order / mill certificatewhen used singly
Ti0.02 max.numeric tolerance not tabulated in BV NR216 – agree on order / mill certificateneed not be reported unless intentionally added
Cu0.35 max.numeric tolerance not tabulated in BV NR216 – agree on order / mill certificate
Cr0.20 max.numeric tolerance not tabulated in BV NR216 – agree on order / mill certificate
Ni0.40 max.numeric tolerance not tabulated in BV NR216 – agree on order / mill certificate
Mo0.08 max.numeric tolerance not tabulated in BV NR216 – agree on order / mill certificate
N—numeric tolerance not tabulated in BV NR216 – agree on order / mill certificatenot specified as a max in AH/DH/EH column

Product (check) analysis column: BV NR216 specify heat (ladle) limits; no numeric product-analysis tolerance is tabulated in the rule text reviewed, so product (check) limits are agreed on the order or taken from the approved mill specification and certificate.

Source: IACS UR W11 higher-strength chemistry tables (ladle samples) — the chemistry Bureau Veritas applies to BV EH32 via NR216. AH/DH/EH share one chemistry column; FH is tighter on C, P, S and adds N control with higher Ni allowance. Toughness is differentiated by impact temperature and supply routes, not by separate C/Mn caps within AH/DH/EH. Product (check) analysis numeric tolerances are not tabulated in UR W11; when required, agree tolerances at enquiry. TMCP steels must also meet the applicable Ceq / Pcm limits on the mill approval — ask for Ceq on the certificate.

BV BV EH32 tensile properties

PropertyRequirement (IACS UR W11)
Tensile strength Rm440–590 N/mm²
Yield strength ReH315 N/mm² min.
Elongation A522 % min.
Impact test temperature−40 °C

Alternative flat-specimen elongations by thickness (indicative UR W11 / industry table for strength 32):

Thickness (mm)≤5>5–10>10–15>15–20>20–25>25–30>30–40>40–50
Elongation min. %1416171819202122

Same tensile band applies to AH/DH/EH/FH 32; only impact temperature and chemistry group (FH vs AH/DH/EH) change across the letter.

BV BV EH32: Charpy at −40 °C and supply condition

ThicknessLong. avg. at −40 °CTrans. avg. at −40 °C
t ≤ 50 mm31 J22 J
50 < t ≤ 70 mm38 J26 J
70 < t ≤ 100 mm46 J31 J

Source: IACS UR W11 impact table for higher-strength Grade EH32 (full-size; either direction acceptable unless specified). Energies rise with thickness — a 60 mm plate must meet higher values than a 20 mm plate at the same −40 °C. Condition of supply and impact lot size depend on grain-refining practice and thickness (AR/CR/N/TM/QT as permitted). For TMCP EH32, respect Ceq caps ≈ 0.36 % (t≤50) / 0.38 % (50

Thickness tolerance and surface condition

Bureau Veritas applies IACS UR W13 thickness tolerances unless the PO states otherwise (often 0.3 mm minus class — confirm on PO; see UNCERTAIN). Plus/flatness/width/length per agreed standard (ASTM A6 or EN 10029). Surface quality per EN 10163 or equivalent accepted by BV; state primer/surface class on receipt if needed.

BV BV EH32 plate stock in China

Thickness (mm)Width (mm)Length (mm)ConditionApprox. quantityLocation
61800 / 20006000 / 8000AR / CR / N / TM100+ tChina
81800 / 20008000 / 12000AR / CR / N / TM200+ tChina
102000 / 22008000 / 12000AR / CR / N / TM200+ tChina
122000 / 2200 / 250012000AR / CR / N / TM200+ tChina
142000 / 220012000AR / CR / N / TM100+ tChina
162000 / 250012000AR / CR / N / TM200+ tChina
202000 / 250012000AR / CR / N / TM100+ tChina
252200 / 250012000AR / CR / N / TM100+ tChina
30220010000 / 12000AR / CR / N / TM100+ tChina
40220010000AR / CR / N / TM50+ tChina
5022008000 / 10000AR / CR / N / TM50+ tChina

Quantities are approximate and change daily (indicative — confirm before booking); all stock plates carry BV EH32 marking and Bureau Veritas–endorsed mill certificates when sold as BV class plate. Sizes outside the table (for example 3000 mm width, 60–100 mm thickness, or fixed lengths for a cutting plan) are produced in the next mill rolling cycle, typically 3–6 weeks including BV survey. Send your size list and we will reply with what is in stock and what must be rolled.

