BV A420 Shipbuilding Steel Plate
BV A420 / BV A420 shipbuilding steel plate — overview
Bureau Veritas titles extra-high-strength plate at 0 °C as BV A420 (BV A420) — official form without H (A420, not AH420). IACS Unified Requirement W16 covers this strength band (yield 420 N/mm²); BV implements corresponding requirements in NR216 Materials rules. Minimum yield is 420 N/mm², tensile 530–680 N/mm², elongation 18 % min., with Charpy at 0 °C. It sits above the AH–FH 40 higher-strength family (max yield 390 N/mm² under UR W11). Commercial enquiries use BV A420 or BV A420 shipbuilding steel plate.
Equivalent grades: BV A420 ≈ ASTM A131 (no direct grade at this strength) ≈ ABS AH42 / AQ43 ≈ DNV NV A420 ≈ LR AH42 ≈ CCS AH420 ≈ NK KA420 ≈ KR RA43 ≈ RINA A420 ≈ GB 712 Grade AH420 (all class-approved, stamped by the issuing society).
Naming note: Bureau Veritas titles this strength band as A420 / BV A420 (no H — write A420, not AH420 or AH42). DNV often titles the same yield as AH420 / DNV NV A420. LR titles AH42. ABS often titles AH42 (official ABS AQ43). ASTM A131 has no grade at this strength. Write BV A420 on the BV purchase order.
BV A420 is almost always produced TM or QT by a BV-approved mill to order rather than taken from open stock. SHH STEEL sources extra-high-strength plate from mills with Bureau Veritas approval for the grade, under Surveyor attendance, with optional multi-class (ABS/DNV/LR) and EN 10204 3.2.
BV BV A420 plate: specification summary
| Item | BV BV A420 / A420 data |
|---|---|
| Rule basis | Bureau Veritas NR216 Materials (extra-high / high-strength hull steel); IACS UR W16 strength band (see UNCERTAIN for NR216 paragraph cross-refs without local BV PDF) |
| Commercial / stamp | BV A420 (BV A420) — official no-H form |
| Yield / tensile / elongation | 420 / 530–680 N/mm² / 18 % min. |
| Impact | 0 °C; ≈ 42 J L or 28 J T average (IACS UR W16 / aligned tables — confirm on mill certificate) |
| Deoxidation | fully killed, fine grain; N-binding elements per manufacturing specification |
| Delivery condition | TM or QT (N/CR routes only where specifically approved) — within mill approval thickness limits |
| Marking | BV A420 / BV A420 (plus delivery-condition / Z / U where ordered) |
| UT | commonly required for thicker EHS plate (e.g. ≥15 mm) — agree standard (EN 10160 / ASTM A578) on PO |
| Thickness tolerance | IACS UR W13 as adopted by BV (confirm class on PO; see UNCERTAIN) |
| Certificate | mill certificate endorsed by the BV Surveyor; includes Ceq/CET/Pcm as applicable; EN 10204 3.1 / 3.2 on request |
Maximum plate thickness depends on delivery condition and the mill’s BV approval sheet — typically TM up to about 100–150 mm and QT higher, but treat the approval limit as governing (UNCERTAIN without local NR216 PDF). Primary commercial scope we quote is within ~100 mm unless the mill approval and BV survey confirm otherwise.
