BV EH460 marine steel plate per Bureau Veritas (BV) rules at SHH STEEL warehouse

BV E460 Shipbuilding Steel Plate

BV BV E460 (E460) extra-high-strength hull structural steel plate, yield 460 N/mm², tensile 570–720 N/mm², Charpy at −40 °C, stamped BV E460 / BV E460 with Bureau Veritas–endorsed certificates. SHH STEEL supplies mill-roll plate in China with cutting, multi-class and 3.2 inspection.
Keywords
BV E460 steel plate, BV E460 shipbuilding steel plate, BV E460 marine plate, E460 extra high strength hull steel, Bureau Veritas E460 plate, BV A420 F690
Equivalent Grades:
ASTM A131 (no direct); ABS EH46 / EQ47; DNV NV E460; LR EH46 / LR/EH46; CCS EH460; NK KE460; KR RE47; RINA per rules; GB 712 Grade EH460
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Impact Test and Condition of Supply
Thickness Tolerance
Stock
Equivalent Grades
Grade Selection
Applications and Fabrication
Testing and Inspection
Specification Mistakes
Buyer Concerns
How to Order
FAQ
Conclusion

BV E460 / BV E460 shipbuilding steel plate — overview

Technical Reviewer: Jack | SHH STEEL Material Solutions Department · Updated: 2026-10-27

Cold-route extra-high scantlings under Bureau Veritas call for BV E460 (BV E460) with −40 °C Charpy — BV’s official EHS naming omits H (E420…E690). IACS Unified Requirement W16 covers this strength band (yield 460 N/mm²); BV implements corresponding requirements in NR216 Materials rules. Minimum yield is 460 N/mm², tensile 570–720 N/mm², elongation 17 % min., with Charpy at −40 °C. It sits above the AH–FH 40 higher-strength family (max yield 390 N/mm² under UR W11). Commercial enquiries use BV E460 or BV E460 shipbuilding steel plate.

Equivalent grades: BV E460 ≈ ASTM A131 (no direct grade at this strength) ≈ ABS EH46 / EQ47 ≈ DNV NV E460 ≈ LR EH46 ≈ CCS EH460 ≈ NK KE460 ≈ KR RE47 ≈ RINA E460 ≈ GB 712 Grade EH460 (all class-approved, stamped by the issuing society).

Naming note: Bureau Veritas titles this strength band as E460 / BV E460 (no H — write A420, not AH420 or AH42). DNV often titles the same yield as EH460 / DNV NV E460. LR titles EH46. ABS often titles EH46 (official ABS EQ47). ASTM A131 has no grade at this strength. Write BV E460 on the BV purchase order.

BV E460 is almost always produced TM or QT by a BV-approved mill to order rather than taken from open stock. SHH STEEL sources extra-high-strength plate from mills with Bureau Veritas approval for the grade, under Surveyor attendance, with optional multi-class (ABS/DNV/LR) and EN 10204 3.2.

BV BV E460 plate: specification summary

ItemBV BV E460 / E460 data
Rule basisBureau Veritas NR216 Materials (extra-high / high-strength hull steel); IACS UR W16 strength band (see UNCERTAIN for NR216 paragraph cross-refs without local BV PDF)
Commercial / stampBV E460 (BV E460) — official no-H form
Yield / tensile / elongation460 / 570–720 N/mm² / 17 % min.
Impact−40 °C; ≈ 46 J L or 31 J T average (IACS UR W16 / aligned tables — confirm on mill certificate)
Deoxidationfully killed, fine grain; N-binding elements per manufacturing specification
Delivery conditionTM or QT (N/CR routes only where specifically approved) — within mill approval thickness limits
MarkingBV E460 / BV E460 (plus delivery-condition / Z / U where ordered)
UTcommonly required for thicker EHS plate (e.g. ≥15 mm) — agree standard (EN 10160 / ASTM A578) on PO
Thickness toleranceIACS UR W13 as adopted by BV (confirm class on PO; see UNCERTAIN)
Certificatemill certificate endorsed by the BV Surveyor; includes Ceq/CET/Pcm as applicable; EN 10204 3.1 / 3.2 on request

Maximum plate thickness depends on delivery condition and the mill’s BV approval sheet — typically TM up to about 100–150 mm and QT higher, but treat the approval limit as governing (UNCERTAIN without local NR216 PDF). Primary commercial scope we quote is within ~100 mm unless the mill approval and BV survey confirm otherwise.

