BS 1501 510 Steel Plate
What is BS 1501 510 plate?
We produce and export BS 1501 510 as alloy steel plate (low-temperature section candidate; 1988 identity not photographed) for pressure purposes. Typical service is alloy pressure equipment that specifies this type.
BS 1501-2:1988 is the last final edition of the alloy-plate part of BS 1501. It was published on 29 July 1988 and superseded on 15 January 1995. It replaced Addendum No. 1 (1973) and Addendum No. 2 (1975) to BS 1501: Part 2: 1970. A photographed 1988 Table 1 was not opened for this page. Clause 3 of the 1988 book is titled Designation, but that clause text was not opened. Clause 19 makes elevated-temperature proof stress an optional requirement for section-two steels. The formal 1988 writing of type, tensile token and any A or B suffix therefore remains unverified. Peer catalogues sometimes write names such as 243 B, 620 B, 621 B or 622-515 B; those B forms are recorded as unverified formal-symbol candidates, not declared absent and not declared commercial-only.
Numeric cells below are taken only from the named public database or peer catalogue opened for this page. They are a reference basis, not a photographed BS 1501-2:1988 table and not an SHH proprietary guarantee. EN 10028-2 values for 16Mo3, 13CrMo4-5 or 10CrMo9-10 are not copied onto this legacy type. Missing chemistry or thickness-banded mechanical fields are project requirements to be agreed against the named edition.
SHH STEEL produces and exports BS 1501 510 plate to the ordered edition, delivery condition, dimensions and extra tests written on the enquiry.
Material specification for BS 1501 510
The items below follow BS 1501-2:1988 as the historical alloy-plate book. Numeric cells in the chemical and mechanical sections are from opened public-database listings and peer catalogues, each labelled by source. They are not photographed 1988 Table 1 values and not 1993 National Annex NC tables (that annex covers 271, 281, 621 and 660 only). Thickness, width, length and the inspection document are stated on the enquiry rather than listed here as stock or capacity ranges.
| Parameter | Detail |
|---|---|
| Standard | BS 1501-2:1988, Steels for pressure purposes — Specification for alloy steels: plates. Numeric cells below are public-database or peer-catalogue references, each labelled by source |
| Designation used here | Working name BS 1501 510 (formal 1988 full symbol unverified) |
| Steel type | Alloy steel plate (low-temperature section candidate; 1988 identity not photographed) |
| Product form | Alloy steel plate for pressure purposes (this part does not cover bars, sections, forgings, tubes or stainless sheet) |
| How designations are listed | This page uses the working name 510. Formal 1988 full symbols (type number plus any tensile token and any A or B suffix) were not photographed. Peer catalogues that print B forms are recorded as unverified formal-symbol candidates; they are not declared absent and not declared commercial-only |
| Applicable thickness in the opened tensile table | Not verified from an official thickness table |
| Usual heat treatment | Quenched at 800–840 °C and tempered at 565–605 °C. |
| Chemical analysis | Opened public cells only, each labelled by source in the chemical table |
| Tensile properties | Database minima only; thickness bands are a project requirement |
| Our supply | We produce and export 510 plate to the ordered edition, delivery condition, dimensions and extra tests |
Chemical composition of BS 1501 510
Numeric cells below are taken only from the named public database or peer catalogue opened for this page. They are a reference basis, not a photographed BS 1501-2:1988 table and not an SHH proprietary guarantee. EN 10028-2 values for 16Mo3, 13CrMo4-5 or 10CrMo9-10 are not copied onto this legacy type. Missing chemistry or thickness-banded mechanical fields are project requirements to be agreed against the named edition. A 1970 Part 2 catalogue abstract lists type 510 among the older imperial alloy plates, alongside 509. Some comparison tables write 1501-509-510 beside X8Ni9. That pairing is recorded as a near-name hint only; nickel and molybdenum were hidden on the opened public-database page and are not invented. One peer catalogue’s mechanical figures for type 510 were inconsistent and are not used.
| Element | Value (wt. %) | Source opened for this cell |
|---|---|---|
| Carbon (C) | 0.10 max | Public database listing opened 8 November 2026 (Asia/Shanghai) |
| Chromium (Cr) | 0.30 max | Public database listing opened 8 November 2026 (Asia/Shanghai) |
| Aluminium (Al) | 0.015–0.055 | Public database listing opened 8 November 2026 (Asia/Shanghai) |
Tensile, impact and elevated-temperature properties for BS 1501 510
Only the opened numeric cells are listed. Thickness-banded values and Charpy energies are a project requirement unless an edition table is named.