BV BV A420 chemical composition (heat analysis — full alloy set)
| Element | Heat (ladle) analysis, % | Product (check) analysis, % | Note |
|---|---|---|---|
| C | 0.21 max. (often 0.14–0.20 by route/condition; TM/QT may tighten) | numeric tolerance not tabulated in BV NR216 – agree on order / mill certificate | TM/QT and letter routes may tighten C — UNCERTAIN exact NR216 table without local PDF |
| Mn | 1.70 max. (typically 1.00–1.70; QT route may differ) | numeric tolerance not tabulated in BV NR216 – agree on order / mill certificate | as per mill approval / UR W16 envelope |
| Si | 0.55 max. (QT may allow up to ~0.80 — confirm on mill approval) | numeric tolerance not tabulated in BV NR216 – agree on order / mill certificate | |
| P | 0.025 max. (some EQ-style routes tighter — confirm) | numeric tolerance not tabulated in BV NR216 – agree on order / mill certificate | EQ-style routes may be tighter |
| S | 0.025 max. (some EQ-style routes tighter — confirm) | numeric tolerance not tabulated in BV NR216 – agree on order / mill certificate | EQ-style routes may be tighter |
| Al (acid soluble / total) | 0.015 min. acid-soluble / ≈0.020 total Al (fine-grain; Al/N control unless other N-binders) | numeric tolerance not tabulated in BV NR216 – agree on order / mill certificate | grain refining / N control |
| Nb | 0.05 max. (when used; combined microalloy caps apply) | numeric tolerance not tabulated in BV NR216 – agree on order / mill certificate | when intentionally added |
| V | 0.10 max. (when used; combined caps apply) | numeric tolerance not tabulated in BV NR216 – agree on order / mill certificate | when intentionally added |
| Ti | 0.05 max. (when used; combined caps apply) | numeric tolerance not tabulated in BV NR216 – agree on order / mill certificate | when intentionally added |
| Cu | 0.50 max. (route-dependent; often ≤0.35 in practice) | numeric tolerance not tabulated in BV NR216 – agree on order / mill certificate | |
| Cr | 0.20–0.25 max. (route-dependent) | numeric tolerance not tabulated in BV NR216 – agree on order / mill certificate | |
| Ni | 2.00 max. or per mill approval (often lower on A/D routes) | numeric tolerance not tabulated in BV NR216 – agree on order / mill certificate | |
| Mo | 0.08–0.50 (route-dependent; QT may allow higher) | numeric tolerance not tabulated in BV NR216 – agree on order / mill certificate | |
| B | 0.005 max. (when intentionally added) | numeric tolerance not tabulated in BV NR216 – agree on order / mill certificate | report when intentionally added |
| N | 0.015 max. (tighter control when Al is the sole N-binder) | numeric tolerance not tabulated in BV NR216 – agree on order / mill certificate | Al/N practice unless other N-binders |
| Nb+V+Ti (combined) | Nb+V+Ti typically < 0.26 % for N/TM routes (not QT) — confirm UR W16 / mill approval | not applicable (calculated from heat analysis) | combined microalloy cap |
| Ceq / CET / Pcm | Ceq / CET / Pcm maxima by category and condition on mill approval — report on certificate | not applicable (calculated from heat analysis) | report on certificate; choice agreed mill/purchaser |
Product (check) analysis column: BV NR216 specify heat (ladle) limits; no numeric product-analysis tolerance is tabulated in the rule text reviewed, so product (check) limits are agreed on the order or taken from the approved mill specification and certificate.
Source: IACS UR W16 chemistry envelope (ABS 2-1-8 Table 4A aligned) as implemented by Bureau Veritas for BV A420 via NR216 — exact ladle limits depend on delivery condition (TM vs QT) and toughness letter. Values above are the rule envelope with every alloy / microalloy row listed; the purchase order and mill approval sheet govern. Product analysis: as per standard and mill certificate. All intentionally added elements and Ceq (or CET/Pcm) are to be reported. Flagged UNCERTAIN where a local BV NR216 PDF was not available to quote paragraph numbers.
BV BV A420 tensile and impact properties
| Property | Requirement (IACS UR W16 aligned) |
|---|---|
| Yield strength ReH (or Rp0.2) | 420 N/mm² min. |
| Tensile strength Rm | 530–680 N/mm² |
| Elongation (transverse, 5.65√A) | 18 % min. |
| Impact test temperature | 0 °C |
| Impact energy (indicative) | 42 J L or 28 J T average |
Final acceptance values are as per standard and mill certificate under BV survey. For thick plate, additional mid-thickness tensile/impact positions may apply — confirm at enquiry. Test frequency is typically each heat-treatment batch of same cast/condition/thickness.
Delivery condition and toughness for BV A420
Charpy temperature is fixed by the grade letter: A → 0 °C. Indicative average energy 42 / 28 J (L/T) from IACS UR W16 aligned tables — confirm exact figures on the BV-endorsed certificate. Unlike UR W11 higher-strength tables, EHS energies are usually stated as a single pair rather than rising through many thickness bands; thick-plate mid-thickness rules may still apply.
Allowed delivery conditions are primarily TM and QT within the mill’s approved thickness. Vacuum degassing is commonly required for higher categories and for thicker plate — follow the mill approval. State TM or QT on the PO; do not leave delivery condition blank for A420.
Thickness tolerance and surface condition
Bureau Veritas applies IACS UR W13 unless the PO states otherwise (confirm minus class on PO; see UNCERTAIN). Surface repair limits follow the applicable BV / UR rules; state primer/surface class on receipt if needed. For QT plate, avoid notching cut edges; follow mill cutting recommendations.