BV BV E460 chemical composition (heat analysis — full alloy set)

ElementHeat (ladle) analysis, %Product (check) analysis, %Note
C0.21 max. (often 0.14–0.20 by route/condition; TM/QT may tighten)numeric tolerance not tabulated in BV NR216 – agree on order / mill certificateTM/QT and letter routes may tighten C — UNCERTAIN exact NR216 table without local PDF
Mn1.70 max. (typically 1.00–1.70; QT route may differ)numeric tolerance not tabulated in BV NR216 – agree on order / mill certificateas per mill approval / UR W16 envelope
Si0.55 max. (QT may allow up to ~0.80 — confirm on mill approval)numeric tolerance not tabulated in BV NR216 – agree on order / mill certificate
P0.025 max. (some EQ-style routes tighter — confirm)numeric tolerance not tabulated in BV NR216 – agree on order / mill certificateEQ-style routes may be tighter
S0.025 max. (some EQ-style routes tighter — confirm)numeric tolerance not tabulated in BV NR216 – agree on order / mill certificateEQ-style routes may be tighter
Al (acid soluble / total)0.015 min. acid-soluble / ≈0.020 total Al (fine-grain; Al/N control unless other N-binders)numeric tolerance not tabulated in BV NR216 – agree on order / mill certificategrain refining / N control
Nb0.05 max. (when used; combined microalloy caps apply)numeric tolerance not tabulated in BV NR216 – agree on order / mill certificatewhen intentionally added
V0.10 max. (when used; combined caps apply)numeric tolerance not tabulated in BV NR216 – agree on order / mill certificatewhen intentionally added
Ti0.05 max. (when used; combined caps apply)numeric tolerance not tabulated in BV NR216 – agree on order / mill certificatewhen intentionally added
Cu0.50 max. (route-dependent; often ≤0.35 in practice)numeric tolerance not tabulated in BV NR216 – agree on order / mill certificate
Cr0.20–0.25 max. (route-dependent)numeric tolerance not tabulated in BV NR216 – agree on order / mill certificate
Ni2.00 max. or per mill approval (often lower on A/D routes)numeric tolerance not tabulated in BV NR216 – agree on order / mill certificate
Mo0.08–0.50 (route-dependent; QT may allow higher)numeric tolerance not tabulated in BV NR216 – agree on order / mill certificate
B0.005 max. (when intentionally added)numeric tolerance not tabulated in BV NR216 – agree on order / mill certificatereport when intentionally added
N0.015 max. (tighter control when Al is the sole N-binder)numeric tolerance not tabulated in BV NR216 – agree on order / mill certificateAl/N practice unless other N-binders
Nb+V+Ti (combined)Nb+V+Ti typically < 0.26 % for N/TM routes (not QT) — confirm UR W16 / mill approvalnot applicable (calculated from heat analysis)combined microalloy cap
Ceq / CET / PcmCeq / CET / Pcm maxima by category and condition on mill approval — report on certificatenot applicable (calculated from heat analysis)report on certificate; choice agreed mill/purchaser

Product (check) analysis column: BV NR216 specify heat (ladle) limits; no numeric product-analysis tolerance is tabulated in the rule text reviewed, so product (check) limits are agreed on the order or taken from the approved mill specification and certificate.