| Item | Value | Source opened for this cell |
|---|---|---|
| Tensile strength Rm | ≥ 690 MPa (minimum only, not a window) | Public database listing opened 8 November 2026 (Asia/Shanghai) |
| Yield / Rp0.2 | ≥ 590 MPa | Public database listing opened 8 November 2026 (Asia/Shanghai) |
| Elongation A | ≥ 18 % | Public database listing opened 8 November 2026 (Asia/Shanghai) |
A database listing showed quenching at 800–840 °C and tempering at 565–605 °C. Hidden public-database fields were not filled. Numeric cells below are taken only from the named public database or peer catalogue opened for this page. They are a reference basis, not a photographed BS 1501-2:1988 table and not an SHH proprietary guarantee. EN 10028-2 values for 16Mo3, 13CrMo4-5 or 10CrMo9-10 are not copied onto this legacy type. Missing chemistry or thickness-banded mechanical fields are project requirements to be agreed against the named edition.
Delivery conditions for BS 1501 510
A public database listing shows quenching at 800–840 °C and tempering at 565–605 °C. Name the required delivery condition on the purchase order.
If the project has moved to EN 10028-2, order the successor designation and edition expressly. A later European name is not by itself a substitute instruction for type 510.
The purchase order should name the official designation, the edition required, thickness, width and length, the delivery condition, any extra tests, and the inspection document required.
This page does not offer heat-treatment or fabrication services.
Welding and thermal cutting
Neither the opened historical book notes nor the later remaining-steel annex set a welding procedure for type 510 on this page. Welding and thermal cutting should be qualified for the alloy content, thickness and the specified delivery condition.
If the project treats type 510 as a 9 % nickel steel, consumables should match the qualified procedure for that nickel family. That identity was not photographed in a 1988 table.
Heat input and any required post-weld heat treatment belong in the project specification.
Form, appearance, dimensions and thickness tolerances
Thickness, width, length, flatness and mass tolerances should be stated on the purchase order against the dimensional standard named by the project. The historical replacement set includes BS EN 10029 for plate tolerances when that standard is specified.
Appearance, repair welding and any ultrasonic class are taken from the enquiry. This page does not list stock sizes or mill capacity.
Applications and specification limits
We produce and export 510 plate as alloy steel plate for pressure purposes. Typical service is alloy pressure equipment that specifies type 510. Low-temperature duty should be stated on the enquiry rather than assumed from later 9 % nickel names.
BS 1501-2:1988 is a historical alloy-plate standard. It is not the current EN 10028-2 or EN 10028-4 order unless that successor standard is written on the enquiry, and it is not a BS 1501-1 carbon, BS 1501-3 stainless, BS 1502 bar or BS 1503 forging order.
Compare BS 1501 510 with other steel plates
BS 1501 510 is a historical BS 1501-2 alloy pressure-vessel plate. The comparison below is for selection only; these materials are not equivalents.
| Material | Alloy / type | Delivery condition | Mechanical requirements | Typical service | Substitution limit |
|---|---|---|---|---|---|
| BS 1501 510 (this plate) | Alloy plate; later 9 % nickel names are near names only | Quenched at 800–840 °C and tempered at 565–605 °C. | Database minima: Rm ≥ 690 MPa, yield ≥ 590 MPa, A ≥ 18 % | Alloy pressure equipment that specifies this type | A later EN name or a different 1988 type is not an automatic substitute |
| EN 10028-4 X8Ni9 | 9 % nickel cryogenic vessel plate, steel number 1.5662 | As specified in EN 10028-4 | Live published yield in the 490 MPa class after QT and tensile 640–840 MPa; impact typically −196 °C | Modern European 9Ni vessel plate | Near name only; those EN numbers are not copied onto type 510 |
| EN 10028-4 12Ni14 | 3.5 % nickel low-temperature vessel plate, steel number 1.5637 | As specified in EN 10028-4 | Live published yield in the 355 MPa class and tensile 490–640 MPa | Modern European 3.5Ni vessel plate | Different nickel level |
| ASTM A203 Grade D | 3.50 % nickel low-temperature vessel plate | As specified in ASTM A203/A203M | Live published yield 255 MPa and tensile 450–585 MPa | ASTM 3.5Ni vessel plate | Different nickel level and strength table |
Equivalent and related grades by country
The designations below are near names, not automatic substitutes. Confirm chemistry, heat treatment, tensile properties, impact temperature and product form.