BV BV A420 plate — mill-roll supply in China
| Thickness (mm) | Width (mm) | Length (mm) | Condition | Approx. quantity | Location |
|---|---|---|---|---|---|
| 10 | 2000 / 2200 | 8000 / 12000 | TM / QT | 200+ t | China |
| 12 | 2000 / 2200 / 2500 | 12000 | TM / QT | 200+ t | China |
| 14 | 2000 / 2200 | 12000 | TM / QT | 100+ t | China |
| 16 | 2000 / 2500 | 12000 | TM / QT | 200+ t | China |
| 20 | 2000 / 2500 | 12000 | TM / QT | 100+ t | China |
| 25 | 2200 / 2500 | 12000 | TM / QT | 100+ t | China |
| 30 | 2200 | 10000 / 12000 | TM / QT | 100+ t | China |
| 40 | 2200 | 10000 | TM / QT | 50+ t | China |
| 50 | 2200 | 8000 / 10000 | TM / QT | 50+ t | China |
Extra-high grades such as BV A420 are rarely held as open stock; the table shows the size bands we quote against scheduled mill rolls. Quantities are indicative. All plates sold as BV class carry BV A420 marking and a Bureau Veritas–endorsed mill certificate. Typical mill lead time including BV survey is about 6–10 weeks (commercial estimate — confirm per quote). Send your size list and we will reply with the next available rolling slot.
Packing. Plates are bundled by size with steel strapping, marked with heat number, grade and BV stamp, and shipped in containers (up to about 11.8 m) or break bulk for longer plates.
BV BV A420 equivalents in other rules and standards
| Standard / society | Designation | Comment |
|---|---|---|
| BV (Bureau Veritas) | BV A420 (BV A420) | this page; BV uses A420…F690 (no H) |
| ASTM A131/A131M | ASTM A131/A131M — no direct Grade A420 | A131 stops at FH40 |
| ABS | ABS AH42 / AQ43 | commercial AH42 / official AQ43 |
| DNV | DNV NV A420 | DNV titles AH420 for this yield band |
| LR | LR AH42 / LR/AH42 | LR titles AH42 (AH69 not AH70 / AH690) |
| CCS | CCS AH420 | CCS follows W16-style naming |
| NK (ClassNK) | NK KA420 | NK KA420 |
| KR | KR RA43 | KR RA43 (KR uses ABS-style category numbers) |
| RINA | RINA (per rules) | EHS name not verified from local RINA PDF |
| GB 712 | GB 712 Grade AH420 | listed in GB 712 EHS band; not class approval alone |
These are comparisons, not substitutions. Always write the BV stamp BV A420 on the PO, plus any additional society stamps you need. Other BV EHS siblings are linked via BV Steel Plates until each product page is live.
BV BV A420 vs higher-strength and other EHS grades
Use A420 when scantlings need yield 420 N/mm². Do not substitute AH40/EH40 (390 N/mm² max under UR W11) without redesign. Within the 420 band, letter choice is toughness: A 0 °C → D −20 °C → E −40 °C → F −60 °C. Neighbouring strengths are AH–FH 40 / 460 — swapping strength needs class approval of the drawing change.
When BV BV A420 is the right choice: typical uses are extra-high-strength hull girder plating and primary members on BV-classed ships and offshore units where 0 °C toughness and yield above 390 N/mm² are specified at extra-high yield — weight-critical hull girder strakes, polar and ice-class primary structure, and offshore units where 420 N/mm² is specified. See offshore platform steel plates for related offshore grades.
Applications and welding notes for BV BV A420
Typical uses: extra-high-strength hull girder plating and primary members on BV-classed ships and offshore units where 0 °C toughness and yield above 390 N/mm² are specified at ReH 420 N/mm²; strength deck and shell of large container ships and gas carriers where EHS is specified; ice-belt and polar primary structure; selected offshore members. See offshore platform steel plates.
Welding: BV A420 is an extra-high-strength steel supplied TM or QT. Welding must follow a procedure qualified for this grade and approved by BV. Ceq/CET/Pcm from the ladle analysis govern hydrogen control, preheat, interpass and heat-input windows. Too much heat input can lower HAZ strength and toughness in QT plate. We send the certificate values before shipment so your welding engineer can confirm the procedure fits. We do not give generic preheat temperatures.
Processing notes: BV A420 owes its strength to TM or QT processing. Hot forming or stress relieving above the tempering temperature can lower the properties, so any heat treatment after delivery must be agreed with the mill and BV. Cold forming and bending radii should follow the mill’s data sheet. Thermal cutting parameters follow mill recommendations so the cut edge is not damaged.