Source: IACS UR W16 chemistry envelope (ABS 2-1-8 Table 4A aligned) as implemented by Bureau Veritas for BV E460 via NR216 — exact ladle limits depend on delivery condition (TM vs QT) and toughness letter. Values above are the rule envelope with every alloy / microalloy row listed; the purchase order and mill approval sheet govern. Product analysis: as per standard and mill certificate. All intentionally added elements and Ceq (or CET/Pcm) are to be reported. Flagged UNCERTAIN where a local BV NR216 PDF was not available to quote paragraph numbers.

BV BV E460 tensile and impact properties

PropertyRequirement (IACS UR W16 aligned)
Yield strength ReH (or Rp0.2)460 N/mm² min.
Tensile strength Rm570–720 N/mm²
Elongation (transverse, 5.65√A)17 % min.
Impact test temperature−40 °C
Impact energy (indicative)46 J L or 31 J T average

Final acceptance values are as per standard and mill certificate under BV survey. For thick plate, additional mid-thickness tensile/impact positions may apply — confirm at enquiry. Test frequency is typically each heat-treatment batch of same cast/condition/thickness.

Delivery condition and toughness for BV E460

Charpy temperature is fixed by the grade letter: E → −40 °C. Indicative average energy 46 / 31 J (L/T) from IACS UR W16 aligned tables — confirm exact figures on the BV-endorsed certificate. Unlike UR W11 higher-strength tables, EHS energies are usually stated as a single pair rather than rising through many thickness bands; thick-plate mid-thickness rules may still apply.

Allowed delivery conditions are primarily TM and QT within the mill’s approved thickness. Vacuum degassing is commonly required for higher categories and for thicker plate — follow the mill approval. State TM or QT on the PO; do not leave delivery condition blank for E460.

Thickness tolerance and surface condition

Bureau Veritas applies IACS UR W13 unless the PO states otherwise (confirm minus class on PO; see UNCERTAIN). Surface repair limits follow the applicable BV / UR rules; state primer/surface class on receipt if needed. For QT plate, avoid notching cut edges; follow mill cutting recommendations.

BV BV E460 plate — mill-roll supply in China

Thickness (mm)Width (mm)Length (mm)ConditionApprox. quantityLocation
102000 / 22008000 / 12000TM / QT200+ tChina
122000 / 2200 / 250012000TM / QT200+ tChina
142000 / 220012000TM / QT100+ tChina
162000 / 250012000TM / QT200+ tChina
202000 / 250012000TM / QT100+ tChina
252200 / 250012000TM / QT100+ tChina
30220010000 / 12000TM / QT100+ tChina
40220010000TM / QT50+ tChina
5022008000 / 10000TM / QT50+ tChina

Extra-high grades such as BV E460 are rarely held as open stock; the table shows the size bands we quote against scheduled mill rolls. Quantities are indicative. All plates sold as BV class carry BV E460 marking and a Bureau Veritas–endorsed mill certificate. Typical mill lead time including BV survey is about 6–10 weeks (commercial estimate — confirm per quote). Send your size list and we will reply with the next available rolling slot.

Packing. Plates are bundled by size with steel strapping, marked with heat number, grade and BV stamp, and shipped in containers (up to about 11.8 m) or break bulk for longer plates.

BV BV E460 equivalents in other rules and standards

Standard / societyDesignationComment
BV (Bureau Veritas)BV E460 (BV E460)this page; BV uses A420…F690 (no H)
ASTM A131/A131MASTM A131/A131M — no direct Grade E460A131 stops at FH40
ABSABS EH46 / EQ47commercial EH46 / official EQ47
DNVDNV NV E460DNV titles EH460 for this yield band
LRLR EH46 / LR/EH46LR titles EH46 (AH69 not AH70 / AH690)
CCSCCS EH460CCS follows W16-style naming
NK (ClassNK)NK KE460NK KE460
KRKR RE47KR RE47 (KR uses ABS-style category numbers)
RINARINA (per rules)EHS name not verified from local RINA PDF
GB 712GB 712 Grade EH460listed in GB 712 EHS band; not class approval alone

These are comparisons, not substitutions. Always write the BV stamp BV E460 on the PO, plus any additional society stamps you need. Other BV EHS siblings are linked via BV Steel Plates until each product page is live.