| Country / region | Standard | Grade or designation | Similarity and key differences | Substitution caveat |
|---|---|---|---|---|
| United Kingdom | BS 1501-2:1988 working name | 510 | This page uses the working name 510. Formal 1988 suffix status is unverified. | This product |
| Europe | EN 10028-4 | X8Ni9 (1.5662) | Later 9Ni vessel plate. Live published tensile 640–840 MPa and yield in the 490 MPa class after QT, against database minima of 690 MPa and 590 MPa for type 510. | Near name only; EN numbers are not used as 510 values |
| United States | — | — | No separately verified ASTM 9 % nickel plate counterpart (for example A353 or A553) was opened as a live compare page for this pairing. | Do not assume a US 9Ni grade is a substitute |
| China | — | — | No separately verified GB plate counterpart was established for type 510 on this page. | Do not assume a Chinese nickel vessel grade is a substitute |
Why choose SHH STEEL for BS 1501 510
- We produce and export BS 1501 510 alloy pressure-vessel steel plate
- We review the enquiry for edition, designation, delivery condition, dimensions and extra tests
- We keep the historical BS 1501-2 type number distinct from later EN 10028-2 names and from Part 1 A/B carbon grades, and we record peer B forms as unverified formal-symbol candidates until a 1988 table is opened
- We match documentation to what the purchase order requires
How to enquire for BS 1501 510 plate
| Item | What to specify |
|---|---|
| Standard and designation | BS 1501 510 and the edition required (BS 1501-2:1988 and/or the 1993 national-annex remaining-steel clauses) |
| Or successor standard | The EN 10028-2 designation and edition, if that is what the project now requires |
| Delivery condition | Quenched at 800–840 °C and tempered at 565–605 °C. |
| Dimensions | Required thickness, width and length |
| Chemistry | Cast analysis to the named edition |
| Mechanical tests | Yield strength, tensile strength, elongation and, where specified, impact or elevated-temperature proof tests to the named edition |
| Other tests | Ultrasonic examination or other extra tests only when written on the order |
| Documentation | State the inspection document type required by the project |
Thickness, width and length are taken from the enquiry. This page does not list stock sizes, mill capacity or fabrication services.
FAQ
-
Is BS 1501-2 still a current product standard?
- No. BS 1501-2:1988 is the last final edition of the alloy-plate part. It was published on 29 July 1988 and superseded on 15 January 1995. EN 10028-2 superseded part of it. Projects still using a historical type number should name the edition required on the order.
-
Which numbers on this page are guaranteed 1988 table values?
- None are presented as a photographed 1988 table. Only visible public-database cells are listed. Other elements, including nickel, were hidden and are not invented.
-
Is type 510 officially a 9 % nickel steel?
- That is unverified. A 1970 abstract lists type 510, and some comparison tables group 509/510 with X8Ni9. Those hints are not used as chemistry cells on this page.
-
Can X8Ni9 replace type 510?
- Only after a project review. Live X8Ni9 is published as a 490 MPa-class yield after QT and 640–840 MPa tensile, typically impacted at −196 °C. It is not an automatic substitute.
-
What should a quotation enquiry include?
- BS 1501 510, the edition required or the successor designation, the delivery condition, plate thickness by width by length, quantity, any extra tests, and the inspection document required.
Request a quotation
Contact SHH STEEL for a quotation for BS 1501 510 steel plate. Please include your required quantity, plate thickness, width and length, delivery destination and preferred delivery schedule so we can review your production and export requirements.
Specify the edition (BS 1501-2:1988 or the later United Kingdom national-annex remaining-steel clauses, or a named EN 10028-2 successor if that is what the project now requires), the delivery condition and any specimen heat treatment. If your project requires ultrasonic examination, a stated impact temperature or another extra test, include the acceptance criteria and the inspection document required.
If you are considering a related designation, send the applicable standard and project specification with your enquiry so we can review chemistry, heat treatment and toughness.
For a detailed quotation, email your material specification, quantity and delivery requirements to our team.