Certificates, BV survey and third-party inspection
BV survey at the mill; certificate includes ladle chemistry (full alloy set + Ceq/CET/Pcm as applicable), tensile (ReH ≥ 420, Rm 530–680, A ≥ 18 %), Charpy at 0 °C, delivery condition, UT if ordered, and plate identity. Optional EN 10204 3.2 and multi-class with ABS/DNV/LR.
On receipt: verify BV A420 stamp, 0 °C impact data, energies ≥ ordered/certified minima, thickness within tolerance, Surveyor endorsement, UT report if required.
Charpy acceptance for BV A420 (IACS UR W16 aligned; actual results as per standard and mill certificate):
| Thickness t (mm) | Test temperature | Average energy, longitudinal (J min.) | Average energy, transverse (J min.) |
|---|---|---|---|
| as per UR W16 / mill approval (typically t/4 position) | 0 °C | 42 | 28 |
For thickness above ~100 mm, additional mid-thickness rules may apply — confirm at enquiry. If the PO asked for 3.2, the inspector’s report must name the witnessed tests and plate numbers.
Common mistakes when ordering BV A420 / BV A420
- Ordering “BV 420” without the letter (A) — toughness missing
- Writing AH420 / AH42 / AH420 on a BV PO — BV official form is A420 (no H)
- Writing ABS AH42 or DNV AH420 or LR AH42 on a BV-class PO without arranging that society’s survey (wrong stamp)
- Leaving delivery condition blank (TM vs QT changes price, mill and properties)
- Expecting ASTM A131 dual-cert at this strength (A131 has no EHS grade)
- Skipping UT on thick EHS plate when the yard specification requires it
- Missing BV endorsement / assuming GB 712 Grade AH420 alone is class approval
- Omitting alloy / microalloy rows (Al, Nb, V, Ti, Cu, Cr, Ni, Mo, B, N) from the certificate check
Write grade ({g}, no H), TM/QT, impact temperature, UT level and certificate type into the PO.
Sourcing BV BV A420: buyer concerns and SHH STEEL solutions
| Concern | How SHH STEEL handles it |
|---|---|
| Fake class plate | BV-approved mills only; traceable BV A420 stamp + certificate; 3.2 on request |
| Payment risk | T/T or L/C; inspection before balance |
| Mill minimum / long lead time | combine sizes on one heat where possible; weekly photo updates; clear rolling-slot confirmation before deposit |
| Welding / heat-input risk | send ladle Ceq/CET/Pcm before shipment; support WPS review with mill data |
| Prep before ship | cutting, bevelling, drilling, machining in our workshop (follow mill cutting notes for QT) |
How to order BV BV A420 plate
Specify BV A420 (BV A420), delivery condition TM or QT, thickness × width × length × qty, Z/U/UT level, multi-class, certificate type, port. Send to SHH STEEL.
Sample PO line: “Steel plate to Bureau Veritas NR216 Materials, Grade A420 (BV A420), delivery condition [TM/QT], 30 × 2500 × 12000 mm, 10 pcs, marked BV A420 / BV A420, certificate endorsed by BV Surveyor, EN 10204 3.2 [if required], UT [EN 10160 / ASTM A578 level], CIF [port].”
FAQ
Conclusion
BV A420 / BV A420 is extra-high-strength hull steel (IACS UR W16 band; BV official no-H naming): yield 420 N/mm², tensile 530–680 N/mm², Charpy at 0 °C, marking BV A420. Lock on the order: TM or QT, UT level, Ceq/CET/Pcm reporting, multi-class and 3.2.
SHH STEEL supplies BV A420 plate rolled by Chinese mills that hold Bureau Veritas works approval for the grade, so every plate carries the BV A420 stamp and a Surveyor-endorsed certificate traceable to its heat. Sizes are scheduled into the mill rolling cycle with BV survey arranged at the mill. On request we add EN 10204 3.2 certificates with third-party witness (TÜV, SGS, LR or another agency) and joint certification with ABS, DNV, LR, CCS, NK, KR or RINA.
We accept T/T or L/C payment, with inspection before the balance is paid. Small quantities in several sizes, or BV A420 with neighbouring EHS sizes or higher-strength AH–FH 40 where the drawing allows, can be combined in one container. A dedicated coordinator sends production and shipping updates with photos, and our own workshop cuts to size, bevels, drills and machines plates before shipment so they arrive ready for fabrication.
Request a quotation: send SHH STEEL the grade (BV A420 / BV A420), thickness, width, length, quantity per size and destination port, plus any multi-class, Z/U or 3.2 certificate requirement. We reply with price, available stock and lead time.