Packing. Plates are bundled by size with steel strapping, marked with heat number, grade and BV stamp, and shipped in containers (up to about 11.8 m) or break bulk for longer plates.

BV BV EH32 equivalents in other rules and standards

Standard / societyDesignationComment
BV (Bureau Veritas)BV EH32 (BV EH32)this page; stamped under BV survey
ASTM A131/A131MASTM A131/A131M Grade EH32A131 lists AH–FH 32/36/40; product standard only
ABSABS EH32IACS UR W11 higher-strength; live product page
DNVDNV NV E32IACS UR W11; live product page
LRLR EH32 / LR/EH32IACS UR W11; live product page
CCSCCS EH32IACS UR W11; category link only
NK (ClassNK)NK KE32ClassNK KE32
KRKR RE32KR RE32
RINARINA Grade EH32confirm exact designation per RINA rules
GB 712GB 712 Grade EH32not class approval by itself
Structural (indicative)S275JRland structural; no class marking

These are comparisons, not substitutions. Multi-class stamps (BV + ABS / DNV / LR) require joint survey before rolling.

BV BV EH32 vs other BV hull grades

Pick EH32 when the drawing specifies higher-strength grade EH32 (or the society equivalent). Do not substitute ordinary Grade A/B unless the designer recalculates scantlings — yield differs (315 vs 235). Within the 32 band, letter choice is toughness: AH 0 °C → DH −20 °C → EH −40 °C → FH −60 °C. Within the EH letter, strength steps 32 → 36 → 40 raise yield from 315 to 355 to 390 N/mm².

For yields above 390 N/mm² Bureau Veritas / IACS move to extra-high strength (UR W16 naming — BV uses A420…F690 without H, not AH420).

When BV BV EH32 is the right choice: typical uses are special and primary category members, crack-arrest strakes, and hull structure for cold-route or ice-strengthened vessels needing −40 °C toughness. The Charpy temperature (−40 °C) is fixed by the letter, and the strength by the number (ReH 315 N/mm²). Pick the strength from the scantling calculation and the letter from the material class and design temperature on the approved drawing.

Applications, cutting and welding of BV BV EH32

Typical uses: special and primary category members, crack-arrest strakes, and hull structure for cold-route or ice-strengthened vessels needing −40 °C toughness; weight-saving vs ordinary-strength plate in large tankers, bulkers and container ships. See offshore platform steel plates when primary offshore grades apply.

Welding: higher-strength hull steels need approved higher-strength consumables matched to −40 °C weld-metal toughness; preheat and heat input follow the approved WPS and often track Ceq/Pcm from the mill certificate. TMCP EH32 must respect the Ceq caps noted above. Cutting by oxy-fuel/plasma/laser is routine; thick FH plate may need hydrogen control — follow mill recommendations.

Processing notes for BV EH32: cold forming is routine within normal shipyard radii. Line heating and fairing of TMCP plate should stay within the temperature limits recommended by the mill, because overheating can reduce the strength gained in controlled rolling. Check the delivery condition on the certificate before planning hot forming.

Certificates, BV survey and third-party inspection

Every plate is tested and marked at the mill under Bureau Veritas survey; the mill certificate lists heat number, ladle chemistry, Ceq where applicable, tensile results (ReH ≥ 315 N/mm², Rm 440–590 N/mm², A ≥ 22 %), Charpy at −40 °C, delivery condition and plate numbers, endorsed by the Surveyor. Optional EN 10204 3.2, UT (U), Z-direction, multi-class with ABS/DNV/LR.

On receipt: verify BV EH32 stamp, −40 °C impact data, energies for the delivered thickness band, thickness within UR W13 / PO tolerance, BV endorsement present.