BV BV E460 vs higher-strength and other EHS grades

Use E460 when scantlings need yield 460 N/mm². Do not substitute AH40/EH40 (390 N/mm² max under UR W11) without redesign. Within the 460 band, letter choice is toughness: A 0 °C → D −20 °C → E −40 °C → F −60 °C. Neighbouring strengths are 420 / 500 — swapping strength needs class approval of the drawing change.

When BV BV E460 is the right choice: typical uses are extra-high-strength special/primary category members and cold-route structure needing −40 °C toughness at elevated yield at extra-high yield — weight-critical hull girder strakes, polar and ice-class primary structure, and offshore units where 460 N/mm² is specified. See offshore platform steel plates for related offshore grades.

Applications and welding notes for BV BV E460

Typical uses: extra-high-strength special/primary category members and cold-route structure needing −40 °C toughness at elevated yield at ReH 460 N/mm²; strength deck and shell of large container ships and gas carriers where EHS is specified; ice-belt and polar primary structure; selected offshore members. See offshore platform steel plates.

Welding: BV E460 is an extra-high-strength steel supplied TM or QT. Welding must follow a procedure qualified for this grade and approved by BV. Ceq/CET/Pcm from the ladle analysis govern hydrogen control, preheat, interpass and heat-input windows. Too much heat input can lower HAZ strength and toughness in QT plate. We send the certificate values before shipment so your welding engineer can confirm the procedure fits. We do not give generic preheat temperatures.

Processing notes: BV E460 owes its strength to TM or QT processing. Hot forming or stress relieving above the tempering temperature can lower the properties, so any heat treatment after delivery must be agreed with the mill and BV. Cold forming and bending radii should follow the mill’s data sheet. Thermal cutting parameters follow mill recommendations so the cut edge is not damaged.

Certificates, BV survey and third-party inspection

BV survey at the mill; certificate includes ladle chemistry (full alloy set + Ceq/CET/Pcm as applicable), tensile (ReH ≥ 460, Rm 570–720, A ≥ 17 %), Charpy at −40 °C, delivery condition, UT if ordered, and plate identity. Optional EN 10204 3.2 and multi-class with ABS/DNV/LR.

On receipt: verify BV E460 stamp, −40 °C impact data, energies ≥ ordered/certified minima, thickness within tolerance, Surveyor endorsement, UT report if required.

Charpy acceptance for BV E460 (IACS UR W16 aligned; actual results as per standard and mill certificate):

Thickness t (mm)Test temperatureAverage energy, longitudinal (J min.)Average energy, transverse (J min.)
as per UR W16 / mill approval (typically t/4 position)−40 °C4631

For thickness above ~100 mm, additional mid-thickness rules may apply — confirm at enquiry. If the PO asked for 3.2, the inspector’s report must name the witnessed tests and plate numbers.

Common mistakes when ordering BV E460 / BV E460

  • Ordering “BV 460” without the letter (E) — toughness missing
  • Writing AH460 / AH46 / AH460 on a BV PO — BV official form is E460 (no H)
  • Writing ABS EH46 or DNV EH460 or LR EH46 on a BV-class PO without arranging that society’s survey (wrong stamp)
  • Leaving delivery condition blank (TM vs QT changes price, mill and properties)
  • Expecting ASTM A131 dual-cert at this strength (A131 has no EHS grade)
  • Skipping UT on thick EHS plate when the yard specification requires it
  • Missing BV endorsement / assuming GB 712 Grade EH460 alone is class approval
  • Omitting alloy / microalloy rows (Al, Nb, V, Ti, Cu, Cr, Ni, Mo, B, N) from the certificate check

Write grade ({g}, no H), TM/QT, impact temperature, UT level and certificate type into the PO.