Charpy acceptance for BV EH32 by thickness (IACS UR W11; actual results as per standard and mill certificate):

Thickness t (mm)Test temperatureAverage energy, longitudinal (J min.)Average energy, transverse (J min.)
t ≤ 50−40 °C3122
50 < t ≤ 70−40 °C3826
70 < t ≤ 100−40 °C4631

If UT or 3.2 was ordered, check the UT report and inspector’s plate list as well.

Common mistakes when ordering BV EH32 / BV EH32

  • Ordering “BV 32” without the letter (EH/…) — toughness class missing
  • Accepting ordinary-strength Grade A/B certificates for a EH32 PO
  • Ignoring TMCP Ceq caps on TM plate
  • Substituting a different letter (e.g. AH for EH) without drawing approval
  • Coil-cut plate without coil approval
  • Missing BV endorsement on the MTC
  • Writing DNV NV E32 or LR/EH32 on a BV-class PO without arranging that society’s survey

Write grade, delivery condition, impact temperature and certificate type into the PO.

Sourcing BV BV EH32: buyer concerns and SHH STEEL solutions

ConcernHow SHH STEEL handles it
Fake class plateBV-approved mills only; traceable BV EH32 stamp + certificate; 3.2 on request
Payment riskT/T or L/C; inspection before balance
Mixed sizes / gradesEH32 combined with BV Grade A/B/D/E or other AH–FH sizes in one container
Lead time visibilityweekly photo updates from dedicated coordinator
Prep before shipcutting, bevelling, drilling, machining in our workshop

How to order BV BV EH32 plate

Specify BV EH32 (BV EH32), delivery condition (AR/CR/N/TM/QT as applicable), thickness × width × length × qty, Z/U, multi-class, certificate type, port. Send to SHH STEEL.

Sample PO line: “Steel plate to Bureau Veritas NR216 Materials, Grade EH32 (BV EH32), delivery condition [AR/CR/N/TM/QT], 20 × 2500 × 12000 mm, 30 pcs, marked BV EH32 / BV EH32, certificate endorsed by BV Surveyor, EN 10204 3.2 [if required], UT [if required], CIF [port].”