Sourcing BV BV E460: buyer concerns and SHH STEEL solutions

ConcernHow SHH STEEL handles it
Fake class plateBV-approved mills only; traceable BV E460 stamp + certificate; 3.2 on request
Payment riskT/T or L/C; inspection before balance
Mill minimum / long lead timecombine sizes on one heat where possible; weekly photo updates; clear rolling-slot confirmation before deposit
Welding / heat-input risksend ladle Ceq/CET/Pcm before shipment; support WPS review with mill data
Prep before shipcutting, bevelling, drilling, machining in our workshop (follow mill cutting notes for QT)

How to order BV BV E460 plate

Specify BV E460 (BV E460), delivery condition TM or QT, thickness × width × length × qty, Z/U/UT level, multi-class, certificate type, port. Send to SHH STEEL.

Sample PO line: “Steel plate to Bureau Veritas NR216 Materials, Grade E460 (BV E460), delivery condition [TM/QT], 30 × 2500 × 12000 mm, 10 pcs, marked BV E460 / BV E460, certificate endorsed by BV Surveyor, EN 10204 3.2 [if required], UT [EN 10160 / ASTM A578 level], CIF [port].”

FAQ

What sizes and minimum order quantity can you supply for BV E460 / BV E460 plate?
BV E460 is ordered as Bureau Veritas extra-high-strength grade E460 (IACS UR W16 strength band; BV official no-H naming). The plate is fully killed, and the maximum thickness depends on the delivery condition (TM or QT) and the mill’s BV approval. In practice BV E460 is nearly always produced by an approved mill to order rather than taken from stock, so a mill minimum per heat or rolling usually applies. Send thickness × width × length × quantity per size and we will say whether the order fits a scheduled rolling or needs its own heat. Small balance quantities can sometimes ride on another E460 order.
How is BV BV E460 certified, and can you arrange EN 10204 3.2 or dual-class with ABS/DNV/LR?
Every plate is made by a BV-approved mill under Bureau Veritas survey. It is die-stamped or stencilled BV E460 / BV E460 with the heat or plate number, and the mill test certificate is endorsed by the BV Surveyor. The certificate gives ladle chemistry (full alloy set including Al, Nb, V, Ti, Cu, Cr, Ni, Mo, B, N where applicable), Ceq/CET/Pcm as applicable, tensile (ReH ≥ 460 N/mm², Rm 570–720 N/mm², A ≥ 17 %), Charpy at −40 °C, delivery condition, UT if ordered, and plate identity. If your contract asks for EN 10204 3.2, we arrange it before rolling. Dual or multi-class (e.g. BV + ABS, DNV or LR) must be booked before testing. 3.2 cannot be added afterwards.
What is the impact test temperature and energy for BV E460 / BV E460, and do thickness limits apply?
BV E460 is tested at −40 °C with an indicative average of at least 46 J longitudinal or 31 J transverse (IACS UR W16 aligned tables). Impact specimens typically come from the quarter-thickness position (t/4). For thicker plates, BV / UR W16 may require additional positions. Rule maximum thickness depends on whether the plate is TM or QT and on mill approval, so give the delivery condition as well as the thickness, and we will check the approved mill’s range before quoting. Final values are as per standard and mill certificate (see UNCERTAIN).
What welding and preheat guidance applies to BV BV E460?
BV E460 is an extra-high-strength steel (yield ≥ 460 N/mm²) supplied TM or QT. Welding must follow a procedure qualified for this grade and approved by BV. Ceq is calculated from the ladle analysis and limited by the approval chemistry; the mill may also report CET or Pcm for low-carbon TM/QT steel. Hydrogen control, preheat, interpass temperature and heat-input windows come from the approved WPS and the mill’s recommendations. Too much heat input can lower HAZ strength and toughness in QT plate. We send the certificate values before shipment so your welding engineer can confirm the procedure fits.
What is the delivery time for BV BV E460 plate?
BV E460 is normally rolled to order. Typical commercial lead time is about 6–10 weeks from confirmed PO and deposit, depending on the mill rolling schedule, QT capacity, UT and any 3.2 witness. Ocean transit comes on top of that. This is a commercial estimate, not a rule value, and we confirm it with each quotation. Every week, your coordinator sends the rolling, heat-treatment, testing and stamping status with photos. Delays are reported as soon as the mill tells us, not at the shipping date.
Which payment terms do you accept for BV E460, and how is my deposit protected?
We accept T/T or L/C at sight. With T/T, the usual terms are a 30 % deposit and the balance against the documents or after inspection. You or your inspector can check the BV E460 stamping, the dimensions and the Surveyor-endorsed certificate before you pay the balance. With L/C, payment is tied to the presented documents. For first orders we can start with a smaller trial lot. The proforma invoice shows the grade (BV E460 / BV E460), TM/QT, sizes and certificate type.
Why does BV write E460 (no H) while DNV/LR/ABS use AH460-style names, and what are the equivalents?
Bureau Veritas lists BV E460 for commercial E460 (official QT/EHS form without H — A420 not AH420). ASTM A131/A131M stops at FH40, so it has no direct equivalent. ABS EH46 / EQ47 is the usual ABS counterpart. DNV NV E460 is the DNV counterpart (DNV titles EH460). LR EH46 / LR/EH46 is the LR counterpart (LR titles EH46). CCS EH460, NK KE460 and KR RE47 are the CCS/NK/KR counterparts. RINA EHS names are written “per rules” until verified. GB 712 Grade EH460 is listed in the GB 712 EHS band but is not class approval by itself. Always write BV E460 on the PO, plus any additional society stamps you need.
Can you cut, bevel or machine BV BV E460 plates, and how are they packed for export?
Yes. In our workshop we can flame, plasma or laser cut E460 to drawings, bevel weld edges (V, X or K preparation to your angle and land), drill and machine. Every cut piece keeps traceability: we transfer the BV E460 marking and heat number before cutting, and the cutting list is tied to the mill certificate. For QT extra-high-strength plate, thermal cutting parameters follow the mill’s recommendations so the cut edge is not damaged. For export, plates are bundled with steel straps and timber spacers, marked with grade, size and heat number, and loaded in containers or as break-bulk. See SHH STEEL for our processing capabilities.

Conclusion

BV E460 / BV E460 is extra-high-strength hull steel (IACS UR W16 band; BV official no-H naming): yield 460 N/mm², tensile 570–720 N/mm², Charpy at −40 °C, marking BV E460. Lock on the order: TM or QT, UT level, Ceq/CET/Pcm reporting, multi-class and 3.2.

SHH STEEL supplies BV E460 plate rolled by Chinese mills that hold Bureau Veritas works approval for the grade, so every plate carries the BV E460 stamp and a Surveyor-endorsed certificate traceable to its heat. Sizes are scheduled into the mill rolling cycle with BV survey arranged at the mill. On request we add EN 10204 3.2 certificates with third-party witness (TÜV, SGS, LR or another agency) and joint certification with ABS, DNV, LR, CCS, NK, KR or RINA.

We accept T/T or L/C payment, with inspection before the balance is paid. Small quantities in several sizes, or BV E460 with neighbouring EHS sizes or higher-strength AH–FH 40 where the drawing allows, can be combined in one container. A dedicated coordinator sends production and shipping updates with photos, and our own workshop cuts to size, bevels, drills and machines plates before shipment so they arrive ready for fabrication.

Request a quotation: send SHH STEEL the grade (BV E460 / BV E460), thickness, width, length, quantity per size and destination port, plus any multi-class, Z/U or 3.2 certificate requirement. We reply with price, available stock and lead time.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *



    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *



      X