FAQ

What sizes and minimum order quantity can you supply for BV EH32 / BV EH32 plate?
IACS UR W11 lists EH32 plate primarily up to 100 mm; thicker plate needs special BV consideration. Most enquiries we receive for EH32 are 8–60 mm thick, 1800–3000 mm wide and 6000–12000 mm long. Popular sizes can come from China stock carrying the BV EH32 marking, with no fixed minimum. A mill rolling for a special width, thickness above roughly 60 mm or a Z-grade normally needs a minimum quantity per size, which we confirm per order. We can combine several sizes, or EH32 with other hull grades, to reach a rolling or container quantity.
How is BV BV EH32 certified, and can you arrange EN 10204 3.2 or dual-class with ABS/DNV/LR?
Every plate is made by a BV-approved mill under Bureau Veritas survey. It is die-stamped or stencilled BV EH32 / BV EH32 with the heat or plate number, and the mill test certificate is endorsed by the BV Surveyor. The certificate gives the ladle chemistry, the tensile results (ReH ≥ 315 N/mm², Rm 440–590 N/mm², A ≥ 22 %), the Charpy results at −40 °C, the delivery condition and the plate identity. If your contract asks for EN 10204 3.2, we arrange it before rolling. Dual or multi-class (BV + ABS, DNV or LR) must be booked before testing. 3.2 cannot be added after testing, so please state it on the enquiry.
What is the impact test temperature and energy for BV EH32 / BV EH32, and do thickness limits apply?
BV EH32 is tested at −40 °C. Required average energies (longitudinal/transverse, J min.) under IACS UR W11 rise with thickness: ≤50 mm 31/22; 50–70 mm 38/26; 70–100 mm 46/31. This matters when you order thick EH32: a 60 mm plate must meet higher values than a 20 mm plate at the same −40 °C. The test lot size and the permitted delivery condition (AR, CR, N, TM or QT) follow the UR W11 / NR216 supply table. Above 100 mm, agree data positions and energies with BV. Results are as per standard and mill certificate.
What welding and preheat guidance applies to BV BV EH32?
BV EH32 needs higher-strength welding consumables approved for −40 °C weld-metal toughness. For TMCP plate, Ceq is commonly capped near 0.36 % (t ≤ 50 mm) and 0.38 % (50 < t ≤ 100 mm) under UR W11 practice; above 100 mm it is agreed at mill approval. N or AR plate of the same grade may have a higher actual Ceq, so the delivery condition affects how easy the plate is to weld. Preheat, interpass temperature and heat input must follow your BV-approved WPS. We send the mill certificate’s ladle analysis and Ceq before shipment so the welding engineer can confirm the procedure qualifies. We do not give generic preheat temperatures.
What is the delivery time for BV BV EH32 plate?
Stock sizes of BV EH32 can usually be cut, inspected and loaded in about 7–15 days. Mill-rolled orders typically take about 3–6 weeks plus inspection, depending on thickness, delivery condition and the mill schedule. These are commercial estimates, confirmed with each quote. If 3.2 witness or multi-class survey is required, we book the inspector when we place the mill order so testing is not delayed. A dedicated coordinator sends weekly progress photos until the bill of lading is issued.
Which payment terms do you accept for BV EH32, and how is my deposit protected?
We accept T/T or L/C at sight. With T/T, the usual terms are a 30 % deposit and the balance against the documents or after inspection. You or your inspector can check the BV EH32 stamping, the dimensions and the Surveyor-endorsed certificate before you pay the balance. With L/C, payment is tied to the presented documents. For first orders we can start with a smaller trial lot. The proforma invoice shows the grade (BV EH32 / BV EH32), sizes and certificate type.
What are the equivalent grades of BV BV EH32 among class societies and GB 712?
BV EH32 corresponds to ASTM A131/A131M Grade EH32, ABS EH32, DNV NV E32, LR EH32 / LR/EH32, CCS EH32, NK KE32, KR RE32, RINA Grade EH32 (confirm RINA designation per rules), and GB 712 Grade EH32. All share yield 315 N/mm², tensile 440–590 N/mm² and a Charpy test at −40 °C under IACS UR W11. Even so, a plate is only accepted by the society whose stamp and certificate it carries. Order BV EH32 for BV class, or ask for multi-class when one stock must serve several projects. GB 712 or A131 certificates alone do not replace the BV EH32 stamp.
Can you cut, bevel or machine BV BV EH32 plates, and how are they packed for export?
Yes. In our workshop we can flame, plasma or laser cut EH32 to drawings, bevel weld edges (V, X or K preparation to your angle and land), drill and machine. Every cut piece keeps traceability: we transfer the BV EH32 marking and heat number before cutting, and the cutting list is tied to the mill certificate. For export, plates are bundled with steel straps and timber spacers, marked with grade, size and heat number, and loaded in containers or as break-bulk. Shot blasting and shop primer are available on request. See SHH STEEL for our processing capabilities.

Conclusion

BV EH32 / BV EH32 is higher-strength hull steel under Bureau Veritas NR216 Materials rules and IACS UR W11: yield 315 N/mm², tensile 440–590 N/mm², Charpy at −40 °C, marking BV EH32. Lock on the order: delivery condition, impact lot size, TMCP Ceq if TM, product analysis if needed, multi-class and 3.2.

SHH STEEL supplies BV EH32 plate rolled by Chinese mills that hold Bureau Veritas works approval for the grade, so every plate carries the BV EH32 stamp and a Surveyor-endorsed certificate traceable to its heat. Common thicknesses are available from stock; other sizes are scheduled into the mill rolling cycle with BV survey arranged at the mill. On request we add EN 10204 3.2 certificates with third-party witness (TÜV, SGS, LR or another agency) and joint certification with ABS, DNV, LR, CCS, NK, KR or RINA.

We accept T/T or L/C payment, with inspection before the balance is paid. Small quantities in several sizes, or BV EH32 mixed with BV Grade A/B/D/E or other AH–FH sizes, can be combined in one container. A dedicated coordinator sends production and shipping updates with photos, and our own workshop cuts to size, bevels, drills and machines plates before shipment so they arrive ready for fabrication.

Request a quotation: send SHH STEEL the grade (BV EH32 / BV EH32), thickness, width, length, quantity per size and destination port, plus any multi-class, Z/U or 3.2 certificate requirement. We reply with price, available stock and lead time.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *



    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *



      X